This application claims benefit of priority to Korean Patent Application No. 10-2017-0180143 filed on Dec. 26, 2017 in the Korean Intellectual Property Office, the disclosure of which is incorporated herein by reference in its entirety.
The present disclosure relates to a wire wound inductor and a manufacturing method thereof.
An inductor, a basic passive element, serves to supply a stable voltage to various components in a product, or to increase or decrease a level of a voltage.
Currently, various types of inductor have been developed and used. Thereamong, a wire wound inductor has a structure in which a winding coil is embedded in a magnetic core. Here, the winding coil and the magnetic core need to be insulated from each other while having sufficient coupling force therebetween.
An aspect of the present disclosure may provide a wire wound inductor.
Another aspect of the present disclosure may provide a manufacturing method of a wire wound inductor.
According to an aspect of the present disclosure, a wire wound inductor may include: a winding coil; a magnetic core embedding the winding coil; and an adhesive portion disposed between the magnetic core and the winding coil and enclosing the winding coil.
According to another aspect of the present disclosure, a manufacturing method of a wire wound inductor may include: attaching a tape on a first surface of a frame which has a hole; loading at least one winding coil in the hole of the frame, the at least one winding coil being attached to the tape; coating a first insulating adhesive film on a second surface of the frame opposing the first surface; and removing tape attached on the first surface of the frame.
The above and other aspects, features, and advantages of the present disclosure will be more clearly understood from the following detailed description taken in conjunction with the accompanying drawings, in which:
Exemplary embodiments of the present disclosure will now be described in detail with reference to the accompanying drawings.
The winding coil 11 is a coil formed by winding a conductive wire at least one turn, and may be stacked in two or more layers, if necessary. The winding coil 11 may be a flat wire coil type, and the wire wound inductor according to the exemplary embodiment in the present disclosure may thus be a chip type. However, the types of the winding coil and the wire wound inductor may be variously changed.
The winding coil 11 may be formed of any one or a mixture of at least two of a noble metal material such as silver (Ag), lead (Pb), platinum (Pt), or the like, nickel (Ni), and copper (Cu) which have excellent conductivity. In addition, the winding coil 11 may further include an insulating film coated on a surface of a wire to secure insulation among wires of the winding coil 11.
Further, an end portion of the winding coil 11 may extend toward the outside of the magnetic core 31, and the extended portion may be electrically connected to an external electrode (not illustrated).
The adhesive portion 21 may be implemented by an insulating adhesive film. For example, the adhesive portion 21 may be formed using an Ajinomoto Build-up Film (ABF). Further, the adhesive portion 21 may be formed to enclose the entire winding coil 11. In addition, the adhesive portion 21 may be formed even in a central portion and an outer side portion of the winding coil 11. The adhesive portion 21 formed in the central portion and the outer side portion of the winding coil 11 may be positioned in the vicinity of a center of the winding coil 11 in a thickness direction. Accordingly, the magnetic core 31 may be formed on and beneath the adhesive portion 21 formed in the central portion and the outer side portion of the winding coil 11. The adhesive portion 21 may insulate the winding coil 11 from the magnetic core 31, and at the same time, improve coupling force between the winding coil and the magnetic core 31. Further, in a process of manufacturing the wire wound inductor, the adhesive portion 21 may secure connectivity between the winding coil 11 and a frame, thereby reducing defects caused by misalignment of the winding coil during manufacture of the wire wound inductor. In addition, in the process of manufacturing the wire wound inductor, the adhesive portion 21 may suppress separation of the frame from the winding coil 11 before stacking a sheet and/or during stacking of a sheet, thereby reducing a defect that the frame is separated.
The magnetic core 31 may be formed of a magnetic resin composite in which metal magnetic powder and a resin mixture are mixed. The metal magnetic powder may be formed of at least one of, for example, Fe—Ni, amorphous Fe, Fe, an Fe—Cr—Si alloy, and an Fe—Si—Al alloy, and the resin mixture may be formed of at least one of, for example, an epoxy, polyimide, and a liquid crystal polymer (LCP), but the materials of the metal magnetic powder and the resin mixture are not limited thereto. The magnetic core 31 may function as a space in which a magnetic path is formed, the magnetic path being a path through which a magnetic flux induced in the winding coil 11 when a current is applied to the winding coil 11 passes. The magnetic core 31 may be formed so that the winding coil 11 is embedded therein. At this time, at least a portion of each of both ends of the winding coil 11 may be exposed to the outside of the magnetic core 31 to be connected to an external electrode.
A winding coil 12 and a magnetic core 32 may be the same as the winding coil 11 and the magnetic core 31 described in
Further, an adhesive portion 22 may be the same as the adhesive portion 21 described in
In the manufacturing method of a wire wound inductor according to an exemplary embodiment in the present disclosure, a plurality of winding coils 10 may be loaded in hollow portions formed in a frame 40.
