Abstract
A multi-platen chemical-mechanical polishing system is used to polish a wafer. The wafer is polished at a first station. During polishing, an endpoint is detected. The endpoint is detected by generating optical radiation by a first light source. The first optical radiation travels through a translucent area in a surface of a first platen and travels through a first polishing pad. After being reflected by the wafer, the optical radiation returns through the first polishing pad through the translucent window to a first optical radiation detector. The first polishing pad has a uniform surface in that no part of the surface of the first polishing pad includes transparent material through which non-scattered optical radiation originating from the first light source can pass and be detected by the first optical radiation detector. Optical radiation that travels through the first polishing pad and is detected by the first optical radiation detector is haze scattered by inclusions within the first polishing pad. Non-scattered light is absorbed by the first polishing pad. The wafer is also polished at a second station. During polishing a final endpoint is detected. The final endpoint is detected by generating optical radiation by a second light source. The second optical radiation travels through a translucent area in a surface of a second platen and travels through a window embedded in a second polishing pad. After being reflected by the wafer, the optical radiation returns through the window embedded in the second polishing pad, through the translucent area in the surface of the second platen, to a second optical radiation detector.
Description




BACKGROUND




The present invention concerns processing of integrated circuits and pertains particularly to a laser interferometry endpoint detection with windowless polishing pad for chemical mechanical polishing process.




In a semiconductor manufacturing process, on a semiconductor wafer small electronic devices are formed of separate dies. The semiconductor wafer is processed using materials that are patterned, doped with impurities, or deposited in layers.




It is often necessary to polish a wafer surface to provide a substantially planar surface. This is done, for example, using a chemical-mechanical polishing process. Chemical-mechanical polishing is performed by pressing semiconductor wafer against a rotating polishing pad under controlled chemical, pressure, and temperature conditions. A chemical slurry, such as alumina or silica can be use as a polishing abrasive. The polishing effect on the wafer results in both a chemical and mechanical action.




In situ laser interferometry can be used to determine the end point of a chemical-mechanical polishing process. For example, an optical laser and optical radiation detector are located in a polishing platen. A transparent window is embedded into the platen surface for radiation transmission. The polishing pad has a matching embedded window made of a material that allows transmission of the laser radiation (“windowed pad”). The window embedded in the polishing pad is aligned to the window embedded on the platen so that radiation may be transmitted through the platen window and through the pad window. The aligned platen and pad windows can be referred to collectively as an “endpoint window.




As the platen rotates, the endpoint window encounters the wafer once per rotation, allowing radiation to be reflected from the wafer back through the window to the detector. During polishing of a transparent film that is coated over a substrate (e.g., silicon dioxide over silicon), as the film is removed from the surface, the intensity of the radiation at the detector has a periodicity governed by Equation 1 below:




Equation 1








d


=λ/(2


n


cos θ)






In Equation 1, “d” is the distance through the film between peak maxima, “n” is the refractive index of the film for the radiation wavelength, “θ” is the collection angle, and “λ” is the radiation wavelength.




A plot of intensity versus polishing time will yield polishing rate and thickness removal information where the polishing rate is the time derivative of “d” in Equation 1 above.




For more information see, for example, U.S. Pat. No. 5,413,941, issued on May 9, 1995 to Daniel A. Koos and Scott Meikle for OPTICAL END POINT DETECTION METHODS IN SEMICONDUCTOR PLANARIZING POLISHING PROCESSES. See also, U.S. Pat. No. 5,609,517, issued on Mar. 11, 1997 to Michael F. Lofaro for COMPOSITE POLISHING PAD.




The Mirra™ chemical mechanical polisher system available from Applied Materials, Inc., having a business address of 2821 Scott Boulevard, Santa Clara, Calif. 95050, utilizes three independent polishing stations. This allows for two-step polishing using two platens for each wafer or three-step polishing using all three platens for each wafer. In the Mirra™ chemical mechanical polisher system, a reactor endpoint detection system is implemented such that each platen and polishing pad utilizes an endpoint window.




