One aspect relates to a method for producing an electrical bushing for an implantable device, another to an implantable medical device, another to an electrical bushing as well as to an implantable device.
DE 697 29 719 T2 describes an electrical bushing for an implantable electrical therapeutic device. Electrical bushings of this type serve to establish electrical connection between a hermetically sealed interior and an exterior of the therapeutic device.
Known examples of implantable therapeutic devices include brain pacemakers, cardiac pacemakers or defibrillators. These devices commonly include a hermetically sealed metal housing which is provided with a connection body, also called header, on one side. The connection body includes a connection socket that serves for connection of electrode leads, which is effected, for example, by means of a bajonet lock. In this context, the connection socket includes electrical contacts that serve to electrically connect electrode leads to control electronics on the interior of the housing of the implantable device.
Hermetic sealing with respect to a surrounding is an essential prerequisite of a corresponding electrical bushing since the control electronics needs to be kept isolated from liquids in order to consistently prevent malfunctions or total failure. Since the conducting wires generally are metal wires or metal pins that are introduced into an electrically insulating ceramic base body of the electrical bushing, the interfaces between the conducting wires and the base body are weak spots. It needs to be ensured, therefore, that the signal-transmitting conducting wires that are introduced into the electrical bushing are introduced into the insulating element such as to be free of gaps.
A gap-free connection between the two elements is commonly generated by metallizing an internal surface of a bore hole in the base body and soldering to it a conducting wire that is guided through it. However, the application of the metallization in the bore hole in the insulating element is a difficult task. Homogeneous metallization of the internal surface of the bore hole in the insulating element are ensured only via cost-intensive procedures.
For these and other reasons there is a need for the present invention.
One embodiment is a method for producing an electrical bushing for an implantable device characterized in that a green blank is produced from an electrically insulating base body and at least one electrically conductive bushing conductor that extends through the base body. It includes forming the base body from a ceramic slurry and introducing a bushing conductor made of a metal powder, metal slurry, cermet powder and/or cermet slurry into the base body. The metal fraction in the bushing conductor is provided to decrease towards the base body. It includes sintering the green blank that includes the base body and the bushing conductor.
The accompanying drawings are included to provide a further understanding of embodiments and are incorporated in and constitute a part of this specification. The drawings illustrate embodiments and together with the description serve to explain principles of embodiments. Other embodiments and many of the intended advantages of embodiments will be readily appreciated as they become better understood by reference to the following detailed description. The elements of the drawings are not necessarily to scale relative to each other. Like reference numerals designate corresponding similar parts.
The invention is described in the following, without limiting its general spirit, by means of exemplary embodiments making reference to the drawings, whereby we wish to explicitly refer to the drawings with regard to any and all details according to the invention that are not elaborated on in more detail in the description. In the figures:
In the following Detailed Description, reference is made to the accompanying drawings, which form a part hereof, and in which is shown by way of illustration specific embodiments in which the invention may be practiced. In this regard, directional terminology, such as “top,” “bottom,” “front,” “back,” “leading,” “trailing,” etc., is used with reference to the orientation of the Figure(s) being described. Because components of embodiments can be positioned in a number of different orientations, the directional terminology is used for purposes of illustration and is in no way limiting. It is to be understood that other embodiments may be utilized and structural or logical changes may be made without departing from the scope of the present invention. The following detailed description, therefore, is not to be taken in a limiting sense, and the scope of the present invention is defined by the appended claims.
It is to be understood that the features of the various exemplary embodiments described herein may be combined with each other, unless specifically noted otherwise.
In the figures below, identical or equivalent elements or corresponding parts are denoted with the same reference numbers such that no presentation thereof is provided again herein.
Based on the above-described prior art, one embodiment provides an electrical bushing for an implantable device, and in one embodiment, an implantable medical device, in which the above-mentioned disadvantages associated with the prior art are averted and the long-lasting hermetic sealing of the electrical bushing is ensured.
One embodiment is a method for producing an electrical bushing for an implantable device that is developed such that a green blank is produced from an electrically insulating base body and at least one electrically-conductive bushing conductor that extends through the base body, comprising the following steps:
In one embodiment, in place of the techniques used previously, in which an electrically conductive wire needed to be guided through a bushing made of a sintered ceramic material and soldered or welded to same, the bushing consists of a sintered material entirely and thus firmly bonded shaping throughout free of sites of fracture and hermetically sealing is attained. The problem that is encountered according to the prior art, being that the seam between a conducting wire and the surrounding sintered material of an insulating base body comes undone and thus breaks the hermetic sealing is thus prevented according to the embodiment, since a predetermined breakage site of this type is no longer present.
