The invention relates to a method and a device for dismantling a multilayer system. The invention particularly relates to a method for recycling multilayer products comprising at least one layer of organic material.
Multilayer systems or products are involved in our daily lives in a wide variety of applications. For example, they are found in:
These multilayer systems generate a lot of waste whose disposal is problematic. In fact, this waste often includes recoverable materials. However, the separation of the different layers of the system is necessary in order to separately recover or recycle each of the components. One of the most telling examples concerns technological waste. Disposal of this electronic component waste poses various problems, among which are:
When seeking to recover each of the components of a multilayer system, it is necessary to perform a step of disassembly or separation of the different layers of the waste, so that each of these layers may undergo appropriate treatment.
In the case of photovoltaic panels with crystalline silicon technology, attempts are made to separate the various layers, i.e. the glass layer, the organic layer(s) (polymers), the crystalline silicon and various metals. The separation of the various layers remains a problem due to the presence of a fluorinated polymeric layer, the rear surface, which requires to take certain precautions during recycling. In fact, the thermal decomposition of the fluorinated polymer generates other fluorinated compounds which are dangerous and toxic. The presence of fluoropolymers therefore limits the recycling processes since there is a risk of formation of these fluorinated derivatives, and this is why attempts are made to separate them before any other recycling step. Thus, the separation of this layer is a priority in order to consider viable recycling techniques. However, when subjected to relatively low temperatures, between 150° C. and 200° C., this fluoropolymer degrades to form dangerous fluorinated compounds. Thus, the use of thermal processes for the removal of this layer does not make it possible to recover the material as a raw material and also requires the implementation of strict procedures for the safety and recycling of gaseous effluents.
One way to proceed is to grind the multilayer system, which allows, for example in the case of a photovoltaic module, the recovery of only a fraction of the glass. The recovered glass requires additional treatment in order to be reused. The recycling of the crystalline silicon or PV c-Si photovoltaic modules generally stops after the grinding/separation step and only allows the recovery of some metals as well as impure glass in the form of ground material that is of an inferior quality compared to the original quality of the material. Many impurities in this ground glass do not allow reuse as solar glass unless, for example, a dry purification process is implemented. To do this, it is possible to carry out a step of purifying the surface of the glass by abrasion in order to eliminate the pollutant, and obtain a glass with sufficient purity for resale (flat glass, quality inferior to the original quality of the material). The non-recovery of solar cells is problematic. The purification of solar cell debris as well as the recovery of other metals requires additional chemical treatment steps. The mechanical processes are simple enough to implement, but remain insufficient to recover all the valuable materials of the module with a sufficient degree of purity.
It is also possible to incinerate the photovoltaic module at high temperature in order to eliminate the different organic layers. However, this technique requires significant amounts of energy to reach the required temperatures ranging from 450° C. to 600° C. and significant safety measures to manage the production of fluorinated compounds. In addition, the glass may be broken due to heat stress during the treatment. The different compounds recovered after this treatment, glass, solar cells (c-Si and metal connections) and metals may be polluted by organic residues and thus require one or more additional treatment steps. Thermal processes are generally excessively energy intensive and expensive. In addition, the recovery of pure materials requires coupling with a mechanical or chemical process due to incineration residues.
Another approach is to use chemical etching of different organic layers to recover glass, solar cells and metals. This technique has many disadvantages. In fact, the chemical etching is carried out in several stages generally involving toxic solvents that are dangerous for the environment, toluene, for example, as well as acids such as sulfuric acid for example. These solvents and acids are expensive and their use leads to the generation of new waste because of their pollution by organic residues. In addition, they may also attack/pollute solar cells and glass, thus degrading the purity of the recovered materials. The chemical treatments have the disadvantage of requiring the use of large quantities of chemicals, such as acids or solvents, which may be problematic from the point of view of method (safety, recycling of solvents . . . ), economy (product prices, regular regeneration . . . ) and environment (creation of possible additional waste).
