Many processes are known in the art for preparing polymer printing plates, such as photopolymer flexographic plates and letterpress printing plates coated with photopolymer material. One known process starts with a plate having an ablatable material thereon, imaging the plate in a digital imager to ablate the ablatable material according to imaging data, and then curing the exposed plate by exposure of the plate to radiation, such as light energy, including but not limited to ultraviolet (UV) light energy.
Various processes for curing the plate on both the imaged side and the back side of the plate by exposure to a functional energy source are known, including methods for providing a blanket exposure (such as with fluorescent light tubes that emit UV light), and methods for providing the desired radiation using light emitting diode (LED) technology, such as is described in U.S. Pat. No. 8,389,203, assigned to the assignee of the present application and incorporated by reference. One particularly useful LED arrangement is shown and described in U.S. Pat. No. 8,578,854, also incorporated herein by reference.
Known processes include exposing the back of a plate, then performing laser ablation on the front side of the plate, then performing front side exposure. Other processes include laser ablating the front side of the plate, then curing one side of the plate using a blanket exposure, manually flipping the plate, and then curing the other side of the plate. Each of the foregoing processes interposes an undefined, variable time delay between the first and second exposure, depending upon the amount of time for the laser ablation step in the first process, or depending upon the time it takes to manually flip the plate, in the second. This variability in elapsed time between first and second exposure leads to undesirable variability in plate quality. Still other processes may include exposing both the back side and the front side of a plate simultaneously, which although it produces more predictable results than a process that imposes a variable time delay, is still not optimal, as discussed more herein later.
In the field of printing, minimizing the size of a dot printed on a substrate is desirable, but smaller dots correspond to smaller printing plate elements, which are more susceptible to damage during use. Accordingly, there is always a need in the art to reduce the size or printed dots, while also providing optimal stability of the printing elements on the plate for making those printed dots.
One aspect of the invention comprises an apparatus for preparing a printing plate, the apparatus comprising a plurality of radiation sources configured to emit the actinic radiation, each of the radiation sources comprises a light emitting diode (LED), such as an LED sources configured to emit actinic ultraviolet (UV) radiation. The plurality of radiation sources includes one or both of a set of front LED sources positioned to emit radiation toward the front side of the plate, with the plate disposed in a stationary position, and a set of back LED sources positioned to emit radiation toward the back side of the plate. The plurality of front LED sources together define a collective irradiation field covering an area at least coextensive with the lateral length and lateral width of the plate, and the plurality of back LED sources together define a collective irradiation field covering an area at least coextensive with the lateral length and lateral width of the plate. One or both of the sets of front and back LED sources may be stationary. A controller is connected to the plurality of radiation sources and configured to activate the plurality of radiation sources to emit the actinic radiation in a predetermined pattern that includes a time difference between activation of at least a portion of the set of back LED sources and activation of at least a portion of the set of front LED sources. A holder may be configured to receive the printing plate in the stationary position to receive incident radiation from the plurality of radiation sources. The holder may comprise a material that transmits the actinic radiation, such as a horizontal surface relative to a ground on which the apparatus is disposed of a holder that defines a cylindrical surface. In another embodiment, the holder may be configured to hold the plate in a vertical orientation relative to a ground on which the apparatus is disposed. The apparatus of may include optics, such as mirrors, for directing and/or confining the radiation emitted from each set of LED sources.
The predetermined pattern may include all of the set of front LED sources emitting actinic radiation simultaneously, all of the set of back LED sources emitting actinic radiation simultaneously, or a combination thereof. The predetermined pattern may include a time difference between activation of at least a portion of the set of back LED sources and activation of at least a portion of the set of front LED sources. The plurality of radiation sources may be individually controllable or controllable in subsets smaller than an entirety of the collective irradiation field corresponding to each set. The predetermined pattern may comprise a sequence that mimics relative motion between the irradiation field and the plate. The predetermined pattern may preclude simultaneously irradiating the front and the back of the plate by respective LEDs spatially aligned with one another relative to a same cross-sectional coordinate of the plate. The predetermined pattern may include activation of multiple portions of the set of front LED sources and the set of back LED sources simultaneously, such as in a pattern that mimics multiple carriages. The predetermined pattern may include activation of all of the plurality of back LED sources simultaneously and then all of the plurality of front LED sources simultaneously, with a predetermined time delay applied between each front and back exposure. The predetermined pattern may include providing a plurality of exposure steps at an intensity that is less than a full amount of actinic radiation required to cure a corresponding side of the plate to a desired degree of curing.
The apparatus may be configured to deliver a first radiation intensity in one exposure step and a second, lesser exposure intensity in another exposure step. The first radiation intensity and the second, lesser exposure intensity may be delivered with the same set of LED sources. The set of front LED sources has a first nominal radiation intensity and the set of back LED sources has a second nominal radiation intensity. The predetermined pattern includes activation of the back LED sources at the second nominal radiation intensity in one exposure step, and activation of the back LED sources at a radiation intensity less than the second nominal intensity another exposure step.
Each set of LED sources comprises a plurality of discrete arrays having a plurality of individual LED point sources on each array, with the plurality of LED point sources arranged in a plurality of lines. The plurality of LED point sources on each array may be controllable together, individually controllable, or controllable in groups, such as each line of LED point sources in each array being separately controllable. The radiation intensity generated by at least one line of LED point sources may differ from a corresponding radiation intensity generated by at least one other line of LED point sources for a same amount of input energy, wherein the controller is configured to control the radiation intensity produced by each line to achieve an intended degree of homogeneity.
