The invention relates to the field of semiconductor processing, and, more particularly, to an apparatus and method for the atomic layer deposition of films onto semiconductor substrates.
Atomic layer deposition (ALD) is a thin film deposition method that allows for the deposition of films having thicknesses on the order of nanometers in a precisely controlled way. Typically, ALD uses two or more gaseous precursors that are alternately and repeatedly applied to a substrate.
A series of sequential steps in which a surface of the substrate is exposed to all precursors is called a deposition cycle. Each deposition cycle grows a single monolayer of film, or a fraction of a monolayer. This is due to the fact that in ALD the film growth depends on chemisorption, a process whereby a precursor molecule adheres to a substrate's surface through the formation of a chemical bond without further thermal decomposition of the precursor molecule taking place. Chemisorption stops naturally when all substrate surface sites available for chemical bonding with a precursor have been covered. Exposing the substrate to the second precursor results in a chemical reaction of the second precursor with the chemisorbed first precursor under the formation of a solid film, until all of the chemisorbed first precursor has been reacted and the substrate is covered with a layer of chemisorbed second precursor in a self-limiting manner. Consequently, ALD is a self-limiting layer-by-layer deposition method that offers highly conformal coating and excellent thickness control. These characteristics make it a method of interest to various industries, among which in particular the semiconductor, and more specifically, the solar cell industry.
In the solar cell industry, ALD may be used to deposit aluminum oxide (Al2O3) films for the passivation of advanced mono-Si solar cells. To this end typical film thicknesses of 5-15 nm are required, which can be achieved using traditional single or multi-wafer ALD systems. Currently, the throughput of the most efficient multi-wafer ALD systems at said film thickness is about 60 wafers per hour. The amount of surface area to be treated in order to obtain—for example—a solar cell panel for use on a rooftop, is considerable however. And with the demand for solar cell panels on the rise, there is an increasing need for ALD apparatus featuring a higher throughput.
The above-described ALD application is exemplary, and merely one of many in which the continual pressure within the semiconductor industry and related industries, such as solar cell industry or flat panel display industry, for an increased throughput is felt. It is therefore on object of the present invention to provide a device and a method for atomic layer deposition offering a much improved throughput capacity.
According to one aspect of the invention, an atomic layer deposition apparatus is provided for depositing a film onto a train of substrates, or a continuous substrate in tape form, in a continuous fashion. The apparatus includes a process tunnel, extending in a transport direction and bounded by at least a first and a second wall. The walls are mutually parallel and spaced apart so as to allow a substantially flat substrate, oriented parallel to the walls, to be accommodated there between. The apparatus further includes a transport system for carrying and moving a train of said substrates or a continuous substrate in tape form, from an entrance of the tunnel, along the transport direction, to an exit thereof. At least the first wall of the process tunnel is provided with a plurality of gas injection channels, which channels are disposed in a spaced apart manner along the transport direction and which channels, viewed in the transport direction, are connected successively to a first precursor gas source, a purge gas source, a second precursor gas source and a purge gas source respectively, so as to create a tunnel segment that—in use—comprises successive zones containing a first precursor gas, a purge gas, a second precursor gas and a purge gas, respectively. Two or more of such segments are disposed behind one another in the transport direction.
According to another aspect of the invention, a method for growing a thin film on a substrate is provided. The method includes providing a process tunnel that extends longitudinally in a transport direction from an entrance to an exit, and that is capable of accommodating one or more substantially flat substrates. The method also includes bringing about a longitudinal division of the process tunnel into two or more functional segments, wherein each segment comprises at least four laterally extending gas zones that successively contain a first precursor gas, a purge gas, a second precursor gas and a purge gas. The method further includes moving a substrate through the process tunnel into the transport direction, such that the substrate is successively subjected to the gases in the successive gas zones, and an atomic layer is deposited onto the substrate when it passes by all at least four zones of a single segment.
These and other features and advantages of the invention will be more fully understood from the following detailed description of certain embodiments of the invention, taken together with the accompanying drawings, which are meant to illustrate and not to limit the invention.
This patent application claims priority from U.S. Non-Provisional patent application Ser. No. 12/993,562, filed Feb. 4, 2011, which is a National Stage Entry of PCT/NL09/50271, filed May 20, 2009, which claims priority from U.S. Non-Provisional patent application Ser. No. 12/123,745, filed May 20, 2008, the disclosures of which are incorporated by reference herein in their entirety.