Most of the recycling methods implemented, therefore, involve high costs and do not make it possible to optimize the recovery of each of the layers constituting a component or a multilayer system comprising at least one organic layer.
The patent application WO 2012101189 proposes a method of recycling photovoltaic modules that consists in separating multi-materials into base materials. The technology is based on the separation of composite materials using microemulsions based on surfactants. The principle of the method is to reduce the interfacial tensions between each component in order to separate them. Several steps are necessary in this separation process:
This method has many economic advantages because it allows a high rate of recycling and recovery of materials with no loss at low energy and financial cost (ambient temperature, water use, . . . ) and allows the recovery of high purity materials (no phase change during treatment). It is also of environmental interest because of the microemulsions but also because the washing water is reusable. Nevertheless, this process involves many steps, while microemulsions use large amounts of water to reduce the proportion of surfactants used.
There is therefore a need for a method for separation in a viable, reliable and safe manner, of the various layers of a multilayer system in order to individually recover them while avoiding their degradation. The clean and clear separation of the various layers of a system comprising several layers including at least one organic layer, remains a key stage to be considered for the optimization of recycling and recovery processes. Thus, the fact of being able to recover the original glass in the case of photovoltaic modules has a much higher economic interest than the recovery of a polluted glass that can only be reused for insulation applications, for example.
A multilayer system according to the invention is a composite material consisting of a stack of inorganic and/or organic layers including at least one organic layer. The bond between two successive layers in the system may be provided by a layer of glue but the interface may also be of a chemical nature, for example one that is obtained by activating a glass surface so that it reacts with an organic layer when assembling the multilayer system. During the method, it will be possible, through the choice of the temperature treatment parameters, pressure and also the choice of fluids, to choose to separate either each layer unitarily or subsets of layers as needed. A layer may itself be composed of several components.
The method according to the invention is based on a new approach to separating at least the various layers or subsets of layers of a multilayer system by using a fluid composed of a gas and a mixture of non-reactive liquids in the ambient conditions of temperature and pressure (25° C. and 0.1 MPa) and to raising it in temperature and pressure, and particularly in a supercritical environment. The term “liquid mixture” will be used to designate a liquid or several non-reactive liquids mixed in variable proportions, wherein the liquids have, in particular, the function of separating the layers without affecting the components.
The invention relates to a method of delamination/dismantling multilayer systems SM comprising several layers including at least one organic layer, the layers being separated by interfaces, characterized in that it comprises at least the following steps:
According to an alternative embodiment, the treatment temperature Tr is chosen to be greater than the critical temperature Tc of the gas and lower than the degradation temperature Tg of the layers of the multilayer system, the treatment pressure Pr is chosen to be greater than the critical pressure Pc of the gas and the volume proportion of liquid mixture relative to the gas is at least 15%.
It is possible to implement the method with a temperature between 30° C. and 150° C. and a pressure between 5 MPa and 50 MPa.
The fluid used is, for example, a CO2/water/acetone mixture with a proportion of water relative to acetone ranging from 0 to 100%.
The treatment temperature may be between 60° C. and 130° C.
The method may be used for the treatment of multilayer systems, for example, a photovoltaic module comprising a fluorinated layer, a packaging, a food packaging, a cosmetic or pharmaceutical packaging, an organic electronic component.
The method may include a step of precutting the multilayer systems and a step of rinsing and drying the layers or subsets of separate layers.
The invention also relates to a device for delamination/dismantling of multi-layer systems comprising several layers including at least one organic layer, the layers being separated by interfaces, characterized in that it comprises at least the following elements in combination:
According to an alternative embodiment, the device may comprise a gas reservoir connected to a cooling device via a first conduit, a high pressure pump whose outlet is connected to a preheater, which itself is connected with a first valve of a gas introduction conduit connected to the first inlet, and a conduit for evacuating gas to an enclosure.
