Fluid ejection devices, such as printheads in inkjet printing systems, may use thermal resistors or piezoelectric material membranes as actuators within fluidic chambers to eject fluid drops (e.g., ink) from nozzles. In either case, fluid flows from a reservoir into the fluidic chambers through a fluid slot that extends through a substrate on which the fluidic chambers and actuators are generally formed. A size of the fluid slot influences a size of the substrate as well as a spacing between fluid slots (i.e., slot pitch).
In the following detailed description, reference is made to the accompanying drawings which form a part hereof, and in which is shown by way of illustration specific examples in which the disclosure may be practiced. In this regard, directional terminology, such as “top,” “bottom,” “front,” “back,” “leading,” “trailing,” etc., is used with reference to the orientation of the Figure(s) being described. Because components of examples of the present disclosure can be positioned in a number of different orientations, the directional terminology is used for purposes of illustration and is in no way limiting. It is to be understood that other examples may be utilized and structural or logical changes may be made without departing from the scope of the present disclosure. The following detailed description, therefore, is not to be taken in a limiting sense, and the scope of the present disclosure is defined by the appended claims.
In general, printhead features such as fluid drop ejection actuators (e.g., thermal resistors, piezoelectric membranes), fluidic firing chambers, and fluidic channels (e.g., fluid slots) that route fluid from fluid supply reservoirs to the firing chambers, are fabricated on or in a substrate using a mixture of integrated circuit and MEMS techniques. In his regard, the present disclosure provides methods of fabrication that result in a fluid slot with a narrow backside width, and result in a fluid slot with a tapered profile or shape at the front side of the substrate. As such, the methods of fabrication provided herein help to reduce fluid slot size such that die size can be reduced and die separation can be increased. As a printhead die may include multiple fluid slots, a reduction in fluid slot width for each of the multiple fluid slots may result in a combined reduction in die size by a corresponding multiple (for example, a reduction in slot width of an amount x for each of four fluid slots of a die may result in a combined reduction of die size in an amount of four times x (i.e., 4x)). Considering substrate cost, such reduction in die size may provided significant cost savings. In addition, by providing a tapered profile or shape of the fluid slot at the front side of the substrate, the methods of fabrication provided herein help to improve passive air management through the slot, as compared to a straight slot. Furthermore, by providing a fluid slot with a narrower throat (i.e., narrower width), the methods of fabrication provided herein help to improve thermal performance, such that a printhead incorporating such a slot may operate at a lower operating temperature. In addition, by providing a fluid slot with a narrower width, the methods of fabrication provided herein may result in reduced spacing between fluid slots (i.e., slot pitch).
In one example, as discussed below and illustrated herein, printhead 114 comprises a thermal inkjet (TIJ) printhead that ejects fluid drops from nozzle 116 by passing electrical current through a thermal resistor ejection element to generate heat and vaporize a small portion of the fluid within a firing chamber. Printhead 114, however, is not limited to being implemented as a TIJ printhead. For example, printhead 114 can be implemented as a piezoelectric inkjet (PIJ) printhead that uses a piezoelectric material ejection element to generate pressure pulses to force fluid drops out of nozzle 116. In either example, nozzles 116 are typically arranged in one or more columns or arrays along printhead 114 such that properly sequenced ejection of ink from the nozzles causes characters, symbols, and/or other graphics or images to be printed on print media 118 as printhead 114 and print media 118 are moved relative to each other.
Mounting assembly 106 positions printhead 114 relative to media transport assembly 110, and media transport assembly 110 positions print media 118 relative to printhead 114. Thus, a print zone 120 is defined adjacent to nozzles 116 in an area between printhead 114 and print media 118. In one example, print engine 102 is a scanning type print engine. As such, mounting assembly 106 includes a carriage for moving printhead 114 relative to media transport assembly 110 to scan print media 118. In another example, print engine 102 is a non-scanning type print engine. As such, mounting assembly 106 fixes printhead 114 at a prescribed position relative to media transport assembly 110 while media transport assembly 110 positions print media 118 relative to printhead 114.