When a wafer is polished in a multi-platen chemical-mechanical polishing (CMP) reactor such as the Mirra™ chemical mechanical polisher system, part of the polishing is performed on one platen, and additional polishing is performed on one or more additional platens. Such sequences are used to optimize wafer throughput. The endpoint traces from platens used to polish one wafer may be “stitched” together into a virtually single trace.




CMP may be performed on wafers that simultaneously have different structures with different film thicknesses and even with different transmitting films. For example, when performing CMP for shallow trench isolation (“STI”), some parts of the reflective wafer surface are coated with silicon dioxide (“SiO


2


”) films (n=1.44) while other parts of the reflective wafer surface are coated with a multi-film structure of SiO


2


on top of silicon nitride (“Si


3


N


4


”, n=2.00). These different structures yield different intensity versus polishing time curves that are independent of one another. However, the lateral dimensions of the structures are microscopic and the radiation collection area is several orders of magnitude larger than the structures. Therefore, a plot of radiation intensity versus polishing time is a convoluted average of the contributions of individual different structures present in the sampling area. Rotational and translational movement of the wafer during polishing result in further averaging the collected signal over a larger area of the wafer.




The embedded window in the polishing pad is made of a material that is transparent to the endpoint radiation wavelength. During manufacture, a rectangular hole is cut into the polyurethane polishing pad and the transparent window is glued into place. This configuration, however, has several disadvantages.




For example, the window material is a different surface material than the rest of the polishing pad. During data collection, when the wafer sweeps over the window in the polishing pad, the surface of the wafer is exposed to a polishing pad surface that is different from the remaining polishing pad surface. With abrasive slurry present, polishing pressure remains applied. This can result in deleterious scratching. Non-uniform polishing may also result.




Another disadvantage of using polishing pads with an embedded window is that extra manufacturing steps and materials are required to produce such polishing pads. This makes polishing pads with embedded more expensive than windowless polishing pads.




SUMMARY OF THE INVENTION




In accordance with the preferred embodiment of the present invention, a multi-platen chemical-mechanical polishing system is presented. A wafer is polished at a first station. During polishing, an endpoint is detected. The endpoint is detected by generating optical radiation by a first light source. The first optical radiation travels through a translucent area in a surface of a first platen and travels through a first polishing pad. After being reflected by the wafer, the optical radiation returns through the first polishing pad through the translucent area to a first optical radiation detector. The first polishing pad has a uniform surface in that no part of the surface of the first polishing pad includes transparent material through which non-scattered optical radiation originating from the first light source can pass and be detected by the first optical radiation detector. Optical radiation that travels through the first polishing pad and is detected by the first optical radiation detector is haze scattered by inclusions within the first polishing pad. Non-scattered light is absorbed by the first polishing pad.




The wafer is also polished at a second station. During polishing a final endpoint is detected. The final endpoint is detected by generating optical radiation by a second light source. The second optical radiation travels through a translucent area in a surface of a second platen and travels through a window embedded in a second polishing pad. After being reflected by the wafer, the optical radiation returns through the window embedded in the second polishing pad, through the translucent area in the surface of the second platen, to a second optical radiation detector.




In one preferred embodiment, for example, each light source is, an optical laser embedded in a platen. Likewise, the translucent area in a platen can consist of, for example, translucent material embedded into the surface of the platen, a hole in the surface of the platen, or an entire surface of the platen.




In the present invention, a windowless pad is used on the first polishing platen, so that the disadvantages of using windowed pads is minimized. The first half of a “stitched” endpoint trace can be collected with low signal-to-noise ratio on the first platen. Although the signal-to-noise ratio may be too low to precisely detect endpoint, when using multi-platen reactors, the actual endpoint of the process always occurs on the second platen. Therefore, a low signal-to-noise signal may be used to initiate the trace on the first platen without danger of detecting a false endpoint due to noise. Radiation source intensity may be increased to compensate for losses in the first pad, so that the average intensity of detected radiation from the first platen is close to that of the second platen. The second half of the “stitched” endpoint trace is collected from the second platen, where the second half of polishing is performed. A windowed pad is used on the second platen for optimum signal-to-noise ratio and accurate endpoint detection.




