1. Field
The present invention generally relates to methods and an apparatus for an atomic layer deposition lithography process, more specifically, to methods and an apparatus for utilizing an atomic layer deposition process along with a lithography process to form features/structures on a substrate surface in the semiconductor field.
2. Description of the Related Art
Integrated circuits have evolved into complex devices that can include millions of components (e.g., transistors, capacitors and resistors) on a single chip. The evolution of chip designs continually requires faster circuitry and greater circuit density. The demands for greater circuit density necessitate a reduction in the dimensions of the integrated circuit components.
As the dimensions of the integrated circuit components are reduced (e.g. to sub-micron dimensions), more elements are required to be put in a given area of a semiconductor integrated circuit. Accordingly, the lithography process has become more and more challenging to transfer even smaller features onto a substrate precisely and accurately without damage. In order to transfer precise and accurate features onto a substrate, a desired high resolution lithography process requires having a suitable light source that may provide a radiation at a desired wavelength range for exposure. Furthermore, the lithography process requires transferring features onto a photoresist layer with minimum structure and/or critical dimension alternation. Recently, an extreme ultraviolet (EUV) radiation source has been utilized to provide short exposure wavelengths so as to further reduce the minimum size printable on a substrate. However, at such small dimensions, the collapse or damage of the photoresist layer often occurs during the subsequent etching process, resulting in failure to successfully transfer structures onto a substrate surface.
In a conventional lithography process, some portions of a photoresist layer disposed on a substrate are exposed to incident radiation to undergo a chemical transformation. In a traditional positive tone exposure process, the exposed portion of the photoresist layer experiencing the chemical transformation is removed during the development process with an aqueous base solution. As the feature sizes formed on microelectronic device continue to shrink, the aqueous base solution developer may become problematic due to image collapse caused by the capillary forces and surface tension of water. Furthermore, solution based developers tend to leave undesired contaminates on the substrate after the development process, thereby adversely effecting the substrate cleanliness.
Therefore, there is a need for a method and an apparatus to control process defects for a lithography process with minimum structure damage so as to obtain a precise structure transfer onto a substrate surface with desired critical dimensions.
Methods and an apparatus for performing an atomic layer deposition lithography process are provided in the present disclosure. In one embodiment, a method for forming features on a material layer in a device includes pulsing a first reactant gas mixture to a surface of a substrate disposed in a processing chamber to form a first monolayer of a material layer on the substrate surface, directing an energetic radiation to treat a first region of the first monolayer, and pulsing a second reactant gas mixture to the substrate surface to selectively form a second monolayer on a second region of the first monolayer.
In another embodiment, a method for forming features on a material layer in a device includes directing a light radiation to treat a first region of a first monolayer of a material layer deposited by a pulse of a first reactant gas mixture performed in an atomic layer deposition process, continuing performing the atomic layer deposition process to form a second monolayer on the first monolayer of the material layer, and removing the first monolayer in the first region treated by the light radiation.
In yet another embodiment, a processing chamber configured to perform an atomic deposition layer process and a lithography process includes a chamber body having a chamber lid disposed on the chamber body defining an interior processing region therein, a pedestal disposed in the interior processing region, a gas delivery system disposed on the chamber body to deliver a reactant gas into the interior processing region, an energy beam source disposed under the chamber lid to direct an energetic radiation toward the interior processing region, and a mask disposed between the energy beam source and the pedestal.
So that the manner in which the above recited features of the present invention can be understood in detail, a more particular description of the invention, briefly summarized above, may be had by reference to embodiments, some of which are illustrated in the appended drawings. It is to be noted, however, that the appended drawings illustrate only typical embodiments of this invention and are therefore not to be considered limiting of its scope, for the invention may admit to other equally effective embodiments.
To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.
It is to be noted, however, that the appended drawings illustrate only exemplary embodiments of this invention and are therefore not to be considered limiting of its scope, for the invention may admit to other equally effective embodiments.
Methods and an apparatus for performing an atomic layer deposition (ALD) lithography process are provided in the present disclosure. The ALD lithography process utilizes an ALD process along with a lithography process to form features onto a substrate surface without using a conventional photoresist layer and/or a hardmask layer. The ALD lithography processing chamber provides a dual function; to deposit an atomic layer deposited layer and to perform a lithography process (e.g., energy beam treatment process) to form features/structures on the atomic layer deposited layer. The substrate may include one or more nonconductive materials, such as silicon, silicon oxide, doped silicon, germanium, gallium arsenide, glass, and sapphire. The substrate may also include dielectric materials such as silicon dioxide, organosilicates, and carbon doped silicon oxides. Further, the substrate can include any other materials such as metal nitrides and metal alloys, depending on the application. In one or more embodiments, the substrate may form a gate structure including a gate dielectric layer and a gate electrode layer to facilitate connection with an interconnect feature, such as a plug, via, contact, line, and wire, subsequently formed thereon. The substrate may be used for integrated circuit, solar, MEMs or other device fabrication.
