Claims
- 1. A curable pulverulent coating composition comprising (a) a polyester containing free carboxyl groups having a softening point of from 40.degree. to 140.degree. C. and an acid number of from 20 to 150 and being derived from at least one polyalcohol and one polycarboxylic acid which is predominantly aromatic and, as the sole crosslinking agent, (b) at least one polyglycidyl ester having an average molecular weight of from 200 to 1000 which is derived from an aromatic polycarboxylic acid, a cycloaliphatic polycarboxylic acid, an alphatic polycarboxylic acid or a mixture of at least two such acids, said (a) and (b) being present in an amount such that 0.7-1.4 equivalents of epoxide groups are present per equivalent of carboxyl groups.
- 2. The composition of claim 1 wherein (a) has an acid number of from 50 to 100.
- 3. The composition of claim 1 wherein (a) has a hydroxyl number of from 0 to 30.
- 4. The composition of claim 1 wherein the polycarboxylic acid of (a) consists of 70 to 100 mole % of aromatic dicarboxylic acid and 30 to 0 mol % of cycloaliphatic dicarboxylic acid, aliphatic dicarboxylic acid or a mixture of at least two such acids.
- 5. The composition of claim 1 wherein (a) is derived from an aromatic dicarboxylic acid anhydride, a cycloaliphatic carboxylic anhydride or a mixture of at least two such anhydrides and a hydroxyl group containing polyester derived from a polyalcohol and a carboxylic acid.
- 6. The composition of claim 5 wherein (a) has a hydroxyl number of from 50 to 150.
- 7. The composition of claim 5 wherein said anhydride is tetrahydrophthalic acid.
- 8. The composition of claim 1 wherein (b) is the bisglycidyl ester of hexahydrophthalic acid, phthalic acid, isophthalic acid, terephthalic acid or a mixture of at least two such acids.
- 9. The composition of claim 1 wherein (a) and (b) are present in an amount such that 0.8-1.0 equivalent of epoxide groups are present per equivalent of carboxyl groups.
- 10. The composition of claim 1 wherein said carable pulverulent coating composition has a particle size of 20 to 120.mu..
- 11. A method of lacquering an article which comprises applying to the article a coating of a pulverulent composition of claim 1 and curing the coating at a temperature of above 130.degree. C.
Priority Claims (1)
Number |
Date |
Country |
Kind |
2232084 |
Jun 1972 |
DEX |
|
CROSS-REFERENCE TO RELATED APPLICATION
This application is a continuation of application Ser. No. 544,123 filed Jan. 27, 1975 and now abandoned which, in turn, is a cntinuation of application Ser. No. 373,470, filed June 25, 1973 and now abandoned.
US Referenced Citations (5)
Continuations (2)
|
Number |
Date |
Country |
Parent |
544123 |
Jan 1975 |
|
Parent |
373470 |
Jun 1973 |
|