The above-described preferred embodiment of the present invention does not completely eliminate the disadvantages introduced by using a polishing pad with a window. However, the above-described preferred embodiment of the present invention does eliminate the deficiencies for at least one polishing station. This can result in the reduction of defects from scratches due to the polishing pad window material, the reduction of non-uniform polishing due to the polishing pad window material, the reduction of added cost of purchasing windowed pads, and the reduction of glazing of the platen windows due to slurry leakage.




Also, when a windowed polishing pad is used, the aqueous medium slurries used for polishing transparent films can be corrosive to the modified polishing pad. For example, in semiconductor manufacturing, inorganic dielectrics are typically polished in basic slurries. In such cases the corrosive medium may attack the glues used to hold the window in place. This can cause leaking behind the polishing pad, causing the quartz window in the platen to become glazed over time. This potential problem is alleviated by the present invention.











BRIEF DESCRIPTION OF THE DRAWINGS





FIG. 1

is a simplified block diagram of a chemical mechanical polisher system that utilizes an endpoint window.





FIG. 2

is a simplified block diagram of a chemical mechanical polisher system in accordance with a preferred embodiment of the present invention.





FIG. 3

is a simplified block diagram of a multi-platen chemical mechanical polisher system in accordance with a preferred embodiment of











DESCRIPTION OF THE PRIOR ART





FIG. 1

is a simplified block diagram of a chemical mechanical polisher system that utilizes an endpoint window. A platen


10


includes an embedded optical laser


15


and an optical radiation detector


16


. A translucent window


12


is embedded into the platen surface for radiation transmission. A polishing pad


11


has a matching embedded window


17


made of a material that allows transmission of the laser radiation. Window


17


embedded in polishing pad


11


is aligned with window


12


of platen


10


so that radiation from embedded optical laser


15


may be transmitted through platen window


12


, through the pad window


17


through a transmitting film


13


of a wafer


18


, reflected by a substrate


14


, back through transmitting film


13


, through pad window


17


, through platen window


12


and detected by optical radiation detector


16


. As platen


10


rotates, the endpoint window composed of window


12


and window


17


, encounters wafer


18


once per rotation, allowing radiation to be reflected from wafer


18


back through the endpoint window to optical radiation detector


16


.




DESCRIPTION OF THE PREFERRED EMBODIMENT





FIG. 2

is a simplified block diagram of a chemical mechanical polisher system. In the system shown in

FIG. 2

, optical radiation used for laser interferometry endpoint detection can be transmitted with low signal-to-noise ratio through polishing pad


21


, which does not include a translucent window. Polishing pad


21


is made of a material which has a high absorption of light. Transmission efficiency and signal-to-noise ratio are degraded because there is no translucent polymer areas (windows or nodes) that allow light to be translucently transmitted through polishing pad


21


.




A platen


20


includes an embedded optical laser


25


and an optical radiation detector


26


. A translucent window


22


is embedded into the platen surface for radiation transmission. Translucent window


22


can be any translucent material. Alternatively, provided platen


20


has sufficient stiffness, translucent window


22


can be merely a hole in platen


20


without any special window material. Alternatively, platen


20


can all be made from translucent material so no window is necessary.




Radiation from embedded optical laser


25


may be transmitted through platen window


22


, through polishing pad


21


, through a transmitting film


23


of a wafer


28


, reflected by a substrate


24


, back through transmitting film


23


, through polishing pad


21


, through platen window


22


and detected by optical radiation detector


26


. As platen


20


rotates, window


22


encounters wafer


28


once per rotation, allowing radiation to be reflected from wafer


28


back through polishing pad


21


and window


22


to optical radiation detector


26


.




While in the preferred embodiment, an optical laser is used to provide optical radiation, any other light source may be used that is capable of generating sufficient optical radiation to be detected by optical radiation detector


26


after passing through polishing pad


21


. The light source may be embedded within platen


20


or may be located below platen


20


.




Polishing pad


21


is composed of materials that absorb light. That is, the pad materials use to manufacture polishing pad


21


have chemical bonds and atomic electrons absorb visible light. If the pad materials were solid, the thicknesses used are sufficient to prevent light transmission with the laser light intensity generated by embedded optical laser


25


. However, the pad materials typically have inclusions to give desirable mechanical properties. The inclusions scatter visible light. Some of the scattered light is transmitted through polishing pad


21


, reflected by reflected by a substrate


24


, and transmitted back through the pad to optical radiation detector


26


. Such scattered light is available for signal processing at reduced signal-to-noise-ratio as compared to using a pad with a transparent window.




