This invention relates generally to the generation and use of high energy, small cross-sectional particle beams and is particularly directed to the use of these types of electron beams arranged in matrix arrays for use in electron beam lithography such as in the fabrication of integrated circuits (ICs) and the chromium masks used in optical lithography.
The fabrication of ICs is accomplished in large volume production by a process called photolithography. Stated simply, this process uses a monochromatic light source of specified wavelength to expose (harden) a photosensitive material covering a silicon wafer. The monochromatic light shines through a chromium stencil (mask) that contains the circuit pattern to be written on the silicon wafer. The shadow of the circuit pattern passes through a complex optical system designed to de-magnify the image and focus it on the silicon wafer. After a short exposure time of about one-quarter to one-half second, the photo-resist chemical hardens effectively transferring the de-magnified image of the mask onto the wafer. The patterns for the various layers of a multi-layer IC are sequentially exposed. The area of a 300 mm diameter wafer is large enough to hold some 176 large scale, 20 mm×20 mm integrated circuit writing fields. With an exposure time on the order of one-quarter to one-half second per IC pattern, the entire wafer can be exposed in 44 to 88 seconds yielding a throughput of approximately 41 to 82 wafers per hour.
The need to improve switching speed and reduce power consumption has driven IC manufacturers to produce ICs with increased component density. This requires increased optical resolution in the photolithography process. It is well known in the manufacture of ICs that the density of components may soon reach a physical limit due to the diffraction effects of light. Diffraction is defined as the apparent bending of light waves around small obstacles and the spreading out of light waves transiting small openings. Diffraction distortion gives rise to a blurring of the shadow of the edge of an object or aperture. In optics, diffraction effects become important when the wavelength of the light used is about the same size as the object being imaged. For example, a standard light optical microscope has a resolving power of approximately 500 nm which is approximately equal to the wavelength of blue visible light. As higher and higher component densities are achieved, the size of individual circuit features decreases. This requires the use of shorter and shorter wavelengths of light to lower diffraction limits. State of the art photolithography machines in use today utilize UV light at a wavelength of 248 nm and employ a costly krypton-fluoride eximer laser as the light source. When combined with phase shifting masks and off-axis optics, the minimum line width that can be written on a wafer is approximately 90 nm. For the next generation of ICs, wavelengths of 193 and 157 nm (extreme UV) such as provided by argon-fluoride lasers will be used to provide line widths possibly down to 45 nm. However, the use of these wavelengths may not be practical due to problems arising from the opaqueness of the conventional glass materials making up the optical lenses. More exotic and costly materials, or the use of totally reflective optics, may be necessary. At a wavelength of 193 nm and below, immersion optics may be used in photolithography equipment to provide additional improvement in resolution. In immersion optics, the air space between the final objective lens and the silicon wafer is replaced by a liquid, such as water, having a higher index of refraction. Since the diffraction limit is also a function of the difference in index of refraction between optical elements and the surrounding medium, immersion optics gives rise to an additional level of improvement in resolution. However, this approach requires resolving not only the opaqueness problem, but also the additional problems associated with a liquid in contact with the silicon. As the wavelength of the incident radiation approaches the X-ray spectrum of approximately 20 nm, standard optical materials will no longer refract or reflect X-rays in the usual manner since the lens materials are now highly transparent at these shorter wavelengths. X-ray lithography devices may be required to use proximity printing techniques which forces the wafer to be in very close proximity to the mask. These difficulties have become technologically insurmountable as well as cost prohibitive.
