Claims
- 1. An aluminum-lithium component formed from a rapidly solidified aluminum-lithium alloy consisting essentially of the formula Al.sub.bal Li.sub.a Cu.sub.b Mg.sub.c Zr.sub.d wherein "a" ranges from about 2.6 to 3.4 wt %, "b" ranges from about 0.5 to 2.0 wt %, "c" ranges from about 0.2 to 2.0 wt % and "d" ranges from about 0.6 to 1.8 wt %, the balance being aluminum, said component having been subjected to a thermal treatment at a temperature greater than 500.degree. C. for a time period greater than 10 hrs. under a protective atmosphere.
- 2. A component as recited by claim 1, having a notched impact toughness from 40 to 250% greater than that prior to said thermal treatment.
- 3. A component as recited by claim 1, wherein said alloy has the composition 2.6 wt % lithium, 1.0 wt % copper, 0.5 wt % magnesium and 0.6 wt % zirconium, the balance being aluminum.
- 4. A component as recited by claim 1, wherein said temperature ranges from about 540.degree. C. to 580.degree. C.
- 5. A component as recited by claim 1, wherein said protective atmosphere is composed of argon or mixtures thereof with hydrogen.
- 6. A component as recited by claim 1 said component having a total toughness greater than the intrinsic toughness thereof prior to said thermal treatment.
CROSS-REFERENCE TO RELATED APPLICATIONS
This application is a division of U.S. application Ser. No. 502,950, filed Apr. 2, 1991, now U.S. Pat. No. 5,045,125.
US Referenced Citations (4)
Divisions (1)
|
Number |
Date |
Country |
Parent |
502950 |
Apr 1991 |
|