This application claims priority from German patent application 10 2015 105 591.0, filed on Apr. 13, 2015. The entire content of that priority application is fully incorporated by reference herewith.
The present disclosure relates to a method for manufacturing a magnetic coil for a magnetic actuator, particularly for an injector. The disclosure further relates to a magnetic coil for a magnetic actuator and to an injector, particularly a fuel injector nozzle for a combustion engine, comprising such a magnetic actuator.
A common fuel injector nozzle is for instance known from EP 0 132 623 A2. The injector nozzle is provided with a magnetic actuator comprising an induction coil which is encapsulated and arranged in a fashion fixed to a housing.
Injectors for the fuel supply for combustion engines are generally known. Injectors of that kind are also referred to as injector nozzles. Modern injectors are provided with mechatronical actors, for instance with magnetic actuators, so as to control the opening and closing of the nozzles in a high-precision fashion. Modern injection systems for diesel engines are configured for maximum injection pressures of several hundred bars up to more than 1000 bar or even up to 2500 bar.
Injectors comprising so-called piezo-actuators are known. Nevertheless, also injectors comprising magnetic actuators are widely used. Injectors of that kind are commonly provided with a magnetic coil which cooperates with a movable armature for controlling the injector.
Actuators for injector nozzles must be manufactured in a high-precision fashion so as to be able to provide a respectively desired injection volume in a repeatedly accurate manner. Accordingly, there are frequently very tight tolerance specifications for the production. Further, it must be noted that the utilized components of the injector have to be considerably fuel-resistant or propellant-resistant so as to be resistant to the fuel which flows through the injector. The fuel may for instance involve diesel fuel, gasoline fuel, ethanol, light oil, heavy oil, kerosene or mixtures thereof.
The frequency at which the actuators of the injectors are controlled typically corresponds to the speed of rotation of the combustion engine. However, there are also injectors known that enable a plurality of injections event in a single combustion cycle. This may involve a further increased load to the injector and to the actuator thereof. Further, injectors are regularly fixedly attached to a cylinder head or a similar housing component of the combustion engine. This involves that the injector and the components provided therein are exposed to heavy vibration exposures, temperature variations and similar environmental impacts. Accordingly, there is a general need to design injectors in a robust fashion so as to ensure a specified minimum lifespan (for instance defined by operating cycles and such like).
For injectors that utilize magnetic actuators, it is a common measure to at least sectionally overmold and/or pot a coil winding of the magnetic coil of the actuator. In this way, the sensitive coil winding may be protected against environmental influences. Generally, such a magnetic coil comprises a coil body made from plastic material which supports a copper winding. For instance, the coil carrier that is provided with the coil winding is arranged in a magnet pot which defines a yoke of the magnetic actuator. By sealing, potting or overmolding the coil carrier that is received at or in the magnet pot, the coil winding is at least sectionally overmolded and/or potted with a (temporarily) fluid filler material.
The armature of such a magnetic actuator which cooperates with the magnet pot and the coil winding is frequently arranged as a plate armature and/or in a similar fashion. A lifting distance of the armature is frequently in a range of a few hundredths of a millimeter up to about 0.1 mm. As a result, even deviations in the range of a few micrometers at the seating surface and/or the abutment surface of the armature have a great influence on the function of the injector. A design goal may therefore involve to avoid, as much as possible, deviations of the armature stroke that is defined by the design.
It has been observed that the required potting and/or the required overmolding of the coil winding may in this respect have a negative impact. Generally, the overmolding and/or potting of the coil winding is performed in connection with the magnet pot, that is, in a state when the coil carrier that is provided with the coil winding is already arranged at the magnet pot in the desired final position. This involves that a molding form and/or potting form for such a procedure has to cooperate with the magnet pot in a high-precision fashion so as to ensure a sufficient sealing. If this is not the case, excess molding material (flash material) may be formed which involves events wherein the filler material (molding compound or potting compound) enters regions which actually shall not be entered for design and/or functional reasons. Even though there exist established solutions for avoiding such excess molding material, these solutions always involve increased production efforts. For instance, the tool which is used for overmolding or potting may be manufactured at an increased accuracy, and the magnet pot which cooperates with the tool may be also provided with an increased precision in a portion thereof that is arranged for contacting such a tool. However, this involves an increased production effort and also an increased wear on the side of the tool.
