1) Field of Invention
The present invention generally relates to nano-indentation measuring instruments and more particularly to a measuring head for such an instrument as well as to its method of use, said head using active referencing of the surface of the sample to be measured.
2) Description of Related Art
The measuring method by instrumented indentation (Depth-Sensing Indentation or DSI) is one of the most used methods for determining certain mechanical properties of materials, such as for example the elastic modulus and hardness. This method consists of applying an increasing and subsequently a decreasing force on a sample via a tip or indentor, with a determined shape in order to investigate and to measure, continuously and simultaneously, the values of the load, of the load alleviation, respectively, applied onto the sample on the one hand, and the penetration depth of the indentor on the other hand. The involved forces may be extremely weak, typically of the order of a few micro-Newtons (μN), and the displacements of the indentor to be measured may be of the order of one nanometer (nm). One then speaks of nano-indentation.
A head for nano-indentation measurements should therefore be capable of applying a force on a sample via an indentor and of determining the applied force as well as the corresponding penetration of the indentor. Among the existing nano-indentation measuring instruments, the Nano Hardness Tester or NHT, may be cited, marketed by the applicant or further the instrument “Triboindenter®” of Hysitron Inc. The technology used for the measuring head of this latter instrument is moreover described in U.S. Pat. No. 5,553,486. The measuring heads of the prior art apply the desired force via an electrodynamic (electromagnet) or electrostatic actuator and they have a displacement sensor (generally a capacitive sensor) but no force sensor. The force applied to the sample is then inferred from the force generated by the actuator, for example calculated from the current or voltage applied to the latter and from the stiffness of the spring strips supporting the indentor. This is therefore a method for indirect measurement of the applied force.
U.S. Pat. No. 4,852,397 describes a measuring instrument by nano-indentation, the measuring head of which includes an indentor, actuating means as well as detecting means of the penetration depth of the indentor in a sample by direct measurement.
The publication entitled “Development of a depth controlling nano-indentation tester with subnanometer depth and submicro-newton load resolutions”, published under the names of Atsushi Shimamoto and Kohichi Tanaka, in Volume 68(9) of September 1997 of the Review of Scientific Instruments, pp. 3494-3503, discloses another example of such a measuring apparatus. The latter comprises a measuring head, including an indentor and a displacement sensor, both submitted to the action of a single actuator, as well as means for measuring the load applied by the actuator, distinct from the measuring head. The displacement sensor described in this publication is of the optical fiber type and with it, direct optical measurement of the displacement of the measuring head may be carried out.
Generally, with the cited devices of the prior art, several problems arise, such as the following:
1) Thermal drift. A standard nano-indentation measurement lasts for about one minute. During this period, any change in temperature will result in a dimensional change of the mechanical components of the measuring instrument (thermal expansion or contraction). The problem is further worsened if the instrument uses an electrodynamic actuator which itself produces heat and this depends on the generated force. For example, in the case of a system without any reference, if a path of 30 cm is considered between the tip of the indentor and the surface of the sample, via the frame of the steel instrument (thermal expansion coefficient of steel equal to 10×10−6/° C.), a variation of 0.1° C. during the measuring period would lead to a depth measuring error of the order of 300 nm, which is disproportioned with regard to the penetration depths which themselves are frequently less than 100 nm. Present answers for minimizing thermal variations combine the use of costly thermostated enclosures with an action consisting of measuring the drift at a given instant and of applying a correction of this drift to the totality of the nano-indentation measurement. Such answers lead to very long cycle times (waiting for thermal stabilization in the enclosure) and are based on the arbitrary assumption that the thermal drift remains constant throughout the measurement.
2) Influence of the stiffness of the frame of the instrument and of the frame-sample connection. When a force is applied on the indentor, it not only causes a penetration of the indentor into the sample but also a deformation of the sample holder/instrument assembly proportional to the compliance (which means the capability of deforming under the effect of a stress) of this assembly. This deformation leads to overestimating the penetration depth and requires subsequent correction by subtraction of the estimated value of the compliance. A solution, already used by the applicant to counter this problem, consists of having the measuring head directly rest on the sample via a reference part and next measuring the penetration depth directly between this reference and the indentor. Any parasitic movement (whether from a thermal origin or because of the compliance of the frame) will thus be greatly attenuated. One of the problems in this case, is that the totality of the weight of the measuring head rests on the sample, which poses problems on soft materials or materials exhibiting creep because, in this case, solving a problem creates new problems.
3) Independence of the force and displacement sensors. As indicated earlier, the existing nano-indentation heads are equipped with a single actuator and a single sensor (displacement sensor). The absence of an independent force sensor poses two problems. First, the force is not directly measured but is estimated, which may be a source of error, and second, several very interesting loading modes—such as an indentation with a constant deformation rate for example—cannot be applied completely because they require a control which takes into account the penetration depth and the applied force simultaneously.
The object of this invention is therefore to allow a nano-indentation measurement, free from the constraints mentioned earlier and to thereby obtain a more accurate and more reliable measurement of the elastic modulus and of the hardness at a nanoscale. This object is achieved by means of the measuring head defined in the independent claim. Particularly advantageous exemplary embodiments are defined in certain dependent claims. A measuring method using the measuring head of the invention is the object of other dependent claims.