Then, an insulating adhesive film 20-1 may be positioned and then compressed on one surface of the frame 40 and an insulating adhesive film 20-2 may be positioned and then compressed on the other surface of the frame 40 to form an adhesive portion (21 in
In addition, at least one magnetic sheet 30-1 may be positioned and then compressed on one surface of the frame 40 and at least one magnetic sheet 30-2 may be positioned and then compressed on the other surface of the frame 40 to form a magnetic core (31 in
After the insulating adhesive film 20-1 is compressed and before the insulating adhesive film 20-2 is attached to the winding coils 10 and compressed, a tape, which is attached on the other surface of the frame 40 to allow the winding coils 10 to be disposed in the accommodation spaces provided by the frame 40 and by the tape, may be removed. In this process, a phenomenon that a portion of the frame 40 is separated from the other portion of the frame 40 may occur, when the tape is removed from the frame. However, in accordance with the manufacturing method of a wire wound inductor according to the exemplary embodiment in the present disclosure, the insulating adhesive film 20-1 increasing a coupling force between the winding coils 10 and the frame 40 may prevent the separation phenomenon, when the tape is removed from the frame 40.
The manufacturing method of a wire wound inductor according to the exemplary embodiment in the present disclosure will be described below with reference to
First, the winding coils 10 and the frame 40 may be prepared (S110).
Next, each of the winding coils 10 may be loaded in a designated position in the frame 40 (S120).
Next, the insulating adhesive film 20-1 may be coated on one surface (e.g., upper surface) of the frame 40 in which the winding coils 10 are loaded (S130). For example, the insulating adhesive film 20-1 may be positioned and then compressed on one surface of the frame 40.
Next, at least one magnetic sheet 30-1 may be positioned and then compressed on one surface of the frame 40 on which the insulating adhesive film 20-1 is coated (S140). As described above, according to the exemplary embodiment in the present disclosure, connectivity between the winding coils 10 and the frame 40 may be sufficiently secured by the insulating adhesive film, such that misalignment of the coil when compressing the magnetic sheet 30-1 may be prevented. Therefore, according to the exemplary embodiment in the present disclosure, a yield may be improved.
Next, the tape attached on the other surface of the frame 40 may be removed (S150). As described above, according to the exemplary embodiment in the present disclosure, adhesive force between the winding coil 10 and the frame 40 is increased by the insulating adhesive film 20-1, thereby suppressing separation of the frame 40. Therefore, according to the exemplary embodiment in the present disclosure, a yield may be improved.
Next, the insulating adhesive film 20-2 may be coated on the other surface (e.g., lower surface) of the frame 40 in which the winding coils 10 are loaded (S160). For example, the insulating adhesive film 20-2 may be positioned and then compressed on the other surface of the frame 40.
Next, at least one magnetic sheet 30-2 may be positioned and then compressed on the other surface of the frame 40 on which the insulating adhesive film 20-2 is coated (S170). An individual structure including a respective magnetic core, a respective winding coil, and respective insulating adhesive films may be separated from the frame 40 and become a wire wound inductor. Accordingly, a plurality of wire wound inductors may be formed when the respective structures are separated from the frame 40.
The manufacturing method of a wire wound inductor according to the exemplary embodiment in the present disclosure will be described below with reference to
First, the winding coils 10 and the frame 40 may be prepared (S210).
Next, each of the winding coils 10 may be loaded in a designated position in the frame 40 (S220).
Next, the insulating adhesive film 20-1 may be coated on one surface (e.g., an upper surface) of the frame 40 in which the winding coils 10 are loaded (S230). For example, the insulating adhesive film 20-1 may be positioned and then compressed on one surface of the frame 40.
Next, the tape attached on the other surface of the frame 40 may be removed (S240). As described above, according to the exemplary embodiment in the present disclosure, adhesive force between the winding coil 10 and the frame 40 is increased by the insulating adhesive film 20-1, thereby suppressing separation of the frame 40. Therefore, according to the exemplary embodiment in the present disclosure, a yield may be improved.
Next, the insulating adhesive film 20-2 may be coated on the other surface (e.g., lower surface) of the frame 40 in which the winding coils 10 are loaded (S250). For example, the insulating adhesive film 20-2 may be positioned and then compressed on the other surface of the frame 40.
Next, the insulating adhesive films 20-1 and 20-2 positioned in a central portion of the winding coil 10 may be removed through laser processing (S260). The laser processing may be performed by irradiating a laser beam on the central portion of the first and second insulating adhesive films 20-1 and 20-2 to remove the central portions of the first and second insulating adhesive films 20-1 and 20-2.