Another aspect of the invention comprises a method for calibrating the apparatus as described herein by periodically characterizing radiation intensity generated by a plurality of lines of LED point sources and adjusting input energy to the respective plurality of lines of LED point sources to account for variations in the lines over time. The characterization may be performed by positioning a sensor that measures incident radiation at a predetermined distance from each line of LED sources. The method may include tailoring radiation intensity of one or more groups of the LED point sources to compensate for variations in transmissivity of a structure that lies between the sources and the printing plate.
Still another aspect of the invention comprises a method for exposing a photopolymer printing plate to actinic radiation from a UV LED light source, the photopolymer printing plate having a non-printing back side and a printing front side with a mask for defining an image to be printed. The method comprises the steps of (a) positioning the photopolymer printing plate in an exposure unit, wherein the exposure unit comprises a plurality of UV LED radiation sources; and (b) exposing the photopolymer printing plate through the mask to actinic radiation from the plurality of UV LED light sources to cure a portion of the photopolymer in the plate in an exposure step during which the plurality of UV LED radiation sources and the photocurable printing plate do not move relative to each other. A first exposure intensity is provided in one exposure step and a second, different exposure intensity is provided in another exposure step. Where the exposure unit has optics, including mirrors, the exposure step may comprise directing the radiation emitted from the plurality of UV LED radiation sources with the mirrors. The plurality of UV LED radiation sources may comprise one or more sets of LED sources, each set of LED sources together defining a collective irradiation field covering an area at least coextensive with a lateral length and lateral width of the plate. The plurality of UV LED radiation sources emit the actinic radiation at a first intensity, wherein the actinic radiation reaching a photocurable surface of the printing plate may be less than the first intensity, such as wherein a portion of the actinic radiation emitted by the plurality of UV LED radiation sources is not transmitted by a surface on which the plate is mounted, blocked by a substrate on which the photocurable polymer is disposed, or a combination thereof.
The first exposure intensity may be provided in one or more back exposure steps and the second exposure intensity may be provided in one or more front exposure steps. The method may include performing the first exposure step with the plurality of UV LED light sources emitting at a nominal intensity, and the second exposure step with the plurality of UV LED light sources emitting at less than the nominal intensity. The first exposure step and the second exposure step may both be back exposure steps. The method may comprise providing a plurality of back exposure steps including at least a first back-only exposure step and a second back exposure step followed by a predetermined time delay followed by a front exposure step, including adjusting the intensity of the one or more of the plurality of UV LED light sources in at least one of the back exposure steps to provide a predetermined ratio Rbf between front side and back side exposure of the printing plate.
Those of skill in the art understand that oxygen is distributed throughout the photopolymer resin of a polymer plate at the time it is typically processed, and that oxygen is an inhibitor of the polymerization reaction commonly harnessed for curing the plates. Although polymerization caused by exposure of the polymer to actinic radiation scavenges this distributed oxygen, ambient oxygen will diffuse back into the resin over time if the plate is in contact with atmospheric air. Surprisingly, in processes in which a back exposure and main exposure are both performed on a plate, it has been found that fine detail on a plate may be optimized by imparting a defined delay between performing the back exposure and the main exposure. Without being held to any particular mechanism, it is believed that in this defined delay time following the back exposure, which scavenges oxygen from the back portion of the plate, oxygen from the front side of the plate starts to diffuse to the back side, thus creating a slightly less oxygen rich concentration in the area of the plate nearest the floor of the plate, such that the polymerization reactions near the floor of the plate react for longer before stopping and therefore create shapes on the plate that taper from the floor toward the top of the plate following the main exposure. It should be noted that a delay that is too long will reset the entire plate to being oxygen saturated, and a delay that is too short may not permit sufficient oxygen diffusion to produce optimal results. Thus, while the amount of the optimal delay may vary depending on any number of characteristics, what is important is that the delay not be too long or too short, for optimal results. This delay may be imparted in any number of ways, described in more detail herein.
An exemplary apparatus 100 for the back exposure of photosensitive printing plate 130 is shown schematically in
In apparatus 100, a UV source of actinic radiation 120 with a predetermined power density is scanned at a specific speed (v) under the bottom of the plate. For the main or front exposure of the photosensitive printing plate a second UV source of radiation 110 with a predetermined power density (irradiance) is scanned above the plate with the same specific speed (v). UV sources of radiation 110 and 120 are configured to scan the printing plate with the same speed (v). Such a configuration may be provided by synchronizing sources 110 and 120 to have a same speed using a controller, or both sources may be attached to a common carriage that traverses the plate, with sources 110 and 120 spaced apart from one another a suitable distance in the direction of carriage travel to provide the desired delay when the carriage moves at a predetermined speed. The predetermined irradiance may be the same for the main side and the back side, or may be different. Preferably the irradiance at the rear side is only a fraction of the irradiance of the front side exposure. Typically, the irradiance at the rear side is in a range of 10% or less of the front side irradiance, but the invention is not limited to any particular ratio of front to back irradiance. The predetermined irradiance is typically a function of the characteristics of the specific type of plate to be exposed, as is known to those of skill in the art, and as is dictated by the manufacturers of such plates.