Moreover, the substrate is not limited to any particular size or shape. The substrate may be a round substrate having a 200 mm diameter, a 300 mm diameter or other diameters, such as 450 mm, among others. The substrate may also be any polygonal, square, rectangular, curved or otherwise non-circular workpiece, such as a polygonal glass substrate used in the fabrication of flat panel displays.
The present invention provides methods for depositing/forming a material layer on a substrate by an ALD process followed by a lithography process (e.g., energy beam treatment process) to form features/structures on the deposited material layer. The process may efficiently forms features/structures with desired small critical dimension onto a substrate surface without using a conventional photoresist layer and/or hardmask layer to assist transferring features/structures onto the substrate surface, thereby improving manufacture cycle time and cost and also reducing manufacture complexity. Advantageously, both the ALD and the lithography process may be performed in a single chamber.
The chamber 134 comprises a chamber body 129 having sidewalls 131 and a bottom 132. A slit valve tunnel 133 formed through the chamber body 129 provides access for a robot (not shown) to deliver and retrieve a substrate 102, such as a 200 mm, 300 mm or 450 mm semiconductor substrate or a glass substrate, from the chamber 134.
A substrate support 192 is disposed in the chamber 134 and supports the substrate 102 during processing. The substrate support 192 is mounted to a lift 114 to raise and lower the substrate support 192 and the substrate 102 disposed thereon. A lift plate 116 is connected to a lift plate actuator 118 that controls the elevation of the lift plate 116. The lift plate 116 may be raised and lowered to raise and lower pins 120 movably disposed through the substrate support 192. The pins 120 are utilized to raise and lower the substrate 102 over the surface of the substrate support 192. The substrate support 192 may include a vacuum chuck, an electrostatic chuck, or a clamp ring for securing the substrate 102 to the surface of the substrate support 192 during processing.
The substrate support 192 may be heated to heat the substrate 102 disposed thereon. For example, the substrate support 192 may be heated using an embedded heating element, such as a resistive heater, or may be heated using radiant heat, such as heating lamps disposed above the substrate support 192. A purge ring 122 may be disposed on the substrate support 192 to define a purge channel 124 which provides a purge gas to a peripheral portion of the substrate 102 to prevent deposition thereon.
A gas delivery apparatus 130 is disposed at an upper portion of the chamber body 129 to provide a gas, such as a process gas and/or a purge gas, to the chamber 134. A pumping system 178 is in communication with a pumping channel 179 to evacuate any desired gases from the chamber 134 and to help maintain a desired pressure or a desired pressure range inside a pumping zone 166 of the chamber 134.
In one embodiment, the gas delivery apparatus 130 includes an expanding channel 190 having gas inlets 137A, 137B to provide gas flows from two similar valves 142A, 142B. The gas flows from the valves 142A, 142B may be provided together and/or separately.
In one configuration, valve 142A and valve 142B are coupled to separate reactant gas sources but are coupled to the same purge gas source. For example, valve 142A is coupled to a reactant gas source 138 and valve 142B is coupled to reactant gas source 139, and both valves 142A, 142B are coupled to purge a gas source 140. Each valve 142A, 142B includes a delivery line 143A, 143B having a valve seat assembly 144A, 144B and includes a purge line 145A, 145B having a valve seat assembly 146A, 146B. The delivery line 143A, 143B is in communication with the reactant gas source 138, 139 and is in communication with the gas inlet 137A, 137B of the expanding channel 190. The valve seat assembly 144A, 144B of the delivery line 143A, 143B controls the flow of the reactant gas from the reactant gas source 138, 139 to the expanding channel 190. The purge line 145A, 145B is in communication with the purge gas source 140 and intersects the delivery line 143A, 143B downstream of the valve seat assembly 144A, 144B of the delivery line 143A, 143B. The valve seat assembly 146A, 146B of the purge line 145A, 145B controls the flow of the purge gas from the purge gas source 140 to the delivery line 143A, 143B. If a carrier gas is used to deliver reactant gases from the reactant gas source 138, 139, the same gas is used as a carrier gas and a purge gas (i.e., an argon gas used as a carrier gas and a purge gas).