In the context of one embodiment, the term, “cermet”, refers to a composite material made of ceramic materials in a metallic matrix. In its unprocessed state, it is a mixture of a ceramic powder and a metallic powder. Cermets are characterized by their particularly high hardness and resistance to wear. Cermets are materials that are related to hard metals, but dispense with the hard material, tungsten carbide, and are produced by powder metallurgical means. The sintering process for cermet proceeds alike the one for homogeneous powders. At identical compression force, the metal is compacted more strongly than the ceramic material. Compared to sintered hard metals, a cermet-containing positional element illustrates higher resistance to thermal shock and oxidation. The ceramic components of the cermet in most cases are aluminum oxide (Al2O3) and zirconium dioxide (ZrO2), whereas niobium, molybdenum, titanium, cobalt, zirconium, and chromium are preferred in one embodiment as metallic components.
The material to be used according to one embodiment can be a dry powder that is compressed into a green blank in the dry state and possesses sufficient adhesion to maintain its compressed green blank shape. In the context of one embodiment, a slurry is a suspension of particles of a powder made of one or more material(s) in a liquid binding agent, commonly in water or in an organic binding agent. A slurry possesses high viscosity and is easy to shape into a green blank without having to apply high pressure.
In the case of green blanks made from slurries, the sintering process, which is generally carried out below the melting temperature of the ceramic, cermet or metal materials that are used, but in individual cases can also be carried out just above the melting temperature of the lower melting component of a multi-component mixture, this usually being the metal component, leads to the binding agent slowly diffusing from the slurry. Overly rapid heating leads a rapid increase of the volume of the binding agent by transition to the gas phase and destruction of the green blank or formation of undesired defects in the work-piece.
During sintering, sintering necks are formed between the particles of the green blank which effects firmly bonded connection of the particles to each other. Simultaneously, the particles of the material move closer together which reduces the size of hollow spaces between the particles until hermetic sealing of the sintered work-piece with respect to gases and liquids is attained. The work-piece shrinks during this process.
It is known that cermet-containing slurries, due to their metal fraction, are subject to more extensive shrinking during the sintering than pure ceramic slurries. Accordingly, there is a risk that the bushing body shrinks more strongly during the sintering than the pure ceramic base body such that no hermetic sealing of the two is established. This is solved according to one embodiment by means of the selection of the shapes of the openings and/or of the green blank bodies that are introduced into the openings as well as by application of a force.
The bushing conductor according to one embodiment in the base body consists of a sintered material, such as a sintered metal and/or cermet slurry or a metal and/or cermet powder, which is introduced into the base body first, before same is sintered in the form of an assembled green blank. In the process, a stepwise or gradually decreasing metal fraction, from the center of the bushing conductor to the base body surrounding the same, is established.
The metal fraction has a dual role. Firstly, the metal powder and/or the metal particles in the metal slurry and/or in the cermet become a continuous metallically and therefore electrically conductive conductor that enables a transmission of electrical current. Secondly, the metal in the cermet and/or in the metal powder also forms a matrix for ceramic particles embedded therein which are thus held therein and result in a particularly durable structure.
What the metal fraction decreasing from inside towards outside, also called gradient, effects is that the different shrinking behavior of a metal and/or cermet slurry or powder with respect to the surrounding ceramic slurry or ceramic powder is balanced out and tensions in the material occurring due to the different shrinkage are balanced out. The tensions are therefore not concentrated in one point and do not lead to defects in the material in said point.
An electrically conductive connection is established if the metal content of the cermet is in one embodiment 80% or more, and in another embodiment is 90% or more.
In a development of the method according to one embodiment, for introduction of the at least one bushing conductor into the base body, a bushing opening is generated in the base body and one or more organic films, such as in a concentric arrangement, which have a low combustion point and separate various volumes from each other, are introduced into the bushing opening, whereby metal powder, cermet powder, metal slurry and/or cermet slurry with different metal fractions are subsequently filled into the various volumes. In the context of one embodiment this means that the metal fraction of the material in one volume differs from that in another volume. In particular, materials with progressively decreasing metal fractions are filled in, progressing from inside towards outside, and thus a gradual gradient of the metal fraction of the material filled into the volumes is generated.
