This application is the U.S. national stage of PCT/JP2018/004416 filed on Feb. 8, 2018, which claims priority of Japanese Patent Application No. JP 2017-036000 filed on Feb. 28, 2017, the contents of which are incorporated herein.
The present disclosure relates to a reactor.
For example, JP 2012-253289A and JP 2013-4531A disclose reactors that are magnetic components used in converters for electric-powered vehicles such as hybrid automobiles. The reactors disclosed in JP 2012-253289A and JP 2013-4531A are provided with a coil with a pair of wound portions, a magnetic core partially arranged inside the wound portions, and a bobbin (insulating interposed member) that ensures insulation between the coil and the magnetic core.
According to the present disclosure, a reactor includes a coil with a wound portion. A magnetic core with an inner core portion is arranged inside the wound portion. An inwardly interposed member is configured to ensure insulation between the wound portion and the inner core portion, wherein the inwardly interposed member has a thin portion that is thin as a result of an inner-circumferential surface of the inwardly interposed member being recessed, and a thick portion that is thicker than the thin portion, the inner core portion has, on an outer circumferential surface that faces the inwardly interposed member, a core-side projection portion that has a shape conforming to the shape of the inner-circumferential surface of the thin portion, the thin portion has a thickness of 0.2 mm to 1.0 mm inclusive, and the thick portion has a thickness of 1.1 mm to 2.5 mm inclusive, and the inner core portion and the inwardly interposed member are in substantially intimate contact with each other, and the inwardly interposed member and the wound portion are in substantially intimate contact with each other.
With recent development of electric-powered vehicles, there is a demand for improvement in performance of a reactor. For example, there is a demand for improvement in heat dissipation properties of the reactor, thereby suppressing changes in magnetic characteristics of the reactor that may be caused by heat accumulated in the reactor. There is also a demand for a reactor that is downsized and has improved magnetic characteristics. In order to meet such requirements, reactor configurations are reviewed.
Therefore, it is an object of the present disclosure to provide a reactor that has improved heat dissipation properties. It is also an object of the present disclosure to provide a reactor that is downsized and has improved magnetic characteristics.
First, embodiments of the disclosure according to the present application will be described sequentially.
Inwardly interposed members are often formed using injection molding. If the inwardly interposed members are thin, the size of the injection molded article is likely to vary. Accordingly, it is conventionally proposed to set the thickness of inwardly interposed members to a given value or more (for example, 2.5 mm or more), or provide ribs or the like on inwardly interposed members as disclosed in Patent Documents 1 and 2, so that the inwardly interposed members have high dimensional accuracy. However, in such a configuration, the distance between a wound portion and an inner core portion is large. Therefore, the dissipation of heat from the inner core portion to the wound portion is constrained, and if the wound portion has a given cross-sectional area, the cross-sectional area of the magnetic path of the inner core portion arranged inside the wound portion cannot be increased to the corresponding given value or more. In view of these issues, the applicants of the present application have accomplished the reactor according to the embodiments below.
According to an embodiment, a reactor includes a coil with a wound portion. A magnetic core with an inner core portion is arranged inside the wound portion. An inwardly interposed member is configured to ensure insulation between the wound portion and the inner core portion, wherein the inwardly interposed member has a thin portion that is thin as a result of an inner-circumferential surface of the inwardly interposed member being recessed, and a thick portion that is thicker than the thin portion, the inner core portion has, on an outer circumferential surface that faces the inwardly interposed member, a core-side projection portion that has a shape conforming to the shape of the inner-circumferential surface of the thin portion, the thin portion has a thickness of 0.2 mm to 1.0 mm inclusive, and the thick portion has a thickness of 1.1 mm to 2.5 mm inclusive, and the inner core portion and the inwardly interposed member are in substantially intimate contact with each other, and the inwardly interposed member and the wound portion are in substantially intimate contact with each other.
