Virtual Frisch-grid detectors represent a class of single-carrier devices for which fast-moving electrons are used to measure energies deposited by X-rays, gamma-rays, ionizing particles, and the like. A main drawback of single carrier devices is that the output signals are influenced by the stationary holes whose effects depend on the locations of interaction points inside the device. Such behavior of the output signals, caused by uncollected holes, is commonly called the “induction effect.” This effect inhibits spectral resolution of single-carrier detectors unless special measures are implemented to neutralize the holes. Two techniques directed to minimizing the induction effect are: (1) subtracting the fraction of the charge signal contributed by the stationary holes and (2) electrostatic shielding of the stationary holes.
In the first technique, the induced charge contributed by the holes is measured and subtracted from the total output signal. The holes-induced signal can be measured with one or several electrodes located adjacent to the collecting electrode. The electrodes can be composed of pixels or strips and, depending on the locations of interaction points, the same electrode can be used for measuring collected or induced-only charges. Coplanar-grid devices proposed for Cadmium Zinc Telluride (CdZnTe or CZT) and fluid Xenon (Xe) detectors are special cases for implementing this technique.
For the second technique, there are two types of devices that employ the electrostatic shielding: Frisch-grid and virtual Frisch-grid detectors. In a classic Frisch-grid ionization chamber, a metal grid (or mesh) is used for electrostatic shielding of the collecting electrode (or several collecting electrodes) from the positive ions. In a virtual Frisch-ring detector, the shielding electrode (or several electrodes) is placed around the sides of the device's sensitive volume but they produce essentially the same shielding effect as if a real Frisch grid were placed inside the detector.
In the past, several designs of virtual Frisch-grid detectors were proposed for CdZnTe semiconductor: CAPture™, hemispherical, Frisch-ring, and pixel detectors. (CAPture™ is a trademark of eV Products, Inc. of Saxonburg, Pa.). CAPture™-type and hemispherical type detectors are generally produced by extending the cathode electrode up the sides of the detector crystal body. In both devices, the extended electrodes are in physical contact with the semiconductor surfaces. As a result, a wide area of the bare detector crystal body surface surrounding the anode is required to keep the surface leakage current below an acceptable level. While these convention devices typically achieve acceptable results for low energy gamma-rays, which normally interact close to the cathode, these conventional devices typically do not perform as well for higher energy gamma-rays that interact closer to the anode. Since the area near the anode is not properly shielded, convention Frisch-grid detectors usually exhibit low energy tails for peaks in the pulse height spectra.
In conventional Frisch-ring detectors, the cathode is also extended along the longitudinal surface of the detector, but the extended portion of the cathode is physically separated from the longitudinal surface by a thin layer of insulating material. The non -contacting electrode, also known as the non-contacting Frisch ring, is the main feature that makes Frisch-ring detectors different from CAPture™ and hemispherical-type devices. The non-contacting electrode is placed along the longitudinal surface of the crystal and is physically connected to the cathode. A common high-voltage bias (with respect to the anode) is applied to the cathode and the non-contacting electrode. The output signal is read out from the anode. Thus, a gap (typically 2-3 mm) of insulating material is generally left between the Frisch-ring and the anode's contact to prevent high leakage current or even possible discharge in the area between these two electrodes. As a result, an electrostatically unshielded area of the surface exists near the anode, which results in a low energy tailing effect discussed above.
Conventional virtual Frisch-grid detectors generally have three common effects that result in degradation of their performance. The first effect that degrades their performance is the presence of an unshielded area near the anode. The second effect that degrades their performance is that the electric field inside the detector (drift field) does not generally direct electrons, liberated by the incident photons or particles, toward the anode (defocusing field). The third effect that degrades their performance is the two-terminal nature of devices in which the cathode signal cannot provide the particle's interaction depth information to correct the electron losses due to trapping.
The preferred embodiments of the present invention relate to high energy detectors, such as X-ray, gamma ray, ionizing particle detectors, and the like, and more particularly to virtual Frisch-grid radiation detectors operating as single-carrier-transport devices that can be operated at room temperature. The high-energy detector can include a first electrical conductor, a second electrical conductor, a third electrical conductor, an insulator, and a detector crystal with a longitudinally extending body.
