1. Field of the Invention
This invention relates to integrated optical devices for modulation, routing, filtering, wavelength conversion, amplification and nonlinear processing of optical signals. Applications include optical communications, optical sensing and high-speed, high-bandwidth analog and digital processing in the optical domain.
2. Prior Art
High-speed optical modulators for telecommunications typically use lithium niobate waveguides, since lithium niobate is an electro-optic material whereby a change in the phase of an optical signal can be induced by applying a voltage across nearby electrodes. Typical lithium niobate waveguides are made using titanium-indiffusion or proton exchange. The resulting waveguides have low optical confinement which effectively means they can only achieve low loss for bend radii larger than about 1 centimeter in the 1400 nm to 1620 nm wavelength range, important for low loss optical fiber transmission, without incurring excess loss. This bend radius restriction substantially limits the number of optical devices and functions that can be fabricated on a single substrate, or on-chip. Consequently, the type and quality of optical filtering that can be realized on-chip is exceedingly limited.
The bend radius, and thus optical circuit size, must be increased further for operating in the mid-infrared, e.g. 2 to 4 micron wavelength range. The mid-infrared wavelengths are important for optical sensing applications where many chemicals. In particular, environmentally-important gases such as carbon monoxide, carbon dioxide, methane, sulfur dioxide and nitrous oxide have ro-vibrational absorption signatures that make them easily identifiable in the mid-infrared.
In addition to increasing the level of integration that can be achieved, it is highly desired to increase the interaction length for high-speed optical modulators in order to lower the drive voltage. One approach is to turn the optical mode by 180 degrees by creating a reflector at the chip facet or etching about ten microns into the lithium niobate and depositing a reflector so that the signal can propagate across the chip multiple times as described in M. Howerton, et al., “Low-loss compact reflective turns in optical waveguides,” U.S. Pat. No. 6,862,387 B2 (2005). The fabrication process for the reflector requires numerous steps and precise alignment to minimize the excess loss. Improvements are needed in reducing the excess loss and circuit size further as well as improving the manufacturability of compact waveguides on electro-optic substrates such as lithium niobate, in particular.
When the optical path lengths are dramatically increased on-chip, a concern arises over compensating the waveguide loss in order to integrate more functionality. Erbium, Er, doping in lithium niobate, LiNbO3, enables integrated optical waveguide amplifiers for applications in the 1550 nm wavelength regime. For example, optical amplification in titanium, Ti, diffused LiNbO3 waveguides has been demonstrated near 1530 nm [for example, see R. Brinkmann et al. in “Erbium-doped single- and double-pass Ti: LiNbO3 waveguide amplifiers,” J. Quant. Electron., pp. 2356-2360 (1994)]. The length of the amplifiers is currently limited by the die size. The ability to turn the waveguide using a compact bend would be highly beneficial in enabling higher gain amplifiers to be implemented, without the concern about unwanted reflections that may be associated with prior art reflection-based waveguide turning approaches.
Wavelength conversion from the 1.5 micron to the mid-infrared (3-5 microns) wavelength range can be performed using periodically poled lithium niobate (PPLN), and similarly for conversion between other wavelength regions. Wavelength conversion from the near-infrared to mid-infrared has been demonstrated in both bulk PPLN and PPLN waveguides. Implementations using bulk PPLN are limited by the fundamental tradeoff between the interaction length and minimum spot size due to beam diffraction. Optical waveguides provide a means of extending the interaction length and the ability to enhance the nonlinear interaction by increasing the optical mode confinement and thereby increasing the intensity of the pump wavelength driving the nonlinear wavelength conversion process. In addition, PPLN waveguide devices offer the potential to be a more compact solution than bulk approaches with more stable and robust packaging.