The apparatus provided by the present disclosure includes a process tunnel through which a substrate, preferably as part of a train of substrates, may be transported in a linear manner. That is, the substrate may be inserted into the tunnel at an entrance thereof to be conveyed to an exit. The tunnel is bounded by at least two, substantially parallel tunnel walls. Preferably, the tunnel walls are located close to both the substrate and each other, to provide an elongate processing space with a minimum of volume. In its longitudinal direction, the process tunnel may be divided into a series of segments, each segment comprising a number—typically four—of laterally extending gas zones. Successive zones within a segment contain gas injection channels for a first precursor gas, a purge gas, a second precursor gas, and a purge gas respectively. As the substrate is transported through the tunnel, its surface is subjected stripwise to contact with the different gases. If the arrangement of the zones and the respective gases are chosen properly, transporting a substrate through one tunnel segment is equivalent to subjecting it to one atomic layer deposition cycle. Since the tunnel may contain as many segments as desired, a film of arbitrary thickness may be grown on a substrate being conveyed from the entrance to the exit of the tunnel. The linear nature of the process tunnel allows for a continuous stream of substrates to be processed, thus delivering an atomic layer deposition apparatus with an appreciably improved throughput capacity.
It is noted that, in the appended figures, the same or similar devices, parts, spaces, orientations etc. may have been indicated by the same reference numeral. Also, for reasons of clarity, reference numerals in some figures may have been omitted when the object of reference is already identified in one or more preceding figures.
Tunnel wall 104 is fitted with a plurality of gas injection channels 102, 102′ etc., the outflow openings of which may be distributed over the wafer facing (i.e. inside) surface of the tunnel wall, both along the lateral and the longitudinal direction thereof. In the illustration of
The gas injection channels 102, 102′, etc. are connected to gas sources (not shown in
In
The dimensions and working parameters of the disclosed atomic layer deposition apparatus may vary, depending on the specific application it is built and used for. For example, depositing a 10 nm film of aluminum oxide onto a standard circular 300 mm silicon wafer may involve two precursors, tri-methyl aluminum (Al(CH3)3, TMA) and water (H2O). As an alternative for water, ozone (O3) may be used. Nitrogen (N2) may be used both as an inert carrier gas in the precursor zones and as purge gas in the purge gas zones. Each of the zones may have a length of several centimeters, typically 2-5 cm, in the transport direction. To accommodate a single stream of wafers having a lateral dimension of 300 mm, the width of the process tunnel needs to measure a little over 300 mm. In case a precursor zone measures 5 cm in length, whereas a purge gas zone measures 2 cm, the length of a single tunnel segment amounts to 0.14 m. As a single tunnel segment is responsible for depositing one monolayer of aluminum oxide of about 0.1 nm thickness, a total of 100 segments is required to grow a 10 nm film. Consequently, the length of the process tunnel comes to approximately 14 meters. Wafers may be transported through the tunnel at a speed as high as 0.25 m/s, which, for this specific example, would lead to a throughput capacity of about 3000 wafers per hour.
A general measure that may be taken to further increase the throughput capacity of a disclosed ALD apparatus is to widen the process tunnel, so as to enable it to accommodate two or more parallel streams of substrates. See for example
Another general measure is providing both the first and the second tunnel wall with gas injection channels, wherein an inert bearing gas may be provided from the bottom wall, as shown in
An alternative configuration is shown in
In
Further, in contrast to any other ALD system known to date, the apparatus may operate at atmospheric pressure. No vacuum pumps are necessary to reduce the pressure in the tunnel space. Operation at around 1 atmosphere is feasible due to the combination of narrow gaps between the substrates 108, 108′, etc. on the one hand, and the tunnel walls 104, 106 on the other, and a high gas flow. In the proposed apparatus, typical gas flow velocities lie in the range of 1-2 m/s.
Due to the absence of tunnel wall deposition and vacuum pumps, said apparatus may be virtually maintenance free.