The scattered light that is transmitted through polishing pad


21


is referred to as haze. “Haze” is the cloudy appearance in a plastic material caused by inclusions that produce light scattering. Haze may be defined as the percentage of transmitted light that is scattered more than 2.5° from the incident beam.




Polishing pad


21


is composed of, for example, polyurethane or some other material or combination of materials with a high absorption of light. In the preferred embodiment, to form polishing pad


21


, polyurethane is laminated onto a base layer of a different polymer material, such as SubaIV material available from Rodel having a business address at 34j06 East Wadkins Street, Phoenix, Ariz. 85034. The polyurethane and polymer material are engineered to give desired mechanical properties (e.g., porosity, compressibility) for CMP. As a result, polishing pad


21


has a high absorbency for visible light, including the 633-nm red helium-neon laser light detected by optical radiation detector


26


. However, because of the above described inclusions in the polyurethane, the luminous transmittance of polishing pad


21


is not zero.




Thus the light that travels through polishing pad


21


and is detected by optical radiation detector


26


is haze, i.e., light that is scattered by inclusions within polishing pad


21


. Non-scattered light is absorbed by the polyurethane and polymer material of which polishing pad


21


is composed.




In one embodiment of the present invention, a multi-platen polishing system is used. Radiation is collected during the initial polishing with low signal-to-noise ratio using a “windowless” polishing pad on a first polishing platen. The polishing is completed, with high signal-to-noise ratio desirable for accurate endpoint determination, using a polishing pad, having a window, placed on a second platen.




For example,

FIG. 3

shows a first station utilizing a platen


30


. Platen


30


includes an embedded optical laser


35


and an optical radiation detector


36


. A translucent window


32


is embedded into the platen surface for radiation transmission. Radiation from embedded optical laser


35


may be transmitted through platen window


32


, through polishing pad


31


, through a transmitting film


33


of a wafer


38


, reflected by a substrate


34


, back through transmitting film


33


, through polishing pad


31


, through platen window


32


and detected by optical radiation detector


36


. As platen


30


rotates, window


32


encounters wafer


38


once per rotation, allowing radiation to be reflected from wafer


38


back through polishing pad


31


and window


32


to optical radiation detector


36


. The light that travels through polishing pad


21


and is detected by optical radiation detector


36


is haze, i.e., light that is scattered by inclusions within polishing pad


31


. Non-scattered light is absorbed by the polyurethane and polymer material of which polishing pad


31


is composed.




A second station utilizes a platen


40


. Platen


40


includes an embedded optical laser


45


and an optical radiation detector


46


. A translucent window


42


is embedded into the platen surface for radiation transmission. Radiation from embedded optical laser


45


may be transmitted through platen window


42


, through polishing pad


41


, through a transmitting film


43


of a wafer


48


, reflected by a substrate


44


, back through transmitting film


43


, through polishing pad


41


, through platen window


42


and detected by optical radiation detector


46


. As platen


40


rotates, window


42


encounters wafer


48


once per rotation, allowing radiation to be reflected from wafer


48


back through polishing pad


41


and window


42


to optical radiation detector


46


.




A third station utilizes a platen


50


. Platen


50


includes an embedded optical laser


55


and an optical radiation detector


56


. A translucent window


52


is embedded into the platen surface for radiation transmission. A polishing pad


51


has a matching embedded window


57


made of a material that allows transmission of the laser radiation. Window


57


embedded in polishing pad


51


is aligned with window


52


of platen


50


so that radiation from embedded optical laser


55


may be transmitted through platen window


52


, through the pad window


57


through a transmitting film


53


of a wafer


58


, reflected by a substrate


54


, back through transmitting film


53


, through pad window


57


, through platen window


52


and detected by optical radiation detector


56


. As platen


50


rotates, the endpoint window composed of window


52


and window


57


, encounters wafer


58


once per rotation, allowing radiation to be reflected from wafer


58


back through the endpoint window to optical radiation detector


56


.




