This application claims priority to Chinese Patent Application No. 200910199993.9, filed Dec. 4, 2010, which is commonly owned and incorporated by reference herein for all purposes.
Embodiments of the present invention generally relate to integrated circuits and their processing for the manufacture of semiconductor devices. More particularly, embodiments of the present invention provide a method and architecture for manufacturing a memory device including a flash memory device, which can be embedded in other applications. For example, embodiments of the invention can be applied to embedded flash memory designs on logic, digital signal processing, microprocessor, micro-controller, and others devices.
A variety of memory devices have been proposed or used in industry. An example of such a memory device is an erasable programmable read-only memory (“EPROM”) device. The EPROM device is both readable and erasable, i.e., programmable. In particular, an EPROM is implemented using a floating gate field effect transistor, which has binary states. That is, a binary state is represented by the presence of absence of charge on the floating gate. The charge is generally sufficient to prevent conduction even when a normal high signal is applied to the gate of the EPROM transistor.
Numerous varieties of EPROMs are available. In the traditional and most basic form, EPROMs are programmed electrically and erased by exposure to ultraviolet light. These EPROMs are commonly referred to as ultraviolet (UV) erasable programmable read-only memories (“UVEPROM”s). UVEPROMs can be programmed by running a high current between a drain and a source of the UVEPROM transistor while applying a positive potential to the gate. The positive potential on the gate attracts energetic (i.e., hot) electrons from the drain-to-source current, where the electrons jump or inject into the floating gate and become trapped on the floating gate.
Another form of EPROM is the electrically erasable and programmable read-only memory (“EEPROM” or “E2 PROM”). EEPROMs are often programmed and erased electrically by way of a phenomenon known as Fowler-Nordheim tunneling. Still another form of EPROM is a “Flash EPROM,” which is programmed using hot electrons and erased using the Fowler-Nordheim tunneling phenomenon. Flash EPROMs can be erased in a “flash” or bulk mode in which all cells in an array or a portion of an array can be erased simultaneously using Fowler-Nordheim tunneling, and are commonly called “Flash cells” or “Flash devices.”
Various types of Flash cells have been proposed and utilized in the semiconductor industry. As merely an example, a split gate structure includes a floating gate, a control gate, and an additional gate known as a select gate. In the split gate structure, the control gate is disposed on top of the floating gate and insulated from it through a dielectric layer. Because of the select gate, the split gate structure is generally larger than a stack-gate structure. For example, the split gate structure has been used by companies such as Silicon Storage Technology, Inc. Unfortunately, a memory cell using a split gate structure cell is often difficult to shrink beyond a certain critical dimension such as 0.25 micron and below. These and other limitations of the conventional split gate cell have been described throughout the present specification and more particularly below.
From the above, it is seen that an improved technique for processing semiconductor devices is desired.
According to embodiments of the present invention, techniques including methods for the manufacture of semiconductor devices are provided. More particularly, embodiments of the invention provide a method and device for manufacturing a memory device including a Flash Memory device, which can be embedded in other applications. For example, embodiments of the invention can be applied to embedded Flash Memory designs on logic, digital signal processing, microprocessor, micro-controller, and others devices.
In a specific embodiment, the invention provides a method for manufacturing memory devices, e.g., Flash memory device. The method includes forming a well region in a substrate, e.g., silicon wafer. The method forms a first polysilicon layer overlying the well region in the substrate and forms a dielectric layer overlying the first polysilicon layer. The method includes depositing a second polysilicon layer overlying the dielectric layer to form a stack layer; the stack layer including the first polysilicon layer, the dielectric layer, and the second polysilicon layer. The method simultaneously patterns the stack layer to form a flash memory device structure, the flash memory device structure including a first portion of the second polysilicon layer overlying a first portion of the dielectric layer, which overlies a first portion of the first polysilicon layer and to form a select device, the select device including a second portion of the second polysilicon layer overlying a second portion of the dielectric layer, which overlies a second portion of the first polysilicon layer. In an embodiment, the select device can be activated by applying a voltage to the second portion of the first polysilicon layer. Preferably, the method forms an electrical connection between the second portion of the second polysilicon layer and the second portion of the first polysilicon layer for the select device, while maintaining isolation between the first portion of the second polysilicon layer and the first portion of the first polysilicon layer for the first flash memory device.
