The present invention relates to the field of metrology, and more particularly, to misregistration metrology procedures.
Various types of devices for metrology and misregistration metrology procedures are known.
The present invention seeks to provide an improved method for measurement of misregistration in the manufacture of semiconductor device wafers and amelioration thereof.
There is thus provided in accordance with a preferred embodiment of the present invention a method for measurement of misregistration in the manufacture of semiconductor device wafers, the method including measuring misregistration between layers of a semiconductor device wafer at a first instance and providing a first misregistration indication, measuring misregistration between layers of a semiconductor device wafer at a second instance and providing a second misregistration indication, providing a misregistration measurement difference output in response to a difference between the first misregistration indication and the second misregistration indication, providing a baseline difference output and ameliorating the difference between the misregistration measurement difference output and the baseline difference output.
Preferably, the ameliorating includes at least one of changing misregistration metrology and changing at least one process step in the manufacture of semiconductor device wafers.
In accordance with a preferred embodiment of the present invention the method for measurement of misregistration in the manufacture of semiconductor device wafers also includes comparing the difference between the misregistration measurement difference output and the baseline difference output with a threshold and the ameliorating occurs when the difference between the misregistration measurement difference output and the baseline difference output exceeds the threshold. Additionally or alternatively, the baseline difference output represents a calculated compilation of differences between the first misregistration indication and second misregistration indication.
In accordance with a preferred embodiment of the present invention the first and second instances include different stages in a manufacturing process of a single batch of semiconductor device wafers intended to be identical from which the semiconductor device wafer is selected.
In accordance with a preferred embodiment of the present invention, the same semiconductor device wafer is measured at the first and second instances. Alternatively, different semiconductor device wafers, which are selected from the single batch of semiconductor devices intended to be identical, are measured at the first and second instances.
Preferably, the first and second instances include different regions of a single target on the semiconductor device wafer.
In accordance with a preferred embodiment of the present invention the misregistration measurement difference output includes an indication of metrology quality.
In accordance with a preferred embodiment of the present invention the misregistration measurement difference output includes an indication of quality of at least one of the different stages.
Preferably, the method also includes using at least one of the first and second misregistration measurement indications to ameliorate misregistration measurement between layers of a semiconductor device at a third instance. Additionally, the third instance includes a later stage in the manufacturing process of the semiconductor device.
In accordance with a preferred embodiment of the present invention the method also includes using the misregistration measurement difference output to ameliorate parameters of the manufacturing process of the single batch of semiconductor devices intended to be identical from which the semiconductor device wafer is selected.
There is also provided in accordance with a preferred embodiment of the present invention a target for use in the measurement of misregistration in the manufacture of semiconductor device wafers and in the calibration of the measurements of misregistration, the target including at least a first structure arranged on a first layer of a semiconductor device wafer and at least a second and a third different structures arranged on a second layer of the semiconductor device.
Preferably, the second and third different structures are formed simultaneously, using identical fabrication tools and methods. Additionally or alternatively, at least one of the first, second and third structures is defined by a plurality of sub-lines and sub-spaces between the sub-lines, the sub-lines being characterized by a pitch.
In accordance with a preferred embodiment of the present invention the second structure is defined by a plurality of second structure sub-lines and a plurality of second structure sub-spaces having a second structure pitch, the third structure is defined by a plurality of third structure sub-lines and a plurality of third structure sub-spaces having a third structure pitch and the second structure pitch and the third structure pitch are different from one another.
In accordance with a preferred embodiment of the present invention the target is characterized by rotational symmetry. Additionally or alternatively, the first, second and third structures are periodic structures.
Preferably, the second and third structures overly the first periodic structure.
In accordance with a preferred embodiment of the present invention the first, second and third structures are bars. Alternatively, the first, second and third structures are rectangular boxes.
In accordance with a preferred embodiment of the present invention the target also includes at least a fourth structure and the first, second, third and fourth structures are characterized by rotational symmetry.
The present invention will be understood and appreciated more fully from the following detailed description, taken in conjunction with the drawings in which:
Reference is now made to
As seen in
Thereafter, at a next step 110, misregistration is measured at a second instance between two layers of a semiconductor device wafer and a second misregistration indication is provided.
It is appreciated that the semiconductor device wafer whose misregistration is measured in steps 100 and 110 may be identical. Alternatively, the semiconductor device wafer measured in the second instance may be a different wafer selected from the same BSDWII 102 from which the semiconductor device wafer measured in the first instance was selected.
