1. Field of the Invention
Embodiments of the present invention generally relate to the fabrication of integrated circuits and to the fabrication of photomasks useful in the manufacture of integrated circuits.
2. Description of the Related Art
The fabrication of microelectronics or integrated circuit devices typically involves a complicated process sequence requiring hundreds of individual steps performed on semiconductor, dielectric and conductive substrates. Examples of these process steps include oxidation, diffusion, ion implantation, thin film deposition, cleaning, etching and lithography. Using lithography and etching (often referred to as pattern transfer steps), a desired pattern is first transferred to a photosensitive material layer, e.g., a photoresist, and then to the underlying material layer during subsequent etching. In the lithographic step, a blanket photoresist layer is exposed to a radiation source through a reticle or photomask containing a pattern so that an image of the pattern is formed in the photoresist. By developing the photoresist in a suitable chemical solution, portions of the photoresist are removed, thus resulting in a patterned photoresist layer. With this photoresist pattern acting as a mask, the underlying material layer is exposed to a reactive environment, e.g., using wet or dry etching, which results in the pattern being transferred to the underlying material layer.
The pattern on a photomask, which is typically formed in a metal-containing layer supported on a glass or quartz substrate, is also generated by etching through a photoresist pattern. In this case, however, the photoresist pattern is created by a direct write technique, e.g., with an electron beam or other suitable radiation beam, as opposed to exposing the photoresist through a reticle. With the patterned photoresist as a mask, the pattern can be transferred to the underlying metal-containing layer using plasma etching. An example of a commercially available photomask etch equipment suitable for use in advanced device fabrication is the Tetra™ Photomask Etch System, available from Applied Materials, Inc., of Santa Clara, Calif. The terms “mask”, “photomask” or “reticle” will be used interchangeably to denote generally a substrate containing a pattern.
During processing, etch rate data from the etching of the photomasks may be used to determine whether the process is operating according to required specifications, and whether the desired results such as etch uniformity are achieved. Since each photomask generally has its own set of features or patterns, different photomasks being etched using the same process recipe may yield different etch rate data, thereby making it difficult to determine if the desired etch results are obtained for a specific photomask.
With ever-decreasing device dimensions, the design and fabrication of photomasks for advanced technology becomes increasingly complex, and control of critical dimensions and process uniformity becomes increasingly more important. Therefore, there is an ongoing need for improved process control in photomask fabrication, such as improved apparatus and methods for collecting etch rate data that would be consistent for each photomask.
The present invention provides a method and apparatus for etching a photomask substrate with enhanced process monitoring, for example, by providing for optical monitoring at different regions of the photomask to obtain desired etch rate or thickness loss. In one embodiment, the method includes etching a first substrate through a patterned mask layer in a plasma etch chamber, the first substrate having a backside disposed on a substrate support and a front side facing away from the substrate support, directing a first radiation source from the backside of the first substrate to a first area covered by the patterned mask layer, directing a second radiation source from the backside of the first substrate to a second area uncovered by the patterned mask layer, collecting a first signal reflected from the first area covered by the patterned mask layer, collecting a second signal reflected from the second area uncovered by the patterned mask layer, and analyzing the combined first and the second signal.
So that the manner in which the above recited features, advantages and objects of the invention are attained and can be understood in detail, a more particular description of the invention, briefly summarized above, may be had by reference to the embodiments thereof which are illustrated in the appended drawings.
It is to be noted, however, that the appended drawings illustrate only typical embodiments of this invention and are therefore not to be considered limiting of its scope, for the invention may admit to other equally effective embodiments.
To facilitate understanding, identical reference numerals have been used, where possible, to designate identical elements that are common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.
It is to be noted, however, that the appended drawings illustrate only exemplary embodiments of this invention and are therefore not to be considered limiting of its scope, for the invention may admit to other equally effective embodiments.
