Claims
- 1. In a process for treating a copper plated substrate, formed by treatment of such substrate with an electroless copper plating solution, with an aqueous acid initiator solution which contains noble metal ions and is substantially free of tin ions, to render said copper plated substrate receptive to a subsequent electroless nickel plating step, wherein said initiator solution has become ineffective due to contamination thereof with complexing agents from said electroless copper plating solution and/or precipitation of noble metal ions therein, the improvement which comprises adding to said initiator solution ferric ions in an amount sufficient to restore said initiator solution to effective operation.
- 2. The process of claim 1 wherein the addition of the ferric ions to the initiator solution is carried out in the presence of an oxidizing medium.
- 3. The process as defined in claim 1 in which said ferric ions are present in an amount of at least about 10 mg/l.
- 4. The process as defined in claim 1 in which said ferric ions are present in an amount below that at which excessive etching of the copper substrate occurs.
- 5. The process as defined in claim 1 in which said ferric ions are present in an amount up to about 5 g/l.
- 6. The process as defined in claim 1 in which said ferric ions are persent in an amount of about 40 to about 500 mg/l.
- 7. The process as defined in claim 1 in which the step of introducing ferric ions into said initiator solution is performed by adding a bath soluble and compatible ferric compound thereto.
- 8. The process as defined in claim 7 in which said compound comprises ferric chloride.
- 9. The process as defined in claim 2 in which said ferric ions are present in an amount of at least about 10 mg/l.
- 10. The process as defined in claim 2 in which said ferric ions are present in an amount below that at which excessive oxidation attack of the copper coating to be plated occurs.
- 11. The process as defined in claim 2 in which said ferric ions are present in an amount up to about 5 g/l.
- 12. The process as defined in claim 2 in which said ferric ions are present in an amount of about 40 to about 500 mg/l.
- 13. The process as defined in claim 2 in which said oxidizing medium is performed by bubbling an oxygen-containing gas through initiator solution for a period of time sufficient in combination with said ferric ions present to effect a redissolution of at least a portion of said precipitate therein thereby restoring effective operation of said solution.
Parent Case Info
This is a continuation-in-part of application Ser. Number 556,417 filed Dec. 2, 1983 now abandoned.
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
556417 |
Dec 1983 |
|