The present invention relates to a tyre retreading method and system.
The present invention may be used to advantage in retreading truck tyres, to which the following description refers purely by way of example.
Cold-retreading of a truck tyre normally comprises removing the worn tread from the tyre, and applying a new tread to the tyre carcass. To apply a new tread to a carcass, a green-rubber intermediate strip or cushion and a pre-cured tread (PCT) strip are wound about the carcass; and the carcass is then inserted inside an autoclave and cured further to achieve optimum adhesion of the tread to the carcass by means of the bonding action of the cushion.
One example of a pre-cured tread strip ready for application to a tyre carcass is described in U.S. Pat. No. 5,277,727A1. And one example of a station for retreading a tyre using the above method is described in U.S. Pat. No. 6,368,439B1.
Before the green-rubber cushion is applied, the lateral surface of the carcass is sprayed with a liquid (so-called cement) with a green-rubber and normalheptane (or other organic solvent) base to assist adhesion of the green-rubber cushion to the carcass for retreading.
Applying cement, however, involves numerous drawbacks, in that, the cement being volatile and potentially highly pollutant, application calls for the use of a high-cost, bulky, insulated cementing booth (normally insulated with rock wool, which must be disposed of using appropriate, high-cost disposal methods); the cement is stored in drums, which must also be disposed of using appropriate, high-cost disposal methods; the presence of cement between the cushion and tread strip, i.e. of a heterogeneous material interposed between two layers of rubber, may impair performance of the retreaded tyre; and, finally, organic solvents such as those contained in the cement being highly pollutant, avoiding application of organic-solvent-based cement greatly reduces overall pollution of the tyre retreading process. In this connection, it is important to note that recent United Europe regulations (VOC 13/1999/EC) call for a 75% reduction in the use of organic solvents in industry by the year 2007.
U.S. Pat. No. 5,635,015A1 describes a tyre retreading method whereby, to avoid using cement, the green-rubber cushion is heated, before being wound onto the carcass, to improve adhesion of the green-rubber cushion, so cement is superfluous. Heating the green-rubber cushion, however, has been found to also soften it, thus making it more difficult to wind about the carcass.
It is an object of the present invention to provide a tyre retreading method and system designed to eliminate the aforementioned drawbacks, and which, in particular, are cheap and easy to implement.
According to the present invention, there are provided a tyre retreading method and system as claimed in the accompanying Claims.
A non-limiting embodiment of the present invention will be described by way of example with reference to the accompanying drawings, in which:
Number 1 in
At preparation station 3, the worn tread (not shown) is removed from tyre 2, and the lateral surface 7 (shown in
The filled carcass 6 is then transferred to winding station 4, where an intermediate strip or cushion 8 of green rubber and a tread strip 9 are wound about carcass 6.
As shown in
Building machine 10 also comprises a heating device 15 located close to drum 11, upstream from feed conveyor 12 (as shown in
In a preferred embodiment, building machine 10 comprises a blower 17 located close to drum 11, upstream from heating device 15 in the rotation direction of drum 11. Prior to heating, blower 17 blows a jet of compressed air in a substantially tangential direction onto lateral surface 7 of carcass 6 or onto the outer surface of green-rubber cushion 8, substantially for the purpose of further cleaning, and particularly removing dust from, lateral surface 7 of carcass 6 or the outer surface of green-rubber cushion 8. In one possible embodiment, the compressed air from blower 17 may be heated by electric resistors to assist heating.
In actual use, carcass 6 is mounted on drum 11, and green-rubber cushion 8 and tread strip 9 are wound about carcass 6 by rotating drum 11; and heating device 15 and blower 17 are activated as drum 11 rotates.
In a preferred embodiment, building machine 10 is used to manually wind green-rubber cushion 8 about carcass 6 separately from tread strip 9, and is then used to wind tread strip 9 about carcass 6 and on top of the previously wound green-rubber cushion 8. In which case, heating device 15 and blower 17 act on both lateral surface 7 of carcass 6 as green-rubber cushion 8 is wound on, and on the outer surface of green-rubber cushion 8 as tread strip 9 is wound on.
In an alternative embodiment, green-rubber cushion 8 is superimposed on tread strip 9, off building machine 10, by means of a pair of known mutually cooperating pressure rollers (not shown), and green-rubber cushion 8 and tread strip 9 are then wound together about carcass 6 on building machine 10. In which case, heating device 15 and blower 17 only act on lateral surface 7 of carcass 6 as green-rubber cushion 8 and tread strip 9 are wound on together.
Lateral surface 7 of carcass 6 and/or the outer surface of green-rubber cushion 8 are/is preferably heated to a temperature ranging between 50° C. and 75° C. It is important to note that below 50° C. fails to provide for sufficiently strong adhesion, and over 75° C. may result in partial, irregular surface curing of green-rubber cushion 8, which impairs not only the success of the retreading process, but also performance of the retreaded tyre 2.
It is important to note that green-rubber cushion 8 may be calendered or extruded. If extruded directly on building machine 10, green-rubber cushion 8 has a temperature of about 75-80° C. as a result of the extrusion process, so lateral surface 7 of carcass 6 may not need heating, or may be heated to a relatively low temperature, when winding on the extruded green-rubber cushion 8.
Once green-rubber cushion 8 and tread strip 9 are wound about carcass 6, tyre 2 is transferred to curing station 5 (shown schematically in
The retreading method described above eliminates cementing of the lateral surface 7 of carcass 6, while still achieving optimum adhesion of green-rubber cushion 8 to carcass 6. Heating lateral surface 7 of carcass 6, before winding on green-rubber cushion 8, in fact, improves adhesion of carcass 6 to green-rubber cushion 8. It should be stressed that only lateral surface 7 of carcass 6, and not green-rubber cushion 8, is heated, thus preventing green-rubber cushion 8 from softening and so being difficult to wind about carcass 6.
As stated, eliminating cementing of lateral surface 7 of carcass 6 greatly reduces both the cost and pollution of the retreading process.
Number | Date | Country | Kind |
---|---|---|---|
TO2006A0499 | Jul 2006 | IT | national |
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/EP2007/056916 | 7/6/2007 | WO | 00 | 6/23/2009 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2008/003786 | 1/10/2008 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
4096008 | Taylor | Jun 1978 | A |
4149926 | Taylor | Apr 1979 | A |
4407220 | Fesmire | Oct 1983 | A |
5277727 | Seiler et al. | Jan 1994 | A |
5568822 | Michelson | Oct 1996 | A |
5635015 | Longo et al. | Jun 1997 | A |
5755904 | Longo et al. | May 1998 | A |
6328836 | Ogawa | Dec 2001 | B1 |
6368439 | Bender et al. | Apr 2002 | B1 |
6758931 | Daugherty et al. | Jul 2004 | B1 |
6998006 | Kessler et al. | Feb 2006 | B1 |
20050034804 | Usami et al. | Feb 2005 | A1 |
Number | Date | Country |
---|---|---|
102 28 372 | Jun 2003 | DE |
0 054 533 | Jun 1982 | EP |
0 730 950 | Sep 1996 | EP |
1 120 235 | Aug 2001 | EP |
Number | Date | Country | |
---|---|---|---|
20090320988 A1 | Dec 2009 | US |