The present invention relates to a surface-mounted chip component which is typically a chip resistor.
A chip resistor, which is an example of a chip component, is designed to mainly include a rectangular parallelepiped insulating substrate, a pair of front electrodes oppositely disposed on the front surface of the insulating substrate with a predetermined interval therebetween, a resistor that bridges the pair of front electrodes, an insulating protective layer that covers the resistor, a pair of back electrodes oppositely disposed on the back surface of the insulating substrate with a predetermined interval therebetween, a pair of end face electrodes formed on both ends of the insulating substrate to bridge the front electrodes and the corresponding back electrodes. The outer face of each of the end face electrodes is covered with an external electrode formed by plating.
A chip resistor thus designed is surface-mounted on a circuit board by the processes of, after application of a solder paste on the lands provided on the circuit board, mounting the external electrodes on the lands with the back electrodes facing downward, and then melting and curing the solder paste in this state.
Here, each of the external electrodes to be soldered to the lands and each of the end face electrodes provided inside thereof is generally formed in a U-shape so as to be exposed at three faces (upper face, end face, and lower face) except for side faces of the chip resistor. On the other hand, as disclosed in Patent Literature 1, it has been also known that the end face electrodes are formed in a cap shape at both ends of the insulating substrate, whereby a chip resistor can be mounted on a circuit board in any posture via four faces (upper face, lower face, and both side faces) thereof.
Patent Literature 1: JP-A-2017-45861
The chip resistor according to Patent Literature 1 is formed by the processes of providing each of the front electrodes connected to both ends of the resistor so as to be exposed at three end faces on the short side and long side of the insulating substrate, respectively, and providing each of the cap-shaped end face electrodes so as to be connected to the end faces of each of the front electrodes which are exposed at the three end faces of the insulating substrate, so as to increase the connection reliability between the front electrodes and the end face electrodes. However, in recent years, downsizing of chip components which are typically chip resistors has been increasingly promoted, and for example, in the case where the outer dimension of a chip resistor is reduced to 0201 size (long side 0.250 mm, short side 0.125 mm), the contact areas between the front electrodes and the end face electrodes are significantly reduced. This causes a problem that the connection reliability of the end face electrodes with respect to the resistor and the front electrodes decreases.
The present invention has been made in view of the circumstances described above of the prior art, and thus an object of the present invention is to provide a chip component suitable for downsizing.
In order to achieve the object described above, the present invention provides a chip component comprising: a rectangular parallelepiped insulating substrate; a strip-shaped conductive film formed on a main surface of the insulating substrate along a longitudinal direction; a pair of electrodes formed on a surface of the conductive film at both ends in the longitudinal direction; an insulating protective layer that entirely covers the main surface of the insulating substrate including the conductive film and the pair of electrodes; and a pair of cap-shaped end face electrodes formed at both ends of the insulating substrate in the longitudinal direction, and each of which is connected to an end face of the conductive film, an end face of corresponding one of the pair of electrodes, and an end face of the protective film, wherein a cross-sectional shape of each of the pair of electrodes is almost a triangle in which a side of the end face has a maximum height, and a shape of an end face of each of the pair of end face electrodes is almost a square.
In the chip component thus designed, the conductive film which is a functional element is formed in a strip shape on the insulating substrate, and the cross-sectional shape of the electrodes formed on the conductive film is almost a triangle in which the side of the end face has the maximum height. Accordingly, even in the case where the outer dimension of the chip component is reduced, it is possible to reliably connect the cap-shaped end face electrodes to the end faces of the conductive film and those of the electrodes. In addition, the protective layer is formed so as to cover the entire main surface of the insulating substrate including the conductive film and the electrodes, and the shape of the end faces of the end face electrodes covering the ends of the protective layer is almost a square. Accordingly, it is possible to realize a chip component in the shape of almost cube, which is very small and excellent in planarity.
In the chip component thus designed, the conductive film may be a conductor having a resistance value of approximately zero ohms such as a jumper chip, however, in the case of a chip resistor in which the conductive film is a resistor, it is preferable that the protective layer is formed of a glass coating layer that covers the resistor and a resin coating layer that covers the glass coating layer.
In the chip component thus designed, in the case where the film thickness of the glass coating layer is set to less than the maximum height dimension of the electrodes, the pair of electrodes is exposed at both ends of the glass coating layer. This enables a trimming groove for adjusting a resistance value in the resistor to be formed during the process of producing the chip resistor by irradiating a laser beam from above the glass coating layer while bringing a probe into contact with the pair of electrodes to measure the resistance value of the resistor.
Furthermore, in the chip component thus designed, each of the electrodes may be connected to the corresponding one of the end face electrodes at least via its end face in the longitudinal direction of the insulating substrate. On the other hand, it is preferable to connect each of the electrodes to the corresponding one of the end face electrodes via the three faces of each of the electrodes including the end face in the longitudinal direction of the insulating substrate and both the side faces adjacent to the end face so as to further enhance the connection reliability between the electrodes and the end face electrodes.
