The present invention relates to a shadow mask frame, especially to a fine shadow mask assembly for an active matrix organic light emitting diode (AMOLED) and a fine shadow mask assembly manufacturing method for an AMOLED. The fine shadow mask assembly for the AMOLED has excellent structure strength and can prevent deformation. Furthermore, when the fine shadow mask assembly for the AMOLED is employed in a vapor deposition process for manufacturing an AMOLED display panel, the structure of the fine shadow mask assembly itself is compact without any gaps and can prevent organic material for vapor deposition from inadvertently passing through the fine shadow mask assembly for the AMOLED and falling onto a glass substrate of the AMOLED display panel.
With reference to
The shadow mask frame 91 is rectangular. The transverse spacer plates 93 are sheet plates, are tensioned and disposed on the shadow mask frame 91 at intervals. The longitudinal supporting plates 92 are sheet plates, are tensioned and disposed on the transverse spacer plates 93 at intervals, each longitudinal supporting plate 92 intersects the transverse spacer plates 93.
The shadow mask plates 94 are disposed on the longitudinal supporting plates 92 and is perpendicular to the transverse spacer plates 93 such that each of the transverse spacer plates 93 is located under a gap between adjacent two of the shadow mask plates 94. Each of the transverse spacer plates 93 mainly serves to cover and block the gap between the adjacent two shadow mask plates 94. When the fine shadow mask assembly for the AMOLED is used in a later vapor deposition process for manufacturing an AMOLED display panel, the transverse spacer plates 93 prevents organic material from falling downward through the gap onto a glass substrate (not shown in the figures) of the AMOLED display panel under the shadow mask plates 94. Furthermore, a plurality of pattern regions 941 are formed on each the shadow mask plate 94 to form pixel units of the AMOLED display panel in later processes of the AMOLED display panel.
However, the above-mentioned fine shadow mask assembly for the AMOLED has the following disadvantages.
1. To ensure that the shadow mask plates 94 are disposed flatly on the shadow mask frame 91 and would not has partial ridges or depressions relative to the shadow mask frame 91, the longitudinal supporting plates 92 need to be sheet plates and cannot include too much thickness. However, the sheet-like longitudinal supporting plates 92 has insufficient supporting strength and is easily deformed, which also makes the shadow mask plates 94 deform easily.
2. The transverse spacer plates 93 is disposed under the longitudinal supporting plates 92 and does not directly contact the shadow mask plates 94. Therefore, a gap exists between each of the transverse spacer plates 93 and a corresponding one of the shadow mask plates 94. The organic material in the vapor deposition can still fall on the lower glass substrate through such gaps.
3. The transverse spacer plates 93 is disposed under the longitudinal supporting plates 92 instead of being supported by the longitudinal supporting plate 92, and therefore deforms easily.
4. The sheet-like longitudinal supporting plates 92 contact the shadow mask plates 94 by surfaces so friction there-between is large, which disadvantages fine adjustment of tension force when the longitudinal supporting plates 92 are tensioned.
Therefore, it is necessary to provide a fine shadow mask assembly for an AMOLED and a fine shadow mask assembly manufacturing method for the AMOLED to solve the issues of the prior art.
A primary objective of the present invention is to provide an active matrix organic light emitting diode (AMOLED) fine shadow mask assembly, the fine shadow mask assembly for the AMOLED has excellent structure strength and can prevent deformation. Furthermore, when the fine shadow mask assembly for the AMOLED is employed in a vapor deposition process for manufacturing an AMOLED display panel, the structure of the fine shadow mask assembly itself is compact without any gaps and can prevent organic material for vapor deposition from inadvertently passing through the fine shadow mask assembly for the AMOLED and falling onto a glass substrate of the AMOLED display panel.
