This invention relates to a steam expander for a loose fill material.
As is known, various types of expanders have been employed for expanding latent foaming loose fill material. Typically, a charge of loose fill material in a latent foaming state is deposited into a chamber which is heated so that the individual elements of the charge are expanded under the heat generated in the chamber. In some cases, it has been known to move a charge of loose fill material by means of a conveyor screw into a heated steam chamber so that the loose fill material can be expanded on a continuous basis. However, use of a conveyor screw to move the elements of the loose fill material causes flaking and cracking of the elements. As a result, dust is created within the moving mass of material. Further, in some cases, the steam chamber has been provided with rotating paddles in order to break up any clumping of the material at the entrance to the steam chamber as well as to convey the material to an outlet of the steam chamber. These paddles, in turn, cause further flaking and cracking of the elements and an accumulation of more dust in the mass of material. Consequently, when the expanded loose fill material is packaged and subsequently placed into use, the accumulated dust creates problems for the user and the environment to which the loose fill material is exposed.
Accordingly, it is an object of the invention to reduce the amount of dust created during the expansion of latent foaming loose fill material.
It is another object of the invention to avoid cracking or splitting of the elements of a charge of latent foaming loose fill material during expansion thereof.
Briefly, the invention provides a steam expander with at least one housing that receives a flow of loose fill material, a steam chamber in communication with an outlet of the housing to receive the loose fill material and a paddle frame rotatably mounted in the steam chamber to rotate about a central axis. In accordance with the invention, the paddle frame has at least one scoop mounted on a periphery thereof that extends longitudinally in spaced parallel relation to the central axis and that is disposed in spaced relation to the outlet of the housing for scooping loose fill material delivered into the steam chamber peripherally of the steam chamber.
Preferably, the paddle frame is provided with a pair of scoops disposed in diametrically spaced apart relation. Each scoop is positioned to pass a short distance, for example, approximately 3 to 4 inches, from the outlet from the housing so that they elements of the loose fill material are gently moved away from the entrance to the steam chamber to avoid clumping thereat and without chipping or flaking of the surfaces of the elements.
In addition, the housing has an inlet to receive a flow of loose fill material and a screw that is rotatably mounted in the housing with a plurality of flights for conveying the loose fill material received towards the outlet of the housing. In accordance with the invention, at least some of the screw flights that are disposed in alignment with the inlet are of a smaller radius than the remainder of the flights. In this way, an annular space is provided about the flights of reduced diameter to allow the elements of the loose fill material to the gently received and conveyed along the remainder of the screw without being unduly compressed. As a result, chipping, cracking and flaking of the elements is avoided.
In order to provide for multiple passes of a latent foaming loose fill material through the steam chamber, the steam expander is provided with a second hopper and a second housing similar to the first housing. In this embodiment, one hopper is used to feed a latent foaming loose fill material into the steam expander for expansion to a first state of expansion. After the expanded material has been cured, the material is passed through the second hopper into the second housing and conveyed in a similar fashion into the steam expander for further expansion. In this regard, the second housing is larger diameter than the first housing in order to accommodate the expanded state of the elements of the loose fill material. After the loose fill material has been expanded and cured in the second stage, the loose fill material may be recycled through the second hopper and second housing into the steam expander for a third and final stage of expansion and curing.
These and other objects and advantages of the invention will be, more apparent from the following detailed description taken in conjunction with the accompanying drawings wherein:
Referring to
As shown in
The manner in which the hoppers 13,14 operate to feed material to the housings 11,12 is well known and need not be further described.
Referring to
The other housing 11 is of smaller diameter than the housing 12 and is provided with a screw (not shown) of similar construction to the screw 19 but of smaller diameter to fit into the housing 11 and need not be further described. Each screw is driven from a separate drive (not shown) from the other located within a motor housing 24 (see
Referring to
Referring to
Additional paddle frames (not shown) may also be provided in the steam chamber 25 for purposes such as described in U.S. Pat. No. 4,379,106.
The spacing of each scoop 28 from the outlet 20 of the housing 12 and the not shown outlet of the housing 11 is sufficient to allow the scoop 28 to gently move the delivered loose fill material away from the inlet end of the steam chamber 25 to avoid accumulation thereat without fracturing, splitting or flaking of the individual elements of the material. In this respect, each scoop 28 has an L shape but made also be made of other suitable shapes, such as a curved or concave shape. Each scoop 24 not only extends longitudinally of the chamber 25 as shown in
As illustrated in
The paddle frame 26 is of skeletal construction being formed of a pair of plates 29 that are secured coaxially to and along the central rotatable shaft 27. These plates 29 support a pair of paddles 30 therebetween which serve to agitate and move the loose fill material delivered into chamber 25. The L-shaped scoops 28 are connected as by welding to the forward plate 29 in line with the paddles 30.
By way of example, the plates 29 have a length of 31 ¼ inches and a width of 3 inches. Each scoop 28 has a height of 4 inches and projects peripherally (i.e. perpendicularly) from the plane of the plates 25 a distance of 4 inches and projects longitudinally forward a distance of 4 inches.
In operation, a mass of latent foaming loose fill thermoplastic material is delivered into the first hopper 11 and passed through the housing 13 into the steam chamber 21. During this time, the elements of loose fill material are heated and expanded. For example, the loose fill elements may be expanded from a bulk density of 30 pounds per cubic foot to achieve an expanded bulk density of 0.6 pounds per cubic foot.
Since the latent foaming loose fill elements are hard, any harsh mechanical working of the elements may cause flaking or cracking of the elements which, in turn, may lead to the formation of dust. Consequently, the working parameters of the housing 11 and paddle frame 26 are such as to minimize the risk of dust formation.
During operation of the screw in the housing 11, the screw 19 in the other housing 12 is also rotating and vice versa to prevent back feed of the loose fill material. In this respect, the speed of the screw in the housing that is not delivering material to the steam chamber 21 is operated at a slow speed, that is at a speed less than the normal operating speed.
After a suitable curing time has passed, the expanded material is delivered into the second hopper 12 via suitable means such as described in U.S. Pat. No. 4,379,106 and passed through the second housing 14 into the steam chamber 25 for a second stage of heat expansion. For example, during this time, the loose fill material is expanded to achieve a bulk density of 0.3 pounds per cubic foot. Again, after a suitable curing time has passed, the loose fill material is re-cycled through the hopper 12 and housing 14 into the steam chamber 25 for a third pass. During this time, the loose fill material is expanded to achieve a bulk density of 0.18 to 0.2 pounds per cubic foot.
Any number of passes may be used to expand the original mass of latent foaming loose fill material. However, three passes should be sufficient to reduce the overall weight per cubic foot of the material to a suitable range for packaging purposes.
During passage through the respective housings 13,14 and steam chamber 25, the loose fill material is gently moved without fracturing, splitting or flaking of the individual elements. In this way, little or no dust is created in the final product. Hence, when the expanded loose fill material is used by the ultimate consumer, there is little or no dust to contend with by the consumer and the surrounding environment.
The invention thus provides a clean and economical apparatus for expanding latent foaming loose fill material without creating dust.