This disclosure relates generally to an apparatus, system and process for vaporizing materials, such as, for example, inorganic salt catalysts from a catalyst roaster conveyer belt using a heat source such as, for example, hot air flow.
Alkylene oxides are known for a multiplicity of utilities. Ethylene oxide, for example, is used to produce ethylene glycol, nonionic surfactants, glycol ethers, ethanolamines, and polyethylene polyether polyols. Ethylene glycol is used as an automotive coolant, as antifreeze, and in preparing polyester fibers and resins. Propylene oxide is used to produce propylene glycol and polypropylene polyether polyols, which are used in polyurethane polymer applications.
Alkylene Oxides, such as, for example ethylene oxide and propylene oxide, are produced by oxidation of an olefin, such as ethylene or propylene, with oxygen at elevated temperature of about 250° over an inorganic catalyst comprising metallic silver supported on alumina. Typically, promoters such as chloride are also included. The production of ethylene oxide or propylene oxide catalyst occurs in an apparatus such as a catalyst roaster which typically includes an acid bath, usually containing nitric acid, to help clean the silver catalyst from the apparatus. The silver nitrate residue is passed through an air knife apparatus to blow the residue from the conveyor. It has been a challenge to manage the acid fumes generated in such a process, and it has been found that in some cases, the acid fumes escape to the interior of the industrial processing building, where they may pose a serious industrial hygiene and safety problem. Thus, a need has arisen for a process that addresses the foregoing issues.
In accordance with one aspect, an apparatus for drying a catalyst roaster belt including a drying vessel having a catalyst roaster belt inlet, a catalyst roaster belt outlet, a heating medium inlet, and a heating medium outlet, wherein the catalyst roaster belt inlet and the catalyst roaster belt outlet are spaced apart along a first direction, the heating medium inlet and the heating medium outlet are spaced apart along a second direction, the heating medium inlet is spaced apart from the catalyst roaster belt inlet in the second direction, and the catalyst roaster belt inlet is disposed between the heating medium inlet and the heating medium outlet along the second direction is provided.
In another aspect, a system is provided for an apparatus as set forth above that includes an acid bath, and a moveable catalyst roaster belt extending from the acid bath through the catalyst roaster belt inlet and through the catalyst roaster belt outlet to vaporize inorganic salts from the conveyer belt.
In another aspect, a process is provided for removing an inorganic salt from a catalyst roaster belt in an apparatus as set forth above includes the steps of providing the catalyst roaster belt with the inorganic salt disposed thereon, wherein the catalyst roaster belt extends between the catalyst roaster belt inlet and the catalyst roaster belt outlet, and supplying a heating medium to a first side of the catalyst roaster belt such that the heating medium flows through the catalyst roaster belt to a second side of the catalyst roaster belt, and such that the inorganic salt is vaporized.
In yet another aspect, there is provided a process of removing a transition metal from a catalyst roaster belt, comprising the steps of passing the catalyst roaster belt through an acid bath to form a salt of the transition metal, removing liquid acid droplets from the catalyst roaster belt; and supplying a heating medium to a first side of the catalyst roaster belt such that the heating medium flows through the catalyst roaster belt to a second side of the catalyst roaster belt to vaporize the inorganic salt.
Referring now to the drawings, illustrative embodiments are shown in detail. Although the drawings represent some embodiments, the drawings are not necessarily to scale and certain features may be exaggerated, removed, or partially sectioned to better illustrate and explain the present invention. Further, the embodiments set forth herein are exemplary and are not intended to be exhaustive or otherwise limit or restrict the claims to the precise forms and configurations shown in the drawings and disclosed in the following detailed description.