A well known method for overcoming the diffraction limits associated with the photolithographic process involves replacing the UV light with an electron beam to write the IC pattern. Although the electron has an associated quantum wavelength, it is much shorter than the wavelength of even deep UV light or X-rays and will not cause a diffraction problem even at the 35 nm line width needed in the future. For lithography, the resolution limit for an electron beam is likely not due to its inherent diffraction limit, but rather is due to electron scattering in the resist material and is estimated to be approximately 10 nm. This is well below that needed for the foreseeable future of IC devices. Conventional electron beam lithography devices generally consist of a single electron beam that is focused and magnetically scanned across the silicon wafer. By turning the electron beam on and off at the appropriate time, the IC pattern can be formed much like the video image produced by scanning an electron beam across the phosphor screen of a cathode ray tube (CRT). The electron optics in these devices are very complex and similar to the beam columns of electron microscopes. Indeed, many e-beam lithography machines are modified electron microscopes. Although these electron beam devices have the ability to focus the electron beam spot far smaller than that needed for IC production, they suffer from three major problems, i.e., low throughput, high beam deflection sensitivity, and spot size enlargement due to deflection distortion. It can be easily calculated that the dwell time of an electron beam required on each pixel of an IC pattern is on the order of 1×10−7 seconds for proper exposure of the electron resist. The next generation of IC patterns will have a feature size approaching 65 nm or a resolution of 15,384 lines per mm (6.0×1010 total pixels in a 16 mm×16 mm IC). This translates to a total writing time on the order of two hours per layer of the IC pattern. In addition, the electron beam column used in conventional systems is very large in size such that only one such column can fit over the area of the wafer and only one chip pattern can be written at a time. Thus, the time to form the roughly 176 ICs on a 300 mm diameter wafer is on the order of several days. This is obviously not compatible with the 41 to 82 wafer/hr level of throughput needed for production. The second problem faced by conventional electron beam writing devices is that of beam positioning. Since the scale of the smallest feature for next generation ICs will be on the order of 65 nm, the positioning accuracy of the electromagnetic scan must be on the order of 10% of the line width, or about 6 nm, in order to guarantee vertical alignment of subsequent IC layers. In these conventional devices the positioning of the beam is controlled by an electromagnetic and/or electro-static deflection system that requires extremely accurate control of voltages and currents. This is a difficult task that can be easily disturbed by external electric or magnetic fields.
Accordingly, it is an object of the present invention to provide a mechanically driven multi-beam electron lithography (MDMBEL) apparatus for IC fabrication that alleviates the problems of low throughput and high beam deflection sensitivity.
Another object of the present invention is to provide for the high-speed, large scale fabrication of ICs by means of stationary beams of energetic particles directed onto a silicon substrate without the use of a mask.
A further object of the present invention is to provide for the simultaneous fabrication of plural ICs located on a silicon substrate by directing plural spaced energetic beams onto the substrate and displacing the substrate and controlling the operation of each of the beams in accordance with the IC design.
A still further object of the present invention is to provide a high throughput, low cost, efficient arrangement for the production of ICs wherein plural, parallel, closely spaced energetic particle beams are directed onto a silicon wafer and the wafer is linearly translated a very short distance on the order of the distance of the inter-beam spacing while the beams are individually controlled for tracing out a sub-micron circuit pattern.
It is still another object of the present invention to form an IC on a silicon wafer by directing plural spaced, fixed, parallel particle beams each having a cross section on the order of the required spatial resolution of the IC onto the wafer and displacing the wafer while turning the beams on and off in accordance with the IC pattern.
It is another object of the present invention to provide an MDMBEL device that is very small in size so that many such devices can fit on a wafer to simultaneously write a large number of individual IC patterns.
A further object of the present invention is to provide an MDMBEL device that is inexpensive to manufacture compared to current photolithography exposure equipment or electron beam lithography exposure equipment.
A still further object of the present invention is to provide an MDMBEL device that uses ultra high precision piezoelectric mechanical X-Y translation tables instead of an electromagnetic scan.
Yet another object of the present invention is to provide an MDMBEL device such that the distance needed for the mechanical translation of an IC wafer is on the order of the spacing between electron beams used to form the IC patterns on the wafer.
Still another object of the present invention is to provide an MDMBEL device that utilizes multiple, closely spaced electron beams arranged in a compact, rectangular array.
Another object of the present invention is to provide an MDMBEL device that uses conventional electron optics design and cathodes.
It is yet another object of the present invention to provide an MDMBEL device wherein the IC pattern is stored in computer software eliminating the need for costly mask sets.
Another object of the present invention is to provide an MDMBEL device wherein the step size for the X and Y piezoelectric linear stages is under software control.