Separated by the organic films, the materials filled into the various volumes do not mix during the sintering. Since the organic films have a combustion temperature below the sintering temperature, they disintegrate during the sintering and diffuse from the green blank. Once the organic films have disintegrated, the adjoining materials of the initially separately filled volumes contact each other and form a firmly bonded sintered connection to each other.
In another embodiment, which can also be used in addition to the embodiment of the method discussed above, for introduction of the at least one bushing conductor into the base body, it is preferable to generate a bushing opening in the base body, form a bushing conductor green blank and insert it into the bushing opening of the base body. Green blanks of bushing conductors and bushing openings in the green blank of the base body can be shaped to a perfect fit and can be placed inside each other after removal from the mold. It is also feasible to introduce a corresponding green blank of a bushing conductor into an organic film according to the above-mentioned variant of the method or to initially wrap it with the film and then to introduce it into the bushing opening.
Prior to inserting it in the bushing opening, the bushing conductor green blank is enveloped in one or more transitional layers made of a cermet slurry whose metal fraction or metal fractions decrease(s) progressively from inside towards outside, in particular with respect to the metal fraction of the bushing conductor green blank. By this means, a gradient of the metal fraction of the bushing conductor from inside towards outside is established.
In another variant of the method according to one embodiment, which can also be used in addition to one or both of the embodiments of the method described above, for introduction of the at least one bushing conductor into the base body, the base body and/or a cermet slurry-filled volume of the bushing opening is punctured with an injection needle and the injection needle is retracted while injecting a metal powder, a metal slurry, a cermet powder and/or a cermet slurry.
In this variant, the material with the highest metal fraction is injected directly into the green blank of the base body or of a bushing conductor. When the injection needle punctures the material, it first generates a channel with the same diameter as the injection needle and the material that was situated in said space is pushed aside. Upon retraction of the injection needle, said channel is filled out with a material with a high metal fraction.
In one embodiment, the injection proceeds under pressure and the injected metal and/or cermet powder and/or the injected metal and/or cermet slurry penetrates into the surrounding material under pressure. Due to the penetration, the material with a high metal fraction mixes more strongly with the surrounding material with a low or non-existent metal fraction as compared to if it is filled-in without pressure such that a gradient and/or metal fraction that gradually decreases from inside towards outside is established in the material. Suitable injectors are known and work, for example, on the basis of piezo elements. Hydraulic or pneumatic pressure generators can also be used according to the embodiment.
The injection needle in one embodiment includes two or more injection channels in a concentric arrangement through which two or more materials with different metal fractions can be co-extruded or co-injected into the base body or into the bushing conductor. By this means, a bushing conductor or the core of a bushing conductor is generated in one procedural step that generates a metal fraction gradient that decreases from inside towards outside. In this context, according to one embodiment, the term, “extrude”, refers to the injection of a metal or cermet slurry, whereas the term, “inject”, refers to both a slurry and a powder.
If, after completing the sintering, at least one surface of the electrical bushing is polished and contacted with a metallic pin or wire in at least one place of the surface at which the at least one bushing conductor is arranged, a stable and hermetically sealed electrical bushing is attained. The contacting is effected by means of soldering or welding, whereby in particular laser welding and resistance welding lead to long-lasting contacting that conducts the electric current well. The contacting is effected by metallic wires or pins. Alternatively, the bushing conductor can be provided to be projecting beyond the electrical bushing and/or the base body and itself form a contacting pin. This means provides for current flow from one side of the bushing conductor to the other side.
A stable connection of an electrical bushing to a housing is achieved if, in addition, prior to the sintering, a wreath-shaped fringe body is formed from a cermet slurry and has a receiving opening for the base body into which the base body is inserted in order to form the green blank. Said green blank with the fringe body is then sintered, whereby the fringe body, having a metal fraction, enables good connection to a metallic housing of an implantable device.
One embodiment is an electrical bushing for an implantable device having an electrically insulating base body and at least one electrically conductive bushing conductor that extends through the base body, whereby the base body is produced from a sintered ceramic material, and which electrical bushing is developed such that the at least one bushing conductor consists of a metal and/or cermet material that has been jointly sintered with the base body and has a metal fraction that decreases from the interior of the bushing conductor towards the outside.
