1. Technical Field
The disclosure relates to a heat spreader/lid, especially for microelectronic flip-chip packaging, in which the heat spreader has an underside surface that includes at least one curvilinear contour. The curvilinear contour improves the heat dissipation and mechanical stress of a thermal interface between the heat spreader or lid and the circuit chip. The disclosure also relates to a microelectronic package that includes the heat spreader/lid.
2. Discussion of the Background
Heat dissipation from a circuit chip to a heat spreader/lid is important for microelectronic packages and depends on the thermal resistance of package components. The thermal resistance is determined by the thermal conductivity, the thickness of materials and the degree of wetting at joining interfaces. The heat dissipation increases with increasing thermal conductivity and the degree of wetting, and decreasing thickness.
The major function of thermal interface materials (TIM) is to dissipate heat from the chip by thermally and mechanically linking the chip to the heat spreader. The thermal interface between the chip and the heat spreader usually has significantly smaller thermal conductivity than any other component of a microelectronic package. The thermal performance of the TIM can be improved by introducing materials with higher thermal conductivity and smaller TIM thickness. Inorganic fillers (metals and mineral oxides) are mixed with TIM gels and pastes to increase the thermal conductivity or decrease the thermal resistance of TIM. As TIM bondline decreases, the mechanical stress increases and can become a design constraint.
A soft or low-modulus TIM adhesive is preferred for flip chip plastic ball grid array (FCPBGA) packages to reduce overall mechanical stresses that are governed by the coefficient of thermal expansion (CTE) mismatched chip, underfill and organic substrate structure as shown in
U.S. Pat. No. 6,091,603, incorporated herein by reference in its entirety, generally discloses that thermal resistance may be reduced by introducing customized lid understructure to reduce the amount of thermally conductive material. In particular, the smaller the TIM volume, the smaller the thermal resistance. U.S. Pat. No. 6,472,762 generally discloses the use of a heat spreader with high coefficient of thermal expansion. U.S. Pat. No. 6,784,535 generally discloses a composite lid consisting of at least two materials. However, the above-mentioned disclosures do not indicate the use of curvilinear contours on a heat spreader underside to locally control the bondline for improvements to both heat dissipation and mechanical stress management in the TIM.
A curvilinear surface of a heat spreader or a lid for a microelectronic package can significantly increase heat dissipation without increasing TIM stress. A curvilinear contour of the heat spreader surface can dissipate more heat by reducing local TIM thickness than a conventionally flat heat spreader. The TIM stress can be controlled and suppressed by selecting appropriate curvilinear contours of the heat spreader based on an understanding of mechanical stresses in the package.
Accordingly, one aspect of the disclosure is a microelectronic package comprising:
The region of highest TIM stress is right at the perimeter of the chip. This region is very susceptible to TIM failure. For this reason, there is a benefit to either increasing the TIM thickness or using a second adhesive with higher strength in this zone. Moving inward, the stress decreases and reaches a minimum. This zone is much less susceptible to failure due to the warping characteristics of FCPBA packages. For this reason, the TIM thickness in this zone can be reduced without affecting overall TIM stress.
As indicated above, the disclosure describes the use of curvilinear contours on the underside of the heat spreader. In the location where the stress in the TIM is low, a protruding or positive curvilinear feature is designed into the heat spreader surface that faces the chip to reduce the TIM bondline thickness and lower thermal resistance. In the location where the stress in the TIM is high, a recessed or negative curvilinear feature is designed into the heat spreader surface that faces the chip to increase the TIM bondline thickness and lower mechanical stress. Alternatively, a second adhesive with higher strength can be used either with or without the negative curvilinear feature.
Another aspect of the disclosure is a heat spreader or lid for a microelectronic package, wherein the heat spreader has an underside surface comprising at least one curvilinear contour, wherein the curvilinear contour selected from at least one positive or protruding curvilinear feature, at least one negative or recessed curvilinear feature, and a combination thereof.