The time delay between the back exposure with UV source of radiation 120 and the main exposure with UV source of radiation 110 may be adjusted by the control system 140 by adjusting the speed of the sources and/or mechanically by setting a constant distance (D) between the sources during the scan process. The time delay t=D/v. Thus, mechanically varying D has an impact on the delay, as does the relative speed between the plate and the sources during exposure. The time delay can be optimized to get smaller single dot elements on the photosensitive printing plate after processing and smaller single element dot sizes printed on the print substrate. It should be understood that the arrangement depicted in
The relative movement between the radiation sources and the plate may be provided by any mechanism known in the art for moving objects relative to a horizontal, vertical, or otherwise disposed stationary surface. For configurations in which the radiation sources move and the plate is stationary, for example, the sources may be disposed on a gantry system having arms that pass the respective sources above and beneath a stationary horizontal plate mounted on a substrate configured to permit a sufficient amount of radiation to pass through, or on either side of a vertically mounted plate. For configurations in which the radiation sources are stationary and the plate is movable, for example, the plate may be mounted on any mechanism known in the art, such as a movable stage configured to move relative to fixed sources on opposite sides of the stage. Mechanisms for rotating a cylinder on which a plate is mounted relative to fixed sources are well known in the field of printing. Similarly, mechanisms for rotating sources relative to a fixed cylinder on which a stationary object is mounted are also well known, such as in the field of medicine (e.g. CAT scan machines). Thus, mechanisms for moving one or more elements relative to another are well known in the art, generally, and the invention is not limited to any particular mechanism.
As shown in
In one embodiment, shown in
The overall mechanism for creating the exposure may comprise a table having an outer frame 1110 that holds a transparent (e.g. glass) inner portion 1112. The upper 1120 and lower 1122 linear radiation sources (e.g. banks of LED point sources, optionally mounted inside a reflective housing) are mounted on a gantry system or carriage 1130. The radiation sources are connected to a power source, such as an electrical power cord having sufficient slack to extend the full range of motion of the carriage. Tracks (not shown) disposed on the outer frame portion provide a defined path for the gantry system or carriage to traverse. The carriage may be moved on the tracks by any drive mechanism known in the art (also coupled to the power supply and the controller), including a chain drive, a spindle drive, gear drive, or the like. The drive mechanism for the carriage may comprise one or more components mounted within the carriage, one or more components fixed to the table, or a combination thereof. A position sensor (not shown) is preferably coupled to the carriage to provide feedback to the controller regarding the precise location of the carriage at any given time. The control signal output from the controller for operating the radiation sources and for controlling motion of the carriage may be supplied via a wired or wireless connection. The controller may be mounted in a fixed location, such as connected to the table with a control signal cable attached to the sources similar to the power cable, or may be mounted in or on the carriage. The control system and drive mechanism cooperate to cause back/forth relative motion in a transverse direction between the light from the radiation sources and the plate. It should be understood that other embodiments may be devised in which the drive mechanism is configured to move the portion of the table containing the plate past stationary upper and lower linear radiation sources, as well as embodiments in which the radiation sources cover less than the full width of the plate and are movable in both the transverse and longitudinal direction to provide total plate coverage (or the plate is movable in both directions, or the plate is movable in one of the two directions and the sources are movable in the other direction to provides the full range of motion required to cover the entire plate).
In one work flow configuration, the table for conducting the exposure step (i.e. exposure table) as described above may be positioned to automatically receive an imaged plate from an imager. For example, an imager may be positioned so that the imaged plate expelled therefrom lands in a first location, and a robotic handling device may be configured to automatically pick up and move the imaged plate from the first location to a processing location on the exposure table, where the exposure process as described herein is then performed using transverse linear sources attached to a carriage that traverses the plate longitudinally.
As discussed in U.S. Pat. No. 8,578,854 and illustrated schematically in
The term “single element structure number” as used herein refers to a square defined by the total number of pixels that comprises that square. For example, a “64-pixel single element structure” comprises square 200, which comprises an 8×8 grid of pixels 202, and has a total of 64 pixels, as illustrated in
The term “dot top diameter” refers to the diameter of the top of a printing plate element or “dot” (i.e. the portion of the element that contacts the printing surface), as illustrated in
For optimization of the time delay, single element structures of various sizes were imaged by a laser into the mask of a photosensitive printing plate at a resolution of 4000 dpi. For this example, a Model No. DPR 045 printing plate, manufactured by DuPont, was used.
The photosensitive printing plates were then back exposed, such as by using UV radiation source 120, and main exposed, such as by using UV radiation source 110, as depicted in
Results of exemplary time delays for exemplary single element structure numbers 64 and 144 are shown in
The optimized results shown in
Although the exemplary system shown in
In one embodiment 700 depicted in
In another exemplary embodiment 800, depicted in
One exemplary control pattern may activate the radiation subsources in a sequence that causes relative motion between the radiation field and the plate, such as a movement that essentially mimics the same light patterns that would be provided by main and back linear sources attached to a carriage, but with the advantage of having no moving parts. The illumination pattern may be configured to illuminate multiple portions of the front and back simultaneously (e.g. such as in a pattern that mimics multiple carriages—one starting at one end of the plate, and one starting in the middle). The illumination pattern in such a configuration is not constrained to patterns that mimic one or more carriages, however, and may be implemented in any pattern that provides the desired time delay, overall exposure, and lack of simultaneous exposure from front and back for any particular cross sectional coordinate of the plate. The pattern may also comprise illuminating the entire back at once and then the entire front, either in a single exposure for each side, or in fractional exposures of the full required exposure for each side, with the desired time delay applied between each front and back exposure. Furthermore, although shown in a flat configuration, it should be understood that systems in which both the plate and the sources are stationary may also be arranged in a cylindrical configuration.
Optionally, the embodiment shown in
In yet another exemplary embodiment 900, a stationary plate 930 may be subjected to irradiation from a single linear source 915 that is configured to pass over both the front side and back side of the plate at a speed that provides the desired time delay, with a controller 940 that, for example, may turn the source on and off at the appropriate times or modulate the amount of radiation between a main exposure intensity and a back side exposure intensity, as needed. The plate may be disposed on a substrate 960 in a horizontal system, as depicted in
It should be understood that the invention is not limited to any particular physical embodiment, and that the method of the invention of incorporating an optimized delay between back side and front side exposure may be performed in any system having any physical configuration.