The purpose of this invention is to provide a low cost, thumbnail-sized electron beam lithography apparatus that alleviates the problems of low throughput and high magnetic deflection sensitivity that prevent current e-beam lithography machines from being used in high volume production. This invention employs a large number of stationary micro column electron guns (MCEG) arranged in an K×L array extending over the length and width of each IC circuit pattern that is to be written on the wafer. Because the footprint of the array is approximately equal to the size of the IC pattern, many such MCEG arrays can fit within the circular area of the silicon wafer. In the invention, one MCEG array will be used to write one IC pattern on the wafer and all the MCEGs will write simultaneously. In conventional electron beam lithography machines, the IC circuit pattern is written by magnetically scanning an electron beam across a stationary silicon wafer. The present invention uses a novel reverse approach wherein the silicon wafer is physically moved by a set of orthogonal, high precision, piezoelectric linear stages disposed under the stationary electron beams. The silicon wafer is mechanically translated in the X and Y directions in a serpentine scan pattern while the individual electron beams are pulsed on and off by precise computer control synchronized with the position of the wafer. The computer control system contains stored IC pattern information that controls the timing of the electron beam pulses in accordance with the X-Y position of the wafer such that any circuit pattern can be written. The maximum travel of the silicon wafer in either the X or Y direction is very small and is approximately equal to the spacing between adjacent electron beams. For example, to write a 16 mm×16 mm circuit pattern with an array of 16×16 beams, the maximum displacement of the wafer need only be 1 mm in both the X and Y directions. Each of the 256 electron beams in the array writes a 1 mm×1 mm sub-field of the IC pattern, where each sub-field can be thought of as an M×N array of pixel elements. One pixel element has a size equal to the smallest feature to be drawn on the wafer. The time required to write one sub-field of the IC pattern is simply the product of the time to mechanically scan one line of the sub-field times the number of lines in the sub-field. Currently available (off the shelf) piezoelectric linear stages are capable of a displacement velocity of 100 mm/sec with a positional accuracy as small as 1 nm. Thus, the time to scan a 1 mm×1 mm sub-field at a resolution of 15384 lines/mm (65 nm resolution) is 154 seconds (15384/100). With 256 individually controlled beams simultaneously writing their individual sub-fields, the complete IC pattern is written in the same time, or 154 seconds. Since one MCEG array can be fitted for each IC pattern on the silicon wafer and all the MCEGs are driven simultaneously, the entire wafer can be written in the time it takes to write one sub-field and with only a 1 mm by 1 mm motion of the wafer. Therefore, the entire wafer is written in approximately 154 seconds or approximately 23 wafers per hour. Thus, high throughput approaching that of optical lithography is realized. This technology is applicable to an even smaller line width of 35 nm simply by modifying the electron optics in the micro column to produce a 35 nm beam diameter and reducing the pixel size (piezo-motor step size) to 35 nm. In this case, the throughput expected would be approximately 12 wafers per hour (28571 lines/mm, 2.1×1011 pixels, 286 seconds/sub-field or about 12 wafers/hour). In any of the above mentioned line widths, it may be necessary to reduce the pixel size in the vertical Y direction to some fraction of that in the X direction to allow for beam overlap when writing continuous features that extend in the Y direction. This would reduce the throughput somewhat. Since these devices would be relatively low in cost compared to current optical lithography equipment, several multi-beam steppers could be run simultaneously to equal or surpass the throughput of current optical lithography devices. The problem of electromagnetic deflection sensitivity is essentially non-existent since the beams are held stationary and the wafer is moved by mechanical means while disposed under the beams. In addition, the electron beam travel distance to the wafer is only on the order of a few millimeters compared to the tens of centimeters typical in conventional e-beam lithography columns. Thus, deflection of the electron beam by any external fields is much less likely. Because of its small size and low cost, each MCEG array can be considered a throw-away/replaceable item.