State-of-the-art waveguide-based wavelength converters using lithium niobate are substantially limited in their conversion bandwidth. High-refractive-index blanket coatings (not waveguides) of As2S3 have been investigated for 1.5 μm-band wavelength converters and z-cut, annealed proton exchange waveguides [see Sato et al., “Efficiency improvement by high-index cladding in LiNbO3 waveguide quasi-phase-matched wavelength converter for optical communication,” in IEEE Photon. Technol. Lett., pp. 569-571 (2003). Different PPLN waveguide fabrication processes have successfully been employed in Ti-indiffusion [see D. Hofmann et al., “Quasi-phase-matched difference-frequency generation in periodically poled Ti:LiNbO3 channel waveguides,” in Opt. Lett., pp. 896-898 (1999)]. Thus, substantial improvements are needed to advance the bandwidth and efficiency of wavelength converters, particularly for mid-infared wavelength generation. Within the 1550 nm telecommunications window, frequency shifting applications using four wave mixing are needed for signal processing applications of wavelength division multiplexed signals.
This invention relates to a novel optical waveguide platform for the high-density integration of multiple linear and nonlinear optical processing functions. Integrated-optic waveguides are preferred over bulk implementations for nonlinear processing because the propagation distance is not diffraction limited and the mode size can be made small without impacting the propagation distance. The level of integration for optical processing functions such as routing, modulation, switching, and filtering in lithium niobate waveguides is substantially hindered by their inherent low mode confinement, preventing optical circuits with tight bend radii (less than a millimeter) to be achieved. Optical filtering, in particular, is rarely done on-chip because it requires coupling between multiple, long optical paths. For nonlinear processing, the refractive index dispersion of nonlinear materials often limits the wavelength range over which the nonlinear process is optimized.
This disclosure provides the foundation for increasing the integration density of optical elements and functionality, for example, on a lithium niobate substrate. The novel waveguide platform that is disclosed offers an unprecedented combination of high-density, high-functionality integration using an exemplar combination of chalcogenide glass waveguides on lithium niobate, which enables high-speed modulation and reconfigurability, low-loss and low-power-consumption phase shifters, as well as amplification through erbium doping of the lithium niobate. This new waveguide platform can be exploited to demonstrate integration of polarization beam splitters and rotators for polarization diversity and polarization tuning.
For the wavelength converter, the necessary course wavelength combiners and splitters are easily integrated on-chip. This combination of high-confinement waveguides and low-loss, low-confinement waveguides for high-efficiency, broadband wavelength conversion, and increased optical integration density will enable a compact and robust wavelength converter package. Thus, this disclosure makes it possible to combine both linear and nonlinear waveguides, optimize their design, and integrate them monolithically.
The advantages, nature and various additional features of the invention will appear more fully upon consideration of the illustrative embodiments now to be described in detail in connection with the accompanying drawings. In the drawings:
a is a cross-sectional view of a multi-functional waveguide and
It is to be understood that these drawings are for illustrating the concepts of the invention and are not to scale.
Referring to the drawings,
Electrode 104a and 104b operate as a pair, whereby one active electrode driven by an applied voltage and a ground electrode form a pair. One or more ground electrodes may be used.
Buffer layer 112 comprises a material with a lower refractive index than the substrate and overlay waveguide material and that is optically transparent in the wavelength range of operation. Silicon dioxide is an example of a suitable buffer layer material to be used with lithium niobate and As2S3. Other glasses and polymers are also suitable. Buffer layer 112 provides a protective overcladding for overlay waveguide 108.
Buffer layer 112 separates the electrodes 104a and 104b from the optical mode traveling in either waveguide 102 or 108 when an electrode is above or in close proximity to the waveguide.