The detector crystal body can have a rectangular cross-section, circular cross-section, or an elliptical cross-section. For the embodiment where the detector crystal body has a rectangular cross-section the ratio of a length of the longest side of the cross-section to the longitudinal length of the detector crystal body can be less than one. The detector crystal body is in electrical contact with, and bounded by, the first electrical conductor formed at a first end, which represents a cathode, and the second electrical conductor formed at a second end, which represents an anode. A different electrical potential can be applied to the first and second electrical conductors to create an electric field within the body that is sufficient to direct liberated electrons towards the second electrical conductor. The first electrical conductor can extend along and be in direct contact with a first portion of the longitudinal surface of the detector crystal body
At least a portion of the longitudinal surface is substantially surrounded by the third electrical conductor, which extends to the second end. The third electrical conductor is electrically isolated from the body and the first electrical conductor by the insulator which is disposed about the longitudinal surface of the detector crystal body. The detector crystal body is electrically shielded by the first, second, and third electrical conductors so that the body is substantially shielded from electrostatic interference.
The third electrical conductor comprises at least one of copper and aluminum and can have an electrical potential that is substantially equal to that of the second electrical conductor. The insulator can extend from the second end to the first end and beyond and can be formed from at least one of polyester, polyethylene, polytetraflouroethylene, and a polyimide. In one embodiment, the insulator is composed of a tube of heat-shrinkable polymer within which the detector crystal body is positioned and to which heat sufficient to shrink said tube is applied so that the tube contracts onto the detector.
For the embodiment where the first electrical conductor extends from the first end of the body along a first portion of the longitudinal surface of the body, the third electrical conductor surrounds a second portion of the longitudinal surface of the body, where the first and second portion can, but do not necessarily overlap. The insulator can surround the longitudinal surface of the detector crystal body so that an inner surface of the first electrical conductor is in direct electrical contact with the longitudinal surface of said body and an outer surface of the first electrical conductor is in contact with the insulator.
In one embodiment high-energy can be detected by applying a first electrical potential at an anode disposed on a first end of a detector crystal body to a first potential, applying a second electrical potential at a cathode disposed on a second end of said detector crystal body, and applying a third electrical potential to an electrically conducting shield, where the third electrical potential is substantially equal to the second electrical potential. An output is read at the anode that corresponds to a number of liberated electrons collected by the anode and an output is read at the cathode that corresponds to a number of trapped electrons. The number of originally liberated electrons is determined based on the number of collected electrons and the number of trapped electrons. For example, the number of originally liberated electrons can be determined by summing the number of collected electrons with the product resulting from multiplying the number of trapped electrons by a correction factor.
The preferred embodiments of the inductive sealing unit, as well as other objects, features and advantages of the present invention will be apparent from the following detailed description, which is to be read in conjunction with the accompanying drawings wherein like reference numerals in the various figures are utilized to designate like components. The scope of the invention will be pointed out in the claims.
The preferred embodiments of the present invention are directed to a high-energy detector that is substantially shielded from electrostatic interference. The high-energy detector can include a detector crystal that is preferably formed using a semiconductor material, such as Cadmium Zinc Telluride (CdZnTe or CZT), Cadmium Telluride (CdTe), Mercury Iodide (HgI2), and the like, which is substantially shielded from electrostatic interference by electrical conductors that can include a cathode, an anode, and a conducting shield where the conducting shield is electrically decoupled from the cathode.
In one application, ionizing radiation and/or high-energy particles impinge upon the detector crystal to create electron-hole pairs. As a result of an electric field created within the detector crystal by electrical potentials applied to the cathode and anode, liberated electrons of the electron-hole pairs are directed towards the anode. In the case of an ideal detector, all liberated electrons drift towards the anode where they are collected and the holes drift towards the cathode where they are collected. In an actual implementation, however, liberated electrons can be trapped by holes or surface states within the detector crystal. Liberated electrons collected by the anode provide information about the high-energy photons and/or particles that impinge on the detector crystal. In the preferred embodiment of the present invention, the holes collected by the cathode can also be used to correct for liberated electrons that are not collected by the anode, for example, because they become trapped or drift to the longitudinal surface of the detector crystal.
The high-energy detectors of the present invention can be configured to generate an electric field within the detectors that directs electrons liberated by photons and/or particles that impinge the detector crystal towards an anode located at one end of the detectors. To achieve this, the high-energy detectors of the present invention can include cathodes that are located at an end of the detectors opposite that of the anode and that can extend along a portion of, and in electrical contact with, the longitudinal surface of the detector crystal body. This configuration can prevent the creation of an undesirable defocusing electric field within the detector, which is generally inefficient in directing liberated electrons towards the anode.
The conducting shield of the preferred embodiments surrounds at least a portion of the longitudinal surface of the detector crystal and is decoupled from the cathode. The conducting shield is preferably held at an electrical potential that is substantially equal to the electrical potential of the anode. Using this configuration, an interaction depth of photons and/or particles that are impinge upon the detector crystal can be determined and electron losses due to, for example, trapping can be corrected.