It is further appreciated that the first and second layers of semiconductor device wafer whose misregistration is measured in steps 100 and 110 may be identical. Alternatively, at least one of the first and second layers of semiconductor device wafer measured in the second instance may be different from the first and second layers of the semiconductor device wafer measured in the first instance.
It is yet further appreciated that misregistration measurements in steps 100 and 110 may be measured either with identical measurement parameters or with different measurement parameters.
As seen at a next step 120, the difference between the misregistration measured in the first instance and the misregistration measured in the second instance is stored, and at a following step 122, a misregistration measurement difference output is generated by comparing the stored difference to a baseline difference output. In a preferred embodiment of the present invention, the baseline difference output represents a calculated compilation of differences between the first and second misregistration indications, such as an average or a mean. In a preferred embodiment of the present invention, such a calculated compilation of differences between first and second misregistration indications is obtained from first and second misregistration indications measured on previously processed semiconductor device wafers, which are selected from BSDWII 102.
At a subsequent step 130, the misregistration measurement difference output, in the form of the difference between the difference between the misregistration measured in the first instance and the misregistration measured in the second instance stored at step 120 and the baseline difference output used at step 122, is compared with a predetermined threshold.
As indicated at a subsequent step 132, if the misregistration measurement difference output of step 130 does not exceed the predetermined threshold, the method continues by checking if there are additional semiconductor device wafers to be processed, the method ends at a step 134. If additional semiconductor device wafers are to be processed, the method continues to a next step 140, whereat the regular fabrication and metrology proceeds for the next semiconductor wafer or wafers in BSDWII 102. As indicated by an arrow 142, the regular fabrication and metrology process includes repetitions of steps 100, 110, 120, 122 and 130.
As indicated at a subsequent step 150, if the misregistration measurement difference output exceeds the predetermined threshold, amelioration of either or both the wafer fabrication and the metrology takes place.
It is a particular feature of an embodiment of the present invention that the first and second instances referenced in the above description of
A plurality of compilations of differences between the misregistration indications 252, 254, 256 and 258 may be made in accordance with steps 120 and 130 described above with reference to
It is appreciated that any of misregistration indications 252, 254, 256 and 258 may be used to optimize misregistration measurement between layers of a semiconductor device in a later stage in the manufacturing process of BSDWII 102.
It is noted that target 300 preferably includes four sets 330 of periodic structures 302, 304 and 306. Each of sets 330 appears in target 300 in a different mutually orthogonal orientation, giving target 300 rotational symmetry. It is appreciated that other than their orientation, each of sets 330 of periodic structures 302, 304 and 306 are preferably identical to each other.
In a preferred embodiment of the present invention, periodic structures 302, 304 and 306 are each defined by a plurality of mutually parallel lines 340, 342 and 344, respectively, and mutually parallel spaces 346, 348 and 350 between respective mutually parallel lines 340, 342 and 346. Mutually parallel lines and spaces 340 & 346, 342 & 348 and 344 & 350 are arranged along axes 352, 354 and 356, respectively.
Preferably, lines 340, 342 and 346 have respective pitches C, D and E, each in the range of 1-3 μm and line widths which are 10%-90% of each respective pitch C, D or E, most typically 50% of C, D or E.
Lines 340, 342 and 346 are typically segmented, though they need not be. In an embodiment wherein lines 340, 342 and 346 are segmented, as seen in enlargement B of
Periodic structures 302, 304 and 306 may be distinguished from one another by any of their respective pitches C, D and E, their respective line widths and their segmentation pitches F, G and H, and most preferably by their segmentation pitches F, G and H.
It is a particular feature of an embodiment of the present invention that the first and second instances referenced in the above discussion of
It is appreciated that since periodic structures 304 and 306 are preferably formed together, any difference in misregistration indications between periodic structures 302 & 304 and 302 & 306 over a predetermined threshold indicates a need for amelioration in the misregistration metrology process.
It is noted that target 400 preferably includes four sets 430 of structures 402, 404 and 406. Each of sets 430 appears in target 400 in a different mutually orthogonal orientation, giving target 400 rotational symmetry. It is appreciated that other than their orientation, each of sets 430 of structures 402, 404 and 406 are preferably identical to each other. In a preferred embodiment of the present invention, structures 402, 404, and 406 are bars.