The transport system based on the floating wafer technology, as shown in
In a first option, a driving force is applied to a train of substrates at a single location, preferably at the entrance of the process tunnel. The force may, for example, be applied by an insertion mechanism that continuously or semi-continuously inserts a new (last) wafer into the tunnel for processing. It may use the new wafer to push the train of substrates already present in the tunnel forward. As all substrates in the tunnel are floating, the force required to do so is relatively small. Each of the substrates already in the tunnel is driven in the transport direction by a next wafer in line, due to physical contact between their edges. As a constant throughput speed is not essential to the self-limiting atomic layer deposition process, hiccups in the supply of new wafers—which would automatically influence the transport speed of the wafers in the tunnel—do not influence the quality or thickness of the deposited layers. This first option is illustrated in
In a second option, illustrated by
A third option is illustrated in
A fourth option is to provide grooves in the tunnel walls, the grooves being elongated in the longitudinal direction and having one end proximate a gas injection channel, as disclosed in U.S. Pat. No. 6,824,619 of applicant, which is incorporated herein by reference, where it is used to impart a rotational movement on a floating substrate. Similarly, this method can be used to impart a linear movement to a substrate.
As the quality of a film may depend on the surface temperature of the substrate during processing, substrates may be preheated before being subjected to the deposition process. Preheating of a substrate may be done by providing the deposition apparatus with a special pre-heat tunnel segment, located upstream of the first reactive tunnel segment, i.e. the first tunnel segment wherein a substrate is subjected to two or more precursors. In the pre-heat tunnel segment, a substrate may be brought into contact with no more than a purge gas, which is kept at the same or at a higher temperature than that of the reactive sections. Similarly, a cool-down segment may be provided at the end of the process tunnel, downstream of the last reactive tunnel segment. As the primary purpose of the purge gas in the pre-heat and cool-down segments is to transfer heat, helium—which has a relatively high thermal conductivity—is a good choice that helps to minimize the length of such a segment.
Further, to facilitate the loading and discharging of substrates into/from the process tunnel by a mechanical substrate handler, a first and a last segment of the tunnel—reactive or non-reactive—may be provided with a larger gap between the tunnel walls to increase the gap between the upper and lower surface of an inserted wafer and the upper and lower tunnel wall respectively. A larger gap between the tunnel walls and the substrate comes at the penalty of an increased gas flow rate, since the force to be delivered by the gas bearing to carry the weight of the substrate does not change.
Entrance section 900 is shown schematically in a lateral cross-sectional view in
Above, the invention has been described in terms of a first and a second precursor. One skilled in the art will recognize, however, that ALD may be performed using more than two precursors. It is emphasized here, that the language of the claims does not intend to exclude an atomic layer deposition apparatus featuring three, four or more precursors. To that end, each segment may comprise three, four or more precursor gas injection zones all separated by purge gas injection zones. Also nanolaminate films may be deposited. For this purpose, a number of successive segments of a first configuration for depositing a number of monolayers of a first film having a first composition, can be alternated by a number of successive segments of a second configuration, for depositing a number of monolayers of a second film having a second composition. And this sequence of segments can be repeated until the desired number of nanofilms is deposited.
The substrate may have a circular form, a square form, a rectangular form or triangular form or any other form that is available. Preferably, the form of the substrate is such that it allows a good filling of a surface area when the substrates are placed adjacent to each other, such as a square or rectangular form.
In an alternative embodiment, the substrate may be a flexible material such as a foil or tape that is fed through the apparatus. The material may be available in tape format, from a roll, and collected at the exit side of the apparatus on a collection roll. The material can be pulled through the apparatus by a pulling force exerted by the collection roll. Gas injection from both the upper and lower tunnel walls make that the tape will flow with very little friction through the apparatus.
Although as an example material only aluminum oxide is disclosed, it will be clear that the apparatus and method of the invention can be applied in combination with all precursor materials and film compositions that are now known in the art.
Further, while the invention has been described with reference to certain embodiments, it will be understood by those skilled in the art that various changes may be made and equivalents may be substituted for elements thereof without departing from the scope of the invention. In addition, many modifications may be made to the teachings of the invention to adapt to a particular situation without departing from the essential scope thereof. Therefore, it is intended that the invention may not be limited to any particular embodiment disclosed for carrying out this invention, but that the invention includes all embodiments falling within the scope of the appended claims.
Number | Date | Country | |
---|---|---|---|
Parent | 12993562 | Feb 2011 | US |
Child | 14969579 | US | |
Parent | 12123745 | May 2008 | US |
Child | 12993562 | US |