According to the present invention, it is possible to reduce the outer dimension of a chip component while obtaining the connection reliability of end face electrodes with respect to a conductive layer and electrodes.
Each
Each
Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
As illustrated in
The insulating substrate 1 is a ceramic substrate mainly composed of alumina. The insulating substrate 1 is obtained with the other multiple pieces of substrates by dicing a large-sized substrate along primary division expected lines and secondary division expected lines which extend to form a grid.
The resistor 2 is formed by screen-printing a resistance paste such as ruthenium oxide on the front surface of the insulating substrate 1 and drying and sintering the paste. Both ends of the resistor 2 in the longitudinal direction are exposed at both end faces of the insulating substrate 1 in the X-direction. Although not illustrated, the resistor 2 is provided with a trimming groove for adjusting a resistance value.
The pair of front electrodes 3 are obtained by screen-printing an Ag-based paste from above the resistor 2 and drying and sintering the paste. The front electrodes 3 are formed at positions so as to overlap both the ends of the resistor 2 in the longitudinal direction, respectively. As apparent from
The protective layer 4 has a double-layer structure of a glass coating layer 7 that covers the resistor 2 and a resin coating layer 8 that covers the glass coating layer 7. The glass coating layer 7 is formed by screen-printing a glass paste from above the resistor 2 and drying and sintering the paste so as to cover the resistor 2, and is exposed at both the end faces of the insulating substrate 1 in the Y-direction. The film thickness of the glass coating layer 7 is set to less than the maximum height dimension of the front electrodes 3. Accordingly, the glass coating layer 7 is not exposed at both the end faces of the insulating substrate 1 in the X-direction, and at both end faces of the glass coating layer 7 in the X-direction, inclined faces of the front electrodes 3 are exposed, respectively.
The resin coating layer 8 is formed by screen-printing an epoxy-based resin paste from above the glass coating layer 7 and heating and curing the paste. The resin coating layer 8 is formed of a transparent or translucent resin material or the like. Since the resin coating layer 8 is formed so as to cover the entire front surface of the insulating substrate 1 including the front electrodes 3 and the glass coating layer 7, as illustrated in
The pair of end face electrodes 5 is formed by dip-coating an Ag paste or Cu paste and heating and curing the paste. Each of the end face electrodes 5 is formed in a cap shape so as to cover the upper face of the resin coating layer 8 and the lower face and both side faces of the insulating substrate 1 from both the end faces in the X-direction of the insulating substrate 1. Thus, the end face electrodes 5 are connected to the end faces of the resistor 2 in the X-direction, respectively, and are connected to the front electrodes 3 exposed at the three end faces of the insulating substrate 1, respectively. Note that the outer shape of a chip element body before the end face electrodes 5 are formed is almost a cube, and at both the end faces in the longitudinal direction of the chip element body having such a shape, the end face electrodes 5 in the shape of a cap are formed, respectively. That is, the insulating substrate 1 has a rectangular parallelepiped shape in which the thickness dimension (length in the height direction in
Although not illustrated, the pair of end face electrodes 5 is covered by the external electrodes, respectively. The external electrodes are formed by electroplating Ni, Sn or the like on the surfaces of the end face electrodes 5, respectively.
Next, a method of producing the chip resistor designed as described above will be explained with reference to
The first process is to prepare a large-sized substrate 10A made of ceramic from which multiple pieces of insulating substrates 1 are to be obtained. The large-sized substrate 10A is not provided with any primary division groove and secondary division groove, on the other hand, as dicing positions during dividing the large-sized substrate 10A into multiple pieces of chip elements in subsequent processes, primary division expected lines L1 and secondary division expected lines L2 are set on the large-sized substrate 10A. That is, where the lateral direction of the large-sized substrate 10A is defined as the X-direction and the vertical direction is defined as the Y-direction in
Then, by screen-printing a resistance paste such as ruthenium oxide on the front surface of the large-sized substrate 10A designed as described above and drying and sintering the paste, as illustrated in
Next, by printing an Ag-based paste on the front surface of the large-sized substrate 10A and drying and sintering the paste, as illustrated in
Next, by screen-printing a glass paste and drying and sintering the paste, as illustrated in
Next, by irradiating a laser beam from above the glass coating layer 7 while bringing a probe for measurement (not illustrated) into contact with the pair of front electrodes 3 exposed at both the ends of the glass coating layer 7 to measure a resistance value of the resistor 2 between the pair of front electrodes 3 in this state, the process of forming a trimming groove (not illustrated) for adjusting the resistance value on the resistor 2 is performed (resistance value adjusting process).