By contrast, in cases where no complete sealing of the magnet pot by the injection molding or potting tool may be ensured, excess molding material (flash material) may be present. Hence, in these cases, an increased scrap/waste or functional deficiencies have to be expected. Excess molding material may be generally referred to as residual flash.
In view of this, it is a first object of the present disclosure to provide a method for manufacturing a magnetic coil for a magnetic actuator which results in an improved quality of the potting and/or molding.
It is a further object to provide a method for manufacturing a magnetic coil for a magnetic actuator which involves an improved reproducibility and process reliability.
It is a further object to provide a method for manufacturing a magnetic coil for a magnetic actuator which prevents excess flash molding material to a great extent or even entirely.
More particularly, it is a further object to provide a method for manufacturing a magnetic coil for a magnetic actuator, wherein residual flash of the filler material at functional surfaces, particularly at contact surfaces or seating surfaces for the armature may be avoided to a considerable extent.
It is a further object to provide a method for manufacturing a magnetic coil for a magnetic actuator that is arranged to utilize robust tools/molds for the potting or overmolding which may achieve a great service life and/or lifespan.
It is a further object to provide a method for manufacturing a magnetic coil for a magnetic actuator that enables a reduction of efforts for quality management and a reduction of scrap production.
It is a further object to provide a method for manufacturing a magnetic coil for a magnetic actuator that enables the production of injectors which provide an increased operation performance and which are arranged to be controlled in a highly-accurate fashion.
It is a further object to present exemplary arrangements of magnetic coils and of injectors that are provided with respective magnetic coils that may profit from exemplary embodiments and aspects of the manufacturing method.
In regard of the manufacturing method, these and other objects of the present disclosure are achieved by a method of manufacturing a magnetic coil for a magnetic actuator, the method comprising the following steps:
In accordance with a further manufacturing related aspect, these and other objects of the present disclosure are achieved by a method for manufacturing a magnetic coil for a magnetic actuator, particularly for an injector, the method comprising the following steps:
Exemplary aspects of the disclosure are based on the insight that the step of overmolding or potting may be combined with a punching procedure by means of which a highly-accurate sealing is enabled. After the punching, the flange contour exactly corresponds to the surrounding inner contour of the die. This is enabled without the necessity to satisfy excessively accurate manufacturing tolerances. Rather, the collar of the coil carrier may comprise an “excess extension” before the punching operation. After the punching, the resulting flange contour is adapted to the inner contour of the die in a highly-accurate fashion.
Hence, the collar of the coil carrier not only serves as a boundary for the coil winding received at the coil carrier. Further, the collar and/or the flange contour which is formed at the collar after the punching forms a tight sealing barrier for the filler material. Hence, the sealing for the overmolding or potting no longer has to be primarily provided by the corresponding molding tool which abuts the coil carrier at this side. Rather, now the flange contour serves as a “sealing element”.
Needless to say, such an arrangement is primarily suited for manufacturing procedures wherein an overmolding with the filler material is performed at a relatively high pressure. In other words, pressure values may be present which generally occur in injection molding procedures for thermoplastic materials. Nevertheless, in the alternative, also a potting procedure is known, i.e. a filling with a fluid potting compound which is not exposed to an increased pressure or which is merely exposed to a slightly increased pressure. However, the increased sealing effect due to the integrated punching procedure may be on option also for these manufacturing steps.
In the context of the following explanations and elucidations of several arrangements and embodiments, reference is primarily made to the overmolding with fluid thermoplastics that are pressurized. However, this shall not be understood as limiting the scope.