Electronic controller 104 typically includes components of a standard computing system such as a processor, memory, firmware, and other printer electronics for communicating with and controlling supply device 108, printhead(s) 114, mounting assembly 106, and media transport assembly 110. Electronic controller 104 receives data 122 from a host system, such as a computer, and temporarily stores the data 122 in a memory. Data 122 represents, for example, a document and/or file to be printed. As such, data 122 forms a print job for inkjet printing system 100 that includes one or more print job commands and/or command parameters. Using data 122, electronic controller 104 controls printhead 114 to eject ink drops from nozzles 116 in a defined pattern that forms characters, symbols, and/or other graphics or images on print medium 118.
In one example, substrate 304 is formed of silicon and, in some implementations, may comprise a crystalline substrate such as doped or non-doped monocrystalline silicon or doped or non-doped polycrystalline silicon. Other examples of suitable substrates include gallium arsenide, gallium phosphide, indium phosphide, glass, silica, ceramics, or a semiconducting material. Substrate 304 may be between 100 and 2000 microns thick and, in one implementation, is approximately 675 microns thick. Substrate 304 has a first or front-side surface 306 and a second or back-side surface 308 opposite front-side surface 306. In one example, an adhesive layer 322 joins substrate 304 at back-side surface 308 to cartridge body 202. In addition, a thin-film structure 310, including one or more thin-film layers such as, for example, a field or thermal oxide layer, is formed on front-side surface 306.
In one example, a barrier layer 312 is formed over thin-film structure 310, and at least partially defines firing or fluid ejection chambers 314. Barrier layer 312 may be formed, for example, of a photo-imagable epoxy. Over barrier layer 312 is an orifice plate or nozzle plate 316 having nozzles 116 through which fluid is ejected. Orifice plate 316 may be formed, for example, of a photo-imagable epoxy or a nickel substrate. In some implementations, orifice plate 316 is the same material as barrier layer 312 and, in some implementations, orifice plate 316 and barrier layer 312 may be integral.
Within each fluid ejection chamber 314 and surrounded by barrier layer 312, is an independently controllable fluid ejection element 318. In the illustrated example, fluid ejection elements 318 comprise thermal firing resistors. When an electrical current is passed through a resistor in a respective fluid ejection chamber 314, a portion of the fluid is heated to its boiling point so that it expands to eject another portion of the fluid through nozzle 116. The ejected fluid is then replaced by additional fluid from a fluid-handling passageway 320 and corresponding fluid-feed or fluid-handling slot 302a, 302b, 302c. As noted above, in different implementations, fluid ejection elements can comprise piezoelectric material ejection elements (i.e., actuators).
In one example, substrate 460 is a silicon substrate and opening 450 is formed in substrate 460 as described below. Substrate 460 has a first side 462 and a second side 464. Second side 464 is opposite of first side 462 and, in one example, oriented substantially parallel with first side 462. Opening 450 communicates with first side 462 and second side 464 of substrate 460 so as to provide a channel or passage through substrate 460. While only one opening 450 is illustrated and described as being formed in substrate 460, it is understood that any number of openings 450 may be formed in substrate 460.
In one example, first side 462 forms a front side of substrate 460 and second side 464 forms a back side of substrate 460 such that fluid flows through opening 450 and, therefore, through substrate 460 from the back side to the front side. Accordingly, in one implementation, opening 450 provides a fluidic channel or fluid (or ink) feed slot for the communication of fluid (or ink) with fluid ejection elements 318 (
In one example, as illustrated in
Also, as illustrated in the example of
In one example, as illustrated in
As illustrated in the example of
In one example, as illustrated in
As illustrated in the example of
In one example, as illustrated in
In one implementation, first portion 452 of opening 450 is formed in substrate 460 by laser processing through sacrificial mask layer 474. Other techniques for forming first portion 452 of opening 450 include, for example, a silicon dry etch such as a plasma enhanced reactive ion etch (RIE) with alternating sulfur hexafluoride (SF6) etching and octafluorobutene (C4F8) deposition, sand drilling and mechanically contacting the substrate material. Mechanically contacting can include, for example, sawing with a diamond abrasive blade.