The corresponding electrical bushing according to one embodiment possesses the advantages mentioned above in relation to the method, for example in one embodiment, the firmly bonded production of the entire electrical bushing with a fully firmly bonded incorporation of the bushing conductor(s) in the insulating base body, whereby tension due to the different shrinking processes of the various metals during the sintering are reduced, in particular, by the metal fraction gradient from the bushing conduction to the material of the base body. This contributes to a long service life of the hermetic seal.
In one embodiment, the base body is connected circumferentially to a wreath-shaped fringe body made of a cermet material through a firmly bonded sintered connection, whereby the fringe body includes a receiving opening, in which the base body is arranged. Having the fringe body enables easy availability and/or ability of the electrical bushing to be connected in a housing of an implantable device.
In one embodiment, the electrical bushing is hermetically sealed for gases and liquids. For this purpose, for example, the sintering process is carried out until the material has compacted to the degree that no patent pores are present any longer.
An electrical bushing according to one embodiment can be or is produced according to any one of the methods according to the embodiments described above.
One embodiment is an implantable device having an electrical bushing of the type described above.
Features, advantages, and details specified in the context of one of the subject matters of one embodiment shall also apply to the respective other subject matters of other embodiments.
The electrical bushing 3 hermetically seals an opening in housing 2. In electrical bushing 3, the bushing conductor 20 is framed sequentially by transitional layers 30 and a base body 10, which includes on its circumference a fringe body 40 next to which the housing 2 is situated. The electrically insulating base body 10 prevents short-circuiting between the electrically conductive, extended conducting wire 5 and the metallic housing 2 and/or the fringe body 40 which is also partly metallic.
The base body 10 is made from an insulating composition of materials. Electrical signals proceeding through the conducting wire 5 are not to be attenuated or short-circuited by contacting the housing 2 of the implantable device 1. Moreover, the base body 10 must include a biocompatible composition to be suitable for medical implantation. For this reason, it is preferred in one embodiment for the base body 10 to consist of a glass-ceramic or glass-like material. Compositions of base body 10 materials that include at least one from the group, aluminum oxide (Al2O3), magnesium oxide (MgO), zirconium oxide (ZrO2), aluminum titanate (Al2TiO5), and piezoceramic materials, are preferred in some embodiments. Said substances possess high electrical resistance and low dielectric losses. In addition, these properties are complemented by high thermal resistance and good biocompatibility. Biocompatible metals include, in some embodiments, metals from the group, titanium (Ti), tantalum (Ta), iridium (Ir), niobium (Nb), platinum (Pt) or an alloy including at least one of these metals.
The insulating composition of materials is a powder mass that illustrates at least minimal adhesion of the powder particles. This is commonly implemented in that a grain size of the powder particles does not exceed 0.5 mm. In this context, the green blank is produced either by compaction of powder masses or by shaping and subsequent drying. Green blanks of an insulating base body 10 and of electrically conductive bushing conductors 20 and, if applicable, of a fringe body 40 are produced in parallel, placed inside each other and fired subsequently.
Bushing conductors 20 are embedded in the base body 10 and jacketed each with a transitional layer 30. The transitional layer 30 consists of a cermet with a metal content of approx. 20% to approx. 70%, whereas the bushing conductor 20 includes a higher metal content and, in one embodiment, consists entirely of a sintered metallic material. Since the entire part illustrated in
The fringe body 40 includes a flange 41, whereby the flange, in one embodiment, is metallically conductive. The flange serves to seal the electrical bushing with respect to a housing 2 of the implantable device 1. The electrical bushing 3 is held in the implantable device 1 by the fringe body 40. The flange 41 forms a bearing that can be engaged by a lid of the implantable medical device 1, in a sealing manner. Accordingly, the fringe body 40 having the flange 41 can have a U- or H-shaped cross-section. Integrating at least one flange 41 into the fringe body 40 ensures secure, shock-resistant, and long-lasting integration of the electrical bushing 3 in the implantable device 1. In addition, the flange can be provided such that a lid of the implantable device 1 is connected to the fringe element 40 in a non-positive fit and/or positive fit manner.
In
The situation illustrated in
Another method of implementing the situation according to
In order to increase the electrical conductivity of the bushing conductor, it is also feasible to proceed according to
All specified features, including those evident from the drawings only, as well as individual features that are disclosed in combination with other features are considered essential for the embodiments both alone and in combination. Embodiments according to the invention can be provided through individual features or a combination of multiple features. Although specific embodiments have been illustrated and described herein, it will be appreciated by those of ordinary skill in the art that a variety of alternate and/or equivalent implementations may be substituted for the specific embodiments shown and described without departing from the scope of the present invention. This application is intended to cover any adaptations or variations of the specific embodiments discussed herein. Therefore, it is intended that this invention be limited only by the claims and the equivalents thereof.
