Claims
- 1. A method for making a black plate by exposing a panchromatically spectral sensitized photosensitive material to a block copy having multicolor continuous tone images and line images, comprising the following steps:
- (1) exposing the photosensitive material in close contact with a contact screen to the block copy, with the line images of the block copy being covered with a black mask (M-1) of 2% or less in optical reflectance and the multicolor continuous tone images of the block copy being covered with a white mask (M-2) of about 50% or more in optical reflectance;
- (2) exposing the photosensitive material to the multicolor continuous tone images without the contact screen and the mask (M-2), and with the line images being covered with mask (M-1); and
- (3) exposing the photosensitive material to the line images without the mask, and with the multicolor continuous tone images being covered with mask (M-1).
- 2. A method according to claim 1 wherein said mask (M-2) has an optical reflectance of about 80% or more.
- 3. A method according to claim 1 wherein the mask (M-2) has an optical reflectance of about 70% or more.
- 4. A method according to claim 1 wherein the photosensitive material (P) has a panchromatically spectral-sensitized silver halide emulsion layer.
Priority Claims (2)
Number |
Date |
Country |
Kind |
60-38082 |
Feb 1985 |
JPX |
|
60-38083 |
Feb 1985 |
JPX |
|
Parent Case Info
This is a continuation of application Ser. No. 832,772, filed Feb. 25, 1986, now abandoned.
US Referenced Citations (5)
Continuations (1)
|
Number |
Date |
Country |
Parent |
832772 |
Feb 1986 |
|