The present invention provides a method and apparatus for etching a photomask substrate with enhanced process monitoring, for example, by providing for optical monitoring at different regions of the photomask to obtain desired etch rate or thickness loss. Although the discussions and illustrative examples focus on the etching rate detection during an etching process of a photomask substrate, various embodiments of the invention can also be adapted for process monitoring of other suitable substrates, including transparent or dielectric substrates, or optical disks.
The etch chamber 10 generally includes a cylindrical sidewall or chamber body 12, an energy transparent ceiling 13 mounted on the body 12, and a chamber bottom 17. The ceiling 13 may be flat, rectangular, arcuate, conical, dome or multi-radius shaped. At least one inductive coil 26 is disposed above at least a portion of the ceiling 13. In the embodiment depicted in
A substrate support member 16 is disposed in the etch chamber 10 to support a substrate 120 during processing. The support member 16 may be a conventional mechanical or electrostatic chuck with at least a portion of the support member 16 being electrically conductive and capable of serving as a process bias cathode. While not shown, a photomask adapter may be used to secure the photomask on the support member 16. The photomask adapter generally includes a lower portion configured to cover an upper portion of the support member and a top portion having an opening that is sized and shaped to hold a photomask. In one embodiment, the top portion of the photomask adapter has a square opening. A suitable photomask adapter is disclosed in U.S. Pat. No. 6,251,217, issued on Jun. 26, 2001, which is incorporated herein by reference.
Process gases are introduced into the etch chamber 10 from a process gas source 48 through a gas distributor 22 peripherally disposed about the support member 16 and/or disposed in the ceiling 13. Mass flow controllers (not shown) for each process gas, or alternatively, for mixtures of the process gas, are disposed between the etch chamber 10 and the process gas source 48 to regulate the respective flow rates of the process gases.
A plasma zone 14 is defined in the etch chamber 10 between the substrate support member 16 and the ceiling 13. A plasma is generated in the plasma zone 14 from the process gases by supplying power from a power supply 27 to the inductive coils 26 through an RF match network 35. The support member 16 may include an electrode disposed therein, which is powered by an electrode power supply 28 and generates a capacitive electric field in the etch chamber 10 through an RF match network 25. Typically, RF power is applied to the electrode in the support member 16 while the body 12 is electrically grounded. The capacitive electric field, which is transverse to the plane of the support member 16, influences the directionality of charged species to provide more anisotropic etching of the substrate 120.
Process gases and etchant byproducts are exhausted from the etch chamber 10 through an exhaust port 34 to an exhaust system 30. The exhaust port 34 may be disposed in the bottom 17 of the etch chamber 10 or may be disposed in the body 12 of the etch chamber 10 for removal of process gases. A throttle valve 32 is provided in the exhaust port 34 for controlling the pressure in the etch chamber 10.
In one embodiment, a detection system 164 operatively coupled to the etch chamber 10 for detecting etch rate and/or endpoint of the etching process. At least one optical access ports or viewports, are provided in different regions of the substrate support member 16. In the example shown in
In general, a larger window facilitates the installation of optical components within the substrate support member 16. However, for apparatus in which the substrate support member 16 is RF biased, the size of the window, especially in the central region 16C of the substrate support member 16, is selected to be sufficiently large for optical monitoring, yet small enough to avoid potential adverse impact for the RF bias. Selecting a small window also improves the lateral temperature uniformity of the support member 16. The optical access port may generally comprise a flat window made of quartz or other materials that transmit light over a broad wavelength spectrum. A more detailed discussion of different optical configurations will be provided further below.
The detection system 164 comprises optical setup for operating in at least one of reflection, interferometry or transmission modes, and is configured for different types of measurements such as reflectance or transmittance, interferometry, or optical emission spectroscopy. Depending on the application of interest, e.g., the material layers or substrate structure being processed, endpoints may be detected based on a change in the reflectance or transmittance intensities, the number of interference fringes, or changes in optical emission intensities at specific wavelengths, or a combination thereof.
