(1) Field of the Invention
The present invention relates to a process for treating a coil end upon automatic winding of the coil used for a motor, relay or transformer, by which each of a portion of the wire (i.e. electric wire) at the front end of the coil and a portion of the wire at the rear end of the coil is bound to a corresponding terminal formed on a winding object.
(2) Description of the Related Art
So far, for example, in case of a multi-spindle automatic winding device of coil, each of the portion of the wire at the front end of the coil and the portion of the wire at the rear end of the coil as insulation-treated has been bound to a corresponding metal terminal formed on a winding object such as a coil bobbin by winding each of the wire around the corresponding terminal with about three to six turns.
An example of the winding object is shown in
In general, a portion of the wire at the front or rear end of the coil, which is bound to the corresponding terminal of the winding object, has been electrically connected to the terminal by arc welding in a downstream process. In the arc welding process, a high voltage electricity is applied between an electrode and a terminal to be welded so as to generate an arc and high heat simultaneously, by which the portion of the wire at the front or rear end of the coil and the terminal are melted and joined together, thereby the electric connection is attained.
In a conventional process for treating a coil end upon winding of the coil as described above, the portion of the wire at the front or rear end of the coil is electrically connected to the terminal by arc welding. In an arc welding, since the arc tends to blow to a position at which the electricity is easily conducted, therefore it is an important subject how to blow a stable arc to a portion to be welded.
However, in the conventional process for treating a coil end as described above, an insulating coating of a wire (i.e. electric wire) affects an arc restraining the arc from blowing, resulting in an incomplete welding. As a result, there has been a possibility that the coils thus manufactured might include a defective coil, which cannot be used for electrical conduction, thereby deteriorating the reliability of the product.
It is therefore an objective of the present invention to solve the above problem and to provide a process for treating a coil end, by which upon automatic winding of the coil, the electric connection between the portion of the wire at the front or rear end of the coil and the terminal by arc welding can be securely carried out.
In order to attain the above objective, the present invention is to provide a process for treating a coil end upon automatic winding of the coil, in which a wire with an insulating coating is wound around a winding object including a terminal to be electrically connected to a portion of the wire at the front end of the coil and a terminal to be electrically connected to a portion of the wire at the rear end of the coil, so that the coil is formed, the process comprising the step of:
stripping the insulating coating off from the portions of the wire at the front and rear ends of the coil while the wire is wound around the winding object and the portions of the wire are bound to the terminal.
With the process described above, since the insulating coating is stripped off from the portions of the wire at the front and rear ends of the coil while the wire is wound around the winding object with the portions of the wire being bound to the terminal, the exposed area of the conductor of each portion of the wire can be increased. Accordingly, upon the arc welding, the arc can be stably blown, that is, the arc welding can securely be carried out, resulting in that the problem of the electric connection described above can be completely solved and a coil having high reliability and high quality can be provided.
Preferably, in the step of stripping, the insulating coating is streakily stripped off from the portions of the wire in an axial direction of the wire.
With the process described above, since the insulating coating can be streakily stripped off from the portions of the wire at the front and rear ends of the coil in an axial direction of the wire, therefore the stripping process can continuously be carried out securely and easily without influencing the path of the wire for making the coil, thereby the productivity of the coil can be raised.
Preferably, the portions of the wire to be bound to the corresponding terminals are subjected to an arc welding so as to be electrically connected to the terminal.
With the process described above, since the insulating coating is stripped off from the portions of the wire at the front and rear ends of the coil, the merit of the arc welding can be sufficiently utilized. Further, the workability can be improved, the electric connection between the portion of the wire at the front or rear end of the coil and the terminal can be securely carried out, and a coil having high reliability and high quality can be provided.
In the following, the preferred embodiments of the present invention will be explained with reference to the attached drawings.
The wire 6 is provided with a specific tension by the tension mechanism 10 and thereafter is conveyed to a stripping section 12, in which the portions of the wire at the front and rear ends of the coil are subjected to a stripping treatment and thereafter, is conveyed to the automatic coil winding section 7 equipped with a winding subject such as the winding subject 1 shown in
The stripping section 12 for stripping an insulating coating off from the wire is constructed as shown in
To the contrary, when the portion of the front or rear end of the coil of the wire 6 passes through the stripping section 12, the passing is automatically detected, and the cutter mechanism 14 starts to act as shown in
As shown in
Each portion of the wire at the front or rear end of the coil, which has been subjected to the stripping process and the binding process to the corresponding terminal continuously as described above, is further subjected to arc welding so as to carry out the electric connection. In the arc welding process, due to the high heat generated as the arc is generated, the portion of the wire at the front or rear end of the coil and the terminal are melted and joined together, thereby the electric connection is attained. Upon the arc welding, since each portion of the wire at the front or rear end of the coil, which has been subjected to the stripping, is bound to the corresponding terminal, therefore an exposed area of the conductor is increased, resulting in that the arc can be stably blown and thus the electric connection can securely be carried out.
Further, since each portion of the wire at the front or rear end of the coil is subjected to the stripping of the insulating coating, therefore an electric connection by soldering can be carried out besides the electric connection by the arc welding as described above. Furthermore, since the solder can easily adhere to the stripped part, therefore a period of time required for soldering can be shortened.
The aforementioned preferred embodiments are described to aid in understanding the present invention and variations may be made by one skilled in the art without departing from the spirit and scope of the present invention.
Number | Date | Country | Kind |
---|---|---|---|
2002-015190 | Jan 2002 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
3765276 | Pollitt | Oct 1973 | A |
3780928 | Shirn | Dec 1973 | A |
4072176 | Friend | Feb 1978 | A |
4687898 | Riordan et al. | Aug 1987 | A |
4860433 | Miura | Aug 1989 | A |
5210928 | Seshita et al. | May 1993 | A |
5977852 | Schoettl | Nov 1999 | A |
6442833 | Mizuno et al. | Sep 2002 | B1 |
Number | Date | Country | |
---|---|---|---|
20030136000 A1 | Jul 2003 | US |