An enclosure shroud 40 is positioned between the drying vessel or second hot zone 56 and the acid bath receptacle through which the belt must travel to get to the drying vessel. The shroud has a top 42 and bottom 44 in generally opposed spaced apart relation separated by sidewalls 46 and 47, and 49 and 43 to define a hollow space 41 through which the belt travels. The shroud is equipped with at least one, and preferably multiple rollers 50, 52 and 54 oriented in the shroud enclosure such that the belt travels into close proximity to air knife system 34 where the belt is subjected to a first phase of drying to begin removal of the warm dilute nitric acid bath solution. The shroud is a substantially sealed system to prevent the acid fumes escape to the interior of the industrial processing building
Air knife system 34 may be utilized to remove acid solution from the belt. In one embodiment, it may consist of a blower mechanism 35 in fluid communication through conduit 37 with an air knife 36 through which it may supply air to blow over the belt as it passes in a first direction from the acid bath through the shroud. In this design aspect, the air knife may be constructed such that it has a thin slit across the whole width of the conveyer belt (thus the name of air knife) through which the air can pass at high velocity (more than 100 meter per second) and impact onto the roaster belt to assist in drying the belt of any residual nitric acid solution as it passes from the acid bath into the shroud area. The air knife system further includes a vent conduit 39 which directs introduced air from the acid bath back to the air knife blower in a manner to be hereinafter described.
As previously stated, the shroud is in substantially sealed relation relative to the interior of the industrial processing building where the system is installed. The drying vessel 56 is a hollow structure comprised of a top 57 and bottom 59 in opposed spaced apart relation separated by opposed exit wall 61 and entrance wall 63 and opposed side walls 65 and 67, to define an interior space 69. Roller 54 is advantageously positioned proximal to roaster belt entrance 51 in entrance wall 63 to assist in guiding the roaster belt into the interior space 69 of the drying vessel. The drying vessel is equipped with a vent 70 in fluid communication with a vacuum source 71 to vent acid fumes and vaporized inorganic salts from the system to a containment zone (not shown) to prevent the acid fumes from building up to any appreciable level in the area where the system is operating. The roaster belt between conduits 85 and 83 and through exit 30 as will be hereinafter described.
Having described one embodiment of the system as contemplated by this disclosure,
As can be seen in
Turning back to
As the air hooks at either the belt inlet or the belt exit are the same, discussion will be made with reference to
As previously described the system includes an air knife system to direct forced air onto the roaster belt as it exits the acid bath. Reference will be made to
Having thus described at least one embodiment of the system, it may be seen that in one aspect, the system can be used in a process for removing an inorganic salt from a catalyst roaster belt using the apparatus and system as described wherein the catalyst roaster belt has an inorganic salt disposed thereon, and wherein the catalyst roaster belt extends between the catalyst roaster belt inlet and the catalyst roaster belt outlet. The system can have heating medium at a first side of the catalyst roaster belt such that the heating medium flows through the catalyst roaster belt to a second side of the catalyst roaster belt, and such that the inorganic salt is vaporized.
In another embodiment, is contemplated that the process for removing an inorganic salt disposed on a catalytic roaster belt includes providing a catalyst roaster belt with the inorganic salt disposed thereon and supplying a heating medium to a first side of the catalyst roaster belt such that the heating medium flows through the catalyst roaster belt to a second side of the catalyst roaster belt, and such that the inorganic salt is vaporized. The catalytic belt may be moving in a first direction and the heated medium flows in a second direction. The first direction and the second direction may or may not be parallel to each other. The heating medium may be air, and the inorganic salt is a nitrate salt, and more specifically may be silver nitrate.
In another embodiment, the process may include an enclosure within which the catalyst roaster belt is partially disposed, and into which the heating medium flows. The enclosure operates at a pressure less than atmospheric pressure, and may preferably operate at no more than about 0.1 in. H2O column vacuum.
In another embodiment, there is contemplated a process for drying a catalytic roaster belt wherein the enclosure includes a catalyst roaster belt inlet, and the process further comprises receiving air through the catalyst roaster belt inlet and diverting the received air away from the catalyst roaster belt. When the heated medium is introduced into the interior of the drying vessel, it may flow in a plurality of directions in the interior of the enclosure before flowing through the catalyst roaster belt. In another embodiment, when the system has two baffles the heating medium comprises supplying the heating medium may be introduced to a first side of the catalyst roaster belt such that the heating medium flows between the baffles.
In another embodiment, the process of removing a transition metal from a catalyst roaster belt may comprise the steps of passing the catalyst roaster belt through an acid bath to form a salt of the transition metal such as silver nitrate, removing liquid acid droplets from the catalyst roaster belt such as forced air by impinging a gas stream on the catalyst roaster belt; and supplying a heating medium to a first side of the catalyst roaster belt such that the heating medium flows through the catalyst roaster belt to a second side of the catalyst roaster belt, and such that the inorganic salt is vaporized. The acid may be nitric acid, and the heating medium temperature is no less than about 450° C. and no greater than about 750° C.
