The present application relates to a method for repairing parts, and more particularly, relates to a method for repairing parts composed of superalloys.
Superalloys are used for various components in gas turbine engines where the components are exposed to high temperatures and pressures for extended periods of time. A typical application is high pressure turbine vanes, where the temperature of the component can rise to about 2000° F. Under these conditions, the component is expected to retain its shape and strength long enough to provide economical operation of the engine without unduly frequent service or replacement requirements.
Typically, superalloy components have been produced by precision casting, which provides a near-net shape component requiring only minimal machining operations to reach final configuration. To provide additional protection for the material from the high temperatures and corrosive environment due to combustion processes, a protective coating is commonly applied. Components with adequate properties for the desired applications have been successfully produced with no heat treatment other than the heating cycle incurred as part of the coating process, which is effectively a precipitation heat treatment of the as-cast material.
Frequently expensive gas turbine engine components, like superalloy turbine blades and vanes, are found with small defects resultant from the casting processes or develop small cracks during engine service. After extended service, some of these components may also incur damage, due to erosion, thermal mechanical fatigue-induced cracking caused by the frequent cycling between ambient and operating temperatures, or creep, which causes the airfoil portions of the turbine blades and vanes to bow or the platform portions of the component to twist away from their original positions, with a resultant change in the operational characteristics of the components. Although such defects may be relatively small, they are often sufficient to cause rejection of the component. In many instances, however, the defect is of such a nature that repairs would be satisfactory. However, lacking a suitable means for reliably repairing such defects, these components are often scrapped.
In an attempt to salvage such parts, many repair techniques have been attempted in the past. For example, although repair by fusion welding has occasionally been successful, its success tends to be sporadic, and the welding technique itself often produces additional cracking due to the typical high crack sensitivity of the cast superalloys.
Brazing procedures have also been utilized in attempts to repair defective turbine components. One method has been to simply flow molten brazing material into an existing crack. At times, oxides or other contaminants may yet still remain in the cracks due to tight or partially closed crevice areas which can prevent complete filling. In such cases, although the cracks may be sealed at the surface, no assurance can be provided that subsurface cracks will be sealed as well. This is, of course, not only detrimental but difficult to detect as well.
A more satisfactory approach to component repair is to first eliminate the cracks by mechanically routing out the entire defective area and then refilling it. However, when braze alloys are employed as the filler for such relatively large volumes; upon solidification they often form quantities of eutectic phases which are weak, brittle and prone to adverse selective oxidation during subsequent component service.
Although the desirability of effecting component repairs has long been evident, it is apparent that no satisfactory repair techniques exist, particularly where such repairs can be made reproducibly and reliably.
A method for repairing parts comprises applying a first repair material in an amount sufficient to fill at least a first portion of a part; welding the first repair material in the portion of the part; blending the first repair material with a contour of the part; inspecting the part; brazing a second repair material in a second portion of the part; blending the second repair material with the contour of the part; and inspecting the part.
A method for repairing parts comprising superalloys comprises applying a first repair material in an amount sufficient to fill at least a first portion of a part, wherein the first portion comprises a depleted area having a depth of greater than about 0.030 inches; welding the first repair material in the portion of the part; blending the first repair material with a contour of the part; inspecting the part; brazing a second repair material in a second portion of the part, wherein the second portion comprises a depleted area having a depth of no more than about 0.030 inches; blending the second repair material with the contour of the part; and inspecting the part.
The details of one or more embodiments of the invention are set forth in the accompanying drawings and the description below. Other features, objects, and advantages of the invention will be apparent from the description and drawings, and from the claims.
Like reference numbers and designations in the various drawings indicate like elements.
The method(s) for repairing a part comprising a superalloy are described herein. The method described herein combines both welding and brazing steps in order to effectively, reproducibly and reliably seal surface and subsurface defects while also removing oxides and other contaminants.
The method of the present invention generally comprises prepping a part having one or more defects in order to receive a repair material. The repair material is applied to the defect, and then welded. The welded repair material is blended to the contour of the part and inspected for additional defects. Upon finding additional defects in the part, a second repair material is applied and the defect and repair material are brazed. The second repair material is then blended to the contour of the part and inspected again for additional defects.
