Claims
- 1. A method of forming an electric cell comprising the steps of:
- (b) providing an electrode material wherein the electrode material is porous carbon black;
- (c) inserting the electrode material into a plasma etcher;
- (d) filling the plasma etcher with a reactive gas mixture;
- (e) exposing the electrode material to a gas plasma for from 0.5 seconds to 5 minutes; and
- (f) installing the electrode material in an electric cell having an electrolyte of the general formula R.sub.p O.sub.r X.sub.t, where R is selected from the group consisting of sulfur, carbon and silicon; O is oxygen; and X is selected from the group consisting of fluorine, chlorine, bromine, and iodine; and the subscripts p, r, and t are greater than 0.
- 2. The process of claim 1 wherein the electrode material is formed into a solid electrode.
- 3. A method of forming an electric cell comprising the steps of:
- (a) providing an electrode material wherein the electrode material is manganese dioxide;
- (b) inserting the electrode material into a plasma etcher;
- (c) filling the plasma etcher with a reactive gas mixture;
- (d) exposing the electrode material to a gas plasma for from 0.5 seconds to 5 minutes; and
- (e) installing the electrode material in an electric cell having an electrolyte of the general formula R.sub.p O.sub.r X.sub.t, where R is selected from the group consisting of sulfur, carbon, and silicon; O is oxygen; and X is selected from the group consisting of fluorine, chlorine, bromine, and iodine; and the subscripts p, r, and t are greater than 0.
- 4. The process of claim 1 wherein the reactive gas mixture is selected from the group consisting of oxygen, ammonia, and a mixture of carbon tetrafluoride and oxygen.
- 5. The process of claim 1 wherein the treatment of electrode material is conducted under a vacuum from 20 to 250 millitorr.
- 6. The process of claim 4 wherein the mixture of carbon tetrafluoride and oxygen contains from 90 to 99 percent by volume of carbon tetrafluoride.
- 7. The process of claim 1 wherein the electrolyte is selected from the group consisting of SOCl.sub.2, SO.sub.2 Cl.sub.2, SOClBr, SO.sub.2 ClBr, SOBr.sub.2, and COCl.sub.2.
- 8. An electric cell made by the method of claim 1.
- 9. The cell of claim 8 wherein the electrode material is formed into a solid electrode.
- 10. An electric cell made by the method of claim 3.
- 11. The cell of claim 8 wherein the reactive gas mixture is selected from the group consisting of oxygen, ammonia, and a mixture of carbon tetrafluoride and oxygen.
- 12. The cell of claim 8 wherein the treatment of electrode material is conducted under a vacuum from 20 to 250 millitorr.
- 13. The cell of claim 11 wherein the mixture of carbon tetrafluoride and oxygen contains from 90 to 99 percent by volume of carbon tetrafluoride.
- 14. The cell of claim 8 wherein the electrolyte is selected from the group consisting of SOCl.sub.2, SO.sub.2 Cl.sub.2, SOClBr, SO.sub.2 ClBr, SOBr.sub.2, and COCl.sub.2.
GOVERNMENT INTEREST
The invention described herein may be manufactured, used, and licensed by or for the Government for governmental purposes without the payment to us of any royalty thereon.