In a method for optimizing the time delay for a specific type of printing plate at a specific set of exposure conditions, also illustrated in
Notably, as illustrated in
Such a configuration may be provided by a spatial configuration as depicted with respect to
Finally, while the time delay may be the same for each area of the plate, it should be understood that depending upon the configuration of the radiation sources, controller, and control scheme, one portion of the plate may be irradiated differently than another, if desired.
Processes for Increasing Back-Exposure
As described above, photo polymer printing plates typically need UV exposure from the front side and the back side. The front side exposure is applied through the mask, which holds the image information that shall be imposed to the printing plate. The rear side is exposed to UV radiation through the rear side plastic substrate without any vignetting in order to build a polymerized support layer over the entire plate for the fine printing details located on the plates front side. This polymerized support layer is called “floor.” The floor thickness determines the relief depth for a given plate thickness.
Recent advances in technology for curing of photopolymer printing plates with UV light has produced a variety of LED-based exposure units from various suppliers. These units comprising LED UV light sources are increasingly replacing so-called “bank” exposure devices that incorporate fluorescent tube technology, in which light from the fluorescent tubes typically covers the complete plate surface at one time. Because LEDs are more expensive and require more complex driver electronics, while delivering a much higher UV power-per-unit-surface-area than fluorescent tubes, many embodiments comprise a light source that covers only one dimension of the polymer plate completely (e.g. width), while using relative motion between the plate and UV head to cover the second dimension (e.g. length), to ensure all surface areas of the plate are exposed to the UV light. One example of a state of the art exposure system is the XPS 5080 system manufactured by ESKO. This exposure system is equipped with 3 identical UV heads: two for front side exposure, and one for rear side exposure.
Thus, in one embodiment of the invention, the exposure system comprises three (typically identical) UV heads (e.g. linear sources) comprising a plurality of LED sources: two heads directed to the front side (also referred to herein as the “main exposure heads”), and one head directed to the rear side (also referred to herein as the “back exposure heads”), as shown in
Using the apparatus and method described above may present a challenge with respect to curing photopolymer printing plates having back sides that are less sensitive to UV radiation. Such lesser sensitivity may arise from relatively higher photo-blocker content in the plate rear-side plastic substrate. One way of overcoming this challenge is to apply back exposure energy to the plate rear side prior to the combined back-main exposure steps.
For common standard polymer plates, the ratio (Rbf) between the predetermined amount of energy applied to the rear (back) side and energy applied to the front side of the plate to achieve desired results, ranges according to plate supplier information from 1:5 to 1:40, respectively 20% to 2.5%, depending on the plate type and the relief depth to be achieved.
A standard polymer printing plate, such as for example, the DuPont® model DPR 045 plate, may require approximately 12 minutes of front exposure and about 60 Seconds of back exposure for complete curing on a bank exposure unit. In an LED UV exposure unit configured such as those described herein, and in particular in the XPS 5080 system manufactured by Esko-Imaging Graphics GmbH, Rbf may be as high as 16%.
In certain highly-UV-sensitive plates, such as EXS model plates from DuPont or FTF plates from Flint, a back exposure of only about 6 seconds would optimally be required using such systems, if the plates were not otherwise adjusted. As most bank exposure units control exposure time in 1-second increments, adjusting the floor thickness with back exposure for such high sensitive plates would be very difficult to achieve, without making some adjustments to the plate structure. Hence, plate suppliers now add a higher content of UV blocker into the rear side UV-transmissive, dimensionally-stable plastic substrate of the plate, which blocks a substantial amount of UV from participating in the curing process from the rear side. Such adjustments by plate suppliers have pushed Rbf closer to, for example, approximately 50%.
Unfortunately, if the content of UV blocker inside the rear side plastic substrate is not controlled very precisely by the plate suppliers and varies from one plate charge to another, it may be necessary to control the resulting floor thickness of the plates periodically by readjusting the back exposure UV-energy accordingly.
Moreover, in many configurations, the plate typically lies flat on a glass table with its rear side adjacent the glass plate and is back-exposed through this glass plate. The glass plate typically has a UV transmission of around 80%, consuming 20% UV, thereby pushing the Rbf as high as, for example, approximately 62.5% for the exemplary plates described above.
Another demand for increase of back exposure power arises from the fact that the exposure may be applied to the plate in several fractions. Using several smaller exposure-energy factions, the curing becomes less efficient, making the total exposure energy required for complete curing higher in comparison to an exposure applied in an uninterrupted step. The loss of efficiency due to using multiple exposure steps results in another increase in Rbf, bringing it close to, for example, approximately 75% for the exemplary plates described above.
An embodiment equipped with three identical heads—one UV head for back exposure and two UV heads for main exposure—as depicted in
It is thus not possible to adjust the floor thickness exclusively through irradiance of the rear side UV Head using three identical heads operating at the same power output, and for reasons described herein later, it may be desirable to use three identical heads with the same nominal power operating at that nominal power, for greatest efficiency and productivity. One method for supplying the missing 25% of back exposure UV power is to provide a back-only exposure step to provide the additional energy in an uninterrupted exposure into the rear side of the plate before the combined main and back exposure steps are commenced.
As shown in
A standard exposure process comprises at least two exposure steps, wherein in each step the exposure heads move from a start position along the polymer plate, exposing the plate to actinic UV radiation with constant speed V in the direction of the arrow shown in
As described herein, total exposure time is determined by UV output aperture of the UV heads in traveling direction, the speed by which the heads travel along the polymer plate and the number of passes the head moved along the plate. The width of the UV output aperture divided by the traveling speed results in the time that a pixel in the plate “sees” UV light. This time is called “pixel time” in the following text.