The reflection mode of operation allows reflectance (or reflectometry) and interferometric measurement to be performed. The detection system 164 generally comprises an optical light source 166, a focusing assembly 168 for focusing an incident optical beam 176 from the optical light source 166 onto a discreet area (e.g., spot) 180 on the backside of substrate 120, and a photodetector 170 for measuring the intensity of a reflected optical beam 178 reflected off the spot 180 of the substrate 120. The photodetector 170 may be a single wavelength or multi-wavelength detector, or a spectrometer. Based on the measured signal of the reflected optical beam 178, a computer system 172 calculates portions of the real-time waveform and compares it with a stored characteristic waveform pattern to extract information relating to the etch process. In one embodiment, the calculation may be based on slope changes or other characteristic changes in the detected signals, either in reflection or transmission mode, for example, when a film is etched to a target depth. Alternatively, the calculation may be based on interferometric signals as the depth of a trench or the thickness of a film changes during etching. In other embodiments, more detailed calculations may be performed based on interferometric signals obtained over a wide spectrum in order to determine the depth or thickness at any point in the etch process to determine etch rate of the object being etched.
The light source 166 may be monochromatic, polychromatic, white light, or other suitable light source. In general, the optical signal from the reflected optical beam 178 may be analyzed to extract information regarding the presence or absence of a layer (e.g., metal-containing layer), or the thickness of certain material layers within the spot 180. The intensity of the incident optical beam 176 is selected to be sufficiently high to provide a reflected optical beam 178 with a measurable intensity. The lamp can also be switched on and off to subtract background light such as from the plasma. In one embodiment, the light source 166 provides polychromatic light, e.g., from an Hg—Cd lamp, an arc lamp, or a light emitting diode (LED) or LED array, which generate light in wavelength ranges from about 170 nm to about 800 nm, or about 200 to 800 nm, for example about 250 nm to about 800 nm respectively. The polychromatic light source 166 can be filtered to provide an incident optical beam 176 having selected frequencies. Color filters can be placed in front of the photodetector 170 to filter out all wavelengths except for the desired wavelength of light, prior to measuring the intensity of the reflected optical beam 178 entering the photodetector 170. The light can be analyzed by a spectrometer (array detector with a wavelength-dispersive element) to provide data over a wide wavelength range, such as ultraviolet to visible, from about 200 nm to 800 nm. The light source 166 can also comprise a flash lamp, e.g., a Xe or other halogen lamp, or a monochromatic light source that provides optical emission at a selected wavelength, for example, a He—Ne or ND-YAG laser. The light source may be configured to operate in a continuous or pulsed mode. Alternatively, the wavelength range may be expanded into the deep UV as low as 170 nm or beyond y using optical materials with stable deep UV transmission and purging air paths with inert gas or other suitable carrier gas, such as nitrogen gas.
One or more convex focusing lenses 174A, 174B may be used to focus the incident optical beam 176 to the spot 180 on the substrate surface, and to focus the reflected optical beam 178 back on the active surface of photodetector 170. The spot 180 should be sufficiently large to compensate for variations in surface topography of the substrate 120 and device design features. This enables detection of etch endpoints for high aspect ratio features having small openings, such as vias or deep narrow trenches, which may be densely present or more isolated. The area of the return optical beam should be sufficiently large to activate a large portion of the active light-detecting surface of the photodetector 170. The incident and reflected optical beams 176, 178 are directed through a transparent window 110 in the etch chamber 10 that allows the optical beams to pass in and out of the processing environment.
The diameter of the beam spot 180 is generally about 2 mm to about 10 mm. However, if the beam spot 180 encompasses large isolated areas of the substrate containing only a small number of etched features, it may be necessary to use a larger beam spot in order to encompass a greater number of etched features. The size of the beam spot can therefore be optimized, depending on the design features for a particular device. If the signal is sufficient, a large beam spot or field of view will enable process control without precisely matching the position of the substrate support hole and the etched area of the substrate giving rise to the signal.
