Claims
- 1. A method of manufacturing a solid optical fiber preform in which disturbance of the refractive index profile is substantially avoided, said method consisting essentially of the steps of:
- providing a hollow optical fiber preform having a longitudinal direction, said hollow preform having an inside wall bounding a central duct, the central duct extending in the longitudinal direction, the inside wall portion of the hollow preform comprising quartz glass doped with a dopant, said dopant being more volatile than quartz glass;
- heating the hollow preform to a temperature at which the duct closes spontaneously to form a solid preform; and
- passing a gaseous etchant through the central duct while the duct is closing, said gaseous etchant consisting of oxygen and 5-30 volume percent C.sub.2 F.sub.6.
- 2. A method as claimed in claim 1, wherein:
- the step of passing the etchant through the duct is started when the duct has closed to a diameter approximately equal to one millimeter; and
- the method further comprises the step of passing oxygen through the duct while the duct is closing and until the diameter of the duct is approximately equal to one millimeter.
- 3. A method as claimed in claim 1, wherein the oxygen content of the gaseous etchant is 70-90% by volume.
- 4. A method as claimed in claim 1, wherein the pressure of the gaseous etchant in the central duct when the duct is closing is approximately equal to atmospheric pressure.
- 5. A method as claimed in claim 1, wherein the gaseous etchant is passed through the closing duct at a rate of 50 to 60 sccm.
- 6. A method of manufacturing a solid optical fiber preform in which disturbance of the refractive index profile is substantially avoided, said method consisting essentially of the steps of:
- providing a hollow optical fiber preform having a longitudinal direction, said hollow preform having an inside wall bounding a central duct, the central duct extending in the longitudinal direction, the inside wall portion of the hollow preform comprising quartz glass doped with a dopant, said dopant being more volatile than quartz glass;
- heating the hollow preform to a temperature at which the duct closes spontaneously to form a solid preform; and
- passing a gaseous etchant through the central duct after the duct has closed to a diameter approximately equal to one millimeter and while the duct is closing, said gaseous etchant consisting of oxygen and 5-30 volume percent and C.sub.2 F.sub.6.
- 7. A method as claimed in claim 6, wherein the oxygen content of the gaseous etchant is 70-90% by volume.
- 8. A method as claimed in claim 6, wherein the pressure of the gaseous etchant in the central duct when the duct is closing is approximately equal to atmospheric pressure.
- 9. A method as claimed in claim 6, wherein the gaseous etchant is passed through the closing duct at a rate of 50 to 60 sccm.
- 10. A method of manufacturing a solid optical fiber preform in which disturbance of the refractive index profile is substantially avoided, said method comprising the steps of:
- providing a hollow opitcal fiber preform having a longitudinal direction, said hollow preform having an inside wall bounding a central duct, the central duct extending in the longitudinal direction, the inside wall portion of the hollow preform comprising quartz glass dopoed with a dopant, said dopant being more volatile than quartz glass;
- heating the hollow preform to a temperature at which the duct closes spontaneously to form a solid preform; and
- passing a gaseous etchant through the central duct while the duct is closing, said gaseous etchant consisting of 48 sccm oxygen and 10 sccm C.sub.2 F.sub.6.
- 11. A method of manufacturing a solid optical fiber preform in which disturbance of the refractive index profile is substantially avoided, said method comprising the steps of:
- providing a hollow optical fiber preform having a longitudinal direction, said hollow preform having an inside wall bounding a central duct, the central duct extending in the longitudinal direction, the inside wall portion of the hollow preform comprising quartz glass doped with a dopant, said dopant being more volatile than quartz glass;
- heating the hollow preform to a temperature at which the duct closes spontaneously to form a solid preform; and
- passing oxygen through the central duct while said duct is closing and thereafter passing a gaseous etchant through the central duct after the duct has closed to a diameter approximately equal to one millimeter and while the duct is closing, said gaseous etchant consisting of 48 sccm oxygen and 10 sccm C.sub.2 F.sub.6.
Priority Claims (1)
Number |
Date |
Country |
Kind |
8300650 |
Feb 1983 |
NLX |
|
Parent Case Info
This is a continuation of application Ser. No. 758,586, filed July 25, 1985, now abandoned which is a continuation of Ser. No. 580,976, filed Feb. 16, 1984 now abandoned.
US Referenced Citations (6)
Foreign Referenced Citations (5)
Number |
Date |
Country |
91173 |
Oct 1983 |
EPX |
2504514 |
Oct 1982 |
FRX |
54-30852 |
Mar 1979 |
JPX |
55-10468 |
Jan 1980 |
JPX |
2067182 |
Jul 1981 |
GBX |
Continuations (2)
|
Number |
Date |
Country |
Parent |
758586 |
Jul 1985 |
|
Parent |
580976 |
Feb 1984 |
|