The present disclosure relates to a method of forming an alloy thin film using an atomic layer deposition (ALD) process including an optimal unit process, and an electronic element manufactured using the same, and more specifically, to a method of forming an alloy thin film using an ALD process including an optimal unit process in a super-cycle ALD process, and an electronic element manufactured using the same.
When an alloy thin film is formed in the related art, an atomic layer deposition (ALD) process should be first performed with a unit material constituting the thin film, it is difficult to deposit a metal thin film including a highly reactive element (such as Ti, Ta, or Al), and it is possible to deposit only materials with high oxidation resistance. Accordingly, there is a limitation in that the scope of technical application is limited to chemically stable materials such as oxides, nitrides, and precious metals.
For example, conventionally, in order to deposit a thin film including two or more types of metal atoms through an ALD process, a super-cycle ALD process in which two or more ALD unit processes are continuously performed in an alternating sequence to form a thin film has been mainly used. However, when a super-cycle ALD is used, two or more ALD unit processes included in the super-cycle ALD process should be first developed, and thus it is impossible to form an alloy thin film including low work function metals such as aluminum (Al), tantalum (Ta), and titanium (Ti), for which it is difficult to develop an ALD-based unit process. Accordingly, an oxide or nitride of low work function metals, which are relatively easy to deposit, are being used as substitutes, but inevitably cause an increase in impurities in a thin film and a degradation in physical and electrical properties.
In addition, when a metal thin film is deposited according to the related art, due to the characteristics of metal materials having high surface energy, an island growth phenomenon in which separate nuclei are generated and grow in the early stage of growth inevitably occurs. Therefore, in order for nuclei to be grown and connected to form a thin film, a thickness of a certain level or more is required, which acts as a critical limiting factor in forming a thin metal film.
The present disclosure is directed to providing a method of forming an alloy thin film using an atomic layer deposition (ALD) process including an optimal unit process in which a unit process used in an existing super-cycle ALD process is optimized to design and cause a surface reaction that is advantageous for thin film formation, thereby forming an alloy film with low impurity concentration and excellent physical and electrical properties using the same material and device as before, and an electronic element manufactured using the same.
According to an aspect of the present disclosure, there is provided a method of forming an alloy thin film including a low work function metal through an ALD process, the method including performing a first unit process of forming an oxide or nitride of a low-work function metal, and performing a second unit process of forming a film of a different type metal on the oxide or nitride, wherein the second unit process includes (a) injecting a precursor of a source of the different type metal for a first time, (b) injecting a purge gas, (c) injecting a reactant, and (d) injecting a purge gas, and the second unit process further includes, prior to the injecting of the precursor of the source of the different type metal, injecting the precursor of the source of the different type metal for a second time to reduce the low work function metal.
The second time may be substantially the same as the first time.
The injecting for the second time may include effectively removing oxygen present in a form of an OH functional group on a surface of the low work function metal immediately after the first unit process.
The injecting for the second time may include sufficiently removing oxygen combined with the low work function metal immediately after the first unit process to allow the alloy thin film to have a low resistivity of 3.5 mΩ·cm or less.
The injecting for the second time may include optimizing a surface reaction of the film of the different type metal and an oxide thin film of the low work function metal to convert the oxide thin film of the low work function metal from an insulating chemical state to a conductive metal sub-oxide.
The oxide thin film of the low work function metal may be continuously formed with respect to the film of the different type metal undergoing island growth to electrically connect islands of the film of the different type metal and then induce layer-by-layer growth of the film of the different type metal deposited thereon to improve continuity of the film itself of the different type metal.
The injecting for the second time may include optimizing a surface reaction of the film of the different type metal and an oxide thin film of the low work function metal to reduce an oxidation number of the low work function metal in the oxide thin film of the low work function metal.
The source of the different type metal may be selected from Ru, Pt, Ir, Ag, Au, Mo, and Co. In addition to the materials listed, the source of the different type metal may be selected from any material capable of metal deposition.
The first unit process may include injecting a precursor of the low work function metal source, injecting a purge gas, injecting a reactant, and injecting a purge gas.