A more complete appreciation of the disclosure and many of the attendant advantages will be readily obtained, as the same becomes better understood by reference to the following detailed description when considered in connection with the accompanying drawings.
It should be understood that the term “curvilinear” means “appearing as a curve or nonlinear” throughout the disclosure.
It should also be understood that the terms “heat spreader” and “lid” are interchangeable terms, having the same meaning and function throughout the disclosure.
In a microelectronic package, the TIM dissipates heat from the chip as a heat conductive material. Because the thermal conductivity of the TIM is small compared to the silicon chip and metal heat spreader, it becomes the limiting path for removing heat from the chip. Thermal management and performance require optimum heat dissipation of the TIM as it is located in between the chip and the heat spreader.
In order to achieve the best heat dissipating performance, the TIM must maintain reliable mechanical contact with the chip and the heat spreader. It is the package warpage that exerts thermal stresses/strains in the TIM and that can initiate delamination or fracture, as shown in
A soft or low-modulus TIM conforms to the warpage of a chip and a substrate, and results in lower thermal stresses in the package compared to a rigid, high modulus TIM. See
A curvilinear surface on the heat spreader can significantly enhance heat dissipation through the TIM. This curvilinear contour allows a local thickness reduction in the TIM at a location where the stresses in the TIM caused by the warpage profile of a chip/substrate package are low. As a consequence, the maximum TIM stress remains the same compared to the maximum stress in the TIM for a flat heat spreader. The low-stress zone can be located by conducting advanced analytical modeling using multi-layered beams on elastic foundation. This predicts the warpage or deflection profile of the chip/substrate package mounted on the heat spreader. This model consistently predicts a curvilinear or sinusoidal contour of the warpage for a wide range of material properties and dimensions. The TIM strain distributions at four different moduli of TIM are shown in
The contour may include at least one positive or protruding curvilinear feature and/or at least one negative or recessed curvilinear feature. In one embodiment, the contour may include one positive or protruding curvilinear feature, and one negative or recessed curvilinear feature, as shown in
In a preferred embodiment, the positive or protruding curvilinear feature aligns with low stress regions in the TIM between the heat spreader/lid and chip, and results in an increase in heat dissipation. The increase in heat dissipation may up to 35%, as indicated below. In another preferred embodiment, the negative or recessed curvilinear feature aligns with a high stress region in the TIM between the heat spreader/lid and circuit chip, and results in a reduction in mechanical stress. The reduction in mechanical stress may be as large as 80%. The positive or protruding curvilinear feature is located, starting 10 to 25% in from an edge of the circuit chip, and further extending inboard up to 25% of a dimension of the chip. The starting location is preferably inboard 20% from the chip edge. In addition, the positive or protruding curvilinear feature has a height up to 80% of the TIM thickness of a flat zone.
In another preferred embodiment, the negative or recessed curvilinear feature is located, starting from an edge of the chip, inboard up to 15% of a dimension of the chip. The negative or recessed curvilinear feature has a height less than or equal to 100% of the thickness of the TIM. The negative or recessed curvilinear feature may have a width of up to 15% of a dimension of the chip.
By increasing the TIM thickness in the high stress zones near the chip perimeter, it is possible to significantly lower the stresses in the TIM. See
One of the advantages of this invention is that no extra assembly step is required. The same assembly process can be used except for a curvilinearly contoured heat spreader. For manufacturing simplicity, grinding, stamping or coining can be used to place a curvilinear contour on the heat spreader surface.
Obviously, numerous modifications and variations of the disclosure are possible in light of the above disclosure. It is therefore understood that within the scope of the appended claims, the disclosure may be practiced otherwise than as specifically described herein.
This application is a divisional of co-pending application Ser. No. 11/857,812 filed on Sep. 19, 2007, the contents of which are hereby incorporation by reference.
Number | Date | Country | |
---|---|---|---|
Parent | 11857812 | Sep 2007 | US |
Child | 13586421 | US |