Embodiments of the present invention generally involve lighting or lamp assemblies and more particularly to a fluorescent lamp (FL) or lamp assembly having improved run-up properties.
The majority of the known and commercially available low-pressure fluorescent discharge lamps are so-called fluorescent lamps (FLs) at present. For example, compact fluorescent lamps (CFLs) are intended to replace incandescent lamps used in a wide field of industry and home applications. In order to provide a CFL that resembles conventional incandescent lamps, a bulb shaped outer envelope may encapsulate the CFLs. The advantages of these lamps are low power consumption and long lifetime. However, one of the main disadvantages of FLs, including CFLs, is their relatively long run-up time.
A number of different solutions currently exist to improve run-up behavior, i.e., the time needed after switching on the supply for the lamp to reach 80% of its stabilized luminous flux (as defined by Energy Star Program Requirements for Compact Fluorescent Lamps 4.3: Section 2, Definition DD, Page 2). This property is also referred to as “lamp warm-up time,” which is the time needed after start-up to emit a defined proportion of its stabilized luminous flux (defined by the Commission Regulation (EC) EuP No 244/2009 Annex l/1/k). By way of example only, long-life fluorescent lamps currently need approximately 0.5 to 1.5 seconds to preheat the cathodes or electrodes before starting. Before preheating is complete, there is no light emission from the lamp. Once the arc discharge is initiated, the fluorescent lamp still requires an additional approximately 20 to 120 seconds or more to reach 80% of its stabilized luminous flux.
Prior attempts to reduce the run-up time of a FL that uses amalgam mercury dosing by incorporating an auxiliary amalgam close to one of the electrodes in the lamp. As a result of this arrangement, mercury stored in the auxiliary amalgam is vaporized shortly after switching on and in this way, the run-up period is reduced. However, one disadvantage of this proposed solution is that it does not provide an instant light feature.
Another known solution combines two lamps in one unit. More particularly, a fluorescent lamp and a conventional incandescent lamp are combined. Although it has been suggested to simultaneously turn on both lamps in order to result in instant light from the incandescent lamp, and then subsequently terminate or switch off the incandescent lamp, these known arrangements do not provide an efficient and effective manner for warming up the mercury source. For example, it has been suggested that a thermally sensitive element be located in the ballast compartment. This arrangement does not provide an accurate assessment of the actual thermal conditions of the discharge vessel. Further, locating a thermally sensitive element in a ballast compartment is potentially impacted by temperature variations caused by different illumination positions of the lamp e.g. vertically upright or inverted. As a result, the thermally sensitive element does not provide an accurate representation of the heat conditions.
Still another known solution is to apply power to the incandescent lamp only when the lamp assembly is turned on or switched on. Once a predetermined temperature is reached, the switch then de-energizes the incandescent lamp and subsequently applies power to the fluorescent lamp. The thermal switch associated with this arrangement aids in starting of the fluorescent lamp in low temperature, ambient conditions; however, it does not improve run-up of the lamp assembly.
In still another known arrangement, a fluorescent lamp is used in conjunction with a small incandescent lamp and AC power line voltage is provided. An inverter-type ballast is combined with the lamp base and is operable to power the fluorescent lamp whenever the base is received in the associated lamp socket. A thyristor or silicon controller rectifier (SCR) causes total light provided from the combination fluorescent-incandescent lamp assembly to remain substantially constant from the moment that AC power line voltage is provided at the lamp socket. When the AC power line voltage is initially provided, light from the incandescent lamp is at its maximum, while light provided from the fluorescent lamp will be at a minimum. Thereafter, light from the incandescent lamp will gradually diminish as the fluorescent lamp gradually increases. After a period, the AC power line voltage is totally disconnected from the incandescent lamp. Unfortunately, due to the SCR, the RMS value of the input power is about 70% of the nominal value and results in a specialized incandescent lamp that has increased cost and complexity.
Consequently, a need exists for a long-life fluorescent lamp that provides energy savings with instant light capabilities and fast warm-up, and overcomes the problems noted with prior proposed solutions.
Aspects and advantages of the invention are set forth below in the following description or may be learned through practice of the invention.
Fluorescent lamps having a number of advantages over known FLs are generally provided, along with their methods of manufacture and use. In one embodiment, the fluorescent lamp includes a discharge tube extending from a first end to a second end; a resistive transparent coating (e.g., a tin oxide thin film layer, such as a fluor-doped tin oxide thin film layer) on the outer surface of the discharge tube; and a pair of electric terminals positioned on the discharge tube such that a first terminal is on the first end and a second terminal is on the second end. The resistive transparent coating has, in one embodiment, a thickness of about 1.2 μm or less.
The resistive transparent coating can, in certain embodiments, have a resistivity of about 10 ohms to about 10,000 ohms. The resistive transparent coating, in one embodiment, can have a variable resistivity such that a middle area of the resistive transparent coating has a greater resistivity than an area of the resistive transparent coating at the first end and/or the second end.