If the inwardly interposed member is produced using injection molding, in which resin is injected into a mold, the resin injected into a wide space of the mold is to serve as a thick portion, and the resin injected into a narrow space of the mold is to serve as a thin portion. The wide space of the mold functions to let the resin promptly move through all spaces of the mold. Therefore, an inwardly interposed member having a thick portion with a predetermined thickness or more can easily be produced according to the designed size, even if it has a thin portion that is thinner than a conventional one. To bring the inner core portion and the inwardly interposed member, and the inwardly interposed member and the wound portion of the coil into substantially intimate contact with each other, a method such as resin molding or press fitting is used. In either case, as a result of being able to produce the inwardly interposed member according to the designed size, the three components can be brought into substantially intimate contact with each other. Here, if resin molding or press fitting is performed, the interface between the inner core portion and the inwardly interposed member, or the interface between the inwardly interposed member and the wound portion may partially include a detached portion. Therefore, even if a portion of the interfaces is a detached portion, the three components are regarded as being in substantially intimate contact with each other as long as the total area of the detached portions in all of the interfaces is small (for example, not greater than 40% or 20%).
As a result of the inwardly interposed member including a thin portion that is thinner than a conventional one, it is possible to reduce the distance between the inner core portion and the wound portion, and to improve the dissipation of heat from the inner core portion to the wound portion. Moreover, since the inner core portion and the inwardly interposed member, and the inwardly interposed member and the wound portion are in intimate contact with each other, thermal conductivity between the three components is favorable, and the dissipation of heat from the inner core portion to the wound portion can be improved. Specifically, in the reactor of the embodiments, since the core-side projection portion of the inner core portion is arranged in the recess of the thin portion (hereinafter, also referred to as “interposition-side recess portion”), the distance of heat dissipation from the core-side projection portion to the wound portion is short, and as a result, the heat dissipation properties of the reactor can be improved.
Furthermore, as a result of the inwardly interposed member including a thin portion that is thinner than a conventional one, it is possible to increase the cross-sectional area of the magnetic path of the inner core portion arranged inside the wound portion, without increasing the size of the wound portion. Specifically, in the reactor of the embodiments, the core-side projection portion of the inner core portion is arranged in the interposition-side recess portion of the inwardly interposed member, and thus the cross-sectional area of the magnetic path of the inner core portion is large. Therefore, it is possible to increase, without changing the size of the wound portion, the cross-sectional area of the magnetic path of the inner core portion compared to a case of a reactor using a conventional inwardly interposed member that includes no interposition-side recess portion.
Furthermore, the configurations of the embodiments include advantages such as being able to suppress expansion and contraction of the wound portion that may be caused by use of the reactor, using the inwardly interposed member that is in intimate contact with the inner circumference of the wound portion, or being able to suppress magnetostrictive vibration of the inner core portion, using the inwardly interposed member that is in intimate contact with the outer circumference of the inner core portion.
A configuration of the reactor according to the embodiment may be such that the inwardly interposed member is made of resin that is molded inside the wound portion.
When the wound portion is arranged in a mold, and resin is molded inside the wound portion to form the inwardly interposed member, the resin injected into a wide space between the wound portion and the core of the mold that is arranged inside thereof is to serve as a thick portion, and the resin injected into a narrow space of the mold is to serve as a thin portion. By molding the resin on the wound portion to form the inwardly interposed member, it is possible to reliably bring the wound portion and the inwardly interposed member into intimate contact with each other. Furthermore, since the wound portion and the inwardly interposed member can be formed as one piece, it is possible to reduce time and effort required in assembling the wound portion and the inwardly interposed member, thus improving the productivity of the reactor.
A configuration of the reactor according to the embodiment may be such that the inner core portion is made of a composite material that contains soft magnetic powder and resin.
With the above-described configuration, it is possible to reliably bring the inwardly interposed member and the inner core portion into intimate contact with each other. Specifically, if a molded coil in which the inwardly interposed member is formed inside the wound portion using resin molding is used, simply by filling the molded coil with a composite material, it is possible to form the inner core portion inside the molded coil, and thus it is possible to improve the productivity of the reactor.
A configuration of the reactor according to the embodiment may be such that a difference in the thickness between the thin portion and the thick portion is not less than 0.2 mm.
As a result of a difference in the thickness between the thin portion and the thick portion being set to be not less than 0.2 mm, it is possible to reduce variations in size of the inwardly interposed member, while sufficiently ensuring the filling properties of resin into a narrow and small space of the mold that corresponds to the thin portion.