The intent of the foregoing method is to obtain a cure of the polymer plate that is superior to a simple front and backside exposure each applied in only one uninterrupted step. “Superior” in this case means the plate holds smaller printing details, which are fixed to the plate floor with higher stability and that do not bend during printing. Producing smaller print dots enables production of lighter highlights in the print.
The back exposure energy is increased or decreased to adjust the floor thickness of the plate. This can be done either by adjusting the irradiance of the back exposure UV head, by adjusting the pixel time, or by adjusting both pixel time and irradiance. Due to the nature of the curing process, changing the pixel time is disfavored, as it can also affect the front exposure results, which may lead to unwanted curing and printing results. Thus the preferred method for adjusting the plate floor thickness is to change the irradiance.
Productivity is a highly desirable characteristic of UV exposure devices, and thus it is favorable to run the UV light sources at the nominal UV output in order to supply the energy to the plate required for curing as fast as possible. As a consequence, both front exposure UV heads in the system depicted in
In the example discussed above, where the irradiance of the back exposure head cannot be increased any further, absent some other remedy, the UV output of the back exposure would have to be set to maximum and the pixel time increased by 50% to reach the required floor thickness (with some corresponding change to the front exposure to adjust for the increased time). This approach may affect the quality of the front exposure curing result, and thus, it may be necessary to evaluate the complete set of exposing parameters to maintain desirable plate printing quality.
Alternatively the number of exposure cycles may be increased until the accumulated rear side exposure energy is sufficient to cure the plate floor to the required thickness. But this approach will also increase the front exposure energy, leading to higher energy input if the front exposure irradiance stays the same as before the increase in the number of cycles, which may lead to different curing and printing results. Also if the irradiance of the front exposure is reduced to maintain the front exposure energy the same as before the increase of the number of exposure cycles, this may lead to different curing and printing results, making this an imperfect solution.
Table 1 below provides a survey of different Rbf ratios for various exemplary plate types. As shown in Table 1, the Rbf ratio increases for thicker plate materials. For thicker plate material and also for the new highly-UV-sensitive materials, like the EXS plate from DuPont or the FTF plate from Flint, there is a need for further improving the efficiency of the XPS exposure device. The plates listed in the table are merely examples, and the invention is not limited only to use with digital flexographic printing plates listed.
One preferred method for bringing more back side exposure energy into the plate, without sacrificing the desired printing results of the plate derived from the proper selection of exposure parameters, comprises executing one or more additional back exposure steps prior to the consecutive combined back and front exposure steps discussed herein. This additional back exposure step is preferably applied directly before starting the consecutive exposure steps.
Thus, for the processes described and depicted relative to
The energy applied by the additional back exposure steps may be controlled by the exposure time, namely by the speed by which the UV head is moved along the plate rear side. In order to keep the time period for this additional exposure step as short as possible, the UV irradiance of the rear exposure UV head is ideally operated at the nominal maximum.
The amount of additional back exposure UV-energy may be controlled by controlling the irradiance of the back exposure UV-heads, by adding more back exposure steps (each step comprising a fractional amount of a total that is predetermined to be required to provide the desired floor thickness adjustment), or by some combination of irradiance, exposure time (the speed by which the UV head is moved along the polymer plate rear side), and the number of additional exposure steps.
Additional back exposure steps are added whenever the nominal back exposure irradiance is not sufficient for complete curing of the floor to the required thickness. The additional back exposure step or steps (as well as any and all of the method steps described herein) may be implemented via the apparatus controller, which controller may be in the form of computer hardware programmed with software instructions for causing the components of the apparatus to perform the subject steps. Although shown and described in connection with a certain embodiments of the invention described herein, it should be understood that exposure processes comprising additional back-exposure steps are not limited to any particular process or apparatus. Similarly, although the use of additional back-only exposure steps may be particularly suitable for UV exposure systems, this aspect of the invention is not limited to any particular radiation system.
Although the invention is illustrated and described herein with reference to specific embodiments, the invention is not intended to be limited to the details shown. Rather, various modifications may be made in the details within the scope and range of equivalents of the claims and without departing from the invention.
While preferred embodiments of the invention have been shown and described herein, it will be understood that such embodiments are provided by way of example only. Numerous variations, changes and substitutions will occur to those skilled in the art without departing from the spirit of the invention. Accordingly, it is intended that the appended claims cover all such variations as fall within the spirit and scope of the invention.
This application is a continuation of U.S. patent application Ser. No. 16/926,076 (status: allowed), titled METHOD AND APPARATUS FOR EXPOSURE OF FLEXOGRAPHIC PRINTING PLATES USING LIGHT EMITTING DIODE (LED) RADIATION SOURCES, filed Jul. 10, 2020, which is a continuation of U.S. patent application Ser. No. 15/926,616, titled PROCESS AND APPARATUS FOR CONTROLLED EXPOSURE OF FLEXOGRAPHIC PRINTING PLATES AND ADJUSTING THE FLOOR THEREOF, filed Mar. 20, 2018 now U.S. Pat. No. 10,732,507, which is a continuation-in-part of PCT Application Ser. No. PCT/IB2016/001660, titled SYSTEM AND METHOD FOR CONTROLLED EXPOSURE OF FLEXOGRAPHIC PRINTING PLATES, filed 26 Oct. 2016, which claims priority to U.S. Provisional Patent Application Ser. No. 62/246,276, filed on 26 Oct. 2015. U.S. patent application Ser. No. 15/926,616 also claims priority to U.S. Provisional Application Ser. No. 62/473,784, titled “PROCESS AND APPARATUS FOR ADJUSTING THE FLOOR OF A FLEXOGRAPHIC PRINTING PLATE IN A CONTROLLED EXPOSURE SYSTEM OR PROCESS,” filed 20 Mar. 2017. All of the foregoing are incorporated herein by reference in their entireties.