The resistive transparent coating can be electrically connected to the pair of electric terminals. For example, the lamp can further include a first electrical connection from the first electric terminal to the resistive transparent coating on the first end of the discharge tube; and a second electrical connection from the second electric terminal to the resistive transparent coating on the second end of the discharge tube.
In one particular embodiment, the lamp can further include a lamp driver electrically connected to a discharge driver and a heating driver. The discharge driver can be electrically connected to the first electrode and the heating driver is electrically connected to the resistive transparent coating on the first end of the discharge tube. The heating driver can be configured to provide about 1 watt to 1000 watts to the resistive transparent coating. In certain embodiments, the heating driver is connected to a controller (e.g., a timer), which can be configured to provide current to the resistive transparent coating for a run-up period upon the fluorescent lamp being turned on by measuring time, temperature, light output or electrical parameters.
A transparent insulating layer can be positioned on the resistive transparent layer in particular embodiments.
Methods are also generally provided for forming a fluorescent lamp. In one embodiment, the resistive transparent layer can be deposited onto an outer surface of a discharge tube (e.g., via chemical vapor deposition); and electrodes can be attached to a first end and a second end of the discharge tube.
Those of ordinary skill in the art will better appreciate the features and aspects of such embodiments, and others, upon review of the specification.
A full and enabling disclosure of the present invention, including the best mode thereof to one skilled in the art, is set forth more particularly in the remainder of the specification, including reference to the accompanying figures, in which:
This detailed description uses numerical and letter designations to refer to features in the drawings. Like or similar designations in the drawings and description have been used to refer to like or similar parts of embodiments of the invention.
Reference will now be made in detail to present embodiments of the invention, one or more examples of which are illustrated in the accompanying drawings.
Each example is provided by way of explanation of the invention, not limitation of the invention. In fact, it will be apparent to those skilled in the art that modifications and variations can be made in the present invention without departing from the scope or spirit thereof. For instance, features illustrated or described as part of one embodiment may be used on another embodiment to yield a still further embodiment. Thus, it is intended that the present invention covers such modifications and variations as come within the scope of the appended claims and their equivalents.
Fluorescent lamps (FLs) having improved properties, including compact fluorescent lamps, are generally provided, along with their methods of manufacture. Referring to
A resistive transparent coating 30 is shown layered on the outer surface 20 of the discharge tube 12. Generally, one particular aspect of the present invention provides that the resistive transparent coating 30 is electrically connected to a pair of heating electrodes 25, 26 to apply a current to the resistive transparent coating 30, which in turn creates an electrical heating affect. This external heating of the discharge tube 12 can increase the rate at which mercury evaporates within the inner cavity 13 during lamp start, thereby reducing the time needed for the lamp to reach maximum lumen output.
In one embodiment, the pair of heating electrodes 25, 26 is electrically connected to the first electrode 21 and the second electrode 22, respectively. For example, a first electrical connection 25 can be present from the first electrode 21 to the resistive transparent coating 30 on the first end 14 of the discharge tube 12, and a second electrical connection 26 can be present from the second electrode 22 to the resistive transparent coating 30 on the second end 16 of the discharge tube 12. For instance, a pair of galvanic contacts can be utilized as the electrical connections 25, 26 through attachment to the resistive transparent coating 30 and to the first electrode 21 and second electrode 22, respectively.
Turning to
The heating driver 104 can also include a controller 106 configured to provide current to the resistive transparent coating 30 for a run-up period following the fluorescent lamp 10 being turned. The controller can include any suitable sensor or combination of sensors that are configured to measure time, temperature, light output, and/or electrical parameters, such as voltage, current, and/or power of the lamp 10 or the discharge driver 102. After this run-up period, the controller 106 can then break the electrical connection within the heating driver 104 such that no electrical current is passed through the resistant transparent coating 30. Generally, the controller 106 can be tuned for each particular lamp 10 to provide sufficient warm-up heating to the discharge tube 12, particularly in the areas away from the ends 14, 16, to allow for quickly reaching full lumens. For instance, the run-up period can be about 5 seconds to about 1 minute. In one embodiment, the controller can include a simple timer configured to provide current to the resistive transparent coating 30 for a run-up period upon the fluorescent lamp 10 being turned on.
According to certain aspects of the present invention, the resistive transparent coating 30 includes a material that is generally resistive in nature, while remaining substantially transparent to light within the visible wavelengths (e.g., about 380 nm to about 780 nm). For example, the resistive transparent coating 30 can have at least about 65% transparent in the UV wavelengths (e.g., about 10 nm to about 400 nm), the visible wavelengths (e.g., about 380 nm to about 750 nm), and/or the near IR wavelengths (e.g., about 750 nm to about 0.1 mm) of light. In one embodiment, the resistive transparent coating 30 can be a thin film layer.