A configuration of the reactor according to the embodiment may be such that the thickness of the thin portion is 0.2 mm to 0.7 mm inclusive, and the thickness of the thick portion is 1.1 mm to 2.0 mm inclusive.
By setting the thickness of the thin portion to be in the above-described range, it is possible to sufficiently reduce the distance between the wound portion and the core-side projection portion of the inner core portion, and improve the heat dissipation properties of the reactor. Furthermore, by setting the thickness of the thick portion to be in the above-described range, it is possible to further reduce variation in size of the inwardly interposed member.
A configuration of the reactor according to the embodiment may be such that a plurality of thick portions and a plurality of thin portions are distributed in the circumferential direction of the inwardly interposed member.
In a mold used to produce the inwardly interposed member having the above-described configuration, resin is likely to move through all spaces of the mold when the resin is injected, and thus it is easy to produce an inwardly interposed member with little variation in size. In other words, the inwardly interposed member having the above-described configuration is an inwardly interposed member with little variation in size, and can improve the heat dissipation properties and the magnetic characteristics of the reactor. Specifically, if narrow spaces and wide spaces are alternately arranged side by side in the circumferential direction of the spaces of the mold into which resin is injected, the resin is more likely to move through all spaces of the mold. With such a mold, it is possible to produce an inwardly interposed member whose thick portions and thin portions are alternately arranged side by side in the circumferential direction of the inwardly interposed member, with dimensional accuracy.
A configuration of the reactor according to the embodiment may be such that at least some of the thick portions reach an end face, in the axial direction of the wound portion, of the inwardly interposed member.
When the inwardly interposed member is produced using injection molding, resin is often injected at a position of the mold at which an end face of the inwardly interposed member is to be formed. In this case, the end face of the inwardly interposed member serves as an entrance for the resin, and thus, if there is a large space that corresponds to the thick portion in the entrance for the resin, the moldability of the inwardly interposed member will be improved. Here, when the inwardly interposed member whose thick portion reaches the end face of the inwardly interposed member is produced, the wide space that corresponds to the thick portion is formed in the entrance for the resin. Therefore, the inwardly interposed member having the above-described configuration has improved moldability, and it is possible to accurately produce the inwardly interposed member even if a thin portion has a reduced thickness.
A configuration of the reactor according to the embodiment may be such that the inwardly interposed member has an outer circumferential surface in a shape that conforms to an inner-circumferential surface of the wound portion.
If the outer circumferential surface of the inwardly interposed member conforms to the inner-circumferential surface shape of the wound portion, there is hardly any gap between the inwardly interposed member and the wound portion, and thus it is easy to reduce the distance between the inner core portion located inside the inwardly interposed member, and the wound portion. As a result, the heat dissipation properties and the magnetic characteristics of the reactor can be improved with ease.
A configuration of the reactor according to the embodiment may be such that the thickness of the inwardly interposed member gradually increases from the thin portion toward the thick portion.
By employing a configuration in which the thickness of the inwardly interposed member gradually increases from the thin portion to the thick portion, it is possible to improve the moldability of the inwardly interposed member. Examples of the configuration in which the thickness gradually increases from the thin portion to the thick portion include an example in which the portion extending from the thin portion to the thick portion is a curved surface or an inclined surface. The reason why the above-described configuration improves the moldability of the inwardly interposed member is that, when the inwardly interposed member is formed using injection molding, resin injected into the portion of the mold in which the thick portion is to be formed is likely to move through toward the portion in which the thin portion is to be formed.
Hereinafter, embodiments of the reactor of the disclosure according to the present application will be described with reference to the drawings. The same reference numerals in the drawings denote a constituent component with the same name. Note that the disclosure according to the present application is not limited to the configurations shown in the embodiments but is defined by the claims, and is intended to encompass all modifications in the scope of the claims and equivalent thereto.