Preferably, structures 402, 404 and 406 have respective widths I, J and K, each in the range of 0.5-1.5 μm. Structures 402, 404 and 406 are typically segmented, though they need not be. In an embodiment wherein structures 402, 404 and 406 are segmented, as seen in enlargement B of
Structures 402, 404 and 406 may be distinguished from one another by any of their respective widths I, J and K and their segmentation pitches L, M and N, and most preferably by their segmentation pitches L, M and N.
It is a particular feature of an embodiment of the present invention that the first and second instances referenced in the above discussion of
It is appreciated that since structures 404 and 406 are preferably formed together, any difference in misregistration indications between structures 402 & 404 and 402 & 406 over a predetermined threshold indicates a need for amelioration in the misregistration metrology process.
Preferably, structures 502, 504 and 506 have respective widths O, P and Q, each in the range of 0.5-1.5 μm. Structures 502, 504 and 506 are typically segmented, though they need not be. In an embodiment wherein structures 502, 504 and 506 are segmented, as seen in enlargement B of
Structures 502, 504 and 506 may be distinguished from one another by any of their respective widths O, P and Q and their segmentation pitches R, S and T, and most preferably by their segmentation pitches R, S and T.
It is a particular feature of an embodiment of the present invention that the first and second instances referenced in the above discussion of
It is appreciated that since structures 504 and 506 are preferably formed together, any difference in misregistration indications between structures 502 & 504 and 502 & 506 over a predetermined threshold indicates a need for amelioration in the misregistration metrology process.
As seen particularly in
As seen particularly in
As seen particularly in
As seen in the embodiment illustrated in
Preferably, lines 640, 642 and 646, in periodic structures 602, 604 and 606, have respective pitches U, V and W, each in the range of 300 nm-1 μm and line widths which are 10%-90% of each respective pitch U, V and W, most typically 50% of U, V and W.
Lines 640, 642 and 646, in periodic structures 602, 604 and 606, are typically segmented, though they need not be. In an embodiment wherein lines 640, 642 and 646 are segmented, as seen in enlargement C of
Periodic structures 602, 604 and 606 may be distinguished from one another by any of their respective pitches U, V and W, their respective line widths and their segmentation pitches α, β and γ, and most preferably their segmentation pitches α, β and γ.
It is a particular feature of an embodiment of the present invention that the first and second instances referenced in the above discussion of
It is appreciated that since periodic structures 604 and 606 are preferably formed together, any difference in misregistration indications between periodic structures 602 & 604 and 602 & 606 over a predetermined threshold indicates a need for amelioration in the misregistration metrology process.
It is further appreciated that structures 701, 702, 704 and 706 may be any structures characterized by rotational symmetry. It is further appreciated that while target 700 is shown in
Structures 701, 702, 704 and 706 are typically segmented, though they need not be. In an embodiment wherein structures 701, 702, 704 and 706 are segmented, as seen in enlargement
It is a particular feature of an embodiment of the present invention that the first and second instances referenced in the above discussion of
It is appreciated that since each of pairs of structures 701 &702 and 704 & 706 are preferably each formed together, any difference in misregistration indications between structures 701 & 704 and 702 & 706 over a predetermined threshold indicates a need for amelioration in the misregistration metrology process.
Reference is now made to
It is appreciated that method 800, described hereinbelow, is performed as part of step 150, of the method described in
As seen at a first step 804, method 800 ascertains if the first and second misregistration indications are post-lithography misregistration indication 252 and post-mask open misregistration indication 254.
If the first and second misregistration indications are post-lithography misregistration indication 252 and post-mask open misregistration indication 254, method 800 proceeds to next step 806 whereat mask opening stage 204 is modified in preparation of processing of further semiconductor device wafers. For example, etching depth of the mask opening stage may be modified or material properties such as index of refraction or dielectric constant of the layers measured may be modified.
If the first and second misregistration indications are not post-lithography misregistration indication 252 and post-mask open misregistration indication 254, method 800 proceeds to a next step 808 at which method 800 ascertains if the first and second misregistration indications are post-lithography misregistration indication 252 and post-etch misregistration indication 256.
If the first and second misregistration indications are post-lithography misregistration indication 252 and post-etch misregistration indication 256, method 800 proceeds to next step 810 whereat etching stage 206 is modified in preparation of processing of further semiconductor device wafers. For example, etching time may be modified or material properties such as index of refraction or dielectric constant of the layers measured may be modified.