Optionally, an optical beam positioner 184 may be used to move the incident optical beam 176 across the substrate 120 to locate a suitable portion of the substrate surface on which to position the beam spot 180 to monitor an etching process. The optical beam positioner 184 may include one or more primary mirrors 186 that rotate at small angles to deflect the optical beam from the light source 166 onto different positions of the substrate surface. Additional secondary mirrors may be used (not shown) to direct the reflected optical beam 178 on the photodetector 170. The optical beam positioner 184 may also be used to scan the optical beam in a raster pattern across the backside of the substrate 120. In this embodiment, the optical beam positioner 184 comprises a scanning assembly consisting of a movable stage (not shown), upon which the light source 166, the focusing assembly 168 and the photodetector 170 are mounted. The movable stage can be moved through set intervals by a drive mechanism, such as a stepper motor or galvanometer, to scan the beam spot 180 across the substrate 120.
The photodetector 170 comprises a light-sensitive electronic component, such as a photovoltaic cell, photodiode, phototransistor, or photomultiplier, which provides a signal in response to a measured intensity of the reflected optical beam 178. The signal can be in the form of a change in the level of a current passing through an electrical component or a change in a voltage applied across an electrical component. The photodetector 170 can also comprise a spectrometer (array detector with a wavelength-dispersive element) to provide data over a wide wavelength range, such as ultraviolet to visible, from about 170 nm to 800 nm. The reflected optical beam 178 undergoes constructive and/or destructive interference which increases or decreases the intensity of the optical beam, and the photodetector 170 provides an electrical output signal in relation to the measured intensity of the reflected optical beam 178. The electrical output signal is plotted as a function of time to provide a spectrum having numerous waveform patterns corresponding to the varying intensity of the reflected optical beam 178.
A computer program on a computer system 172 analyzes the shape of the measured waveform pattern of the reflected optical beam 178 to determine the endpoint of the etching process. The waveform generally has a sinusoidal-like oscillating shape, with the trough of each wavelength occurring when the depth of the etched feature causes the return signal to be 180 degrees out of phase with the return signal reflected by the overlaying layer. The endpoint may be determined by calculating the etch rate using the measured waveform, phase information of the measured waveform and/or comparison of the measured waveform to a reference waveform. As such, the period of the interference signal may be used to calculate the depth and etch rate. The program may also operate on the measured waveform to detect a characteristic waveform, such as, an inflection point indicative of a phase difference between light reflected from different layers. The operations can be simple mathematic operations, such as evaluating a moving derivative to detect an inflection point.
In one embodiment, the patterned metal-containing layer 202 may be a chromium layer, or a composite layer including a chromium oxide disposed on chromium. Alternatively, a phase shifting material layer 250, e.g., molybdenum silicide (MoSi), may be optionally disposed between the metal-containing layer 202 and the quartz layer 204 as needed. The molybdenum silicide (MoSi) layer 250 may be etched with the patterned metal-containing layer 202 as a hardmask. The etch rate detection for etching the quartz layer 204 can be monitored either in reflection or transmission mode, and reflectance, transmittance and/or interferometric signals can be performed.
Halogen-containing gases are typically used for etching different materials found on the photomask structure 200. For example, a process gas containing chlorine may be used for etching a chromium layer, while a fluorine-containing gas such as trifluoromethane (CHF3) or tetrafluoromethane (CF4) may be used for etching quartz.