Overall Configuration
A reactor 1 shown in
Coil
The coil 2 of the present embodiment is provided with the pair of wound portions 2A and 2B, which are arranged in parallel to each other, and a coupling portion that couples the two wound portions 2A and 2B. End portions 2a and 2b of the coil 2 are drawn from the wound portions 2A and 2B, and are connected to not-shown terminal members. An external device such as a power supply that supplies electric power to the coil 2 is connected via the terminal members. The wound portions 2A and 2B of the coil 2 of the present example have substantially square tubular shapes with the same number of turns and the same winding direction, and are arranged in parallel to each other so that the axial directions thereof are in parallel to each other. The wound portions 2A and 2B may also have different numbers of turns or different cross-sections of the winding wires. Furthermore, the coupling portion of the present example is formed by bending a winding wire that connects the wound portions 2A and 2B in a flatwise manner, and is covered by a later-described coupling portion covering portion 71 so as not to be viewed from the outside.
The coil 2 including the wound portions 2A and 2B can be formed by a coated wire, which is a conductor, such as a rectangular wire or round wire made of a conductive material such as copper, aluminum, magnesium, or an alloy thereof provided with, on its outer circumferential surface, an insulating coating made of an insulating material. In the present embodiment, the wound portions 2A and 2B are formed by winding a coated rectangular wire in an edge wise manner, the coated rectangular wire having a conductor made of a copper rectangular wire and an enamel (typically, polyamide-imide) insulating coating.
As shown in
Magnetic Core
The magnetic core 3 can be classified into outer core portions 32 arranged outside the wound portions 2A and 2B (see
Each outer core portion 32 is divided by a gap portion 42g in a direction in which the wound portions 2A and 2B are arranged in parallel to each other. The gap portion 42g is formed by part of a later-described end-face interposed member 42. Here, the gap portion 42g is not limited to a portion that divides an outer core portion 32 into a plurality of core pieces without a coupled portion, and may be any portion as long as it can divide the main portion of a magnetic path of the outer core portion 32. In other words, the gap portions 42g do not need to be provided at positions of the outer core portions 32 at which the magnetic path is not affected. For example, even if the gap portions 42g have a length in the axial direction of the wound portions 2A and 2B such that they do not reach the end faces of the outer core portions 32, it is sufficient that they are arranged at a position in the magnetic path. Note that, in the configuration of the present example, the gap portions 42g are provided, but the gap portions 42g are not essential.
The magnetic core 3 is made of a composite material that contains soft magnetic powder and resin. The soft magnetic powder is an aggregation of magnetic grains made of an iron group metal such as iron or an alloy thereof (such as a Fe—Si alloy, a Fe—Si—Al alloy, or a Fe—Ni alloy). The magnetic grains may also have, on their surface, an insulating coating made of phosphoric salt or the like. Furthermore, as the resin, a thermosetting resin such as an epoxy resin, a phenol resin, a silicone resin, or an urethane resin, a thermoplastic resin such as a polyphenylene sulfide (PPS) resin, a polyamide (PA) resin such as nylon 6 or nylon 66, a polyimide resin, or a fluorine resin, or the like may be used, for example. This magnetic core 3 is formed by accommodating the coil 2 in a casing 6, and then filling the casing 6 with the composite material, as illustrated in the later-described manufacturing method of the reactor. Accordingly, the outer core portions 32 of the magnetic core 3 are joined to the inner circumferential surface of the casing 6.
The content of the soft magnetic powder in the composite material may be from 50% by volume to 80% by volume inclusive, out of 100% of the composite material. If the content of the magnetic powder is not less than 50% by volume and the ratio of the magnetic component is thus sufficiently high, it is easy to increase the saturation flux density. If the content of the magnetic powder is not greater than 80% by volume, the composite of the magnetic powder and the resin may have high fluidity, resulting in a composite material with improved moldability. The lower limit of the content of the magnetic powder may not be less than 60% by volume. Furthermore, the upper limit of the content of the magnetic powder may not be greater than 75% by volume, and more specifically not greater than 70% by volume.