Number | Name | Date | Kind |
---|---|---|---|
3981583 | Tsuchida et al. | Sep 1976 | A |
4927723 | Cusdia | May 1990 | A |
5073792 | Paccagnella et al. | Dec 1991 | A |
5386268 | Ohlig et al. | Jan 1995 | A |
6238837 | Fan | May 2001 | B1 |
6266134 | Gelbart | Jul 2001 | B1 |
6326127 | Morren et al. | Dec 2001 | B1 |
6352815 | Feil et al. | Mar 2002 | B1 |
6355395 | Zwez et al. | Mar 2002 | B1 |
6383690 | Vargas | May 2002 | B1 |
6683421 | Kennedy et al. | Jan 2004 | B1 |
6700598 | Hull | Mar 2004 | B1 |
6903809 | Donahue et al. | Jun 2005 | B2 |
6908726 | Korionoff et al. | Jun 2005 | B2 |
6931992 | Hull et al. | Aug 2005 | B1 |
7358026 | Dudek et al. | Apr 2008 | B2 |
7632625 | Roberts et al. | Dec 2009 | B2 |
7682775 | Rapp et al. | Mar 2010 | B2 |
7691550 | Goldfarb | Apr 2010 | B2 |
7709183 | Watanabe et al. | May 2010 | B2 |
7767383 | Roberts et al. | Aug 2010 | B2 |
7875321 | Verhoest et al. | Jan 2011 | B2 |
8034540 | Zwadlo | Oct 2011 | B2 |
8114569 | Holt | Feb 2012 | B2 |
8153347 | Veres et al. | Apr 2012 | B2 |
8227769 | Sievers | Jul 2012 | B2 |
8389203 | Sievers | Mar 2013 | B2 |
8399178 | Bertrand et al. | Mar 2013 | B2 |
8501391 | Yoshida et al. | Aug 2013 | B2 |
8524442 | Recchia et al. | Sep 2013 | B1 |
8578854 | Sievers | Nov 2013 | B2 |
8790864 | Baldwin | Jul 2014 | B2 |
8820234 | Sievers | Sep 2014 | B2 |
8900798 | Savariar-Hauck et al. | Dec 2014 | B2 |
8994916 | Mei et al. | Mar 2015 | B2 |
9040226 | Boukaftane | May 2015 | B2 |
9057958 | Armstrong et al. | Jun 2015 | B2 |
9063426 | Ramakrishnan et al. | Jun 2015 | B2 |
9134612 | Blomquist et al. | Sep 2015 | B2 |
9463617 | De Caria | Oct 2016 | B2 |
9671695 | Fronczkiewicz et al. | Jun 2017 | B2 |
9703201 | Vest | Jul 2017 | B2 |
9740099 | Boukaftane | Aug 2017 | B2 |
9740103 | Vest | Aug 2017 | B2 |
9849663 | Sievers | Dec 2017 | B2 |
9889640 | Boyksen | Feb 2018 | B2 |
9937703 | Stebani et al. | Apr 2018 | B2 |
10025183 | Baldwin et al. | Jul 2018 | B2 |
10036956 | Baldwin et al. | Jul 2018 | B2 |
10175580 | Fronczkiewicz et al. | Jan 2019 | B2 |
10732507 | Wolterink et al. | Aug 2020 | B2 |
11333980 | Wolterink | May 2022 | B2 |
20010052924 | Steinke et al. | Dec 2001 | A1 |
20020192569 | Ulland et al. | Dec 2002 | A1 |
20050011382 | Donahue et al. | Jan 2005 | A1 |
20050116176 | Aguirre et al. | Jun 2005 | A1 |
20060124008 | Kessenich et al. | Jun 2006 | A1 |
20060154180 | Kannurpatti | Jul 2006 | A1 |
20070071953 | Nakamura | Mar 2007 | A1 |
20070084368 | Vest et al. | Apr 2007 | A1 |
20070146430 | Nakamura et al. | Jun 2007 | A1 |
20070148582 | Hayashi et al. | Jun 2007 | A1 |
20070218372 | Zalevsky et al. | Sep 2007 | A1 |
20080063981 | Ohnishi | Mar 2008 | A1 |
20080197300 | Kayser et al. | Aug 2008 | A1 |
20080280227 | Sievers | Nov 2008 | A1 |
20090188308 | Rudolph | Jul 2009 | A1 |
20090267269 | Lim et al. | Oct 2009 | A1 |
20090272286 | Wolterink et al. | Nov 2009 | A1 |
20090290891 | Sievers | Nov 2009 | A1 |
20100028815 | Zwadlo | Feb 2010 | A1 |
20100143840 | Veres et al. | Jun 2010 | A1 |
20100173135 | Choi et al. | Jul 2010 | A1 |
20110014573 | Matzner et al. | Jan 2011 | A1 |
20110104615 | Sievers | May 2011 | A1 |
20110230585 | Chen | Sep 2011 | A1 |
20120157561 | Gould et al. | Jun 2012 | A1 |
20120171434 | Herlihy | Jul 2012 | A1 |
20120266767 | Klein et al. | Oct 2012 | A1 |
20120281408 | Owen | Nov 2012 | A1 |
20130209939 | Recchia et al. | Aug 2013 | A1 |
20130242276 | Schadebrodt et al. | Sep 2013 | A1 |
20130340637 | Wolterink et al. | Dec 2013 | A1 |
20140057207 | Baldwin | Feb 2014 | A1 |
20140335456 | Boukaftane | Nov 2014 | A1 |
20140373742 | Ramakrishnan | Dec 2014 | A1 |
20150004530 | Ramakrishnan et al. | Jan 2015 | A1 |
20150030984 | Ramakrishnan | Jan 2015 | A1 |
20150086928 | Ramakrishnan et al. | Mar 2015 | A1 |
20160207299 | Stebani et al. | Jul 2016 | A1 |
20160229173 | Boyksen | Aug 2016 | A1 |
20160368260 | De Caria | Dec 2016 | A1 |
20180004093 | Fronczkiewicz et al. | Jan 2018 | A1 |
20180210345 | Wolterink et al. | Jul 2018 | A1 |
20180217502 | Dietz et al. | Aug 2018 | A1 |
20200023632 | Boyksen | Jan 2020 | A1 |
Number | Date | Country |
---|---|---|
2374207 | Oct 2009 | CA |