Each valve 142A, 142B may be a zero dead volume valve to enable flushing of a reactant gas from the delivery line 143A, 143B when the valve seat assembly 144A, 144B of the valve is closed. For example, the purge line 145A, 145B may be positioned adjacent the valve seat assembly 144A, 144B of the delivery line 143A, 143B. When the valve seat assembly 144A, 144B is closed, the purge line 145A, 145B may provide a purge gas to flush the delivery line 143A, 143B. In the embodiment shown, the purge line 145A, 145B is positioned as slightly spaced from the valve seat assembly 144A, 144B of the delivery line 143A, 143B so that a purge gas is not directly delivered into the valve seat assembly 144A, 144B when open. A zero dead volume valve as used herein is defined as a valve which has negligible dead volume (i.e., not necessary zero dead volume.) Each valve 142A, 142B may be adapted to provide a combined gas flow and/or separate gas flow of the reactant gas 138, 139 and the purge gas 140. The pulses of the purge gas may be provided by opening and closing a diaphragm of the valve seat assembly 146A of the purge line 145A. The pulses of the reactant gas from the reactant gas source 138 may be provided by opening and closing the diaphragm valve seat 144A of the delivery line 143A.
A power source 103 is coupled to a lid 105 disposed on the chamber body 129. The power source 103 is configured to provide power to an energy beam source 106 disposed under the power source 103 connected through an aperture 104 formed therebetween. In one embodiment, the energy beam source 106 may be any suitable energetic radiation source that may provide UV light or other energetic radiation, such as mercury microwave arc lamps, pulsed xenon flash lamps, high efficiency UV light emitting diode arrays, and electron beam generators. The UV lamp bulbs may be sealed plasma bulbs filled with one or more gases, such as xenon (Xe) or mercury (Hg) for excitation by the power source 103. Light emitted from the energy beam source 106 enters the substrate surface by passing through a window 111 disposed below the energy beam source 106. The window 111 may be made of a quartz glass having sufficient thickness to maintain vacuum without cracking. A photomask and/or a feature transfer shield 113 is disposed between the substrate 102 and the window 111. The position of the feature transfer shield 113 can be adjusted between the window 111 and the surface of the substrate 102 so as to assist in transferring features/structures onto the substrate 102 surface. The photomask/the feature transfer shield 113 disposed in the processing chamber 134 may assist by allowing only a portion of the light from the energy beam source 106 to pass therethrough to certain regions of the substrate 102, protecting some other regions from being exposed to light when the energy beam source 106 is turned on. The energy beam source 106 along with the photomask/feature transfer shield 113 serve as a features/structures transferring mechanism configured to perform a lithography process to transfer features/structures onto a material layer disposed on the substrate surface without breaking vacuum during and/or after a deposition process.
In one embodiment, the photomask/the feature transfer shield 113 may provide features/structures formed therein with a dimension less than 180 nm so as to transfer similar features/structures onto the substrate surface with or without image reduction. Details regarding how the lithography process may be performed utilizing the energy beam source 106 along with the photomask/feature transfer shield 113 will be further discussed below with reference to
In
The process 200 starts at block 202 by providing a substrate, such as the substrate 102 depicted in
The substrate 102 has a first surface 302 exposed upward facing the energy beam source 106 and the gas inlets 137A, 137B readily to have the ALD lithography process to be performed thereon.
At block 204, after the substrate 102 is transferred into the processing chamber 134, a pulse of a first reactant gas mixture is supplied into the processing chamber 134 to form a first monolayer 304 of a material layer 305 on the surface 302 of the substrate 102, as shown in
During the pulse of the first reactant gas mixture at block 204, the pulse of the first reactant gas mixture lasts for a predetermined time interval. The term pulse as used herein refers to a dose of material injected into the process chamber. Between each pulse of the first reactant gas mixture or of the first and a second reactant gas mixture, which will be discussed further below, the purge gas mixture may be pulsed into the processing chamber in between each or multiple pulses of the first and/or second reactant precursor gas mixture to remove the impurities or residual precursor gas mixture which is unreacted/non-absorbed by the substrate surface (e.g., unreacted impurities from the reactant gas mixture or others) so they can be pumped out of the processing chamber.
In operation at block 204, a pulse of the first reactant gas mixture is pulsed into the processing chamber 134 to form a first monolayer 304 of the material layer 305. Each pulse of the first reactant precursor gas mixture pulsed into the processing chamber 134 may deposit the first monolayer 304 of the material layer 305 having a thickness between about 3 Å and about 5 Å.