The low work function metal source may be selected from Ti, Al, Ta, Hf, Zr, Nb, Sn, Mo, Pt, Ru, and Ir. In addition to the materials listed, the low work function metal source may be selected from any material that can be deposited by ALD.
According to another aspect of the present disclosure, there is provided a method of forming an alloy thin film including a low work function metal through an ALD process, the method including performing a first unit ALD process of forming an oxide of a low-work function metal, and performing a second unit ALD process of forming a film of different type metal on the oxide, wherein the second unit ALD process includes injecting a subsequent precursor to form a sub-oxide of the low work function metal.
According to still another aspect of the present disclosure, there is provided an electronic element including an alloy thin film manufactured through the method of forming an alloy thin film including a low work function metal through a super-cycle ALD process.
The above and other objects, features and advantages of the present disclosure will become more apparent to those of ordinary skill in the art by describing exemplary embodiments thereof in detail with reference to the accompanying drawings, in which:
The advantages and features of the present disclosure and methods of accomplishing the same will become apparent from the following description of embodiments in detail, taken in conjunction with the accompanying drawings. However, the present disclosure is not limited to the embodiments disclosed herein but will be implemented in various forms. The embodiments are provided so that the present disclosure is completely disclosed, and a person of ordinary skilled in the art can fully understand the scope of the present disclosure. Therefore, the present disclosure will be defined only by the scope of the appended claims. Like reference numerals refer to like elements throughout the specification.
Terms used herein are for the purpose of describing embodiments only and are not intended to limit the present disclosure. As used herein, the singular forms are intended to include the plural forms as well, unless the context clearly indicates otherwise. It will be further understood that the terms “comprise” and/or “comprising” used in this specification specify the presence of stated components, steps, operations, and/or elements, but do not preclude the presence or addition of one or more other components, steps, operations, and/or elements thereof.
In addition, embodiments described herein will be described with reference to cross-sectional views and/or plan views which are ideal exemplary views of the present disclosure. In drawings, thicknesses of films and regions are exaggerated for effective description of technical contents. Therefore, the form of the exemplary views may be modified by manufacturing techniques and/or tolerances, an allowable error, or the like. Therefore, the embodiments of the present disclosure are not limited to a specific form which is shown but include variations according to the manufacturing process. For example, an etching region shown at a right angle may be rounded or have a shape with a certain curvature. Accordingly, the regions illustrated in the drawings are schematic in nature, and the shapes of the regions illustrated in the drawings are intended to illustrate the specified shape of a region of a device and are not intended to limit the scope of the present disclosure.
In a method of forming an alloy thin film according to an embodiment of the present disclosure, in a super-cycle atomic layer deposition (ALD) process, a unit process is performed for forming a thin film of compounds such as an oxide and a nitride that are easy to deposit to form a thin film, and impurities such as oxygen and nitrogen are removed by optimizing a subsequent unit process in consideration of a surface reaction. Thus, without a deposition process of a single metal that is difficult to deposit, an alloy thin film including the single metal can be deposited. According to the present disclosure, while the same material and device used in the conventional ALD process are used, material limitations are overcome through surface reaction control, and an alloy thin film, which is difficult to form with existing technologies, can be deposited.
As described above, conventionally, in order to deposit a thin film including two or more types of metal atoms through an ALD process, a super-cycle ALD process in which two or more ALD unit processes are continuously performed in an alternating sequence to form a thin film has been mainly used. However, when a super-cycle ALD process is used, two or more ALD unit processes included in the super-cycle ALD process should be first developed, and thus it is impossible to form an alloy thin film including low work function metals such as aluminum (Al), tantalum (Ta), and titanium (Ti), for which it is difficult to develop an ALD-based unit process. Accordingly, an oxide or nitride of low work function metals, which are relatively easy to deposit, are being used as substitutes, but inevitably cause an increase in impurities in a thin film and a degradation in physical and electrical properties.