The device may also comprise one or more liquid introduction lines connected to a second inlet of the reactor, a line comprising at least a second conduit equipped with a third control valve, a pump which receives the mixture of liquids stored in a reservoir, a drain circuit connected to a second outlet of the reactor connected to a conduit equipped with a third valve and a reservoir or a drain pipe.
Other characteristics and advantages of the present invention will become clearer upon reading the description of exemplary embodiments given in the appended figures by way of illustration and in no way limiting, wherein:
In order to clearly understand the steps and operation of the method according to the invention, the following example is given in the context of dismantling a photovoltaic module. There are a number of photovoltaic module technologies. Photovoltaic modules based on crystalline silicon dominate the photovoltaic module market. These photovoltaic modules with c-Si technology are multilayer systems whose recycling and recovery require the separation of the different layers in order to extract the materials of interest.
An example of a photovoltaic module with crystalline silicon technology shown in
The presence of fluoropolymers in the backsheet today represents a technological block to the recycling of the various layers. In fact, the thermal decomposition of fluorinated polymers, such as PVF or PVDF, results in the generation of toxic and dangerous fluorinated compounds for the operator, the environment and the method.
Upstream of the reactor 20, the carbon dioxide or any other gas used during the process may be stored in a bottle (not shown), or else via a circuit comprising a CO2 reservoir 31 that is connected to a cooling device 32 via a first conduit 33, and a high pressure pump 34, whose output is connected to a preheater 35, which itself is connected to the first valve 24.
The liquid mixture may be introduced directly into the reactor 20 with the multilayer system to be treated. One or more lines for introduction of the liquid or liquid mixture may equip the device for this purpose.
In
The photovoltaic modules PV are placed directly in the reactor 20 with the liquid mixture, for example. The reactor is then closed and the CO2 is injected. The preheater 35 facilitates the rise in temperature of the CO2 medium. The presence of the high pressure pump 34 coupled to the cryostat 33 makes it possible to reach higher pressures, thereby ensuring that the CO2 is in the liquid state. Once the treatment parameters have been reached, i.e. the temperature Tr and the pressure Pr, an adjustment is made for a predetermined period. At the end of this stage, the system is cooled, then depressurization is carried out before opening the reactor. The various separated layers of the multilayer system without degradation and the mixture of liquids are then recovered. The layers or the subset of layers separated at the end of the method are subsequently rinsed with water and dried in air (ambient temperature, compressed air or natural air), for example, in order to eliminate liquid residues. It will also be possible to introduce the liquid mixture for continuous treatment through the liquid introduction circuits described above.
The gas used for the implementation of the method fills, for example, three functions, simultaneous or not:
The mixture of non-reactive liquids will be chosen for its ability to separate either each layer unitarily or subsets of layers comprising the multilayer system, in addition to the action of the gas, regardless of the function performed by the latter according to the definition above, and without modification of the components of interest of the multilayer system. The volume proportion of the liquid mixture with respect to the gas will be at least 15%.
In the case of presence of glue ensuring bonding between the layers, the mixture of liquids will allow dissolution and/or extraction of glues without changing the components of interest.
The conditions of pressure Pr and temperature Tr for carrying out the treatment will, for example, be chosen from the following ranges; the temperature range [31° C., 150° C.]; the pressure range Pr [5 MPa, 50 MPa]. The value of the temperature Tr to which the reactor is raised will be chosen at a value lower than the degradation temperature Tg of the components constituting a layer of the multilayer system.
The mixture of liquids or fluid mixed with CO2 will comprise, for example, ethanol, acetone, water, etc., i.e. any non-reactive fluid having the effect of separating either each layer unitarily or subsets of layers comprising the multilayer system in addition to the action of CO2 at the interface of the layers constituting the multilayer system. The volume proportion of this mixture of liquids within the gas/liquid mixture fluid will be at least 15%.
The liquid mixture used for the treatment comprises, for example, acetone, and the value of the treatment temperature Tr is moderate, for example 90° C., between 30° C. and 150° C.