The preceding description has been presented only to illustrate and describe exemplary embodiments of the methods and systems of the present invention. It is not intended to be exhaustive or to limit the invention to any precise form disclosed. It will be understood by those skilled in the art that various changes may be made and equivalents may be substituted for elements thereof without departing from the scope of the invention. In addition, many modifications may be made to adapt a particular situation or material to the teachings of the invention without departing from the essential scope. Therefore, it is intended that the invention not be limited to the particular embodiment disclosed as the best mode contemplated for carrying out this invention, but that the invention will include all embodiments falling within the scope of the claims. The invention may be practiced otherwise than is specifically explained and illustrated without departing from its spirit or scope. The scope of the invention is limited solely by the following claims.
This application claims the benefit of U.S. Provisional Application No. 61/255,591, filed on Oct. 28, 2009, which is hereby incorporated by reference in its entirety.
Number | Name | Date | Kind |
---|---|---|---|
1982756 | Roesen | Dec 1934 | A |
3437605 | Keith | Apr 1969 | A |
3849904 | Villalobos | Nov 1974 | A |
3909953 | Hemsath et al. | Oct 1975 | A |
3913241 | Chaikin et al. | Oct 1975 | A |
4107378 | Bourguignon et al. | Aug 1978 | A |
4135308 | Benson | Jan 1979 | A |
4248741 | Wernli et al. | Feb 1981 | A |
4365423 | Arter et al. | Dec 1982 | A |
4472624 | Janning | Sep 1984 | A |
4538899 | Landa et al. | Sep 1985 | A |
4696115 | Spadafora | Sep 1987 | A |
4715912 | Tillotson | Dec 1987 | A |
4825561 | Cornell | May 1989 | A |
4916243 | Bhasin et al. | Apr 1990 | A |
4984594 | Vinegar et al. | Jan 1991 | A |
5008413 | Liu | Apr 1991 | A |
5024319 | Dixon et al. | Jun 1991 | A |
5071540 | Culross et al. | Dec 1991 | A |
5270519 | Higgins | Dec 1993 | A |
5343632 | Dinh | Sep 1994 | A |
5553189 | Stegemeier et al. | Sep 1996 | A |
5600899 | Stevens et al. | Feb 1997 | A |
5641722 | Mitchell et al. | Jun 1997 | A |
5651191 | Walunas et al. | Jul 1997 | A |
5680713 | Forbert et al. | Oct 1997 | A |
5881476 | Strobush et al. | Mar 1999 | A |
5967770 | Heine et al. | Oct 1999 | A |
6157002 | Schjerven, Sr. et al. | Dec 2000 | A |
6184175 | Rizkalla | Feb 2001 | B1 |
6589417 | Taciuk et al. | Jul 2003 | B2 |
6735882 | Takahashi | May 2004 | B2 |
7214903 | Curatolo | May 2007 | B2 |
7401417 | Rydell et al. | Jul 2008 | B2 |
7410104 | MacPherson | Aug 2008 | B2 |
7432483 | Wilson | Oct 2008 | B2 |
20040025366 | Soucy | Feb 2004 | A1 |
20070023413 | Wilson | Feb 2007 | A1 |
20110094120 | Bai et al. | Apr 2011 | A1 |
Number | Date | Country |
---|---|---|
1299667 | Jan 1965 | DE |
10301738 | Jul 2004 | DE |
07165932 | Jun 1995 | JP |
2003066732 | Mar 2003 | JP |
WO 9604989 | Feb 1996 | WO |
WO 2007104268 | Sep 2007 | WO |
Entry |
---|
International Search Report dated Mar. 10, 2011 for International Application No. PCT/US2010/054091. |
Written Opinion of the International Searching Authority mailed Mar. 10, 2011 for International Application No. PCT/US2010/054091. |
EP Office Action for International Application No. 10776003.5, dated Apr. 23, 2013, 8 pages. |
Number | Date | Country | |
---|---|---|---|
20110094120 A1 | Apr 2011 | US |
Number | Date | Country | |
---|---|---|---|
61255591 | Oct 2009 | US |