As illustrated in the example of
In one example, first portion 452 of opening 450 includes substantially parallel sidewalls from second side 464 to depth D. In another example, first portion 452 of opening 450 includes sidewalls at angles greater than ninety degrees (relative to second side 464) to the extent that width w of first portion 452 does not exceed width W (
Next, as illustrated in the example of
In one implementation, second portion 454 of opening 450 is formed in substrate 460 by a dry etch process, and is performed through first portion 452 of opening 450 to first side 462 of substrate 460. In one example, the dry etch process is a reactive ion etch (RIE) using a fluorine-based plasma etch such as, for example, sulfur hexafluoride.
As illustrated in the example of
In one example, third portion 456 of opening 450 is formed in substrate 460 using an anisotropic chemical etch process. More specifically, the chemical etch process is a wet etch process and, in one implementation, uses a wet anisotropic etchant such as tetra-methyl-ammonium hydroxide (TMAH), potassium hydroxide (KOH), or other alkaline etchant. Wet etching is achieved by immersing substrate 460 in an anisotropic etchant for a period of time sufficient to form opening 450. Etchants can include any anisotropic wet etchant that has selectivity to hard masks and exposed thin-film and other layers. In one implementation, a single instance of wet etching is used to remove the additional substrate material and form opening 450. In other implementations, the etching can include multiple instances of wet etching. In addition to forming third portion 456 of opening 450, the anisotropic wet etch process also removes sacrificial mask layer 474 (
With the anisotropic wet etch process, third portion 456 of opening 450 follows and is defined by crystalline planes of substrate 460 as a silicon substrate. More specifically, as illustrated in the example of
In one example, opening 450 is generally defined by sidewalls that are substantially symmetrical from one side to the other side. In one example, sidewalls of opening 450 are substantially parallel over at least a portion of opening 450 between second side 464 of substrate 460 and first side 462 of substrate 460, and converge toward and to first side 462. As such, a dimension (e.g., width) of opening 450 is substantially constant over at least a portion of opening 450 between second side 464 of substrate 460 and first side 462, and decreases toward first side 462. In one example, a length L of the converging sidewalls of upper portion 484, as measured in a direction substantially perpendicular to first side 462, is in a range of approximately five percent to approximately fifteen percent of thickness t of substrate 460.
In one example, substrate 560 is a silicon substrate and opening 550 is formed in substrate 560 as described below. Substrate 560 has a first side 562 and a second side 564. Second side 564 is opposite of first side 562 and, in one example, oriented substantially parallel with first side 562. Opening 550 communicates with first side 562 and second side 564 of substrate 560 so as to provide a channel or passage through substrate 560. While only one opening 550 is illustrated and described as being formed in substrate 560, it is understood that any number of openings 550 may be formed in substrate 560.
In one example, first side 562 forms a front side of substrate 560 and second side 564 forms a back side of substrate 560 such that fluid flows through opening 550 and, therefore, through substrate 560 from the back side to the front side. Accordingly, in one implementation, opening 550 provides a fluidic channel or fluid (or ink) feed slot for the communication of fluid (or ink) with fluid ejection elements 318 (
In one example, as illustrated in
Also, as illustrated in the example of
In one example, as illustrated in
In one example, as illustrated in
In one example, as first portion 552 of opening 550 is formed in substrate 560, backside layer or stack 570 is patterned such that select portions of backside layer or stack 570 are removed to expose areas of second side 564 of substrate 560. As such, backside layer or stack 570 defines where opening 550 is to be formed in substrate 560 at second side 564. A dimension of the exposed area of second side 564 of substrate 560 is represented by width W such that a width w of first portion 552 of opening 550 at second side 564 of substrate 560 is less than width W. As such, first portion 552 forms a subset of opening 550 of width w.