Insulating Interposed Member
The insulating interposed member 4 is a member that ensures insulation between the coil 2 and the magnetic core 3. In the present example, the insulating interposed member 4 is formed as part of the coil molded portion 7 obtained by molding resin on the wound portions 2A and 2B. The coil molded portion 7 includes the insulating interposed member 4, turn covering portions 70 that integrate turns into one piece at curved corner positions on the outer circumferential side of the wound portions 2A and 2B, and the coupling portion covering portion 71 that covers the coupling portion (not shown) of the wound portions 2A and 2B.
The insulating interposed member 4, which is formed as the coil molded portion 7, is provided with a pair of inwardly interposed members 41 and a pair of end-face interposed members 42. Each inwardly interposed member 41 is formed inside the wound portion 2A (2B), and is interposed between the inner circumferential surface of the wound portion 2A (2B) and the outer circumferential surface of the inner core portion 31 (
The internal areas of dashed-two dotted lines (
Each end-face interposed member 42 is frame-shaped while protruding away from the coil 2 in the axial directions of the wound portions 2A and 2B. An outer-side surface (surface in a direction in which the wound portions 2A and 2B are arranged in parallel to each other) 420 of each of the frame-shaped end-face interposed members 42 abuts against edge portions 600 of core opposing portions 61A and 61B of the later-described casing 6.
The end-face interposed members 42 further include a gap portion 42g provided between the pair of through holes 41h. The gap portion 42g is a plate member that protrudes away from the coil 2 in the axial directions of the wound portions 2A and 2B. As has been described, the gap portion 42g forms a gap at a position of an outer core portion 32. By adjusting the thickness of the gap portion 42g, it is possible to adjust the magnetic characteristics of the magnetic core 3. If adjustment of the magnetic characteristics using the gap portions 42g is not needed, the gap portions 42g do not need to be provided.
The insulating interposed member 4 having the above-described configuration can be formed of, for example, a thermoplastic resin such as a PPS resin, a polytetrafluoroethylene (PTFE) resin, a liquid crystal polymer (LCP), a PA resin such as nylon 6 or nylon 66, a polybutylene terephthalate (PBT) resin, or an acrylonitrile butadiene styrene (ABS) resin. Alternatively, the insulating interposed member 4 can also be formed of a thermosetting resin such as an unsaturated polyester resin, an epoxy resin, a urethane resin, or a silicone resin. A ceramic filler may also be added to the above-described resin to improve the heat dissipation properties of the insulating interposed member 4. As the ceramic filler, a non-magnetic powder such as alumina or silica may be used, for example.
Casing
As shown in
The bottom plate portion 60 is provided with a coil placement portion 60b on which the wound portions 2A and 2B are placed, and core contact portions 60s that are located on the upper side of the coil placement portion 60b, and come into contact with the bottoms of the outer core portions 32 (
The side wall portion 61 is constituted by the pair of core opposing portions 61A and 61B that oppose the outer circumferential surfaces of the outer core portions 32 (
As shown in
Relationship Between Inwardly Interposed Member, Inner Core Portion, and Wound Portion
As shown in an enlarged view in the circle in
The shape of the inner-circumferential surfaces of the interposition-side recess portions 411 in a cross section that is orthogonal to a direction in which the interposition-side recess portions 411 extend (that is a direction of depth of the paper of
The thin portions 41a have a thickness t1 of 0.2 mm to 1.0 mm inclusive, and the thick portions 41b have a thickness t2 of 1.1 mm to 2.5 mm inclusive. Here, the thickness t1 of the thin portions 41a refers to the thickness of the portions of the interposition-side recess portions 411 that correspond to the deepest position as shown in
If the inwardly interposed members 41 having the above-described configuration are produced inside the wound portions 2A and 2B using injection molding, the resin injected into wide spaces of a mold for use in the injection molding is to serve as the thick portions 41b, and the resin injected into narrow spaces of the mold is to serve as the thin portions 41a. The wide spaces of the mold function to let the resin promptly move through all spaces of the mold. Therefore, inwardly interposed members 41 having thick portions 41b with a predetermined thickness or more can easily be produced according to the designed size even if they have thin portions 41a that are thinner than conventional ones, thus making it possible to bring the inwardly interposed members 41 into substantially intimate contact with the inner circumferences of the wound portions 2A and 2B. As a result of the inwardly interposed members 41 having the thin portions 41a that are thinner than conventional ones, it is possible to reduce the distance between the inner core portions 31 and the wound portions 2A and 2B, and improve the dissipation of heat from the inner core portions 31 to the wound portions 2A and 2B.
