Claims
- 1. A process of manufacturing a sheet-like thermoplastic structure having a reduced permeability to gases comprising a continuous phase consisting essentially of polyvinyl chloride and a discontinuous phase consisting essentially of polyvinyl alcohol, incompatible with the polyvinyl chloride phase, comprising lamellar layers distributed in the continuous polyvinyl chloride phase parallel to the surface of said sheet-like structure, which comprises:
- (a) mixing polyvinyl chloride with polyvinyl alcohol to provide a polymer mixture;
- (b) gelling said mixture under the combined effects of pressure and heat, and
- (c) extruding the gelled mixture by subjecting the gelled mixture to laminar flow through at least one die, said die providing between a die inlet and a die outlet a flow path for said mixture, at least a portion of which flow path is defined by the interval between two spaced parallel surfaces, the ratio of the length of said surfaces in the direction of flow to the distance between said surfaces being greater than 10.
- 2. The process of claim 1, wherein said ratio of the length of said parallel surfaces to the distance therebetween is greater than 20.
- 3. The process of claim 1 or 2, wherein said die outlet has a rectangular configuration.
- 4. The process of claim 1 or 2, wherein said die outlet has an annular configuration.
- 5. The process of claim 1 or 2, wherein said polymer mixture is prepared by mixing 100 parts by weight of polyvinyl chloride with about 5 to 30 parts by weight of polyvinyl alcohol.
- 6. The process of claim 1 or 2, wherein the K value of the polyvinyl chloride is comprised between about 50 and about 80, the extent of hydrolysis of the polyvinyl alcohol being comprised between about 50% and about 100%, and the viscosity of a 4% aqueous solution of the polyvinyl alcohol being comprised between about 2 cP and about 70 cP.
- 7. The process of claim 5, wherein the K value of the polyvinyl chloride is comprised between about 50 and about 80, the extend of hydrolysis of the polyvinyl alcohol being comprised between about 50% and about 100%, and the viscosity of a 4% aqueous solution of the polyvinyl alcohol being comprised between about 2 cP and about 70 cP.
- 8. The process of claim 1, further comprising the step of incorporating in said polymer mixture at least one of the compounds selected from the group consisting of stabilizers, lubricants, coloring agents and shock resisting agents.
- 9. The process of claim 5, further comprising the step of incorporating in said polymer mixture at least one composition selected from the group consisting of stabilizers, lubricants, coloring agents and shock resisting agents.
- 10. The process of claim 6, further comprising the step of incorporating in said polymer mixture at least one composition selected from the group consisting of stabilizers, lubricants, coloring agents and shock resisting agents.
- 11. The process of claim 7, further comprising the step of incorporating in said polymer mixture at least one composition selected from the group consisting of stabilizers, lubricants, coloring agents and shock resisting agents.
Priority Claims (1)
Number |
Date |
Country |
Kind |
76 32792 |
Oct 1976 |
FRX |
|
Parent Case Info
This is a division, of application Ser. No. 844,310, filed Oct. 21, 1977, pending in group (160).
US Referenced Citations (9)
Divisions (1)
|
Number |
Date |
Country |
Parent |
844310 |
Oct 1977 |
|