During pulsing of the first reactant precursor gas mixture, several process parameters are also regulated. In one embodiment, the process pressure is controlled at between about 7 Torr and about 30 Torr. The processing temperature is between about 125 degrees Celsius and about 450 degrees Celsius. The RF power may be controlled at between about 100 watts and about 2000 watts. The reactant gas supplied in the first reactant gas mixture may be controlled at between about 5 sccm and about 10 sccm. The reducing gas, such as the NH3 gas, may be supplied at between about 100 sccm and about 700 sccm.
At block 206, a light beam 308 is directed from the energy source 106 to the first monolayer 304 of the material layer 305 to treat a first region 310 of the first monolayer 304, as shown in
In one embodiment, the light beam 308 directed from the energy beam source 106 may be an extreme UV light, deep UV light, electron beam, x-ray, ion beam, or other suitable beams. In one example, the light beam 308 directed from the energy beam source 106 may be a UV light having a wavelength between about 5 nm and about 400 nm.
It is believed that the light energy directed to form the treated layer 306 may damage, cure, modify or alter the chemical bonding or atomic structure of the material layer 305, thereby forming the treated layer 306 having film properties different from the untreated material layer 305 on the substrate surface 302. By doing so, a selective film alternation process may be obtained to only selectively alter the film properties of a portion of the material layer 305 and keep another portion of the material layer 305 remains unchanged. Thus, a selective etching/film removal process may be later performed to only selectively remove a portion (i.e., the treated or untreated depending on the process) of the material layer from the substrate surface 302 as needed.
At block 208, after the light treatment process performed on the first region 310 of the material layer 305, a pulse of a second reactant gas mixture is supplied into the processing chamber 134 to form a second monolayer 314 of the material layer 305 on the surface 302 of the substrate 102, as shown in
In one embodiment, a suitable second reactant gas mixture that may be supplied into the processing chamber 134 may include a silicon containing gas, such as SiH4, Si2H6, or other suitable silicon containing compounds, oxygen containing gas, such as H2O, O2, or O3, tantalum containing gas, titanium containing gas, cobalt containing gas, tungsten containing gas, aluminum containing gas, nickel containing gas, copper containing gas, boron containing gas, phosphorus containing gas, nitrogen containing gas, or other suitable gases that may deposit a monolayer on the substrate surface suitable for using in semiconductor devices. Examples of the alternative reagents (i.e., reducing agents used with reactant precursors for forming the monolayer during the deposition process) as described herein may include hydrogen (e.g., H2 or atomic-H), nitrogen (e.g., N2 or atomic-N), ammonia (NH3), hydrazine (N2H4), a hydrogen and ammonia mixture (H2/NH3), borane (BH3), diborane (B2H6), triethylborane (Et3B), silane (SiH4), disilane (Si2H6), trisilane (Si3H8), tetrasilane (Si4H18), methyl silane (SiCH6), dimethylsilane (SiC2H8), phosphine (PH3), derivatives thereof, plasmas thereof, or combinations thereof.
During the pulse of the second reactant gas mixture at block 208, the pulse of the second reactant gas mixture lasts for a predetermined time interval. The term pulse as used herein refers to a dose of material injected into the process chamber. Between each pulse of the second reactant gas mixture or of the first and the second reactant gas mixture performed at blocks 204 and 206, the purge gas mixture may be pulsed into the processing chamber in between each or after multiple pulses of the first and/or second reactant precursor gas mixture to remove the impurities or residual precursor gas mixture which is unreacted/non-absorbed by the substrate surface (e.g., unreacted impurities from the reactant gas mixture or others) so they can be pumped out of the processing chamber.
In operation at block 208, a pulse of the second reactant gas mixture is pulsed into the processing chamber 134 to selectively form the second monolayer 314 on the first monolayer 304 untreated in the protected region 312. Each pulse of the second reactant precursor gas mixture pulsed into the processing chamber 134 may deposit the second monolayer 314 of the material layer 305 having a thickness between about 3 Å and about 5 Å.
During pulsing of the second reactant precursor gas mixture, several process parameters are also regulated. In one embodiment, the process pressure is controlled at between about 5 Torr and about 30 Torr. The processing temperature is between about 125 degrees Celsius and about 450 degrees Celsius. The RF power may be controlled at between about 100 watts and about 800 watts. The reactant gas supplied in the second reactant gas mixture may be controlled at between about 5 sccm and about 20 sccm. The reducing gas, such as the NH3 gas, may be supplied at between about 100 sccm and about 700 sccm.
In between each or after several pulses of reactant precursor gas mixtures, a purge gas mixture is then supplied into the processing chamber 134 to purge out the residuals and impurities from the processing chamber. Several process parameters are also regulated during pulsing of the purge gas mixture. In one embodiment, the process pressure is controlled at between about 1 Torr and about 100 Torr. The processing temperature is between about 125 degrees Celsius and about 450 degrees Celsius. The RF power may be controlled at between about 100 watts and about 800 watts. The Ar or N2 gas may be supplied at between about 200 sccm and about 1000 sccm.