Taking the moldability of the inwardly interposed members 41 into consideration, the plurality of interposition-side recess portions 411 are preferably distributed in the circumferential direction of the inner-circumferential surfaces 410 of the inwardly interposed members 41. In other words, this configuration is such that the plurality of thick portions 41b and the plurality of thin portions 41a are distributed in the circumferential direction of the inwardly interposed members 41. The mold used to produce the inwardly interposed members 41 is such that a narrow space and a wide space are alternately arranged side by side in the circumferential direction of the spaces of the mold into which resin is injected. With such a mold, when resin is injected, the resin is likely to move through all spaces of the mold, and it is easy to produce inwardly interposed members 41 with little variation in size. Specifically, with the configuration, as in the present example, in which the thin portions 41a and the thick portions 41b extend in the axial direction of the inwardly interposed member 41, it is easier to fill the mold with resin at the time of molding.
Furthermore, taking the moldability of the inwardly interposed members 41 into consideration, at least some of the thick portions 41b preferably reach the end faces, in the axial direction of the wound portions 2A and 2B, of the inwardly interposed members 41. It is preferable that, as shown in
On the other hand, the inner core portions 31 that are arranged inside the inwardly interposed members 41 (through holes 41h) can be produced by inserting a composite material into the through holes 41h. Each of the inner core portions 31 is provided with core-side projection portions 311 formed on the outer circumferential surface thereof (core outer circumferential surface 319) (see
An outer circumferential surface 419 of the inwardly interposed member 41 preferably has a shape that conforms to the shape of the inner-circumferential surface of the wound portions 2A and 2B. With this, there is hardly any gap between the inwardly interposed member 41 and the wound portions 2A and 2B, and it is thus possible to reduce the distance between the inner core portions 31 to the wound portions 2A and 2B. As a result, it is possible to improve the dissipation of heat from the inner core portions 31 to the wound portions 2A and 2B, and to ensure a large cross section of the magnetic path of the inner core portion 31.
More Preferable Configuration
Taking the wide spaces of the mold that correspond to the thick portions 41b realizing favorable moldability of the inwardly interposed members 41 into consideration, a difference between the thickness t1 of the thin portions 41a and the thickness t2 of the thick portions 41b (thickness t2−thickness t1) is preferably set to be not less than 0.2 mm. If specific numerical values are to be defined for the thin portions 41a and the thick portions 41b, the thickness t1 of the thin portions 41a is preferably 0.2 mm to 0.7 mm inclusive, and the thickness t2 of the thick portions 41b is preferably 1.1 mm to 2.0 mm inclusive. The thickness t1 of the thin portions 41a is more preferably 0.2 mm to 0.5 mm inclusive, and the thickness t2 of the thick portions 41b is more preferably 1.1 mm to 2.0 mm inclusive.
By employing a configuration in which the thickness of the inwardly interposed members 41 gradually increases from a thin portion 41a toward a thick portion 41b, it is possible to improve the moldability of the inwardly interposed member 41. This is because, when the inwardly interposed member 41 is molded using injection molding, resin injected into the portion of the mold in which the thick portions 41b are to be formed easily enters the portion in which the thin portions 41a are to be formed. As a specific example of this configuration, as shown in, for example,
Reactor Manufacturing Method
To manufacture the reactor 1 of Embodiment 1, the coil 2 with the coil molded portion 7, and the casing 6 are prepared, as shown in
By inserting the coil 2 into the casing 6, a space is formed between the inner-circumferential surface of the core opposing portion 61A (61B) and the end-face interposed member 42. This space is filled with a composite material from above (filling step). The composite material filling up the casing 6 from the space accumulates in the space between the core opposing portion 61A (61B) and the end-face interposed member 42 to form the outer core portion 32 (
With the above-described manufacturing method, simply by arranging the coil 2 in the casing 6, and filling the casing 6 with a composite material, the reactor 1 can be produced. Therefore, it is possible to improve the productivity of the reactor 1. Furthermore, by forming gap portions 42g for adjusting the magnetic characteristics of the magnetic core 3 on the end-face interposed members 42, which are part of the coil molded portion 7, it is possible to reduce time and effort for preparing separate gap materials, and arranging the separate gap materials.
