Claims
- 1. A process for the preparation of an electroconductive zinc oxide sintered body, which comprises the steps of:
- mixing powdery zinc oxide and a powdery hydrate of at least one oxide of an element having a positive valency of at least 3, and
- sintering the mixture at a temperature of at least 1,300.degree. C.;
- said element being selected from the group consisting of Sc and Y of groups IIIB of the Periodic Table, B, Al, Ga, In and Tl of the group IIIA, Ti, Zr, Hf and Th of the group IVB, C, Si, Ge, Sn and Pb of the group IVA, V, Nb, Ta and Pa of the group VB, As, Sb and Bi of the group VA, Cr, Mo, W and U of the group VIB, Se, Te and Po of the group VIA, Mn, Tc and Re of the group VIIB, Fe, Co, Ni, Ru, Rh, Pd, OS, Ir and Pt of the group VIII, lanthanide elements, and actinide elements, and the amount of said element being from 0.1 to 20 atomic % based on the amount of the zinc of the zinc oxide.
- 2. The process according to claim 1, wherein the amount of the element having a positive valency of at least 3 is from 0.5 to 5 atomic % based on the amount of the zinc of the zinc oxide.
- 3. The process according to claim 1, wherein the mixture of the oxide of the element having a positive valency of at least 3 and the zinc oxide is first molded, and the resulting molded mixture is then subjected to sintering.
- 4. The process according to claim 1, wherein the sintering is carried out at a temperature of from 1,400.degree. C. to 1,500.degree. C. for from 5 to 20 hours.
- 5. The process according to claim 1, wherein the sintering is carried out at a temperature of from 1,450.degree. C. to 1,500.degree. C.
Priority Claims (2)
Number |
Date |
Country |
Kind |
1-205573 |
Aug 1989 |
JPX |
|
2-106599 |
Aug 1990 |
JPX |
|
Parent Case Info
This is a division of application Ser. No. 07/563,153, filed Aug. 6, 1990, pending.
US Referenced Citations (6)
Divisions (1)
|
Number |
Date |
Country |
Parent |
563153 |
Aug 1990 |
|