The method according to the invention may operate online, continuously or batchwise. In the case of an online operation, the steps or phases of setting the temperature and pressure, introduction and “emptying” of the recovered components, will be performed according to principles known to a person skilled in the art.
According to another embodiment, the fluid is a CO2/water/acetone mixture. The temperature Tr is for example 90° C.
These last three explicit variant embodiments make it possible to completely dismantle a PV module using a CO2/water/acetone mixture, without waste or degradation of the PVDF or Kynar® layers by optimizing the temperature between 90° C. and 120° C.
In the case of recycling non-fluorinated backsheet photovoltaic modules, the temperature Tr may be chosen equal to 60° C. The treatment will be carried out in the presence of CO2 at 60° C. or in the presence of a CO2/water mixture at 90° C. in order to separate the backsheet. The use of a mixture of CO2/water/acetone at 120° C. will allow the separation of the backsheet and the recovery of the glass. Without departing from the scope of the invention, it is possible to work at lower temperatures, in the order of 60° C., 90° C., for example, especially for the CO2/water/acetone mixture.
In general, the operating parameters of the method according to the invention will be as follows:
The method described above may be implemented in the recycling of many multilayer systems. The multilayer system may be, for example, a cosmetic packaging waste composed of a polymer layer coated with one or more metals. It is also possible to treat pharmaceutical packaging waste consisting of a plastic layer and an aluminum film, the treatment allowing a clear separation of the layers.
The method is also used to recycle waste, for example:
The method may also be used to separate the layers present in c-SI PV cells, OLEDs (organic light emitting diodes), display devices, etc.
For the treatment of this waste, this waste is, for example, precut before subjecting it to the two treatments described above:
The pre-cutting step makes it possible, in particular, to promote and/or allow access of the gas/liquid mixture fluid to the interfaces of the different layers of the system and thus the separation of the layers. This results among other things in a reduction in processing times. It also makes it easier to handle multilayer systems.
For the treatment of cosmetic packaging waste, consisting of a plastic film coated with a metal deposit, it is possible to recover in solution the metals present on the cosmetic packaging waste.
In the case of pharmaceutical packaging treatment, the method makes it possible to recover the aluminum.
The treatment of compote packaging will lead to the separation of organic layers from aluminum.
In order to minimize the energy costs related to the method, and to avoid thermal decomposition of certain components of the layers, the operating temperature will be at most equal to 150° C., below the degradation temperature Tg of the compounds. In this way, it is possible to treat multilayer systems comprising at least one organic layer that could generate toxic or environmentally hazardous compounds, such as fluoropolymer of the PVF or PVDF type. This temperature value does not limit the use of the method to higher temperatures if the separation of the layers of the system requires it.
The method according to the invention advantageously makes it possible to recover the various components of a multilayer system without harming the environment, or at least minimizing the impact on the environment. It finds its use in many fields, including household waste, electronic waste,
The method according to the invention makes it possible, in particular, to easily recover glass while retaining both its optical and chemical surface properties.
Number | Date | Country | Kind |
---|---|---|---|
15 58185 | Sep 2015 | FR | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/EP2016/070767 | 9/2/2016 | WO | 00 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2017/037260 | 3/9/2017 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
6306564 | Mullee | Oct 2001 | B1 |
7909959 | Tada | Mar 2011 | B2 |
20020081250 | Lord | Jun 2002 | A1 |
20100086788 | Tsuji | Apr 2010 | A1 |
20160214368 | Kernbaum et al. | Jul 2016 | A1 |
Number | Date | Country |
---|---|---|
H0892411 | Apr 1996 | JP |
WO-9703802 | Feb 1997 | WO |
Entry |
---|
International Search Report for PCT/EP2016/070767, dated Sep. 22, 2016. |
Written Opinion of the International Searching Authority for PCT/EP2016/070767, dated Sep. 22, 2016. |
Preliminary Search Report for FR 1558185, dated Jan. 21, 2016. |
Number | Date | Country | |
---|---|---|---|
20180257267 A1 | Sep 2018 | US |