Modification 1-1
In Embodiment 1, the thick portions 41b are a series of projections that extend from one end face to the other end face in the axial directions of the wound portions 2A and 2B. Alternatively, thick portions 41b that reach one end face of the wound portions 2A and 2B and thick portions 41b that reach the other end face of the wound portions 2A and 2B are displaced relative to each other in the circumferential direction of the inwardly interposed members 41. Also, in this case, when the inwardly interposed members 41 are formed inside the wound portions 2A and 2B, and resin is injected from both end face sides of the wound portions 2A and 2B, the entrance for the resin is wide, and thus the inwardly interposed members 41 can be produced with dimensional accuracy.
By inserting a composite material into the inwardly interposed members 41 to produce an inner core portion 31, the inner core portion 31 as shown in
Modification 1-2
The divided state of the magnetic core 3 is not limited to the example of Embodiment 1. For example, an assembly is produced by filling the coil 2 with the coil molded portion 7 with a composite material to form the inner core portions 31 inside the inwardly interposed members 41. Then, the assembly may be combined with outer core portions 32 prepared separately from the assembly, and the reactor 1 may be completed. In this case, the outer core portions 32 may also be molded articles of the composite material, or compressed powder molded articles obtained by compressing and molding soft magnetic powder.
Modification 1-3
The casing 6 of Embodiment 1 is not essential. For example, the coil 2 with the coil molded portion 7 is arranged in the mold, and the mold is filled with a composite material for forming the magnetic core 3. Then, when the resin of the composite material is cured, the assembly 10 may be taken out from the mold, and the reactor 1 may be realized.
Embodiment 1 described a configuration in which the coil 2 is provided with the pair of wound portions 2A and 2B. Alternatively, the same configuration as in Embodiment 1 may be applied to a reactor that includes a coil provided with a single wound portion.
If a coil provided with a single wound portion is used, resin is molded on the coil, and a molded coil assembly is produced that is provided with an inwardly interposed member and an end-face interposed member that are integrated with the coil. Similar to Embodiment 1, the inwardly interposed member is obtained by molding resin so that it has thin portions and thick portions. This molded coil assembly is arranged in the casing, and the casing is filled with a composite material. In this case, of the composite material filling up the casing, the resin that is inserted into the inwardly interposed member serves as an inner core portion, and the resin that moves to the outside of the wound portion serves as an outer core portion.
Usage
The reactor according to the embodiments is applicable to a power conversion device such as a bidirectional DC/DC converter installed in an electric-powered vehicle such as a hybrid automobile, an electric automobile, or a fuel-cell-powered automobile.
Number | Date | Country | Kind |
---|---|---|---|
JP2017-036000 | Feb 2017 | JP | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/JP2018/004416 | 2/8/2018 | WO | 00 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2018/159254 | 9/7/2018 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
3463196 | Richardson | Aug 1969 | A |
20120092120 | Yoshikawa et al. | Apr 2012 | A1 |
20120126928 | Yoshikawa et al. | May 2012 | A1 |
20120154093 | Yoshikawa et al. | Jun 2012 | A1 |
20130181801 | Yoshikawa et al. | Jul 2013 | A1 |
20140125308 | Yoshikawa et al. | May 2014 | A1 |
20150352965 | Inaba | Dec 2015 | A1 |
20150365015 | Ito | Dec 2015 | A1 |
20180358172 | Yamamoto | Dec 2018 | A1 |
Number | Date | Country |
---|---|---|
2012-253289 | Dec 2012 | JP |
2013-004531 | Jan 2013 | JP |
2016-149453 | Aug 2016 | JP |
Entry |
---|
International Search Report, Application No. PCT/JP2018/004416, dated Apr. 24, 2018. ISA/Japan Patent Office. |
Number | Date | Country | |
---|---|---|---|
20210202149 A1 | Jul 2021 | US |