The seating surface may be generally referred to as seating side. It is not necessarily required to provide an areal (flat) seating. The tubular section of the coil carrier may be also referred to as a section that is formed in a tube-like fashion. The tubular section may involve a closed cross-sectional profile. In accordance with alternative embodiments, the tubular section is at least sectionally provided with an open profile along the longitudinal extension or axial extension thereof. This may be the case for instance when a groove-like recess or a plurality thereof is formed at the tubular section. The recesses may serve for instance for preventing eddy current-related losses.
Also the coil carrier, particularly the collar thereof, at which the flange contour is formed by the punching procedure, is generally made from a plastic material, particularly by injection molding. The die is generally made from metal materials. Hence, in the punching operation, a cutting or shearing off of the “overhang” of the collar may be performed in a simple fashion in such a way that the then remaining flange contour is adapted to the inner contour of the die in a highly-accurate fashion. It goes without saying that embodiments of the method may be envisaged wherein the step of punching at least partially also involves a flow and/or a flow plastic deformation of the material of the coil carrier, for instance due to friction which involves a temperature increase in the area of a punching edge. However, insofar as reference is made to punching within the context of this disclosure, also embodiments of that kind shall be covered. It is essential that a separating procedure or cutting procedure is involved and that a remainder of the collar is present after the punching which is separated from the resulting flange contour. It may be envisaged that annular or at least ring segment-shaped scrap pieces are formed by the punching of the collar. The scrap pieces may be also referred to as punching slugs.
The punch used for the punching operation is generally adapted to the inner contour of the die. However, it is not necessary that the punch is adapted to the inner contour in such a highly-accurate fashion as it would be the case in an injection molding tool which would have to ensure the required sealing for the overmolding without the provision of a flange contour formed by punching in a highly-accurate fashion.
Even in cases when for instance an outer contour of the punch which is adapted to the inner contour of the die is offset from the inner contour in such a way that a sufficiently large play is present, the tight fitting flange contour may be formed in a highly-accurate fashion and at a great reproducibility.
According to an exemplary embodiment, the die is arranged as a magnet pot and provided with an annular or ring segment-shaped circumferential section which surrounds the inner contour and forms the seating surface or seating side, wherein the coil carrier remains in the magnet pot after the punching procedure. In other words, the magnet pot itself forms the die or punching die. Hence, a part of the punching tool is provided by the magnetic actuator itself, namely by the magnet pot. This enables a highly-efficient manufacturing. As the magnet pot itself defines the inner contour, the flange contour of the coil carrier which is formed by the punching procedure is always adapted to the magnet pot in a highly-accurate fashion. Excess molding material (flash material) and/or undesired residues of the filler material may be avoided in a high probability fashion. The coil carrier that is provided with the coil winding is permanently bonded with the magnet pot by the overmolding procedure.
According to a further embodiment of the method, the flange contour is arranged in a fashion recessed with respect to the seating surface after the punching. In an exemplary embodiment, the flange contour and/or also the coil carrier remain after the overmolding in this state. Due to the recessed arrangement, an offset between a frontal surface of the flange contour and the seating surface is provided. This may be for instance a design goal for the magnetic coil so as to ensure the functional safety of the magnetic actuator. For instance, the recessed arrangement of the flange contour may ensure that the armature may always abut the seating surface and not the flange contour, provided that the flange contour would extend beyond the seating surface. At least the probability of defective parts of that kind may be significantly reduced.
According to a further embodiment, the potting or overmolding involves a feeding of the filler material from a feeding side which faces away from a collar side of the coil carrier defined by the collar, wherein the barrier that is provided by the flange contour ensures a sealing of the filler material. Hence, the flange contour seals off the to-be-filled and/or to-be-overmolded space and prevents a transfer and/or an over-filling of the filler material to the side of the flange contour at which for instance the punch engages the collar of the coil carrier in the punching step.