Next, by print-screening an epoxy-based resin paste, to which a white pigment is added, from above the front electrodes 3 and the glass coating layer 7 and heating and curing the paste, as illustrated in
Next, after fixing the large-sized substrate 10A, through an adhesive 12, to a base member 11 for fixing made of a hard material such as ceramic, by cutting the large-sized substrate 10A with dicing blades 13 along the primary division expected lines L1 and the secondary division expected lines L2, as illustrated in
In this dicing process, since the positions of the front electrodes 3 and resistor 2 provided inside can be viewed through the protective layer 4 covering the entire front surface of the large-sized substrate 10A, it is possible to accurately determine the dicing positions (primary division expected lines L1 and secondary division expected lines L2). Note that the primary division expected lines L1 and the secondary division expected lines L2 are virtual lines to be set with respect to the large-sized substrate 10A, and thus as mentioned above, any primary division groove and secondary division groove corresponding to the division expected lines are not provided on the large-sized substrate 10A.
Next, by washing the adhesive 12 and peeling off the base member 11 for fixing from the large-sized substrate 10A, as illustrated in
Although the subsequent steps are not illustrated, by dip-coating a conductive paste such as an Ag paste or Cu paste on end faces of each of the chip element body 10B and heating and curing the paste, the process of forming the cap-shaped end face electrodes which wrap from both end faces in the longitudinal direction to predetermined positions on both end faces in the lateral direction of the chip element body 10B is performed (end face electrode forming process). At this time, since the external shape of the chip element body 10B is almost a cube, each of the end face electrodes wrapping around the four faces of the chip element body 10B has a rectangular shape in which the face in contact with the surface of the protective layer 4 and the remaining three faces in contact with the three ceramic surfaces have the same size.
Finally, by providing each of the chip element bodies 10B with an electroplating layer such as Ni, Sn, and the like, the process of forming the external electrodes that cover the end face electrodes, respectively, is performed (external electrode forming process). Through these processes, a chip resistor as illustrated in
As described above, in the chip resistor according to the present embodiment, the resistor 2 which is a functional element is formed in a strip shape on the insulating substrate 1, and the cross-sectional shape of each of the front electrodes 3 formed on both the end of the resistor 2 is almost a triangle in which the side of the end face has the maximum height. Accordingly, even in the case where the outer dimension of the chip resistor is reduced, it is possible to reliably connect the cap-shaped end face electrodes 5 to the end faces of the resistor 2 and those of the front electrodes 3. In addition, the protective layer 4 is formed so as to cover the entire front surface of the insulating substrate 1 including the resistor 2 and the front electrodes 3, and the shape of the end faces of the end face electrodes 5 covering the ends of the protective layer 4 is almost a square. Accordingly, it is possible to realize a chip component in the shape of almost cube, which is very small and excellent in planarity.
In the chip resistor according to the present embodiment, within the protective layer 4 having a double-layer structure formed of the glass coating layer 7 and the resin coating layer 8, the film thickness of the glass coating layer 7 is set to less than the maximum height dimension of the front electrodes 3, whereby the pair of front electrodes 3 is exposed at both ends of the glass coating layer 7. Accordingly, in the resistance value adjusting process of adjusting the resistance value of the resistor 2, it is possible to form a trimming groove in the resistor 2 by irradiating a laser beam from above the glass coating layer 7 while bringing a probe into contact with the pair of front electrodes 3 to measure the resistance value of the resistor 2.
Furthermore, in the chip resistor according to the present embodiment, each of the front electrodes 3 is exposed not only at the end face of the insulating substrate 1 in the longitudinal direction, but also exposed at both the side faces of the insulating substrate 1 in the lateral direction. Thus, each of the end face electrodes 5 is connected to the corresponding one of the front electrodes 3 via these three faces, and accordingly, it is possible to increase the connection reliability between the front electrodes 3 and the end face electrodes 5.
In the embodiment above, the case where the present invention is applied to a chip resistor whose conductive film as a functional element is a resistor has been described. However, the conductive film may be the one other than a resistor, for example, a conductor having a resistance value of approximately zero ohms such as a jumper chip. In such a case, since the resistance value adjustment of the conductive film is not necessary, the protective layer may have a single-layer structure of only the resin coating layer.
Number | Date | Country | Kind |
---|---|---|---|
JP2021-097359 | Jun 2021 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
6856234 | Kuriyama | Feb 2005 | B2 |
6943662 | Tanimura | Sep 2005 | B2 |
8193899 | Takeuchi | Jun 2012 | B2 |
9508473 | Yoneda | Nov 2016 | B2 |
10083781 | Smith | Sep 2018 | B2 |
10438729 | Wyatt | Oct 2019 | B2 |
20030117258 | Kim | Jun 2003 | A1 |
Number | Date | Country |
---|---|---|
2017-45861 | Mar 2017 | JP |
Number | Date | Country | |
---|---|---|---|
20220399140 A1 | Dec 2022 | US |