According to certain aspects of the present invention, the transparency of the resistive transparent coating 30 can be controlled as desired, depending on the end use of the lamp 10. For example, the resistive transparent coating 30 can be configured to be about 65% transparent or greater (e.g., about 85% or greater) in a particular range of wavelength, such as in the near IR wavelengths, the visible wavelengths, and/or the UV wavelengths.
The resistance of the resistive transparent coating 30 can be adjusted to the electronic driver by changing the deposition parameters and/or the chemical composition of the precursor material. In certain embodiments, the resistive transparent coating 30 can have a resistivity of about 10 ohms to about 10,000 ohms. In one embodiment, the resistivity of the resistive transparent coating 30 can vary across the surface area defined by the resistive transparent coating 30.
In one embodiment, the resistive transparent coating 30 can include a tin oxide. In certain other embodiments, the resistive transparent coating 30 can further include another element (e.g., be doped with) to adjust the resistivity as desired, including but not limited to fluorine (i.e., a fluor-doped tin oxide), an indium tin oxide, a zinc tin oxide, or the like, or mixtures thereof. In one embodiment, the weight ratio of tin to the dopant (e.g., fluorine) can be about 1:1 to about 30:1. For instance, the dopant material can be present in an amount sufficient to control the resistivity of the resistive transparent coating 30, such as up about 30% wt. by weight dopant to the weight of tin.
The resistive transparent coating 30 can generally be deposited by any suitable deposition method, including but not limited to chemical vapor deposition, sputtering, sublimation, evaporation, spray pyrolysis, etc. For instance, in one embodiment, the resistive transparent coating 30 can be deposited via chemical vapor deposition onto a heated discharge tube 12. The resistive transparent coating 30 can generally define a thin film, which can, in certain embodiments, have a thickness of about 1.2 μm or less (e.g., about 100 nm to about 1.1 μm). The resistive transparent coating 30 can be a single layer or may be formed from a plurality of layers.
Although shown as having a tubular shape in
In the present disclosure, when a layer is being described as “on” or “over” another layer or substrate, it is to be understood that the layers can either be directly contacting each other or have another layer or feature between the layers, unless expressly stated to the contrary. Thus, these terms are simply describing the relative position of the layers to each other and do not necessarily mean “on top of” since the relative position above or below depends upon the orientation of the device to the viewer.
It is to be understood that the ranges and limits mentioned herein include all sub-ranges located within the prescribed limits, inclusive of the limits themselves unless otherwise stated. For instance, a range from 100 to 200 also includes all possible sub-ranges, examples of which are from 100 to 150, 170 to 190, 153 to 162, 145.3 to 149.6, and 187 to 200. Further, a limit of up to 7 also includes a limit of up to 5, up to 3, and up to 4.5, as well as all sub-ranges within the limit, such as from about 0 to 5, which includes 0 and includes 5 and from 5.2 to 7, which includes 5.2 and includes 7.
This written description uses examples to disclose the invention, including the best mode, and also to enable any person skilled in the art to practice the invention, including making and using any devices or systems and performing any incorporated methods. The patentable scope of the invention is defined by the claims, and may include other examples that occur to those skilled in the art. Such other and examples are intended to be within the scope of the claims if they include structural elements that do not differ from the literal language of the claims, or if they include equivalent structural elements with insubstantial differences from the literal languages of the claims.
Number | Name | Date | Kind |
---|---|---|---|
5438235 | Sommerer et al. | Aug 1995 | A |
5808414 | Wharmby et al. | Sep 1998 | A |
6064155 | Maya et al. | May 2000 | A |
6114809 | Winsor | Sep 2000 | A |
7511431 | Lesch et al. | Mar 2009 | B2 |
7550925 | Lesch et al. | Jun 2009 | B2 |
7928644 | Tokes et al. | Apr 2011 | B1 |
7969074 | Stockwald et al. | Jun 2011 | B2 |
20050035700 | Yano et al. | Feb 2005 | A1 |
20060226781 | Allen et al. | Oct 2006 | A1 |
20110012509 | Wursching et al. | Jan 2011 | A1 |
20110089832 | Kelly | Apr 2011 | A1 |
20110234094 | Wursching et al. | Sep 2011 | A1 |
20120019136 | Wursching et al. | Jan 2012 | A1 |
20130221849 | Koronya et al. | Aug 2013 | A1 |
Number | Date | Country |
---|---|---|
2144260 | Sep 1995 | CA |
0673057 | Sep 1995 | EP |
0767340 | Apr 1997 | EP |
2597936 | May 2013 | EP |
2008029369 | Mar 2008 | WO |
WO 2008029369 | Mar 2008 | WO |
Entry |
---|
European Search Report and Opinion issued in connection with corresponding EP Application No. 13195793.8 on Jan. 14, 2015. |
Number | Date | Country | |
---|---|---|---|
20140159574 A1 | Jun 2014 | US |