According to a further embodiment, the method involves an overmolding of the coil carrier which is provided with the coil winding with a thermoplastic material. In an exemplary embodiment, the overmolding is performed with the material from which also the coil carrier is made. The thermoplastic material may be for instance polyphenylene sulfide (PPS). Alternative materials are for instance polyamide (PA), polyoxymethylene (POM) and similar thermoplastics. For instance, polyphenylene sulfide is high-temperature resistant and sufficiently media-resistant. In an exemplary embodiment, the coil carrier and the filler material for the overmolding are formed from the same material. In this way, a material interoperability may be improved. There is no huge likelihood of a different swelling behavior, temperature behavior, and such like. Overall, the coil carrier and the molding compound thus basically have the same characteristics which may further increase the lifespan, the robustness and the operational safety of the magnetic coil.
According to a further embodiment, the method further comprises providing a hold-down device for the potting or overmolding of the coil carrier, wherein the hold-down device is adapted to the inner contour of the die. In an exemplary embodiment, the hold-down device comprises a defined offset with respect to the inner contour. The hold-down device forms a part of the injection molding tool for overmolding of the coil carrier. However, as the coil carrier itself, due to the flange contour, ensures a sealing during the overmolding, the hold-down device merely has to provide a reduced accuracy. Rather, the hold-down device may comprise a frontal surface which is deliberately arranged and defined to be smaller than the inner contour of the die. This does not involve adverse effects on the sealing as the barrier function is ensured by the flange contour. It is sufficient to design the hold-down device in a sufficiently accurate fashion so as to prevent that the flange contour is excessively deformed during the overmolding procedure, due to the molding pressure. This may be however ensured by a hold-down device which is not adapted to the inner contour in a highly-accurate fashion. As the hold-down device provides a sufficiently large offset and/or a sufficiently large play with respect to the inner contour of the die and/or the magnet pot, only little wear occurs. Hence, the hold-down device may have a very long service life.
According to a further embodiment of the method, there is further provided forming a defined cutting edge at the die. The cutting edge may be arranged as a circumferential cutting edge and may surround the inner contour of the die. The cutting edge may be formed at a transition between the inner contour and the seating surface. Nevertheless, the cutting edge does not have in each case to be arranged in a completely circumferential (interruption-free circumferential) fashion. In an exemplary embodiment, the cutting edge comprises a defined sharp-edged form. In other words, the cutting edge may be arranged in a burr-containing or edge-containing fashion. However, as the coil carrier is made from a sufficiently soft thermoplastic material, there are no excessively high requirements for the cutting edge. It is further noted that the cutting edge of the die that is arranged as a magnet pot is only once used for cutting or punching in the manufacturing procedure for the magnetic coil. Hence, wear-related aspects do not play a considerable role.
According to a further embodiment of the method, there is further provided a counter holder for accommodating the coil carrier. In an exemplary embodiment, the counter holder defines the position of the coil carrier in the die. The counter holder may be for instance referred to and arranged as a support bolt. Generally, the counter holder may form part of the magnet pot. It may be however also envisaged to use a separate counter holder. The counter holder may be arranged for guiding the coil carrier when the same is inserted in the die and/or the magnet pot and, eventually, processed by the step of punching. In an exemplary embodiment, the counter holder may define the actual position of the coil carrier in the die which involves also the offset of the flange contour and/or of the frontal surface thereof with respect to the seating surface of the magnet pot. Generally, the magnet pot may comprise a tubular outer wall and a tubular inner wall between which the coil carrier is arranged that is provided with the coil winding. In this respect, the inner wall of the magnet pot may form the counter holder.