Referring generally now to
Upon determining the routing step removed the defect(s) from that portion, a repair material 14 is applied to fill at least the routed portion of the part as shown in the photograph of
Once the first repair material is applied to the routed portion and surrounding area, the material is welded using a welding method known to one of ordinary skill in the art. Preferably, a gas tungsten arc welding method or laser welding method under inert atmospheric conditions is utilized. The weld formed encompasses the filled in routed portion along with the area surrounding the welded portion. The welded portion and surrounding area may then be blended to the contour of the part. The contour of the part generally constitutes the shape and features originally present. Blending the welded portion may be accomplished using any method known to one of ordinary skill in the art including but not limited to milling, grinding, sanding, super-abrasive machining, and combinations comprising at least one of the foregoing methods. Preferably, the welded area is blended by manually grinding or super-abrasive machining the area until the welded portion and surrounding area conform to the contour of the part. In the alternative, a preform may be utilized in order to accurately restore the welded portion and surrounding area to the original contour of the part. The preform may be applied to the surface of the part including the welded portion prior to blending the welded portion and surrounding area.
Upon completing the welding and blending steps, the part may be inspected to determine whether any cracks, subsurface cracks and/or microcracks still remain in the areas where the first repair material was welded and blended. Preferably, a fluorescent penetration inspection of the part is performed as is known to one of ordinary skill in the art as shown in the photograph of
As described earlier, the second portions of the part having defects comprising a depth of less than 0.030 inches are routed. Once routed, the part may be cleaned by any method known to one of ordinary skill in the art. Preferably, the part is submersed in a hydrogen fluoride bath to remove contaminants and prevent oxidation from occurring in the routed second portions of the part. After being cleaned, a second repair material may be applied to the second routed portions of the part. Preferably, the amount of second repair material applied is sufficient to fill the routed second portion and leave extra repair material in and around the localized area. For example, the amount of repair material may comprise enough material to fill and overflow a surface defect having a depth of about 0.10 inch. The repair material may be applied using any conventional methods known to one of ordinary skill in the art. This second repair material may comprise any nickel-based alloy, and preferably comprises Turbofix® braze repair formula, a transient liquid phase bonding alloy (“TLP”), as described in U.S. Pat. No. 4,008,844 to Duvall, assigned to United Technologies Corporation, and incorporated by reference herein in its entirety.
For repair of the superalloys, preferably the TLP alloy is employed in the form of homogenous powder. This powder comprises an alloy substantially corresponding in composition to at least the major constituents of the substrate material, excluding therefrom any elements known to form deleterious phases which may interfere with character of the finished repair area, and typically containing 1-3 percent boron, as the temperature depressant element. This TLP powder is thoroughly blended with the correct proportion of homogeneous metal powder of the substrate material composition, forming the filler powder mix. Substrate powder/TLP powder ratios of 2-9/1 have been used. This filler powder mix is placed in the void to be filled and the component is heated to the bonding temperature. When the TLP powder melts, it wets and flows around the base metal powder particles and throughout the repair area, completely filling it. The remaining, unmelted substrate powders assist and accelerate the isothermal solidification by acting, as previously described, as local diffusion sinks for the melting point depressant (e.g. boron) in the TLP alloy. Once the repair area has completely solidified, the substrate metal powders further aid in subsequent homogenization by providing short-range distances for mutual diffusion between materials of the TLP and substrate metal compositions.
Preferably, the second repair material comprises a Turbofix® braze repair formula comprises a nickel-based powder in an amount of about fifty percent by weight of the material and a bonding alloy in an amount of about fifty percent by weight of the material. The nickel-based powder is preferably INI-939 powder, and the bonding alloy is preferably PWA 1180 powder. At the completion of the homogenization cycle, the surface of the part may be restored by blending the brazed portion 20 to the desired or original contour as shown in
Upon completing the brazing step as shown in the photograph of
It is to be understood that the invention is not limited to the illustrations described and shown herein, which are deemed to be merely illustrative of the best modes of carrying out the invention, and which are susceptible to modification of form, size, arrangement of parts, and details of operation. The invention rather is intended to encompass all such modifications which are within its spirit and scope as defined by the claims.