Number | Date | Country | Kind |
---|---|---|---|
10 2010 006 689 | Feb 2010 | DE | national |
This application is a divisional of U.S. patent application Ser. No. 13/018,882, entitled “METHOD OF PRODUCING AN ELECTRICAL BUSHING WITH GRADIENT CERMET,” having a filing date of Feb. 1, 2011, which claims priority to German Patent Application No. DE 10 2010 006 689.3, filed on Feb. 2, 2010, all of which are incorporated herein by reference. This Patent Application is also related to Utility patent application Ser. No. 13/018,847 filed on Feb. 1, 2011, entitled “METHOD FOR SINTERING ELECTRICAL BUSHINGS”, which is incorporated herein by reference.
Number | Name | Date | Kind |
---|---|---|---|
4352951 | Kyle | Oct 1982 | A |
4362792 | Bowsky et al. | Dec 1982 | A |
4456786 | Kyle | Jun 1984 | A |
4488673 | Hopper, Jr. | Dec 1984 | A |
4678868 | Kraska et al. | Jul 1987 | A |
4737601 | Gartzke | Apr 1988 | A |
4774953 | Foote | Oct 1988 | A |
4816621 | Huebner et al. | Mar 1989 | A |
4991582 | Byers et al. | Feb 1991 | A |
4992910 | Evans | Feb 1991 | A |
5046262 | Kerbaugh | Sep 1991 | A |
5245999 | Dahlberg et al. | Sep 1993 | A |
5272283 | Kuzma | Dec 1993 | A |
5513793 | Malmgren | May 1996 | A |
5654106 | Purnell et al. | Aug 1997 | A |
5683435 | Truex et al. | Nov 1997 | A |
5738270 | Malmgren | Apr 1998 | A |
5750926 | Schulman et al. | May 1998 | A |
5769874 | Dahlberg | Jun 1998 | A |
5782891 | Hassler et al. | Jul 1998 | A |
5821011 | Taylor et al. | Oct 1998 | A |
5851222 | Taylor et al. | Dec 1998 | A |
5855711 | Araki et al. | Jan 1999 | A |
5861714 | Wei et al. | Jan 1999 | A |
5866851 | Taylor et al. | Feb 1999 | A |
6232004 | Lasater | May 2001 | B1 |
6284080 | Haq et al. | Sep 2001 | B1 |
6414835 | Wolf et al. | Jul 2002 | B1 |
6579492 | Wehler | Jun 2003 | B2 |
6586675 | Bealka et al. | Jul 2003 | B1 |
6660116 | Wolf et al. | Dec 2003 | B2 |
7068491 | Burdon et al. | Jun 2006 | B1 |
7107099 | O'Phelan et al. | Sep 2006 | B1 |
7222419 | Horng et al. | May 2007 | B2 |
7480988 | Ok et al. | Jan 2009 | B2 |
7569452 | Fu et al. | Aug 2009 | B2 |
7668597 | Engmark et al. | Feb 2010 | B2 |
7818876 | Suaning | Oct 2010 | B2 |
7901761 | Jiang et al. | Mar 2011 | B1 |
7930032 | Teske et al. | Apr 2011 | B2 |
7970474 | Starke | Jun 2011 | B2 |
8000804 | Wessendorf et al. | Aug 2011 | B1 |
8155743 | Rundle et al. | Apr 2012 | B2 |
8163397 | Ok et al. | Apr 2012 | B2 |
8189333 | Foster | May 2012 | B2 |
8494635 | Troetzschel et al. | Jul 2013 | B2 |
8528201 | Troetzschel et al. | Sep 2013 | B2 |
8886320 | Troetzschel et al. | Nov 2014 | B2 |
8929987 | Troetzschel et al. | Jan 2015 | B2 |
9048608 | Pavlovic | Jun 2015 | B2 |
9088093 | Reisinger | Jul 2015 | B2 |
9126053 | Kempf | Sep 2015 | B2 |
9129747 | Pinwill | Sep 2015 | B2 |
20010018012 | Harmand et al. | Aug 2001 | A1 |
20020166739 | Naerheim | Nov 2002 | A1 |
20030109903 | Berrang et al. | Jun 2003 | A1 |
20040023101 | Jacobson et al. | Feb 2004 | A1 |
20040128016 | Stewart | Jul 2004 | A1 |