According to a further embodiment of the method, there is further provided forming an undercut contour at the coil carrier, particularly forming at least one undercut opening at the collar of the coil carrier, wherein the step of potting or overmolding the coil carrier involves a penetration of the filler material into the undercut contour. In this way, the filler material may be joined with the coil carrier after the overmolding in a positive fit and bonded fashion. As a result, a high-strength compound of the coil carrier and the filler material may be present. For instance, the undercut contour may involve dip holes or stepped recesses which are tapered in a direction towards the side of the collar at which the coil winding is received. During the overmolding procedure, the hold-down device may abut the collar and/or the flange contour of the coil carrier in an areal fashion in such a way that the filler material may penetrate into the undercut contour, wherein, due to the areal contact, the likelihood of excess molding material or residual material is significantly reduced. The hold-down device may completely cover the undercut contour which may be ensured in spite of the deliberately play-involving arrangement of the hold-down device in relation to the inner contour.
According to a further embodiment of the method, there is further provided a position securing section at the inner contour of the die, wherein the formed flange contour provides a rotation orientation feature in such a way that the coil carrier is arranged to be coupled with the die in a fashion fixed against rotation. Both the magnet pot and the coil carrier that is provided with the coil winding may be arranged in a basically rotationally symmetric fashion and/or may comprise rotationally symmetric sections. However, a defined angular orientation between the coil carrier and the magnet pot may be necessary. This applies for instance in regard of a contacting of the coil winding. Generally, this arrangement may also serve as a mounting aid. For instance, the flange contour may comprise radially protruding lugs which are arranged to engage respective recesses at the seating surface. Also the rotation orientation feature at the flange contour may be simply formed by the step of punching when the die, particularly the die that is arranged as a magnet pot, provides a counter contour, namely the at least one position securing section.
An arrangement involving a punched flange contour is that more complex mating geometries may be provided within the context of the present disclosure. Generally, the flange contour may comprise a plurality of design elements, provided that they may be reflected by a “negative” at the magnet pot. This may for instance involve positive and negative radii and edges, and similar transitions. The flange contour does not necessarily have to be arranged in a circular fashion and may nevertheless ensure a sufficient sealing.
According to a further embodiment of the method, the coil carrier further comprises an opposite flange which is arranged at an end of the tubular section facing away from the collar, wherein the coil winding is arranged between the collar and the opposite flange. In contrast to the flange contour, the opposite flange is, however, not arranged as a sealing opposite flange. This is necessary so as to enable the desired injection of the filler material in the intermediate space between the flange contour and the opposite contour. Put simply, the coil carrier may be arranged as a rotation body or a nearly rotation body comprising a C-shaped rotational cross-section. Between outer legs of the C, the coil winding is received.
In regard of the magnetic coil, these above and other objects of the disclosure are achieved by a magnetic coil for a magnetic actuator, particularly for an injector, wherein the magnetic coil comprises:
In an exemplary embodiment, the magnetic coil is manufactured in accordance with at least some aspects of the above-described manufacturing method.
According to a refinement of the magnetic coil, at least one undercut contour is formed at the coil carrier, for instance at the collar of the coil carrier, wherein the undercut contour is facing away from the coil winding and at least partially filled with the filler material.
According to a further embodiment of the magnetic coil, the die comprises at least one position securing section arranged at a front end, wherein at least one rotation orientation feature is formed at the collar of the coil carrier which is coupled with the at least one position securing section.
In an exemplary embodiment, a magnetic coil in accordance with one of the afore-mentioned aspects is used in a magnetic actuator which forms part of an injector, for instance a part of a fuel injector nozzle for a combustion engine.
It is understood that the above-mentioned features of the disclosure and those to be explained in the following can be applied, not only in the respective specified combination, but also in other combinations or singly, without departing from the scope of the present disclosure.
Further features and advantages of the disclosure are disclosed by the following description of a plurality of exemplary embodiments, with reference to the drawings, wherein:
Further embodiments of injectors may be readily envisaged. Regularly, the injectors 10 are provided with an actuator 28 which is frequently arranged as an electromagnetic actuator 28 and provided with a coil winding 32. The coil winding 32 is regularly overmolded and/or potted. In this way, the coil winding 32 may be efficiently protected against environmental influences.