The preferred embodiments of the present invention are configured to electrically shield the detector crystal to substantially reduce or eliminate electrostatically unshielded area, making the detector resilient to electrostatic interference. The high-energy detectors described herein can be configured to focus an electric field within the detector so that liberated electrons flow towards the anode and can be configured to enable determining interaction depth information of photons and/or particles that impinge upon the detector to correct the electron losses due to trapping. As a result of the above, the preferred embodiments of the present invention can detect photons and/or particles efficiently and with high resolution. For example, the preferred embodiments of the present invention can have an energy resolution of better than 0.7% at 662 keV.
The cathode 330 can be disposed at, and in direct electrical contact with, a first end 332 of the detector crystal body 310 and the anode 350 can be disposed at, and in direct electrical contact with, a second end 352 of the detector crystal body 310. In one application, a negative voltage bias can be applied to the cathode 330 and the anode 350 and conducting shield 390 can be held at 0 volts (V). For example, an electrical potential magnitude of about 1000-3000 V can be used for the cathode 330 and a ground potential (e.g., about 0 V) can be used for the anode 350. The cathode 330 and anode 350 preferably cover the surface of the first end 332 and second end 352 of the detector crystal body 310, respectfully. In addition, the cathode 330 preferably has an extended portion 334 that extends from the first end 332 of the detector crystal body 310 along a first portion 336 of the longitudinal surface 312 of the detector crystal body 310 to at least partially and preferably substantially surround the first portion 336 of the longitudinal surface 312.
In one example, the detector 300 can have a longitudinal length L of 10-mm or longer and the cathode 330 can extend 2-3 mm along the longitudinal surface 312 of the detector crystal body 310, about 20%-30% of the detector crystal length. By extending the cathode 330 along a first portion 336 of the longitudinal surface 312 of the detector crystal body 310, a higher electric field gradient can be created on the surface of the detector crystal body 310 than along the detector crystal body's central axis 314, ensuring that a focusing drift electric field is created within the detector crystal body 310.
The cathode 330 and anode 350 can be disposed on the first end 332 and the second end 352, respectively, using deposition techniques known to those skilled in the art, such as physical vapor deposition or chemical vapor deposition. In a preferred embodiment, the cathode 330 and the anode 350 are disposed on the first end 332 and the second end 352 using a physical vapor deposition technique commonly referred to as sputter deposition. The extended portion 334 of the cathode 330 can be formed by deepening the first end 332 of the detector crystal in a solution, such as a gold chloride solution. The cathode 330 and anode 350 can be formed using an electrical conductor, such as a metal including, but not limited to gold, silver, copper, aluminum, or the like.
The insulator 370 surrounds the longitudinal surface 312 of detector crystal body 310 and preferably extends from the first end 332 of the detector crystal body 310 to the second end 352 of the detector crystal body. Where the cathode 330 extends along the first portion 336 of the longitudinal surface 312 of the detector crystal body 310, the insulator 370 surrounds the cathode 330 in this portion 336 so that the insulator 370 is separated from the longitudinal surface 312 of the detector crystal body 310 by the cathode 330. The insulator 370 can be formed using an electrically insulating material that substantially impedes the electric current flow between electrical conductors separated by the insulator 370. The thickness T of the insulator 370 is minimized to ensure acceptable electrostatic shielding of the detector crystal body 310 by the conducting shield 390 and is preferably less than about 100 um thick. The insulator 370 can be formed by, for example, at least one of polyester, polyethylene, polytetrafluoroethylene, a polyimide, or the like, and can be formed by dipping, wrapping, and/or depositing an insulating material. For example, the detector 300 can be dipped in a polymer solution and/or wrapped in a polytetrafluoroethylene or a polyimide tape. Alternatively, or in addition, the insulator 370 can be deposited on the detector using deposition techniques known to those skilled in the art, such as sputtering. In a preferred embodiment, the detector 300 is positioned within a tube of a heat-shrinkable insulating material, such as polyester, and the tube is heated until the tube contracts around the detector 300, after which excess the insulating material may be trimmed.