b illustrates a serpentined electro-optic phase modulator composed of substrate 100 with waveguide 102 and electrode 104a and 104b. An optical source is coupled to waveguide 102, typically through a singlemode optical fiber. For low loss coupling to a singlemode fiber, it is advantageous for waveguide 102 to be relatively low-confinement so that the mode couples efficiently to a singlemode fiber. Titanium-diffused lithium niobate waveguides are low-confinement waveguides and couple well to singlemode optical fiber. The phase of the optical signal is modulated by applying a voltage to electrode pair 110. The optical signal is then coupled to waveguide 108 via a mode coupler 106 that comprises a small waveguide width for the end point of the overlay material, typically 0.5 to 1.0 microns for As2S3 on LiNbO3, and tapers to a larger waveguide width, typically a few microns for As2S3 on LiNbO3. Waveguide 108 is a high-confinement waveguide that is capable of low-loss bend radii down to tens to hundreds of microns. Buffer layer 112 protects the overlay waveguide material and provides a buffer, separating the optical mode from the electrodes, which is particularly important where the electrodes are on top of or in close proximity to either the overlay waveguide or electro-optic waveguide. For x-cut lithium niobate substrates, the electrodes are placed to either side of the electro-optic waveguide. Traveling wave electrodes, which are designed for predetermined impedance, are used to maximize the modulation bandwidth and minimize reflections of the high-speed electrical drive signal. One end of the electrode pair is driven with a radio frequency or microwave source, while the other is terminated in a matching impedance load 111 to minimize reflections. For z-cut lithium niobate substrates (not shown), one electrode is positioned directly above the electro-optic waveguide while a second electrode is offset from it. The phase modulator illustrates in
By using a chalcogenide glass such as arsenic trisulfide to fabricate a high-confinement waveguide on lithium niobate, simulations show that low-loss bend radii on the order of 100 microns can be achieved. For a bend radius of 150 microns and a group index of 2.2, ring resonators with a free spectral range (FSR) up to 145 GHz can be realized. For optical filtering, it is desirable to have FSRs that are larger than the modulated signal bandwidth, thus achieving low-loss waveguides with small bend radii is critical for enabling advanced optical filtering on-chip. For larger index contrasts, for example by using a different chalcogenide composition with a higher refractive index, tighter bend radii and even larger FSRs can be realized.
To couple between the waveguide layers, one solution is to use adiabatic mode transforming tapers from the low-confinement substrate waveguide into a high-confinement overlay (e.g. As2S3) waveguide. Simulations using a beam propagation method show that efficient transfer of light, better than 95% mode transfer, can be achieved between the vertically integrated waveguides.
While previous optical filters have employed symmetric Mach-Zehnder interferometers with allpass filters in each arm [for example see C. Madsen in “Efficient Architectures for Exactly Realizing Optical Filters with Optimum Bandpass Designs,” in IEEE Photonics Technol. Lett., pp. 1136-1138 (1998)], the disclosed novel design uses polarization converters to tune the filter parameters in
Multiple rings can be incorporated in a Mach-Zehnder interferometer to produce frequency responses identical to elliptic, Butterworth and Chebyshev filter designs [see previous reference to C. Madsen (1998)], to name a few of the possibilities. The elliptic infinite impulse response (IIR) filter, in particular, gives the most efficient boxlike bandpass filter amplitude response for the fewest stages. For higher-order filters, multiple rings are needed in each arm of the interferometer. To do this with birefringent waveguides and polarization mode coupling, we propose to cascade stages of the basic architecture shown in
To realize programmable filters, both the optical phase of the delay path and the coupling into the feedback path must be tunable.
Power consumption is negligible for the electro-optic electrodes that are used for polarization conversion and phase control since they are high impedance with practically zero leakage current. In contrast, traveling-wave modulators need to have a 50-ohm impedance to match the electrical driver. In which case, achieving modulators with low Vπ voltages (the voltage required to shift the phase by π) is critical to reducing the power consumption. Switching energies are estimated at 30 mW per polarization converter section and 20 mW per phase controller. By using the electro-optic effect, the power consumption associated with thermal tuning or current injection, that are typical with other dielectric and semiconductor integrated-optic platforms, is avoided.
Integrated Optical Devices with Gain
The incorporation of gain in the feedback path offers a unique capability for the design of high-order optical filters compared to passive filters. First, the gain can offset the feedback path loss. Thus, ideal allpass optical filters may be realized with a unity magnitude response. A novel device results when gain is employed in a feedback path that is coupled to two input/output waveguides. With sufficient gain in the feedback path, one of the thru-port responses can be made allpass, i.e. the response will demonstrate no amplitude variation with frequency but its phase response can be made to vary dramatically with frequency. This is not possible with a passive filter because there is loss associated with transmission through the second coupler (compared to an allpass ring with a single coupler).
In general, increasing the gain in the feedback path will increase both the pole and zero magnitudes in an IIR filter. The pole magnitudes must be kept less than unity to insure stability. Increasing the loss in the delay path will likewise decrease both the pole and zero magnitudes. The magnitude response may exceed unity, particularly as the pole approaches the unit circle. For a single pole and zero, the architecture with an amplifier in the feedback path allows tuning without requiring a tunable filter in the ring's feedback path. By tuning the gain, it is possible to achieve a range of pole magnitudes without changing the coupling into the feedback path.