With reference to the exemplary embodiments explained in more detail further below, exemplary arrangements and embodiments of magnetic coils 30 for electromagnetic actuators 28 of that kind and exemplary method aspects for the manufacturing thereof will be elucidated and described in more detail.
Generally, the magnet pot 50 is made from a ferrous material or a ferrous-containing material. The coil winding 32 is received at a coil carrier 58. The coil carrier 58 simplifies the manufacturing, particularly the formation of the coil winding 32. The coil carrier 58 may be for instance arranged as an injection molded part, for instance from a thermoplastic material, such as polyphenylene sulfide (PPS). By way of example, the coil carrier 58 comprises a tubular section 60 wherein a collar 62 is arranged at an end thereof, wherein the collar 62 is radially outwardly extending as a circumferential collar. In a non-assembled state of the coil carrier 58, the tubular section 60 delimits or surrounds an opening 64, refer also to
It can be further seen from the exemplary embodiment of
The magnet pot 50 comprises a seating surface 68 which is for instance arranged as a contact surface for an associated magnet armature. Nevertheless, embodiments may be envisaged wherein, by design measures, a remaining air gap is provided between the seating surface and the magnet armature. At the collar 62 of the coil carrier 58, a frontal surface 70 is formed. A design goal for the magnetic coil 30 may involve that the frontal surface 70 of the coil carrier 58 is deliberately recessed with respect to the seating surface 68 so as to ensure that no filler material 66 may protrude. Such an arrangement namely might involve adverse effects on the function of an actuator that is provided with the magnetic coil 30. In a transition area 90 between the collar 62 and the magnet pot 50, particularly the outer wall 52 thereof, occasionally there may be excess molding material or flash protrusions 72. A reason for this is often that the collar 62 cannot be adapted to the magnet pot 50 in a highly-accurate and sealing fashion. However, as for instance the overmolding of the coil winding 32 with the filler material 66 is performed at an increased pressure, filler material 66 may enter the transition area 90 and/or may extend through the transition area 90. The axial flush protrusions 72 which potentially may occur may have the result that the respective instant of the magnetic coil 30 is classified as junk. An offset and/or a deliberate recess of the coil carrier 58 with respect to the seating surface 68 is also an option when a remaining air gap is provided as a design measure so as to ensure the operational safety.
In the following, several embodiments will be elucidated which address this issue and which propose respective solutions therefor.
The coil carrier 58 illustrated in
The magnet pot 50 illustrated in
In other words, a die 94 for the punching of the flange contour 76 is provided which is provided by the magnet pot 50 itself. This ensures in any case that a nearly perfect free-of-play adaptation of the flange contour 76 to the inner contour 84 may be accomplished. In this way, gaps in the transition area 90 (refer also to
With reference to
In accordance with the embodiment elucidated with reference to
In combination, it can be seen in
Further, in
In an exemplary embodiment, the magnet pot 50 itself is arranged as die or punching die 94. By the stamping procedure, a flange contour 76 is formed at the collar 62 the shape of which is basically defined by the application of the magnet pot 50 as a die 94. As a result, at least a portion of the collar 62 is disconnected and/or separated, refer for instance to scrap elements 116 indicated in
It goes without saying that the coil carrier 58 does not necessarily have to be moved by the punch 104 itself further towards the seat 98. This displacement may be also effected by another punch or hold-down device.
In the
In
Generally, the potting or overmolding may involve a filling or a displacement of an empty filling volume 130.
With reference to
According to the embodiments elucidated with reference to
In the overmolded and/or potted state illustrated with reference to
By means of a hold-down device 120 which is indicated by dashed lines in
The method comprises a step S10 which involves a provision of a coil carrier. The step S10 may involve sub-steps S12, S14. The sub-step S12 involves forming the coil carrier by means of injection molding. The sub-step S14 may follow which involves a winding of a coil winding which is received at the coil carrier. The coil carrier further comprises a tubular section and a collar adjoining the tubular section.