As used herein the “conducting shield 390” refers to a non-contacting ring, or Frisch ring, around, and electrically insulated from, the detector crystal body 310. The “rings” need not be circular in cross section, and may conform to the cross section of the detector crystal body 310. The conducting shield 390 can be formed from a continuous conductive material or multiple discrete sections of one or more conductive materials so that the conducting shield 390 surrounds at least a portion of the longitudinal surface of the detector 300. The conducting shield 390 is preferably formed from aluminum. However, those skilled in the art will recognize that other electrically conductive materials, such as gold, silver, copper, or the like, can be used to for the conducting shield 390. In a preferred embodiment, the conducting shield 390 surrounds a second portion 392 of the longitudinal surface 312 of the detector crystal body 310 that extends from the second end 352 of the detector crystal body 310 to the first portion 336 of the longitudinal surface 312 of the detector crystal body 310 so that there is no space between the conducting shield 390 and the anode 350 along the longitudinal surface. In some embodiments, the conducting shield 390 can extend into the first portion 336 and/or can extend from the second end 352 to the first end 332 of the detector crystal body 310. The conducting shield 390 is electrically isolated from the detector crystal body 310 and the cathode 330 by the insulator 370 and is preferably at a electrical potential that is substantially equal to the electrical potential of the anode 350. In this manner, the conducting shield 390 and the cathode 330 are electrically decoupled and a high differential bias, for example in excess 3000 V between the cathode 330 and the conducting shield 390, can be achieved.
The conducting shield 390 can be wrapped around the longitudinal surface 312 of detector crystal body 310 or may be physically deposited thereon by, for example, physical or chemical vapor deposition. Thus, the inner surface 338 of the extended portion 334 of the cathode 330 is in contact with the detector crystal body 310, while the outer surface 340 of the extended portion 334 of the cathode 330 is covered by the insulator 370. Similarly, the portion of the detector crystal body 310 not in direct contact with the cathode 330, i.e., not covered by the extended portion 334 of the cathode 330, is covered by the insulator 370 and electrically shielded by the conducting shield 390. There need be no longitudinal gap between the conducting shield 390 and the anode 350, both of which can be kept at substantially the same electrical potential. Electrical contact can be made on cathode 330 and the anode 350 at the first end 332 and second end 352, respectively, which preferably remain bare of insulator 370, so that output signals can be read.
In the preferred embodiment, the conducting shield 390 forms a non-contacting Frisch ring that covers the longitudinal surface 312 which is not covered by the extended portion 334 of the cathode 330. Acting together, the extended portion 334 of the cathode 330 and the decoupled conducting shield 390 substantially shield the longitudinal surface 312 of the detector crystal from electrostatic interference. Since the conducting shield 390 is at an electrical potential that is substantially equal to the electrical potential of the anode 350, the conducting shield 390 can be extended up to the anode 350 to substantially reduce or eliminate any electrically unshielded area around the anode 350. In this manner, the detector crystal body 310 is electrically shielded by the cathode 330, anode 350, and conducting shield 390 to substantially reduce or eliminate electrically unshielded area of the detector crystal body 310. As a result of the configurations described herein, the detector 300 is resilient to electrostatic interference and can have an energy resolution of better than 0.7% at 662 keV.
The electric field distribution inside the detector 300 is determined by the boundary conditions (i.e. potential distribution on the longitudinal surface 312), which in turn is determined by the surface leakage current. Depending on the surface potential distributions, there can be three outcomes for the electric field distribution inside the device based on predictions from simulations. These electric field distributions are illustrated in
A focusing drift-field as shown in
The insulator 370′ surrounds the longitudinal surface 312′ of detector crystal body 310′ and preferably extends from the second end 352′ of the detector crystal body 310′ to beyond the first end 332′ of the detector crystal body 310′. In one embodiment, the insulator 370′ extends about 2-3 mm beyond the first end 332′ of the detector crystal body 310′.
The conducting shield 390′ surrounds the longitudinal surface 312′ of the detector crystal body 310′ and extends from the second end 352′ of the detector crystal body 310′ to the first end 332′ of the detector crystal body 310′ of the detector crystal body 310′. The conducting shield 390 is electrically isolated from the detector crystal body 310 and the cathode 330′ by the insulator 370′. Extending the insulator beyond the first end 332′ of the detector crystal body ensures that leakage current and discharge paths between the cathode and the conducting shield are minimized to an acceptable level and are preferably eliminated. In this manner, the conducting shield 390′ and the cathode 330′ are electrically decoupled and a high differential bias, for example in excess 3000 V between the cathode 330′ and the conducting shield 390′ can be achieved.
The high-energy gamma-rays 700 can impinge upon the detector crystal body 310 from any direction, however, it is preferably for the gamma-rays 700 to impinge on the detector crystal body 310 through the first end 332.
One or more electron-hole pairs 704 are created at or near the interaction depth 702. As a result of the electric field generated within the detector 300, liberated electrons 706 of the one or more electron-hole pairs 704 drift towards the anode 350 and holes 708 of the one or more electron-hole pairs 704 drift towards the cathode 330. The anode 350 collects the liberated electrons 706 and an anode signal 710 can be obtained from the anode 350 that represents a number of liberated electrons 706 collected. Some of the liberated electrons 706 can become trapped before reaching the anode 350, and therefore, do not contribute to the anode signal 710. The cathode 330 collects the holes 708 and a cathode signal 712 can be obtained from the cathode 330 that represents a number of holes 708 collected.