1315677 | Oct 2001 | CN |
1702557 | Nov 2005 | CN |
1236361 | Jan 2006 | CN |
101019073 | Aug 2007 | CN |
101772424 | Jul 2010 | CN |
102470662 | May 2012 | CN |
204086810 | Jan 2015 | CN |
204679755 | Sep 2015 | CN |
104865390 | Oct 2015 | CN |
205644018 | Oct 2016 | CN |
105637419 | Mar 2018 | CN |
202004017044 | Jan 2005 | DE |
102012109130 | Mar 2014 | DE |
0007127 | Dec 1982 | EP |
1804243 | Jul 2007 | EP |
2124104 | Nov 2009 | EP |
2128702 | Dec 2009 | EP |
2313270 | Apr 2011 | EP |
2317387 | May 2011 | EP |
2508948 | Oct 2012 | EP |
3035123 | Jun 2016 | EP |
3054352 | Aug 2016 | EP |
3086178 | Oct 2016 | EP |
3086179 | Oct 2016 | EP |
3121653 | Jan 2017 | EP |
08305006 | Nov 1996 | JP |
2003154628 | May 2003 | JP |
3562865 | Sep 2004 | JP |
2010091867 | Apr 2010 | JP |
2011154080 | Aug 2011 | JP |
2012145869 | Aug 2012 | JP |
2013029739 | Feb 2013 | JP |
201501594 | Jan 2015 | TW |
02093285 | Nov 2002 | WO |
2007012023 | Jan 2007 | WO |
2008094607 | Aug 2008 | WO |
2008135865 | Nov 2008 | WO |
2008135866 | Nov 2008 | WO |
2013158942 | Oct 2013 | WO |
2014031146 | Feb 2014 | WO |
2014035566 | Mar 2014 | WO |
2015012880 | Jan 2015 | WO |
2015044437 | Apr 2015 | WO |
2015047444 | Apr 2015 | WO |
2015112478 | Jul 2015 | WO |
2017072588 | May 2017 | WO |
2018096144 | May 2018 | WO |
2018172374 | Sep 2018 | WO |
2019018376 | Jan 2019 | WO |
Entry |
---|
Chinese Office Action for Chinese Application No. 201880033332.6, dated May 19, 2021, with translation, 14 pages. |
Columbian Office Action for Columbian Application No. NC2018/0004325, dated Sep. 5, 2019, 21 pages. |
Datasheet—“DuPont Cyrel 1000 ECLF,” 2013, 2 pages. |
Digital Flexo Platemaking Using Flint Group's nyloflex NExT, downloaded at https:///www.youtube.com/watch?v=fB-eaQleHh8, Feb. 25, 2020, 2 pages. |
Digital UV Sleeve User Manual, 2012, 42 pages. |
DuPont Processing Manual for Cyrel, 1998, 142 pages. |
Esko Technical Paper, Flexographic Printing Forms at the Push of a Button, with translation, 2012, 10 pages. |
Esko, FullHD-Flexo Standard Operation Procedure for Labels, 2014, 38 pages. |
Esko Full HD Fiexo 1.1 Standard Operation Procedure, 2013, 35 pages. |
EskoWorld Digital Flexo Plate Room Automation, 2014, 20 pages. |
EskoWorld Digital Flexo Roadmap, 2014, 41 pages. |
European Communication for European Application No. 16 816 384.8, dated Jan. 25, 2021, 11 pages. |
European Communication for European Application No. 18 713 604.9, dated May 26, 2021, 7 pages. |
Extended European Search Report for European Application No. 20 209 977.6, dated Jan. 29, 2021, 9 pages. |
Extended European Search Report for European Application No. 21 165 620.2, dated Jul. 20, 2021, 8 pages. |
“Flexodruckformen auf Knopfdruck,” Flexo + Tief Druck, Jan. 4, 2013, German original, with translation (“Flexographic Printing Forms at the Push of a Button,” 2012), 10 pages. |
Flint Group User's Manual 2013, 28 pages. |
Harri, L., “Microscopic Studies of the Influence of Main Exposure Time on Parameters of Flexographic Printing Plate Produced by Digital Thermal Method”, Microscopy Research Technique, vol. 72, Issue 10, 2009 (abstract only). |
Indian Examination Report for Indian Application No. 201847014990, dated Jun. 12, 2020, with translation, 5 pages. |
International Preliminary Report on Patentability for International Application No. PCT/IB2016/001660, dated May 1, 2018, 6 pages. |
International Preliminary Report on Patentability and Written Opinion for International Application No. PCT/EP2018/057060, dated Sep. 24, 2019, 10 pages. |
International Search Report and Written Opinion for International Application No. PCT/IB2016/001660, dated Apr. 24, 2017, 7 pages. |
International Search Report and Written Opinion for International Application No. PCT/EP2018/057060, dated Jul. 6, 2018, 15 pages. |
Japanese Notification of Reason for Rejection for Japanese Application No. 2018-540233, dated Feb. 7, 2019, 5 pages. |
Nichia LED Ever Research for a Brighter World Catalogue, 2009, 7 pages. |
Sasa et al., “A Novel UV Sensitive Photopolymerization System with Microgel Matrix”, Polymers Advanced Technologies, vol. 5, Issue 2, 1994. 2 pages. (abstract only). |