For high-order optical filters, it is desirable to implement a filter from well-known “unit cells”, analogous to “unit cells” in electronic field programmable gate arrays (FPGA). The “unit cells” may then be connected as necessary to form a programmable array. An optical filter “unit cell” is disclosed in
This invention provides design control over the mode confinement, mode effective index, and mode group index as a function of wavelength by using two optical waveguiding materials with different refractive indices. The wavelength conversion bandwidth is a major limitation for the generation of mid-IR wavelengths using periodically poled lithium niobate (PPLN). By overlaying a high-refractive-index material on the PPLN waveguide and optimizing the width and thickness that allows us to match the group index of the signal and idler wavelengths, over an order of magnitude conversion bandwidth improvement can be achieved. The wavelength conversion bandwidth compared to that with no overlay, for both a waveguide and bulk configuration shows over a factor of 20 improvement in simulation.
For wavelength conversion, we disclose a fully integrable optical parametric oscillator (OPO) solution, shown in
Having described the invention, the following example is given as a particular embodiment thereof and to demonstrate the practice and advantages thereof. It is understood that the example is given by way of illustration and is not intended to limit the specification of the claims in any manner.
An example of the fabrication steps for multi-functional integrated waveguides are set forth below for operation at 1.55 microns.
An optical amplifier may be fabricated in lithium niobate by sputtering a thin layer (e.g. 90 angstrom-thick) of erbium on the surface of the lithium niobate substrate. A mask is used to localize the Er deposition, or dopant, to predetermined regions so that the whole substrate is not doped. Regions which are doped require optical pumping; otherwise, large optical losses result in un-pumped regions, especially near 1530 nm. After Er deposition, diffusion is carried out in an oxygen ambient at 1100° C. temperature for 100 hours in an open tube furnace. Optical channel waveguides are then fabricated using a standard Ti-diffusion and waveguide patterning processes. An example process for making LiNbO3 waveguide devices involves (1) deposition of thin (120 nm) layer of Ti film on the surface of the substrate, (2) patterning the Ti film by a process of photolithography and etching, and (3) diffusing the Ti into the substrate at 1025° C. for 11 hours in wet ambient. For the PPLN section, the waveguide fabrication steps involve forming the domain-inverted grating after the Ti-indiffused waveguides. Standard photolithography techniques are used, to localize the PPLN region and create the periodic pattern to be poled. Electric-field poling is used to invert the domains.
After the substrate processing, As2S3 is deposited using an RF sputtering method that is least vulnerable to compositional difference between the target and the deposited film compared to other deposition techniques such as electron beam evaporation and pulsed laser deposition. The overlay films are annealed at 135° C. for two hours afterwards. Since As2S3 is attacked by developer solutions due to their alkali content, a SiO2 and titanium layers of thicknesses 230 nm and 15 nm are coated on top of As2S3 as a protective layer before the lithography step. The final waveguide structures are obtained after reactive-ion etching and photoresist removal. A protective overcladding of silicon dioxide is sputtered, or deposited by electron beam evaporation, to protect the As2S3 waveguides and to provide a buffer oxide layer on which to deposit electrodes.
For electro-optic control, phase shifters are implemented using a 200-nm-thick SiO2 buffer layer, deposited by RF sputtering. The electrodes may be delineated by liftoff using Cr/Au metal layers. Other electro-optically controlled devices such as an active Y-junction [for example, see H. Sasaki and I. Anderson, “Theoretical and experimental studies on active Y-junctions in optical waveguides,” in IEEE J. Quant. Electron., pp. 883-892 (1978)] may be implemented using these processes. The samples are polished as a last step before optical testing by coupling light into the waveguides.
While presently preferred embodiments have been shown of the optical waveguide devices and method for their fabrication and operation, persons skilled in this art will readily appreciate that various additional changes and modifications can be made without departing from the spirit of the invention as defined and differentiated by the following claims.
This application claims the benefit of provisional patent application Ser. No. 61/020,709, filed 2008 Jan. 12, by the present inventors.