The invention is based on the idea of using a measuring axis and a reference axis each having their own actuating means and their own means for measuring the displacement, and of measuring the applied force. The indentation measurement may therefore be conducted relatively to a reference, for which the force applied on the sample is controlled. Thus it is possible to achieve what is called active referencing of the surface of the sample to be measured, i.e., by independently controlling the reference axis, it is possible to get rid of any parasitic movement of the surface of the sample and/or of the measuring instrument itself, for example as a result of a change in temperature, of a deformation of the frame or of the frame-sample connection.
The measuring head according to the invention is further designed so as not to generate any heat and to be also as insensitive as possible to any change in room temperature. Its application does therefore not require it being placed in a thermostated enclosure.
Other objects, features and advantages of the present invention will become apparent upon reading the following description made as a non-limiting example and with reference to the appended drawings wherein:
a and 3b illustrate a piezoelectric actuator with amplification and a spring, respectively, as used in the measuring head of
An exemplary embodiment of a measuring head by nano-indentation according to the principles of the invention is schematically illustrated in
The bodies 100 and 200 should be perfectly stiff, have a mass as low as possible and also have a thermal expansion coefficient as small as possible. Ceramic glass, as marketed by Schott under the brand Zerodur®, meets the stated conditions. This material will advantageously also be used for making the rods 101 and 201, as well as the transverse components 102, 202 and 203. The material of the indentor 105 and that of the reference head will depend on the application. As a non-limiting example, the indentor may be in diamond and the reference head in steel. As indicated earlier, the actuators A1 and A2 will preferably be of the piezoelectric type in order to avoid any generation of heat. An exemplary embodiment of such actuators will be described with reference to
As for the measuring head as described above, it is further important that it meets the following conditions:
the total suspended mass should be as low as possible;
both measuring and reference axes should be as symmetrical as possible (same length and same materials used); and
the critical path or length of the measuring loop (dotted line CC from the tip of the indentor to the tip of the reference head) should be minimal, which implies that the distance between the indentor and the reference tip is also minimal.
The operation of the measuring head of the invention and in particular that of the sensors may be explained with the diagram of
a shows a so-called “amplification” actuator which may be used in the measuring head according to the invention. Such an actuator is of the APA 120S type, as marketed by Cedrat Technologies, Aix, France. It is controlled by a DC voltage which may attain 150 volts and has a stroke of 100 μm. It consists of a bar 301 in piezoelectric material (to which the DC voltage is applied via suitable electrodes) and of a frame 300 with a rhombic shape and transforming a horizontal elongation of the bar into a vertical displacement of the free angles of the rhombus. The actuator is laid out in such a way that the vertical displacement is larger than the elongation of the bar, whence its name of amplification actuator. It is understood that other actuators may be used from the moment that they meet the conditions stated earlier.
b shows a type of spring which may be used in the measuring head according to the invention. It includes several rectangular structures (such as 401 and 402), formed with two flexible strips (such as 401a and 401b) joined by stiff end components (401c and 401e). The rectangular structures are joined to each other by interfaces (403) fixed at the center of the flexible strips. Under the effect of an applied force between the external portions of these interfaces, the flexible strips deform linearly. The material advantageously used for making these springs is invar, which is an iron and nickel alloy well-known for its exceptional thermal properties. There again, the exemplary embodiment described above is non-limiting and other types of spring may also be used.
According to an advantageous alternative of the invention, a servo-control circuit is also provided for the servo-control of the actuator A1 of the measuring axis. However, in this case, the set force may not be constant but may change during a same measuring cycle or even from one cycle to the other.
According to another alternative of the invention, the actuator A1 of the measuring axis is controlled in such a way that the displacement of the indentor is servo-controlled to a given value.
The method for using the measuring head according to the invention includes the following steps:
the piezoelectric actuators A1 and A2 are pre-positioned so that the tip of the indentor is first slightly retracted relatively to the reference head;
next, the sample E is displaced vertically until it is brought into contact with the reference head;
the piezoelectric actuator A2 is consequently controlled so that a selected force is applied to the reference head and this during the whole measuring period;
the indentor is then, by means of the actuator A1, brought into contact with the sample E, the contact force being controlled by the force sensor (C2, K2);
starting the measuring cycle consisting of applying a given force to the indentor (a simply variable static force or variable according to a repetitive sequence, etc.) and of simultaneously measuring the penetration depth of the indentor;
retracting, at the end of the measurement or of the measuring cycles, first the indentor, and then the reference head and finally the sample.
Although the present invention was described with reference to particular exemplary embodiments, it is by no means limited to said examples and may undergo changes and/or alternatives without however departing from its scope. In particular, if in the preceding description, the stiffnesses of the springs K1 and K2 were supposed to be equal, it is also conceivable to make them different, this would, by swapping the measuring axis and the reference axis (which amounts to exchanging the indentor and the reference tip) very easily provide two different measurement ranges on the same instrument.
Number | Date | Country | Kind |
---|---|---|---|
04405798.2 | Dec 2004 | EP | regional |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/EP05/56026 | 11/16/2005 | WO | 00 | 6/18/2007 |