Next, at least one magnetic sheet 30-1 may be positioned and then compressed on one surface of the frame 40 on which the insulating adhesive film 20-1 is coated (S270). As described above, according to the exemplary embodiment in the present disclosure, connectivity between the winding coils 10 and the frame 40 may be sufficiently secured by the insulating adhesive films, such that misalignment of the coil when compressing the magnetic sheet 30-1 may be prevented. Therefore, according to the exemplary embodiment in the present disclosure, a yield may be improved.
Next, at least one magnetic sheet 30-2 may be positioned and then compressed on the other surface of the frame 40 on which the insulating adhesive film 20-2 is coated (S280). An individual structure including a respective magnetic core, a respective winding coil, and respective insulating adhesive films may be separated from the frame 40 and become a wire wound inductor. Accordingly, a plurality of wire wound inductors may be formed when the respective structures are separated from the frame 40.
As set forth above, the wire wound inductor and the manufacturing method thereof according to exemplary embodiments of the present disclosure, insulation between the winding coil and the magnetic core may be secured, and at the same time, coupling force therebetween may be enhanced, such that durability of the wire wound inductor may be enhanced. Further, in a process of manufacturing the wire wound inductor, connectivity between the coil and the frame may be secured, such that defects caused by misalignment of the coil may be reduced. In addition, separation of the frame from the coil may be suppressed, such that a defect that the frame is separated at the time of stacking the magnetic sheet may be reduced.
While exemplary embodiments have been shown and described above, it will be apparent to those skilled in the art that modifications and variations could be made without departing from the scope of the present invention as defined by the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
10-2017-0180143 | Dec 2017 | KR | national |
Number | Name | Date | Kind |
---|---|---|---|
7012784 | Sasaki | Mar 2006 | B2 |
8174349 | Yoshida | May 2012 | B2 |
9142343 | Ohkubo | Sep 2015 | B2 |
9437363 | Choi | Sep 2016 | B2 |
9490656 | Kurz | Nov 2016 | B2 |
9659709 | Chang | May 2017 | B2 |
10026539 | Yang | Jul 2018 | B2 |
10074473 | Kim | Sep 2018 | B2 |
10211137 | Chen | Feb 2019 | B2 |
10529476 | Park | Jan 2020 | B2 |
10553346 | Ryu | Feb 2020 | B2 |
10902991 | Moon | Jan 2021 | B2 |
10916366 | Lee | Feb 2021 | B2 |
20080236870 | Kuwajima | Oct 2008 | A1 |
20090280153 | Hunter | Nov 2009 | A1 |
20130181668 | Tabata | Jul 2013 | A1 |
20140159228 | Teh | Jun 2014 | A1 |
20140285305 | Yoo | Sep 2014 | A1 |
20150102889 | Choi | Apr 2015 | A1 |
20150145635 | Kurz | May 2015 | A1 |
20150255206 | Han et al. | Sep 2015 | A1 |
20150270053 | Cha | Sep 2015 | A1 |
20160086721 | Park | Mar 2016 | A1 |
20160155556 | Ohkubo | Jun 2016 | A1 |
20160268040 | Kim et al. | Sep 2016 | A1 |
20160276088 | Kwon et al. | Sep 2016 | A1 |
20160372259 | Banba | Dec 2016 | A1 |
20170032885 | Lee et al. | Feb 2017 | A1 |
20170178798 | Yoon et al. | Jun 2017 | A1 |
20170194226 | Chen | Jul 2017 | A1 |
20190326047 | Yamaguchi | Oct 2019 | A1 |
Number | Date | Country |
---|---|---|
104900374 | Sep 2015 | CN |
105448465 | Mar 2016 | CN |
106898479 | Jun 2017 | CN |
2004-040001 | Feb 2004 | JP |
2005-347542 | Dec 2005 | JP |
2015187260 | Oct 2015 | JP |
10-1153954 | Jun 2012 | KR |
10-2014-0083733 | Jul 2014 | KR |
10-2016-0051695 | May 2016 | KR |
10-2016-0134633 | Nov 2016 | KR |
10-2017-0015103 | Feb 2017 | KR |
10-2017-0090144 | Aug 2017 | KR |
Entry |
---|
Office Action issued in corresponding Chinese Patent Application No. 201811097372.5 dated Jul. 16, 2020, with English translation. |
Second Office Action issued in corresponding Chinese Patent Application No. 201811097372.5 dated Mar. 3, 2021, with English translation. |
Office Action issued in corresponding Chinese Patent Application No. 201811097372.5 dated Oct. 25, 2021, with English translation. |
Korean Office Action dated Jul. 1, 2022, issued in corresponding Korean Patent Application No. 20217567.5. |
Korean Office Action dated Jul. 1, 2022, issued in corresponding Korean Patent Application No. 10-2017-0180143. |
Number | Date | Country | |
---|---|---|---|
20190198235 A1 | Jun 2019 | US |