In the embodiment depicted in
A first return beam 207 and a second return beam 209, resulting from the interaction between the first and the second incident beam 206, 208 and the photomask structure 200, e.g., reflecting off the back surface of metal-containing layer 202 in the first area 216 (or interface 212 between the metal-containing layer 202 and the quartz layer 204) and reflecting off from the interface 218 where the quartz layer 204 being etched and exposed, is detected by the photodetector 170 of the detection system 164. The interface 212 causes a phase change in the reflected beam 207. In the case of a quartz/chromium interface 212, the phase change is approximately 115 degrees. The interface 218 of quartz to vacuum causes a phase change of about zero degrees. During etching of the quartz layer 204, the intensity of the reflected optical beam 209 remains constant, as does the optical beam 207. However, as the thickness of the quartz layer 204 shrinks due to etching, the phase of the reflected beam 209 relative to the phase of the reflected beam 207 changes over time. The vector sum of these two produces the interferometric signal. The time-varying sum at a particular wavelength as well as the reflection section obtained from these two different areas may be analyzed to determine at least one of the depth etched, the etch rate and the end point of the quartz etching process.
Depth(D)=fλ/(2n)
In the embodiment depicted here, as the material being etched is quartz, the refractive index of quartz is between about 1.54-1.56 under a light source at wavelength about 230 nm, varied by different manufacture process. In one embodiment, the refractive index of the quartz layer 204 as depicted here is about 1.54.
In the embodiment depicted in
Alternatively, it can also be calculated by the following equation.
Etch Rate(E)=λ/(2n)/(t2−t1)
and
Total time (tendpoint)=Depth(Dendpoint)/Etch Rate (E)
As the example depicted in
In another embodiment, the endpoint may be determined by counting the number of fringes (f) to determine when the etch depth is less than a predetermined depth (for example, just less than the target depth), then etching the last portion of the layer using the etch rate calculated using one or more wavelengths in the spectrum. Since the fringes (f) are accurate indicators of a known depth, using the etch rate to etch the final portion of the layer minimizes potential error. Combining etch rates determined at different wavelengths can yield improved accuracy.
The accuracy of the method described above and the methods described below may be improved by utilizing a metric indicative of etching within the chamber. For example, a sensor or other device may be utilized to determine when the plasma is ignited within the chamber or when etched material is present in the plasma and/or chamber exhaust. This information may be utilized to commence counting of the time t3 to that the endpoint is determined during the time of actual etching, and not during the time in which gases and/or power is provided to the chamber but physical etching of the substrate has not begun.
The differences between the reference substrate waveform 402 and the production substrate waveform 402 may be utilized to improve the accuracy of the endpoint determination. For example, the production substrate real-time waveform 402 is compared with the reference substrate waveform 404 to determine the difference or offset in time when the trough is reached for each waveform 402, 404. If the troughs are reached at different times, this is indicative of the production substrate etching at a different rate than the reference substrate. As shown in the exploded view of the waveforms 402, 404 around a second trough 408 depicted in
Subsequently, the production substrate reflection spectrum 504 may be obtained by transferring a production substrate into the etching chamber using the similar manner discussed above with referenced to
In one embodiment, the minima and maxima in reflection spectrum 504 can be used to determine loss of thickness depth (D) by comparing the minimum wavelength shifts during etching process in accordance with the referenced spectrum 502 of the referenced substrate. As shown in the magnified view of
Furthermore, based on the calculation and prediction of the etch rate/loss of thickness of the quartz layer using the methods discussed above, the process parameters may be real-time adjusted using in-line statistical process control (in-line SPC) for optimization of the process.
By applying one or more optical light source measurement techniques for simultaneous monitoring at different locations of the substrate, embodiments of the present invention provide an improved apparatus and method with enhanced process monitoring and control capabilities. These improvements also allow reliable etch rate/loss of thickness for photomask etching applications.
While the foregoing is directed to embodiments of the present invention, other and further embodiments of the invention may be devised without departing from the basic scope thereof, and the scope thereof is determined by the claims that follow.
This application claims benefit of U.S. Provisional Application Ser. No. 61/551,122 filed Oct. 25, 2011 (Attorney Docket No. APPM/16187L), which is incorporated by reference in their entirety.
Number | Date | Country | |
---|---|---|---|
61551122 | Oct 2011 | US |