According to the present disclosure, a precursor injection time of unit processes that constitute a super-cycle ALD process is optimized to maximize a surface reaction between unit processes, thereby removing oxygen and nitrogen from a thin film of a low work function metal oxide and nitride. In this case, a precursor injection operation in the unit process includes a precursor injection operation of reducing a lower film in addition to existing precursor injection. As a result, an alloy thin film in which oxygen or nitrogen impurities are minimized in the thin film may be formed through a super-cycle ALD process using an ALD process for a low work function metal compound. In addition, when a metal thin film is deposited according to the related art, due to the characteristics of metal materials having high surface energy, an island growth phenomenon in which separate nuclei are generated and grow in the early stage of growth inevitably occurs. Therefore, in order for nuclei to be grown and connected to form a thin film, a thickness of a certain level or more is required, which acts as a critical limiting factor in forming a thin metal film. According to the present disclosure, a thin film in the form of oxide and nitride, which are very easy to deposit as compared to pure metals, may be used in a process to improve the continuity of the thin film, thereby forming a thin film having high conductivity even at a very thin thickness. In addition, the electrical properties of the thin film can be freely controlled according to the properties and composition of each metal that constitutes the thin film.
According to the present disclosure, by optimizing an ALD precursor injection time in consideration of an interaction between unit processes constituting a super-cycle ALD process, even while an ALD-based alloy thin film, which has been impossible to form with the related art, is formed, and since the same process sequence and material as the related art are used, there has a special advantage in that additional devices or materials are not required for application of the present disclosure. These features may be suitable for next-generation products, which are currently undergoing extreme miniaturization, in the semiconductor industry and may contribute to securing future market competitiveness.
Since a super-cycle ALD process according to an embodiment of the present disclosure relates to a method of forming an alloy thin film including a low work function metal, and in the present disclosure, may be referred to as a method of forming an alloy thin film including a low work function metal through a super-cycle ALD process. In addition, the super-cycle ALD process may include an optimal unit process and thus may be referred to as a method of forming an alloy thin film using ALD including an optimal unit process. However, hereinafter, for convenience of description, a super-cycle ALD process will be referred to.
Referring to
More specifically, as shown in
According to an embodiment of the present disclosure, the operation Ru′ of injecting the additional Ru precursor and the operation Ru of injecting the Ru precursor may use the same precursor, and thus the same process may be performed for a longer time. Although both the operation Ru′ and the operation Ru may be separate processes, since the operation Ru′ and the operation Ru use the same precursor, it is more advantageous to perform one process for a long time. Each operation may have a certain duration time, and when a duration time of the operation Ru of injecting the Ru precursor is assumed to be a first time, a duration time of the operation Ru′ of injecting the additional Ru precursor may be a second time. Considering the temporal order, the second time is a time that is earlier than the first time, but for the sake of comparison with
In the first unit process, TaCl4, TaBr4, TaF4, t-butylimino-tris(diethylamino)tantalum (TBTDET), pentakis(ethylmethylamino)tantalum (PEMAT), pentakis(dimethylamino)tantalum (PDMAT), pentakis(diethylamino)tantalum (PDEAT), tertiary amyl imido-tris-dimethylamido tantalum (TAIMATA), or the like may be used as the Ta precursor, in addition to N2, an inert gas such as Ar, Ne, He, or H2 may be used as the purge gas, and H2O, H2O2, O2, O3, NH3, H2, N2, tBuNH2, AyNH2, Me2NNH2, or a mixed gas thereof may be used as the reactant.
In the second unit process, Ru(EtCp)2, Ru(i-PrCp)2, RuCp2, Ru(OD)3, Ru(THD)3, Ru(THD)2COD, Ru(MeCp)2, RuCl3, CpRu(CO)3, Ru3(CO)12, Ru(acac)3, dicarbonyl-bis(5-methyl-2,4-hexane-diketonato)Ru(II) (Carish), Ru2{μ2-η3—N(tBu)—C(H)—C(iPr)}(CO)6 (T-Rudic), or the like may be used as the Ru precursor, in addition to N2, an inert gas such as Ar, Ne, or He, or H2 may also be used as the purge gas, and O2, O3, H2O, H2O2, NH3, H2, N2, tBuNH2, AyNH2, Me2NNH2, or a mixed gas thereof may be used as the reactant.