If the first and second misregistration indications are not post-lithography misregistration indication 252 and post-etch misregistration indication 256, method 800 proceeds to a next step 812 at which method 800 ascertains if the first and second misregistration indications are post-mask open misregistration indication 254 and post-etch misregistration indication 256.
If the first and second misregistration indications are post-mask open misregistration indication 254 and post-etch misregistration indication 256, method 800 proceeds to next step 814 whereat etching stage 206 is modified in preparation of processing of further semiconductor device wafers. For example, etching time may be modified or material properties such as index of refraction or dielectric constant of the layers measured may be modified.
If the first and second misregistration indications are not post-mask open misregistration indication 254 and post-etch misregistration indication 256, method 800 proceeds to a next step 816 at which method 800 ascertains if the first and second misregistration indications are post-lithography misregistration indication 252 and post-polish misregistration indication 258.
If the first and second misregistration indications are post-lithography misregistration indication 252 and post-polish misregistration indication 258, method 800 proceeds to next step 818 whereat at least one of etching stage 206 and polishing stage 208 is modified in preparation of processing of further semiconductor device wafers. For example, any of etching time, polish time, polish angle and materials used in the polishing stage may be adjusted or material properties such as index of refraction or dielectric constant of the layers measured may be modified.
If the first and second misregistration indications are not post-lithography misregistration indication 252 and post-polish misregistration indication 258, method 800 proceeds to a next step 820 at which method 800 ascertains if the first and second misregistration indications are post-mask open misregistration indication 254 and post-polish misregistration indication 258.
If the first and second misregistration indications are post-mask open misregistration indication 254 and post-polish misregistration indication 258, method 800 proceeds to next step 822 whereat polishing stage 208 is modified in preparation of processing of further semiconductor device wafers. For example, any of polish time, polish angle and materials used in the polishing stage may be adjusted or material properties such as index of refraction or dielectric constant of the layers measured may be modified.
If the first and second misregistration indications are not post-mask open misregistration indication 254 and post-polish misregistration indication 258, method 800 proceeds to a next step 824 at which method 800 ascertains if the first and second misregistration indications are post-etch misregistration indication 256 and post-polish misregistration indication 258.
If the first and second misregistration indications are post-etch misregistration indication 256 and post-polish misregistration indication 258, method 800 proceeds to a next step 826 whereat polishing stage 208 is modified in preparation of processing of further semiconductor device wafers. For example, any of polish time, polish angle and materials used in the polishing stage may be adjusted or material properties such as index of refraction or dielectric constant of the layers measured may be modified.
Reference is now made to
It is appreciated that method 900, described below, is performed as part of step 150, of the method described in
As seen at a first step 902, method 900 ascertains if non-zero offset (NZO) calibration should be performed. If NZO calibration should be performed, for example, in embodiments described hereinabove with reference to
If NZO calibration should not be performed, method 900 proceeds to a next step 908, wherein method 900 ascertains if the first and second misregistration indications are post-lithography misregistration indication 252 and post-mask open misregistration indication 254.
If the first and second misregistration indications are post-lithography misregistration indication 252 and post-mask open misregistration indication 254, method 900 proceeds to next step 910 whereat at least one of post-lithography and post-mask open misregistration measurement parameters are modified.
For example, region of interest at which misregistration is measured, wavelength of light utilized in misregistration measurement, polarization of light utilized in misregistration measurement, numerical aperture, diffraction mask and diffraction aperture may be adjusted to reduce the difference between post-lithography misregistration indication 252 and post-mask open misregistration indication 254. As an additional example, outlying measurement results may be identified and removed from misregistration measured at at least one of post-lithography and post-mask open misregistration measurements.
If the first and second misregistration indications are not post-lithography misregistration indication 252 and post-mask open misregistration indication 254, method 900 proceeds to a next step 912 at which method 900 ascertains if the first and second misregistration indications are post-lithography misregistration indication 252 and post-etch misregistration indication 256.
If the first and second misregistration indications are post-lithography misregistration indication 252 and post-etch misregistration indication 256, method 900 proceeds to next step 914 whereat at least one of post-lithography and post-etch misregistration measurement parameters are modified.
For example, region of interest at which misregistration is measured, wavelength of light utilized in misregistration measurement, polarization of light utilized in misregistration measurement, numerical aperture, diffraction mask and diffraction aperture may be adjusted to reduce the difference between post-lithography misregistration indication 252 and post-etch misregistration indication 256. As an additional example, outlying measurement results may be identified and removed from misregistration measured at at least one of post-lithography and post-etch misregistration measurements.