A plot of intensity versus polishing time, as discussed above, yields polishing rate and thickness removal information. When monitoring polishing rate of a single wafer polished using two platens, the first half of a “stitched” endpoint trace is collected with low signal-to-noise ratio on the first platen using a windowless polishing pad. Although the signal-to-noise ratio may be too low to precisely detect an endpoint, this is not necessary since there is still another polishing step. The final polishing step is performed using a platen with a polishing pad that has an embedded window.




Likewise, when monitoring polishing rate of a single wafer polished using three platens, the two parts of a “stitched” endpoint trace is collected with low signal-to-noise ratio on a first platen and a second platen which each have a windowless polishing pad. The low signal-to-noise ratio allow for enough precision in endpoint detection because there is still another polishing step. The final polishing step is performed using a platen with a polishing pad that has an embedded window.




In an alternative embodiment of the present invention, a wafer is polished in a multi-platen polishing system where none of the polishing pads used to polish the wafer have translucent windows. Radiation is collected during the initial polishing with low signal-to-noise ratio using a “windowless” polishing pad on a first polishing platen. The polishing is completed, with low signal-to-noise ratio using a “windowless” polishing pad on a second platen or a third platen. The low signal-to-noise ratio is overcome by using more efficient signal filtering techniques.




The foregoing discussion discloses and describes merely exemplary methods and embodiments of the present invention. As will be understood by those familiar with the art, the invention may be embodied in other specific forms without departing from the spirit or essential characteristics thereof. Accordingly, the disclosure of the present invention is intended to be illustrative, but not limiting, of the scope of the invention, which is set forth in the following claims.