The appended claims set forth those novel features which characterize the invention. However, the invention itself, as well as further objects and advantages thereof, will best be understood by reference to the following detailed description of a preferred embodiment taken in conjunction with the accompanying drawings, where like reference characters identify like elements throughout the various figures, in which:
a is a top view of a silicon wafer showing its circular area divided into a rectangular array AIJ of IC circuit pattern regions, where one MCEG array is positioned 1 mm above each region;
b is a magnified view of a single IC region as shown in
c is a magnified view of one sub-field as shown in
The following discussion assures that 176, 16 mm×16 mm IC circuit patterns are to be written on a silicon wafer that is 300 mm in diameter using a line width of 65 nm. The concept discussed in the following paragraphs, however, is applicable to any size wafer, IC pattern size and resolution within the scope of the device.
Referring to
The construction of an MCEG array 5 is depicted in
Perhaps the most important aspect of the described invention is the method used to simultaneously write 176 complete IC patterns on the wafer. Referring to
Stored within IC circuit bank 14a are the data files that relate the IC circuit pattern with the X, Y pixel position of the wafer as reported by position controllers 14b and 14d. One data file contains the circuit pattern information for one of the 256 sub fields and controls the beam blanking signals sent by beam blanking controller 14c to each of the 256 cathodes. The circuit pattern information for each sub field is stored in the form of a list of the beam blanking condition (on or off) for each pixel in the sub field and listed in sequential order in accordance with the serpentine scan. Thus, the writing pattern for an IC is completely under software control eliminating the requirement for a costly set of photo exposure masks. Because each of the 176 MCEG arrays is writing the same circuit pattern, like positioned cathodes in each array are electrically tied together and receive the same bias and blanking data signals. Thus, cathode C11 of MCEG11 is electrically tied to and run in parallel with cathode C11 of MCEG21 which is electrically tied to and run in parallel with cathode C11 of MCEG31, and so on. It is important to realize since there are K×L beams per MCEG array and there are I×J MCEG arrays per wafer, all 176 IC circuit patterns can be written by moving the silicon wafer no more than the 1 mm span of a sub-field and within the time to scan one sub-field. In other words, the preferred embodiment has 176×256, or 45056, electron beams writing simultaneously as the wafer is displaced 1 mm in the X and Y directions.
Details of the electron optics for a micro column electron gun used in the present invention are shown in the simplified sectional view of
M=(q/p)sqrt(V2/V3), (1)
where:
Using the above computer derived voltages with an image distance q, of 1 mm, equation (1) requires an object distance p of approximately 5.3 mm to achieve a magnification of 0.065. The total length of the described micro column electron gun is given by the sum of spacings 21, 22, 23, p and q yielding an electron gun length of approximately 7-8 mm.
The last characteristic of an electron beam used in the present invention to be discussed is the beam current required for proper exposure of the electron resist material. The level of exposure is determined by the total charge in micro coulombs that is deposited on a square centimeter of the resist area. Standard electron resist materials presently used in electron beam lithography require a charge of approximately 200 uC/cm2 for complete exposure. The beam current I required to deposit 200 uC/cm2 of charge with an electron beam diameter D over an exposure time T per pixel is given by equation (2) as follows:
I=200×10−6*π(D/2)2/T (2)
Using a pixel time T of 6.5×10−7 sec (derived from the linear stage velocity of 100 mm/sec) and a beam diameter D equal to the pixel size, or 65 nm, a 1.02×10−8 Ampere beam current I is required to properly expose the resist. This is the beam current that must pass through the limiting aperture and be focused to a 65 nm diameter spot on the silicon wafer.
While particular embodiments of the present invention have been shown and described, it will be obvious to those skilled in the relevant arts that changes and modifications may be made without departing from the invention in its broader aspects. For example, variations in the design of the mechanical scan displacement arrangement, the MCEG array, the electron beam scan pattern and electron optics described herein are possible in carrying out the present invention. Thus, any such variations are within the scope and spirit of the broad concept and implementation of the present invention described herein. Therefore, the aim in the appended claims is to cover all such changes and modifications as fall within the true spirit and scope of the invention. The matter set forth in the foregoing description and accompanying drawings is offered by way of illustration only and not as a limitation. The actual scope of the invention is intended to be defined in the following claims when viewed in their proper perspective based on the prior art.