If the first and second misregistration indications are not post-lithography misregistration indication 252 and post-etch misregistration indication 256, method 900 proceeds to a next step 916 at which method 900 ascertains if the first and second misregistration indications are post-mask open misregistration indication 254 and post-etch misregistration indication 256.
If the first and second misregistration indications are post-mask open misregistration indication 254 and post-etch misregistration indication 256, method 900 proceeds to next step 918 whereat at least one of post-mask open and post-etch misregistration measurement parameters are modified.
For example, region of interest at which misregistration is measured, wavelength of light utilized in misregistration measurement, polarization of light utilized in misregistration measurement, numerical aperture, diffraction mask and diffraction aperture may be adjusted to reduce the difference between post-mask open misregistration indication 254 and post-etch misregistration indication 256. As an additional example, outlying measurement results may be identified and removed from misregistration measured at at least one of post-mask open and post-etch misregistration measurements.
If the first and second misregistration indications are not post-mask open misregistration indication 254 and post-etch misregistration indication 256, method 900 proceeds to a next step 920 at which method 900 ascertains if the first and second misregistration indications are post-lithography misregistration indication 252 and post-polish misregistration indication 258.
If the first and second misregistration indications are post-lithography misregistration indication 252 and post-polish misregistration indication 258, method 900 proceeds to next step 922 whereat at least one of post-lithography and post-polish misregistration measurement parameters are modified.
For example, region of interest at which misregistration is measured, wavelength of light utilized in misregistration measurement, polarization of light utilized in misregistration measurement, numerical aperture, diffraction mask and diffraction aperture may be adjusted to reduce the difference between post-lithography misregistration indication 252 and post-polish misregistration indication 258. As an additional example, outlying measurement results may be identified and removed from misregistration measured at at least one of post-lithography and post-polish misregistration measurements.
If the first and second misregistration indications are not post-lithography misregistration indication 252 and post-polish misregistration indication 258, method 900 proceeds to a next step 924 at which method 900 ascertains if the first and second misregistration indications are post-mask open misregistration indication 254 and post-polish misregistration indication 258.
If the first and second misregistration indications are post-mask open misregistration indication 254 and post-polish misregistration indication 258, method 900 proceeds to next step 926 whereat at least one of post-mask open and post-polish misregistration measurement parameters are modified.
For example, region of interest at which misregistration is measured, wavelength of light utilized in misregistration measurement, polarization of light utilized in misregistration measurement, numerical aperture, diffraction mask and diffraction aperture may be adjusted to reduce the difference between post-mask open misregistration indication 254 and post-polish misregistration indication 258. As an additional example, outlying measurement results may be identified and removed from misregistration measured at at least one of post-mask open and post-polish misregistration measurements.
If the first and second misregistration indications are not post-mask open misregistration indication 254 and post-polish misregistration indication 258, method 900 proceeds to a next step 928 at which method 900 ascertains if the first and second misregistration indications are post-etch misregistration indication 256 and post-polish misregistration indication 258.
If the first and second misregistration indications are post-etch misregistration indication 256 and post-polish misregistration indication 258, method 900 proceeds to a next step 930 whereat at least one of post-etch and post-polish misregistration measurement parameters are modified.
For example, region of interest at which misregistration is measured, wavelength of light utilized in misregistration measurement, polarization of light utilized in misregistration measurement, numerical aperture, diffraction mask and diffraction aperture may be adjusted to reduce the difference between post-etch misregistration indication 256 and post-polish misregistration indication 258. As an additional example, outlying measurement results may be identified and removed from misregistration measured at at least one of post-etch and post-polish misregistration measurements.
It will be appreciated by persons skilled in the art that the present invention is not limited to what has been particularly shown and described hereinabove. The scope of the present invention includes both combinations and subcombinations of various features described hereinabove as well as modifications thereof, all of which are not in the prior art.
This application is a continuation of U.S. application Ser. No. 16/467,968 filed Jun. 8, 2019, which is a national stage application of PCT/US19/30776 filed May 6, 2019, which claims priority to the provisional patent application U.S. App. No. 62/825,262 filed Mar. 28, 2019, the disclosures of which are hereby incorporated by reference.
Number | Date | Country | |
---|---|---|---|
62825262 | Mar 2019 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 16467968 | Jun 2019 | US |
Child | 17688856 | US |