A further step S20 of the method involves the provision of a magnet pot. In an exemplary embodiment, the magnet pot also serves as a die or punching die in the manufacturing of the magnetic coil. In an exemplary embodiment, the magnet pot is arranged for a single punching operation which relates to the coil carrier, particularly to the collar thereof. A sub-step S22 involves a formation of the magnet pot, for instance by an appropriate molding operation. This may for instance involve a casting operation, a sinter operation or a similar method. Further, a machining of the magnet pot may follow.
In a further sub-step S24, a punching contour at the magnet pot is provided. This may involve the formation of a defined cutting edge. The punching contour may be basically also already formed—so to say as a by-product—by the original formation of the magnet pot as such.
A step S30 follows the steps S10 and S20 which may be also referred to as joining step or pre-assembly step. The coil carrier that is provided with the coil winding is inserted into the magnet pot. In an exemplary embodiment, the collar of the coil carrier is too large for a receiving contour or inner contour of the magnet pot. In other words, the collar may rest on a front end of the magnet pot at a seating surface. Hence, the coil carrier is prepared for a punching operation. Before the actual stamping operation (step S34), a feeding of a punching tool, particularly of a punch, may be provided which is accomplished in a step S32. After the execution of the step S34, a flange contour is formed at the collar which is adapted to the inner contour of the magnet pot.
A subsequent step S36 involves a retraction of the coil carrier in the magnet pot. This is enabled as the collar which was originally too large, is adapted by the punching operation accordingly. The retracting step involves the formation of a desired offset dimension between the flange contour and a seating surface of the magnet pot.
A further step S38 may follow which may be however arranged as a voluntary or an optional step. The optional step S38 involves a deburring procedure or a brushing procedure by means of a deburring tool or a brushing tool. This may already take place at the pre-assembled arrangement of the magnet pot and the coil body. In the step S38, burrs and similar remainders at the cutting edge of the magnet pot may be removed, if necessary. Also any remainders of the coil carrier may be removed in this way. The deburring or brushing may involve a cleaning operation so as to remove any remaining particles.
By way of example, a handling step S40 may follow. In connection with the handling step S40, in a step S42, the punch and/or the punching tool may be lead away. A step S44 may involve an insertion of the magnet pot that is provided with the coil carrier into a molding tool. This may also involve the provision and an approaching of a hold-down device which approaches the flange contour so as to support the flange contour. In this way, a preparation for a further step S46 may be accomplished. The step S46 involves an overmolding or potting with a filler material, for instance with a fluid thermoplastic material. In an exemplary embodiment, the filler material is inserted by injection molding. This involves that the filler material is pressurized. The hold-down device protects the flange contour during the molding operation against excessive deformations. As the flange contour is adapted to the inner contour of the magnet pot in a highly-accurate fashion, there is no likelihood or only little likelihood of a transfer of filler material beyond the flange contour. The flange contour acts as a barrier for the filler material at the magnet pot.
Number | Date | Country | Kind |
---|---|---|---|
10 2015 105 591 | Apr 2015 | DE | national |
Number | Name | Date | Kind |
---|---|---|---|
4575008 | Kaczynski | Mar 1986 | A |
6371270 | Matsumoto | Apr 2002 | B1 |
20040090294 | Just et al. | May 2004 | A1 |
20050232803 | Kuttler et al. | Oct 2005 | A1 |
20090250836 | Fukui | Oct 2009 | A1 |
20110115330 | York et al. | May 2011 | A1 |
20110128103 | Baba | Jun 2011 | A1 |
Number | Date | Country |
---|---|---|
10032328 | Mar 2001 | DE |
10151955 | May 2003 | DE |
102004008450 | Sep 2005 | DE |
0132623 | Feb 1985 | EP |
59103308 | Jun 1984 | JP |
08250357 | Sep 1996 | JP |
2012-174903 | Sep 2012 | JP |
Number | Date | Country | |
---|---|---|---|
20160298582 A1 | Oct 2016 | US |