Along with the cathode 330 and the anode 350, the conducting shield 390 electrically shields the detector crystal body 310 from electrostatic interference. Applying an electrical potential to the conducting shield 390 that is substantially equal to that electrical potential of the anode 350 allows the conducting shield 390 to extend to the second end 352 of the detector 300 without generating a substantial amount of leakage current between the conducting shield 390 and the anode 350. A large differential potential (e.g., in excess of 3,000 V) between the cathode 330 and the conducting shield 390 can be achieved because the conducting shield 390 is electrically insulated from the cathode 330. Also, because the cathode 330 is electrically decoupled from the conducting shield 390, the cathode 330 can be used for sensing the depth of interaction by reading the cathode signals 712 from therefrom. This allows the preferred embodiments of the present invention to implement a charge-loss correction technique that can improve the spectral response as compared to conventional high-energy detectors. The correction of charge loss can be particularly advantageous for detectors having a long longitudinal length (e.g., >10 mm) where electron trapping can be more significant.
The cathode signal 712 provides information pertaining to a number of liberated electrons that have been trapped based on the number of holes collected. By monitoring the number of liberated electrons with the anode 350 and the number of trapped electrons with the cathode 330, it is possible to apply a correction factor that allows for reconstruction of the number of liberated electrons originally created by incident high-energy particles or radiation (e.g., gamma-rays).
In some embodiments, a rise-time or bi-parametric correction technique can be used. To estimate the fraction of particles or photons absorbed inside a drift region of the detector 300, the attenuation of gamma-rays inside the detector 300 is considered.
Acorrected=Aanode+K(Acathode), (1)
where K is the slope of the correlation curve (e.g., slope 906). Moreover, the ratio between the cathode and anode signals, Acathode/Aanode, can be used to reject the events interacting close to the anode. Such events, represented by the dots located close to the y-axis 904, degrade the spectral response of virtual Frisch-grid detectors.
In some embodiments, a signal from the conducting shield 390 can be substituted for the cathode signal. For embodiments that substitute the signal Ashield from the conducting shield for the cathode signal, the cathode signal (Acathode) in equation (1) can be replaced by the right-hand side of the following equation:
Acathode=1−Aanode+Ashield. (2)
As an example of the correction technique,
In some embodiments, the detectors disclosed herein can be used to form an array 1100 (or matrix) of detectors as shown in
The preferred embodiments can be used in a fixed and/or portable application where the detection of high-energy particles is desired and can operate at room temperature. In one example, the preferred embodiments of the detectors described herein can be used in a laboratory where samples may be place in proximity to the detectors and for which the detectors can determine the composition of the samples based on the high-energy radiation or particles emitted from the samples. In another example, the high-energy detectors described herein can be used in a portable field application where the detectors can be used to determine the composition of materials associated with, for example, a dirty bomb. As a result of the preferred embodiments of the present invention, operators of the high-energy detectors described herein can locate and identify radioactive material with more resolution and more accurately than convention high-energy detectors.
While the foregoing description has been made with reference to individual embodiments of the invention, it should be understood that those skilled in the art, making use of the teaching herein, may propose various changes and modifications without departing from the invention in its broader aspects. For example, although the detectors have been described as having an aspect ratio less than one, it is possible to use detector crystals with aspect ratios equal to or greater than one. Similarly the detectors described herein may be of any practical length rather than be limited to 10 mm. The foregoing description being illustrative, the invention is limited only by the claims appended hereto.
This application claims priority to U.S. Provisional Application No. 60/909,023 filed on Mar. 30, 2007, which is incorporated by reference herein in its entirety for all purposes.
This invention was made with Government support under contract number DEACO2-98CH10886, awarded by the U.S. Department of Energy. The Government has certain rights in the invention.
Number | Name | Date | Kind |
---|---|---|---|
5530249 | Luke | Jun 1996 | A |
6175120 | McGregor et al. | Jan 2001 | B1 |
6528797 | Benke et al. | Mar 2003 | B1 |
6781132 | McGregor | Aug 2004 | B2 |
Number | Date | Country |
---|---|---|
1264723 | Sep 1990 | SU |
Number | Date | Country | |
---|---|---|---|
20090026371 A1 | Jan 2009 | US |
Number | Date | Country | |
---|---|---|---|
60909023 | Mar 2007 | US |