Subsequent to the pulse of the purge gas mixture, additional cycles starting from the pulsing of the first and/or second reactant gas mixtures followed by the pulse of the purge gas mixture can then be repeatedly performed until a desired thickness range of the material layer 305 is reached, as indicated by loop 210 depicted in
It is noted that the blocks 204, 206, and 208 may be performed in different chambers providing different functions as needed. For example, at block 204, the deposition process for forming a first monolayer may be performed in a first deposition chamber. Subsequently, at block 206, the substrate may then be transferred to a second chamber having the light source with desired wavelength range to perform the light exposure process. Afterwards, at block 208, the substrate can then be transferred back to the first chamber to finish depositing the second monolayer on the first monolayer. Alternatively, at block 208, the substrate may be transferred to a third processing chamber to finish forming the second monolayer on the substrate as needed. It is noted that the first, the second and/or the third processing chamber may all be incorporated in a cluster tool and the substrate may be transferred among the first, the second and/or the third processing chamber (or back to the first processing chamber) without breaking vacuum and exposing the substrate to atmosphere.
At block 212, after the material layer 305 reaches a predetermined thickness, the substrate 102 may be removed from the processing chamber 134 to perform a removal process to remove the treated layer 306 from the substrate surface 302, as shown in
In one embodiment, the removal process may be any suitable etching/development process configured to remove the treated layer 306 from the substrate 102. Suitable examples of the removal process include a dry etching process, a wet etching process, a development process, an ashing process, or other suitable film removal processes. Any conventional suitable etching process that is available to remove the treated layer 306 may be utilized. After the removal process is completed, the treated layer 306 remained on the substrate 302 is removed exposing the underlying surface 303 of the substrate 102 in the exposed region 310.
In one embodiment, the removal process may be performed by a dry etching process providing a halogen containing gas to remove the treated layer 306 from the substrate 102. Suitable examples of the halogen containing gas include chlorine gas (Cl2), nitrogen trifluoride (NF3), sulfur hexafluoride gas (SF6), carbon and fluorine containing gas, such as CF4, CHF3, or C4F8, chlorine gas (Cl2), boron chloride (BCl3), and hydrogen chloride (HCl), among others. In some embodiment, some reducing agents may be supplied with the halogen containing gas to perform the removal process. Suitable reducing agents include, but are not limited to, hydrocarbon gases, such as carbon monoxide (CO), oxygen gas (O2), methane (CH4), ethane (C2H6), ethylene (C2H4), and combinations thereof, among others.
After the removal process is performed and completed on the substrate 102, a material layer with desired features formed thereon may be obtained. By doing so, a conventional lithography process along with a development process utilizing a photoresist layer and/or hardmask layer is eliminated since the features/structures can now be directly transferred onto the material layers without using additional photoresist layer and/or hardmask layer. Therefore, manufacture complexity, cost and cycle time are then efficiently reduced and improved.
Thus, methods and apparatus for performing an ALD lithography process are provided in the present disclosure. The ALD lithography process utilizes an ALD process along with a lithography process to form features on a substrate surface without using conventional masks formed from a photoresist layer and/or a hardmask layer. The ALD lithography process as described herein efficiently reduces manufacturing complexity, cost and cycle time and improves manufacturing flexibility and productivity.
While the foregoing is directed to embodiments of the present invention, other and further embodiments of the invention may be devised without departing from the basic scope thereof, and the scope thereof is determined by the claims that follow.
This application claims priority to U.S. Patent Application Ser. No. 61/601,511, filed on Feb. 21, 2012, which is incorporated by reference in its entirety.
Number | Name | Date | Kind |
---|---|---|---|
7601652 | Singh et al. | Oct 2009 | B2 |
20080283830 | Ahn et al. | Nov 2008 | A1 |
20100227458 | Chung et al. | Sep 2010 | A1 |
20110120542 | Levy | May 2011 | A1 |
Number | Date | Country |
---|---|---|
06-120156 | Apr 1994 | JP |
06-208965 | Jul 1994 | JP |
10-026820 | Jan 1998 | JP |
2010-0100186 | Sep 2010 | KR |
Entry |
---|
International Search Report and Written Opinion for PCT/US2013/022988 dated May 15, 2013. |
Number | Date | Country | |
---|---|---|---|
20130224665 A1 | Aug 2013 | US |
Number | Date | Country | |
---|---|---|---|
61601511 | Feb 2012 | US |