Meanwhile, in the embodiments of
Referring to
In an embodiment of the present disclosure, considering the ECT and the resistivity at the ECT, a Ru—Ta thin film having a cycle ratio of about 1:8 to 1:9 may have the lowest resistivity at a thickness of about 2.2 nm, which corresponds to an optimal process for use in the application field according to the embodiment of the present disclosure presented above. Meanwhile, since physical properties change according to a composition of a deposited thin film, when applied to other fields, a process with a different cycle ratio may be used as an optimal process according to the purpose of a thin film.
Meanwhile, in the embodiment of the present disclosure, description has been provided using Ru, but since island growth is a phenomenon that commonly occurs when most metal films are formed, the embodiment of the present disclosure may be applied when all metal films of Pt, Ir, Ag, Au, Mo, and Co as well as Ru are formed.
In addition, the above-described embodiment is an example of a Ru—Ta thin film using Ru and Ta2O5, but since the present disclosure relates to a method of controlling a surface reaction between unit processes, the scope of application is not limited to the above-described materials, and any material such as Ti, Al, Ta, Hf, Zr, Nb, Sn, Mo, Pt, Ru, or Ir, and an oxide and nitride thereof may be used. Additionally, the order in which the unit processes are performed may be changed in various ways in consideration of surface reactions.
The method of forming an alloy thin film according to the embodiment of the present disclosure described above can be applied to all electronic devices such as logic circuits, display devices, memory devices, and sensors, and all devices to which an ALD process is used. The method can be applied to transistors, dynamic random access memories (DRAMs), NAND flash memories, and various sensors. In addition, a method of forming an alloy thin film using an ALD process including an optimal unit process according to an embodiment of the present disclosure can be applied to all ALD processes of a super-cycle ALD type including two or more unit processes. In addition, the method of forming an alloy thin film using an ALD process including an optimal unit process according to the embodiment of the present disclosure may be an ALD process including a process optimization operation in which a surface reaction between unit processes is considered when a super-cycle ALD process is performed. In addition, the method of forming an alloy thin film using an ALD process including an optimal unit process according to the embodiment of the present disclosure may be an ALD process including a subsequent precursor injection operation of forming a metal sub-oxide when a super-cycle ALD process is performed. In addition, the method of forming an alloy thin film using an ALD process including an optimal unit process according to the embodiment of the present disclosure may be a thin film manufacturing process in which materials having both high surface energy and conductivity which are advantageous in forming a metal thin film, are mixed and used when thin film is formed.
According to the present technology, a unit process used in an existing super-cycle ALD process is optimized to design and cause a surface reaction that is advantageous for thin film formation, thereby forming an alloy film with low impurity concentration and excellent physical and electrical properties using the same material and device as before.
In addition, since the present technology uses the same material and device as existing technologies, the present technology has broad potential for immediate application without separate device investment.
Although the technical idea of the present disclosure has been described in detail according to the above-described exemplary embodiments, it should be noted that the above embodiments are intended to illustrate the present disclosure, not to limit the scope of the present disclosure. Additionally, a person skilled in the art will appreciate that various embodiments are possible within the scope of the technical idea of the present disclosure.
| Number | Date | Country | Kind |
|---|---|---|---|
| 10-2022-0089008 | Jul 2022 | KR | national |
| 10-2022-0126372 | Oct 2022 | KR | national |
This application is a continuation of pending PCT International Application No. PCT/KR2023/010338, which was filed on Jul. 19, 2023, and which claims priority to and the benefit of Korean Patent Application No. 10-2022-0089008, which was filed in the Korean Intellectual Property Office on Jul. 19, 2022, and Korean Patent Application No. 10-2022-0126372, which was filed in the Korean Intellectual Property Office on Oct. 4, 2022, the disclosures of which are incorporated herein by reference in their entirety.
| Number | Date | Country | |
|---|---|---|---|