To achieve the above-mentioned objective, the fine shadow mask assembly for the AMOLED of the present invention comprises:
a shadow mask frame;
a plurality of longitudinal supporting bars disposed on the shadow mask frame and arrange at intervals, each of the longitudinal supporting bars comprising a circular rod portion and two flat portions, and the two flat portions formed on two ends of the circular rod portion respectively, disposed on a top edge of the shadow mask frame, and located at two opposite sides of the shadow mask frame respectively;
a plurality of transverse spacer plates disposed on the circular rod portions of the longitudinal supporting bars, supported by the longitudinal supporting bars, intersecting the longitudinal supporting bars, and arranged at intervals; and
a plurality of shadow mask plates disposed on the transverse spacer plates, supported by the longitudinal supporting bars, and paralleling the transverse spacer plates, wherein each of the transverse spacer plates is located under a gap between adjacent two of the shadow mask plates, contacts the adjacent two of the shadow mask plates, and covers the gap.
In the present invention, pairs of fixing notches are defined in the shadow mask frame, the pairs of the fixing notches correspond to the longitudinal supporting bars, the two fixing notches of each pair are defined in the top edge of the shadow mask frame, are located on the two opposite sides of the shadow mask frame respectively, and fix and receive the two flat portions of a corresponding one of the longitudinal supporting bars.
In the present invention, a top edge of the circular rod portion of each of the longitudinal supporting bars is flush with the top edge of the shadow mask frame.
In the present invention, a diameter of the circular rod portion of each of the longitudinal supporting bars is greater than a thickness of the flat portion.
In the present invention, a diameter of the circular rod portion of each of the longitudinal supporting bars is less than a width of the flat portion.
In the present invention, each of the flat portions of each of the longitudinal supporting bars comprises two soldering sides.
In the present invention, each of the flat portions of each of the longitudinal supporting bars comprises a truncated distal end.
In the present invention, a diameter of the circular rod portion of each of the longitudinal supporting bars is 0.6 mm, a thickness of the flat portions is 0.3 mm, and a depth of each of the fixing notches is 0.45 mm.
Another objective of the present invention is to provide an active matrix organic light emitting diode (AMOLED) fine shadow mask assembly manufacturing method comprising:
a shadow mask frame providing step, providing a shadow mask frame;
a longitudinal supporting bar disposing step, disposing a plurality of longitudinal supporting bars on the shadow mask frame, wherein each of the longitudinal supporting bars comprises a circular rod portion and two flat portions, the two flat portions are formed on two ends of the circular rod portion and are disposed on a top edge of the shadow mask frame;
a transverse spacer plates disposing step, disposing a plurality of transverse spacer plates on the circular rod portions of the longitudinal supporting bars, wherein the transverse spacer plates intersect the longitudinal supporting bars; and
a shadow mask plate disposing step, disposing a plurality of shadow mask plates on the transverse spacer plates, wherein each of the transverse spacer plates is located under a gap between adjacent two of the shadow mask plates, contacts the adjacent two of the shadow mask plates, and covers the gap.
In the present invention, the fine shadow mask assembly for the AMOLED manufacturing method further comprises a longitudinal supporting bar tensioning step, the longitudinal supporting bar tensioning step is implemented before the transverse spacer plates disposing step, and comprises tensioning the longitudinal supporting bars.
In the present invention, the fine shadow mask assembly for the AMOLED manufacturing method further comprises a transverse spacer plate tensioning step, the transverse spacer plate tensioning step is implemented before the shadow mask plate disposing step, and comprises tensioning the transverse spacer plates.
In the present invention, the fine shadow mask assembly for the AMOLED manufacturing method further comprises a shadow mask plate tensioning step comprising tensioning the shadow mask plates.
