The present disclosure relates generally to a protective coating, and more specifically to three layer conformal coating for electronic components.
Aircraft commonly employ electrical components for a variety of functions. Today's aircraft rely more and more on electrical components and their reliability. Electrical components are sometimes covered in Parylene in order to protect them from the elements. However, Parylene is known to have issues as well, its composition makes it particularly prone to tracking, which can lead to excessive creepage distance requirements at the combination of high voltage and altitude, which in turn results in larger component size. Moreover, it has poor resistance to ozone, which will also be exacerbated at high voltages and requires abrasion and toxic, and possibly flammable solvents for removal, which creates hazardous conditions during servicing.
Although conventional electrical and electromagnetic components have been protected and functioned safely by using conventional methods, there is still a need in the art for improved protective coatings. The present disclosure provides a solution for this need.
A protective coating system includes a first protective layer, a second protective layer covering at least a portion of the first protective layer, wherein the second protective layer includes Parylene, and a third protective layer covering at least a portion of the second protective layer. The third protective layer can be silicone based. The protective coating can be used to cover electric circuit boards and other electronic components having conductive elements and tracts.
The first protective layer can include a UV breakable adhesive. The third protective layer can be a transparent layer. The third protective layer and the second protective layer can transmit UV light at a greater than 350 nm frequency.
A method of applying a protective coating is also disclosed. The method includes covering at least a portion of the circuit board with a first protective layer, covering at least a portion of the first protective layer with a second protective layer including Parylene, and covering at least a portion the second protective layer with a third protective layer. Each of the layers can be different.
The third protective layer can be cured at 170 degrees Fahrenheit for at least 30 minutes. The second protective layer can be coated with a fourth protective layer, an adhesion promoter, before the third protective layer. The method can further include plasma etching the second protective layer, wherein the plasma etching take place before coating with the third protective layer.
The first protective layer can be removed while maintaining the second protective layer and maintaining the third protective layer by shining a UV ray at at least 350 nm frequency to degrade the first protective layer.
These and other features of the systems and methods of the subject disclosure will become more readily apparent to those skilled in the art from the following detailed description of the preferred embodiments taken in conjunction with the drawings.
So that those skilled in the art to which the subject disclosure appertains will readily understand how to make and use the devices and methods of the subject disclosure without undue experimentation, embodiments thereof will be described in detail herein below with reference to certain figures, wherein:
Reference will now be made to the drawings wherein like reference numerals identify similar structural features or aspects of the subject disclosure. For purposes of explanation and illustration, and not limitation, a partial view of an exemplary embodiment of a protective coating in accordance with the disclosure is shown in
The first protective layer 102 includes a UV breakable adhesive so that it can be broken and the entire coating system can be removed without having to perform other, possibly hazardous, abrasive, and time-consuming cleaning exercises. The third protective layer 106 is a transparent layer and along the second protective layer, 104 can pass UV light of at least 350 nm in order to activate the breakup of the first protective layer 102.
The method can further include plasma etching the second protective layer 104 in order to solidify it. When applying the third protective layer 106, it is cured at approximately 170 degrees Fahrenheit for at least 30 minutes or can also be left at ambient room temperature conditions for an hour. It is also considered that a fourth protective layer, an adhesion promoter, can be placed between the second protective layer 102 and the third protective layer 106.
The methods and systems of the present disclosure, as described above and shown in the drawings, provide for a coating having superior protection and cleaning properties. The coating and methods of the subject disclosure have been shown and described with reference to preferred embodiments, those skilled in the art will readily appreciate that changes and/or modifications may be made thereto without departing from the scope of the subject disclosure.
Number | Name | Date | Kind |
---|---|---|---|
4979803 | McGuckin | Dec 1990 | A |
5134015 | Ohtake | Jul 1992 | A |
5654084 | Egert | Aug 1997 | A |
6295112 | Kabe | Sep 2001 | B1 |
6334761 | Tai | Jan 2002 | B1 |
6620233 | Seeger | Sep 2003 | B1 |
6737753 | Kumar et al. | May 2004 | B2 |
7118693 | Glatkowski et al. | Oct 2006 | B2 |
8182892 | Huang et al. | May 2012 | B2 |
10103359 | Ramadas et al. | Oct 2018 | B2 |
20010052752 | Ghosh | Dec 2001 | A1 |
20020086188 | Halsey, IV | Jul 2002 | A1 |
20020106522 | McCormack | Aug 2002 | A1 |
20040032466 | Deguchi | Feb 2004 | A1 |
20050112650 | Chang | May 2005 | A1 |
20050121763 | Ucok | Jun 2005 | A1 |
20050175670 | Aoyagi | Aug 2005 | A1 |
20060003090 | Rodger | Jan 2006 | A1 |
20060102829 | Rieve | May 2006 | A1 |
20080039792 | Meng | Feb 2008 | A1 |
20080185173 | Bedinger | Aug 2008 | A1 |
20080185174 | Bedinger | Aug 2008 | A1 |
20090240215 | Humayun | Sep 2009 | A1 |
20100147192 | Huang | Jun 2010 | A1 |
20120223237 | Takeda | Sep 2012 | A1 |
20130180909 | Zheng | Jul 2013 | A1 |
20130248712 | Abdolvand | Sep 2013 | A1 |
20140183669 | Xu | Jul 2014 | A1 |
20160000602 | Meng | Jan 2016 | A1 |
20160262261 | Toting et al. | Sep 2016 | A1 |
20170100054 | Tai | Apr 2017 | A1 |
20170246847 | Scurtescu et al. | Aug 2017 | A1 |
20190106547 | Lin et al. | Apr 2019 | A1 |
20190113475 | Fan | Apr 2019 | A1 |
20200319135 | Fan | Oct 2020 | A1 |
Entry |
---|
Extended European Search Report for European Patent Application No. EP21215604.6, dated May 27, 2022. |
Number | Date | Country | |
---|---|---|---|
20220201869 A1 | Jun 2022 | US |