Claims
- 1. A glass-silicon column, comprises
a pair of outer silicon members, a glass member located intermediate the outer silicon member, an embedded electrode, at least one fluid channel, and alignment means for said silicon members and said glass member.
- 2. The glass-silicon column of claim 1, wherein said glass-member is composed of a plurality of bonded glass layers.
- 3. The glass-silicon column of claim 2, wherein said bonded glass layers are bonded by anodic bonding.
- 4. The glass-silicon column of claim 2, wherein said electrode is embedded intermediate two of said plurality of bonded glass layers.
- 5. The glass-silicon column of claim 1, wherein each of said outer silicon members are anodically bonded to said glass member.
- 6. The glass-silicon column of claim 1, wherein said glass member comprises a pair on anodically bonded glass layers, wherein said embedded anode is located intermediated the pair of anodically bonded glass layer.
- 7. The glass-silicon column of claim 6, wherein each of said pair of anodically bonded glass layers is anodically bonded to one of said silicon members.
- 8. The glass-silicon column of claim 7, wherein said at least one fluid channel is located intermediate one of said pair of glass layers and an associated silicon member.
- 9. The glass-silicon column of claim 7, wherein said alignment means includes at least one hole in each of said of glass layers, and at least one silicon posting extending from at least one of said silicon members into said hole in each of said pair of glass layers.
- 10. The glass-silicon column of claim 1, wherein said alignment means includes at least one hole in said glass member, and at least one silicon post extending from at least one of said silicon members into said at least one hole.
- 11. The glass-silicon column of claim 1, wherein said at least fluid channel is located partially in an inner surface of one of said silicon members and partially in an adjacent outer surfaces of said glass member.
- 12. The glass-silicon column of claim 1, wherein said electrode comprises a heater for said column.
- 13. The glass-silicon column of claim 12, wherein said electrode additionally function for anodic bonding of components of the column.
- 14. A silicon-glass-silicon column comprising:
a first outer silicon member, at least one glass member, a second outer silicon member, an electrode embedded in said glass member, at least one flow-channel intermediate said glass member and one of said silicon members, and a self-alignment structure located intermediate said first and second silicon members.
- 15. The column of claim 14, wherein said at lest one glass member is anodically bonded to each of said silicon members.
- 16. The column of claim 14, wherein said at least one glass member is composed of a plurality of glass members anodically bonded together.
- 17. The column of claim 16, wherein said electrode is located intermediate a pair of said plurality of glass members.
- 18. The column of claim 14, wherein said electrode is constructed to provide heat for anodic bonding of the column components and for providing heat for at least one fluid channels.
- 19. The column of claim 14, wherein said glass member is composed of a plurality of glass layers anodically bonded together, with each glass layer having a thickness of 10-20 mils.
Government Interests
[0001] The United States Government has rights in this invention pursuant to Contract No. W-7405-ENG-48 between the United States Department of Energy and the University of California for the operation of Lawrence Livermore National Laboratory.