Still another objective of the present invention is to provide an active matrix organic light emitting diode (AMOLED) fine shadow mask assembly comprising:
a shadow mask frame;
a plurality of longitudinal supporting bars disposed on the shadow mask frame and arrange at intervals, each of the longitudinal supporting bars comprising a circular rod portion and two flat portions, and the two flat portions formed on two ends of the circular rod portion respectively, disposed on a top edge of the shadow mask frame, and located at two opposite sides of the shadow mask frame respectively;
a plurality of transverse spacer plates disposed on the circular rod portions of the longitudinal supporting bars, supported by the longitudinal supporting bars, intersecting the longitudinal supporting bars, and arranged at intervals; and
a plurality of shadow mask plates disposed on the transverse spacer plates, supported by the longitudinal supporting bars, and paralleling the transverse spacer plates, wherein each of the transverse spacer plates is located under a gap between adjacent two of the shadow mask plates, contacts the adjacent two of the shadow mask plates, and covers the gap;
wherein pairs of fixing notches are defined in the shadow mask frame, the pairs of the fixing notches correspond to the longitudinal supporting bars, the two fixing notches of each pair are defined in the top edge of the shadow mask frame, are located on the two opposite sides of the shadow mask frame respectively, and fix and receive the two flat portions of a corresponding one of the longitudinal supporting bars;
wherein a top edge of the circular rod portion of each of the longitudinal supporting bars is flush with the top edge of the shadow mask frame;
wherein a diameter of the circular rod portion of each of the longitudinal supporting bars is greater than a thickness of the flat portion;
wherein the diameter of the circular rod portion of each of the longitudinal supporting bars is less than a width of the flat portion;
wherein each of the flat portions of each of the longitudinal supporting bars comprises a truncated distal end.
Compared to the prior art, the fine shadow mask assembly for the AMOLED of the present invention has the following advantages.
1. Each of the longitudinal supporting bars provides excellent supporting capability through the circular rod portion with the greater diameter such that the longitudinal supporting bars can stably support the shadow mask plates without deformation. Therefore, flatness of the shadow mask plates on the shadow mask frame is maintained.
2. Each of the transverse spacer plates directly contacts corresponding adjacent two of the shadow mask plates, closes the gap between the adjacent two shadow mask plates, and effectively prevents organic material in a later vapor deposition process from inadvertently passing through the gap between the adjacent shadow mask plates and falling onto a glass substrate of the AMOLED display panel, which improves yield of the later process.
3. The transverse spacer plates are disposed on the longitudinal supporting bars and are supported by the longitudinal supporting bars without deformation.
4. Each of the shadow mask plates contacts the circular rod portions of the longitudinal supporting bars in lines instead of surface contact as in the prior art, and therefore effectively reduce friction between the shadow mask plates and the longitudinal supporting bars, which facilitates fine adjustment to tension of the longitudinal supporting bars, the transverse spacer plates and the shadow mask plates.
To make the above content of the present invention clearer and understandable, preferred embodiments accompanied with drawings are described in detail as follows.
With reference to
With reference to
With reference to
With reference to
In a preferred embodiment, each of the flat portions 23 of each of the longitudinal supporting bars 20 comprises two soldering sides 231 and a truncated distal end 233. The two soldering sides 231 can be attached with soldering material such as tin solder. The truncated distal end 233 can be flush with one side 11 of the shadow mask frame 10.
In a preferred embodiment, the diameter of the circular rod portion 21 of each of the longitudinal supporting bars 20 is 0.6 mm, the thickness of the flat portion 23 is 0.3 mm, and a depth of each of the fixing notches 110 is 0.45 mm.
The transverse spacer plates 30 are disposed on the circular rod portions 21 of the longitudinal supporting bars 20, are supported by the longitudinal supporting bars 20, intersect the longitudinal supporting bars 20, and are arranged at intervals\.
The shadow mask plates 40 are disposed on the transverse spacer plates 30, are indirectly supported by the longitudinal supporting bars 20, and parallel the transverse spacer plates 30. Each of the transverse spacer plates 30 is located under a gap 45 of adjacent two of the shadow mask plates 40, contact the adjacent two shadow mask plates 40, and covers the gap 45, as shown in
With reference to
The shadow mask frame providing step S01 comprises providing a shadow mask frame 10.