20060025866 | Serafin, Jr. et al. | Feb 2006 | A1 |
20060247714 | Taylor et al. | Nov 2006 | A1 |
20070041164 | Greenberg et al. | Feb 2007 | A1 |
20070217121 | Fu et al. | Sep 2007 | A1 |
20070276389 | Franke et al. | Nov 2007 | A1 |
20080060834 | Eck et al. | Mar 2008 | A1 |
20090281586 | Lim | Nov 2009 | A1 |
20100121438 | Jarvik | May 2010 | A1 |
20110032658 | Iyer | Feb 2011 | A1 |
20110034965 | Troetzschel et al. | Feb 2011 | A1 |
20110034966 | Troetzschel et al. | Feb 2011 | A1 |
20110048770 | Reiterer et al. | Mar 2011 | A1 |
20110094768 | Davis et al. | Apr 2011 | A1 |
20110186349 | Troetzschel et al. | Aug 2011 | A1 |
20110190885 | Troetzschel et al. | Aug 2011 | A1 |
20110232961 | Teske | Sep 2011 | A1 |
20110232962 | Teske | Sep 2011 | A1 |
20130299233 | Troetzschel et al. | Nov 2013 | A1 |
20140008121 | Troetzschel et al. | Jan 2014 | A1 |
20140144014 | Troetzschel et al. | May 2014 | A1 |
Number | Date | Country |
---|---|---|
697 297 19 | Jul 2005 | DE |
102009035971 | Feb 2011 | DE |
102009035972 | Apr 2011 | DE |
Entry |
---|
Advisory Action for U.S. Appl. No. 12/850,412 mailed Apr. 14, 2014 (3 pgs.). |
Office Action for U.S. Appl. No. 12/850,412 mailed May 8, 2014 (11 pgs.). |
Notice of Allowance for U.S. Appl. No. 12/850,412 mailed Sep. 2, 2014 (11 pgs.). |
Restriction Requirement for U.S. Appl. No. 14/171,275 mailed Nov. 2, 2015 (6 pgs.). |
Final Office Action for U.S. Appl. No. 13/942,685 mailed Apr. 14, 2014 (22 pgs.). |
Notice of Allowance for U.S. Appl. No. 13/942,685 mailed Jul. 7, 2014 (5 pgs.). |
Office Action for U.S. Appl. No. 12/850,406 mailed Sep. 17, 2012 (11 pages). |
Final Office Action for U.S. Appl. No. 12/850,406 mailed Feb. 25, 2013 (16 pages). |
Office Action for U.S. Appl. No. 12/850,406 mailed Sep. 12, 2013 (16 pages). |
Dictionary definition of a cermet found at The Free Dictionary site http://www.thefreedictionary.com/cermets. |
Notice of Allowance for U.S. Appl. No. 12/850,406 mailed Feb. 5, 2014 (9 pages). |
Office Action for U.S. Appl. No. 12/850,412 mailed Sep. 17, 2012 (11 pages). |
Final Office Action for U.S. Appl. No. 12/850,412 mailed Feb. 25, 2013 (18 pages). |
Office Action for U.S. Appl. No. 12/850,412 mailed Sep. 11, 2013 (13 pages). |
Final Office Action for U.S. Appl. No. 12/850,412 mailed Jan. 31, 2014 (8 pages). |
Restriction Requirement for U.S. Appl. No. 13/018,882 mailed Dec. 20, 2012 (5 pages). |
Notice of Allowance for U.S. Appl. No. 13/018,882 mailed May 10, 2013 (25 pages). |
Notice of Allowability for U.S. Appl. No. 13/018,882 mailed Jul. 16, 2013 (6 pages). |
Office Action for U.S. Appl. No. 13/018,847 mailed Dec. 5, 2012 (24 pages). |
Notice of Allowance for U.S. Appl. No. 13/018,847 mailed Mar. 25, 2013 (25 pages). |
Office Action for U.S. Appl. No. 13/942,685 mailed Dec. 23, 2013 (10 pages). |
Number | Date | Country | |
---|---|---|---|
20140008121 A1 | Jan 2014 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 13018882 | Feb 2011 | US |
Child | 14023096 | US |