Specifications for Nichia UV LED Cooling Module, Model: NLBU21P02, 12 pages. |
Textbook, “Technik des Flexodrucks,” 1999, ISBN 3-85599-003-4, 4th Edition, 3 pages. |
Toma{hacek over (s)}egovic et al., “Modification of Flexographic Printing Plate's Surface Properties By Variation of UVC Finishing”, Materials Science, 2013 (abstract only). |
Toma{hacek over (s)}egovic, T., “Functional Model of Photopolymer Printing Plate Production Process,” Doctoral Thesis, Jan. 1, 2016, 240 pages, University of Zagreb. |
Urano et al. “Photopolymerization System Thermally Accelerated by a Laser Diode”, Journal of Imaging Science and Technology, vol. 41, No. 4, 1997, 2 pages, (abstract only). |
User's Manual—“Concept 302 ECDLF,” Sep. 2014, 41 pages, Glunz & Jensen. |
Entire patent prosecution history of U.S. Appl. No. 15/926,616, filed Mar. 20, 2018, entitled, “Process and Apparatus for Controlled Exposure of Flexographic Printing Plates and Adjusting the Floor Thereof.” |
Entire patent prosecution history of U.S. Appl. No. 16/926,076, filed Jul. 10, 2020, entitled, “Method and Apparatus for Exposure of Flexographic Printing Plates Using Light Emitting Diode (LED) Radiation Sources.” |
Brazilian Office Action for Application No. 112018008024-1, dated Oct. 10, 2022 with translation, 14 pages. |
German Intermediate Decision for German Application No. 20 2018 006 543.9, dated Sep. 15, 2022. |
FlintGroup Printing Plates, User Manual FV Exposure, Edition AA, Mar. 2009, 39 pages. |
Order Confirmation, Aug. 25, 2009, 2 pages. |
FlintGroup Flexographic Graphics, Invoice 35014, Oct. 23, 2009, two pages. |
FlintGroup Flexographic Graphics, Invoice 35015, Oct. 23, 2009, two pages. |
FlintGroup Flexographic Graphics, Invoice 35016, Oct. 23, 2009, two pages. |
FlintGroup Flexographic Products, Handover Confirmation 35014, Jan. 22, 2010, one page. |
FlintGroup Flexographic Products, Handover Confirmation 35015, Jan. 28, 2010, one page. |
FlintGroup Flexographic Products, Handover Confirmation 35016, Dec. 17, 2009, one page. |
Trial and Error, Sep. 27, 2022, 5 pages, Wikipedia. |
Applicant's Letter for European Application No. 16 816 384.8, dated Jul. 9, 2021, 9 pages. |
Applicant's Letter for European Application No. 16 816 384.8, dated Oct. 13, 2020, 7 pages. |
European Communication of a Notice of Opposition for European Application No. 16 816 384.8, dated Nov. 23, 2022, 47 pages. |
Extended European Search Report for European Application No. 22 196 254.1, dated Jan. 5, 2023, 10 pages. |
Esko Next Generation Flexo Plate Making, dated Apr. 24, 2023, 8 pages. |
German Communication of Cancellation of Utility Model for German Application No. 20 2018 006 543.9, dated Jan. 1, 2022 with translation, 64 pages. |
Esko CDI Crystal 5080 XPS, dated Apr. 20, 2023, 5 pages with translation. |
Zwischenbescheid DE543 for German Application No. 20 2018 006 543.9, dated Sep. 15, 2022, 34 pages with translation. |
Zwischenbescheid DE961 for German Application No. 20 2016 008 961.8, dated Sep. 19, 2022, 32 pages with translation. |
SS basysPrint (Quintuplik), dated Apr. 20, 2023, 64 pages with translation. |
European Communication of a Notice of Opposition for European Application No. 18713604.9, dated Jun. 27, 2023, 39 pages. |
User Manual FV Exposure, 4 pages. |
Declaration of Eva Freudenthaler, dated Feb. 3, 2023, 1 page. |
Brief Communication with Submission in Opposition Proceedings, dated Aug. 11, 2023, 32 pages. |
European Communication pursuant to Article 94(3) for European Application No. 22 196 254.1, dated Sep. 28, 2023, 5 pages. |
Chinese Office Action with Search Report for Chinese Application No. 202111270256.0, dated Sep. 5, 2023 with translation, 25 pages. |
Number | Date | Country | |
---|---|---|---|
20220269178 A1 | Aug 2022 | US |
Number | Date | Country | |
---|---|---|---|
62246276 | Oct 2015 | US | |
62473784 | Mar 2017 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 16926076 | Jul 2020 | US |
Child | 17742003 | US | |
Parent | 15926616 | Mar 2018 | US |
Child | 16926076 | US |
Number | Date | Country | |
---|---|---|---|
Parent | PCT/IB2016/001660 | Oct 2016 | WO |
Child | 15926616 | US |