Claims
  • 1. A method for performing chemical-mechanical polishing of a wafer using a multi-platen system, the method comprising the following steps:(a) polishing the wafer at a first station, including the following substep: (a.1) detecting an endpoint during polishing, the endpoint being detected by generating optical radiation by a first light source, the first optical radiation traveling through a translucent area in a surface of a first platen, traveling through a first polishing pad and after being reflected by the wafer returning through the first polishing pad through the translucent area to a first optical radiation detector, wherein the first polishing pad has a uniform surface in that no part of the surface of the first polishing pad includes transparent material through which non-scattered optical radiation originating from the first light source can pass and be detected by the first optical radiation detector, wherein optical radiation that travels through the first polishing pad and is detected by the first optical radiation detector is haze scattered by inclusions within the first polishing pad, non-scattered light being absorbed by the first polishing pad; and, (b) polishing the wafer at a second station, including the following substep: (b.1) detecting a final endpoint during polishing, the final endpoint being detected by generating optical radiation by a second light source, the second optical radiation traveling through a translucent area in a surface of a second platen, traveling through a window embedded in a second polishing pad and after being reflected by the wafer returning through the window embedded in the second polishing pad, through the translucent area in the surface of the second platen, to a second optical radiation detector.
  • 2. A method as in claim 1, wherein in step (a) the first polishing pad comprises polyurethane.
  • 3. A method as in claim 1, additionally comprising the following step performed after step (a) and before step (b):(c) polishing the wafer at a third station, including the following substep: (c.1) detecting an endpoint during polishing, the endpoint being detected by generating optical radiation by a third light source, the third optical radiation traveling through a translucent area in a surface of a third platen, traveling through a third polishing pad and after being reflected by the wafer returning through the third polishing pad through the translucent area to a third optical radiation detector, wherein the third polishing pad has a uniform surface, in that no part of the surface of the third polishing pad includes transparent material through which non-scattered optical radiation originating from the third light source can pass and be detected by the third optical radiation detector, wherein optical radiation that travels through the third polishing pad and is detected by the third optical radiation detector is haze scattered by inclusions within the third polishing pad, non-scattered light being absorbed by the third polishing pad.
  • 4. A method for performing chemical-mechanical polishing of a wafer using a multi-platen system, the method comprising the following steps:(a) polishing the wafer at a first station, including the following substep: (a.1) detecting a first endpoint during polishing, the first endpoint being detected by generating optical radiation by a first light source, the first optical radiation traveling through a translucent area in a surface of a first platen, traveling through a first polishing pad and after being reflected by the wafer returning through the first polishing pad through the translucent area to a first optical radiation detector, wherein the first polishing pad has a uniform surface in that no part of the surface of the first polishing pad includes transparent material through which non-scattered optical radiation originating from the first light source can pass and be detected by the first optical radiation detector, wherein optical radiation that travels through the first polishing pad and is detected by the first optical radiation detector is haze scattered by inclusions within the first polishing pad, non-scattered light being absorbed by the first polishing pad; and, (b) polishing the wafer at a second station, including the following substep: (b.1) detecting a second endpoint during polishing, the second endpoint being detected by generating optical radiation by a second light source, the second optical radiation traveling through a translucent area in a surface of a second platen, traveling through a second polishing pad and after being reflected by the wafer returning through the second polishing pad through the translucent area to a second optical radiation detector, wherein the second polishing pad has a uniform surface in that no part of the surface of the second polishing pad includes transparent material through which non-scattered optical radiation originating from the second light source can pass and be detected by the second optical radiation detector, wherein optical radiation that travels through the second polishing pad and is detected by the second optical radiation detector is haze scattered by inclusions within the second polishing pad, non-scattered light being absorbed by the second polishing pad.
  • 5. A method for performing chemical-mechanical polishing of a workpiece using a multi-platen system; the method comprising the following steps:(a) polishing the workpiece at a first station, including the following substep: (a.1) detecting an endpoint during polishing, the endpoint being detected by generating optical radiation by a first light source, the first optical radiation traveling through a translucent area in a surface of a first platen, traveling through a first polishing pad and after being reflected by the workpiece returning through the first polishing pad through the translucent area to a first optical radiation detector, wherein the first polishing pad has a uniform surface in that no part of the surface of the first polishing pad includes transparent material through which non-scattered optical radiation originating from the first light source can pass and be detected by the first optical radiation detector, wherein optical radiation that travels through the first polishing pad and is detected by the first optical radiation detector is haze scattered by inclusions within the first polishing pad, non-scattered light being absorbed by the first polishing pad; and, (b) polishing the workpiece at a second station, including the following substep: (b.1) detecting a final endpoint during polishing, the final endpoint being detected by generating optical radiation by a second light source, the second optical radiation traveling through a translucent area in a surface of a second platen, traveling through a window embedded in a second polishing pad and after being reflected by the workpiece returning through the window embedded in the second polishing pad, through the translucent area in the surface of the second platen, to a second optical radiation detector.
  • 6. A method as in claim 5, wherein in step (a) the first polishing pad comprises polyurethane.
  • 7. A method as in claim 5, additionally comprising the following step performed after step (a) and before step (b):(c) polishing the workpiece at a third station, including the following substep: (c.1) detecting an endpoint during polishing, the endpoint being detected by generating optical radiation by a third light source, the third optical radiation traveling through a translucent area in a surface of a third platen, traveling through a third polishing pad and after being reflected by the workpiece returning through the third polishing pad through the translucent area to a third optical radiation detector, wherein the third polishing pad has a uniform surface, in that no part of the surface of the third polishing pad includes transparent material through which non-scattered optical radiation originating from the third light source can pass and be detected by the third optical radiation detector, wherein optical radiation that travels through the third polishing pad and is detected by the third optical radiation detector is haze scattered by inclusions within the third polishing pad, non-scattered light being absorbed by the third polishing pad.
CROSS REFERENCE TO RELATED APPLICATION;

This is a divisional of copending application Ser. No. 09/340,487, filed on Jun. 30, 1999 now U.S. Pat. No. 6,224,460.

US Referenced Citations (8)
Number Name Date Kind
5413941 Koos et al. May 1995 A
5605760 Roberts Feb 1997 A
5609517 Lofaro Mar 1997 A
5838447 Hiyama et al. Nov 1998 A
5893796 Birang et al. Apr 1999 A
5899792 Yagi May 1999 A
6014218 Bradl et al. Jan 2000 A
6068539 Bajaj et al. May 2000 A
Foreign Referenced Citations (2)
Number Date Country
0 663 265 Nov 1994 EP
0738 561 Mar 1996 EP