In one implementation, first portion 552 of opening 550, and the patterned and removed portions of backside layer or stack 570, are formed in substrate 560 by laser processing through backside layer or stack 570. In one example, the laser processing includes a first laser process of a first width w1 to a first depth d1 followed by a second laser process of a second width w2 for an additional, second depth d2, where first width w1 is greater than second width w2, and second depth d2 is less than first depth d1 and is to depth D of first portion 552. In one implementation, the first laser process includes a six-wide laser process, and the second laser process includes a four-wide laser process.
Other techniques for forming first portion 552 of opening 550 include, for example, a silicon dry etch such as a plasma enhanced reactive ion etch (RIE) with alternating sulfur hexafluoride (SF6) etching and octafluorobutene (C4F8) deposition, sand drilling and mechanically contacting the substrate material. Mechanically contacting can include, for example, sawing with a diamond abrasive blade.
As illustrated in the example of
In one example, first portion 552 of opening 550 includes substantially parallel sidewalls from second side 564 to depth D, including substantially parallel sidewalls of depth d1 and depth d2. In another example, first portion 552 of opening 550 includes sidewalls at angles greater than ninety degrees (relative to second side 564) to the extent that width w of first portion 552 does not exceed width W whereby a width of first portion 552 at depth D, including at depth d1 and depth d2, is less than a width of first portion 552 at second side 564.
Next, as illustrated in the example of
In one example, second portion 554 of opening 550 is formed in substrate 560 using an anisotropic chemical etch process. More specifically, the chemical etch process is a wet etch process and, in one implementation, uses a wet anisotropic etchant such as tetra-methyl-ammonium hydroxide (TMAH), potassium hydroxide (KOH), or other alkaline etchant. Wet etching is achieved by immersing substrate 560 in an anisotropic etchant for a period of time sufficient to form opening 550. Etchants can include any anisotropic wet etchant that has selectivity to hard masks and exposed thin-film and other layers. In one implementation, a single instance of wet etching is used to remove the additional substrate material and form opening 550. In other implementations, the etching can include multiple instances of wet etching.
With the anisotropic wet etch process, second portion 554 of opening 550 follows and is defined by crystalline planes of substrate 560 as a silicon substrate. More specifically, as illustrated in the example of
In one example, opening 550 is generally defined by sidewalls that are substantially symmetrical from one side to the other side. In one example, sidewalls of opening 550 are substantially parallel over at least a portion of opening 550 between second side 564 of substrate 560 and first side 562 of substrate 560, and converge toward and to first side 562. As such, a dimension (e.g., width) of opening 550 is substantially constant over at least a portion of opening 550 between second side 564 of substrate 560 and first side 562, and decreases toward first side 562. In one example, a length L of the converging sidewalls of upper portion 584, as measured in a direction substantially perpendicular to first side 562, is in a range of approximately five percent to approximately fifteen percent of thickness t of substrate 560.
While the above description refers to the inclusion of substrate 460 or 560 having opening 450 or 550 formed therein in an inkjet printhead assembly, it is understood that substrate 460 or 560 having opening 450 or 550 formed therein may be incorporated into other fluid ejection systems including non-printing applications or systems as well as other applications having fluidic channels through a substrate, such as medical devices or other micro electro-mechanical systems (MEMS devices). Accordingly, the methods, structures, and systems described herein are not limited to printheads, and are applicable to any slotted substrates. In addition, while the above description refers to routing fluid or ink through opening 450 or 550 of substrate 460 or 560, it is understood that any flowable material, including a liquid such as water, ink, blood, or photoresist, or flowable particles of a solid such as talcum powder or a powdered drug, or air may be fed or routed through opening 450 or 550 of substrate 460 or 560.
Although specific examples have been illustrated and described herein, it will be appreciated by those of ordinary skill in the art that a variety of alternate and/or equivalent implementations may be substituted for the specific examples shown and described without departing from the scope of the present disclosure. This application is intended to cover any adaptations or variations of the specific examples discussed herein. Therefore, it is intended that this disclosure be limited only by the claims and the equivalents thereof.
Number | Date | Country | |
---|---|---|---|
Parent | 14766925 | Aug 2015 | US |
Child | 15947197 | US |