The longitudinal supporting bar disposing step S02 comprises disposing a plurality of longitudinal supporting bars 20 on the shadow mask frame 10. Each of the longitudinal supporting bars 20 comprises a circular rod portions 21 and two flat portions 23. The two flat portions 23 are formed on two ends of the circular rod portions 21 respectively and are disposed on a top edge of the shadow mask frame 10.
The longitudinal supporting bar tensioning step S03 comprises tensioning the longitudinal supporting bars 20.
The transverse spacer plates disposing step S04 comprises disposing a plurality of transverse spacer plates 30 on the circular rod portions 21 of the longitudinal supporting bars 20. The transverse spacer plates 30 intersect the longitudinal supporting bars 20.
The transverse spacer plate tensioning step S05 comprises tensioning the transverse spacer plates 30.
The shadow mask plate disposing step S06 comprises disposing a plurality of shadow mask plates 40 on the transverse spacer plates 30 such that each of the transverse spacer plates 30 is located under a gap 45 between adjacent two of the shadow mask plates 40, contacts the adjacent two shadow mask plates 40, and covers the gap 45.
The shadow mask plate tensioning step S07 comprises tensioning the shadow mask plates 40.
Compared to the prior art, the fine shadow mask assembly for the AMOLED of the present invention has the following advantages.
1. Each of the longitudinal supporting bars 20 provides excellent supporting capability through the circular rod portion 21 with the greater diameter such that the longitudinal supporting bars 20 can stably support the shadow mask plates 40 without deformation. Therefore, flatness of the shadow mask plates 40 on the shadow mask frame 10 is maintained.
2. Each of the transverse spacer plates 30 directly contacts corresponding adjacent two of the shadow mask plates 40, closes the gap 45 between the adjacent two shadow mask plates 40, and effectively prevents organic material in a later vapor deposition process from inadvertently passing through the gap 45 between the adjacent shadow mask plates 40 and falling onto a glass substrate of the AMOLED display panel, which improves yield of the later process.
3. The transverse spacer plates 30 are disposed on the longitudinal supporting bars 20, are supported by the longitudinal supporting bars 20 without deformation.
4. Each of the shadow mask plates 40 contacts circular rod portions 21 of the longitudinal supporting bars 20 in lines instead of surface contact as in the prior art, and therefore effectively reduce friction between the shadow mask plates 40 and the longitudinal supporting bars 20, which facilitates fine adjustment to tension of the longitudinal supporting bars 20, the transverse spacer plates 30 and the shadow mask plates 40.
5. In the above fine shadow mask assembly manufacturing method for the AMOLED, because the longitudinal supporting bars 20, the transverse spacer plates 30 and the shadow mask plates 40 are sequentially tensioned, it is ensured that the longitudinal supporting bars 20 can support the transverse spacer plates 30 and the shadow mask plates 40 to prevent the transverse spacer plates 30 and the shadow mask plates 40 from drooping and deforming.
Number | Date | Country | Kind |
---|---|---|---|
201810637584.1 | Jun 2018 | CN | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/CN2018/110126 | 10/12/2018 | WO | 00 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2019/242171 | 12/26/2019 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
6407489 | Lee | Jun 2002 | B1 |
6407490 | Shin | Jun 2002 | B1 |
20010018309 | Nishiki | Aug 2001 | A1 |
20010033130 | Ha | Oct 2001 | A1 |
20020135286 | Ha | Sep 2002 | A1 |
20030117058 | Reed | Jun 2003 | A1 |
20040028875 | Van Rijn | Feb 2004 | A1 |
20100192856 | Sung | Aug 2010 | A1 |
20110139069 | Ahn | Jun 2011 | A1 |
20130286151 | Wakabayashi | Oct 2013 | A1 |
Number | Date | Country |
---|---|---|
105839051 | Oct 2016 | CN |
Number | Date | Country | |
---|---|---|---|
20210226128 A1 | Jul 2021 | US |