In an alternative specific embodiment, the invention provides a semiconductor integrated circuit memory device structure, e.g., Flash memory cell. The structure includes a semiconductor substrate, e.g., silicon wafer. The structure also includes a well region in a substrate and a dielectric layer formed over the well region. A flash memory device structure is formed overlying a first portion of the dielectric layer. The flash memory device structure further includes a first portion of a second polysilicon layer overlying a first portion of the dielectric layer overlying a first portion of a first polysilicon layer. The structure also includes a select device formed over a second portion of the dielectric layer. In an embodiment, the select device may be coupled to the flash memory device structure through a source/drain region. In another embodiment, the select device may include a second portion of the second polysilicon layer overlying a second portion of the dielectric layer, which overlies a second portion of the first polysilicon layer. The structure further includes a contact region that electrically couples the second portion of the second polysilicon layer to the second portion of the first polysilicon layer.
In a specific embodiment, the flash device has a tunnel oxide layer between the first portion of the first polysilicon layer and the well region, and the select device has a gate oxide layer between the second portion of the first polysilicon layer and the well region. Depending on the embodiment, the gate oxide may have a different thickness than the tunnel oxide.
Many benefits can be achieved by way of the present invention over conventional techniques. For example, embodiments of the present technique provide an easy to use process that relies upon conventional technology. In some embodiments, the method provides higher device yields in dies per wafer. Additionally, the method provides a process that is compatible with conventional process technology without substantial modifications to conventional equipment and processes. Depending upon the embodiment, one or more of these benefits may be achieved. These and other benefits will be described in more throughout the present specification and more particularly below.
Various additional embodiments, features, and advantages of the present invention can be more fully appreciated with reference to the detailed description and accompanying drawings that follow.
According to embodiments of the present invention, techniques including methods for the manufacture of semiconductor devices are provided. More particularly, embodiments of the invention provide a method and structure for manufacturing a memory device including a Flash Memory device, which can be embedded in other applications. For example, the invention can be applied to embedded Flash Memory designs on logic, digital signal processing, microprocessor, micro-controller, and others devices.
The Flash memory device includes a floating gate 115 defined by poly-1 and an overlying control gate 117 defined by poly-2. An ONO layer 116 is interposed between the floating gate and the control gate, as shown. The Flash device also included source/drain region 111 and a source/drain region 119, which coupled to each other through a channel region 121. The present gate structure is commonly called an “ETOX” gate structure, but can also be others. The channel region can include a length of 0.18 microns and less, and 0.15 microns and less, as well as other dimensions. Each of the devices is formed on the gate oxide layer overlying the semiconductor substrate. In an embodiment, the semiconductor substrate can be a silicon wafer or any other suitable material.
In an embodiment, the floating gate (i.e., the first polysilicon layer) has a thickness of about 1000 Angstroms to about 2000 Angstroms; the dielectric layer has a thickness of about 50 Angstroms to about 200 Angstroms; and the control gate (i.e., the second polysilicon layer) has a thickness of about 1500 Angstroms to about 2500 Angstroms.
In some embodiments, the flash device includes a tunnel oxide layer between the first portion of the first polysilicon layer and the well region and the select device includes a gate oxide layer between the second portion of the first polysilicon layer and the well region. Although the tunnel oxide and gate oxide are both shown as layer 120 in
In operation, a voltage is applied to poly 1 of the select gate, which causes the voltage to be applied to source/drain region 111. Alternatively, poly 1 and poly 2 in the select gate are electrically connected to each other. Accordingly, the voltage may also be applied to poly 2 of the select gate, which provides the same voltage potential to poly 1 of the select gate. That is, poly 1 and poly 2 are connected to each other electrically. The Flash device operates in a conventional manner. Further details of the present invention are found throughout the present specification and more particularly below.
A method according to an embodiment of the present invention may be outlined as follows:
1. Provide a semiconductor substrate, e.g., a silicon wafer;
2. Form a well region in the substrate;
3. Form field isolation regions (e.g., LOCOS, STI);
4. Form a gate dielectric layer overlying the well region;
5. Deposit a first polysilicon layer overlying the gate dielectric layer;
6. Deposit a first oxide layer overlying the first polysilicon layer;
7. Deposit a nitride layer overlying the oxide layer;
8. Deposit a second oxide layer overlying the nitride layer, where the ensemble of the first oxide layer, the nitride layer and the second oxide layer forms an oxide-on-nitride-on-oxide (“ONO”) layer;
9. Deposit a second polysilicon layer overlying the ONO layer, thereby the first polysilicon layer, the ONO layer, the second polysilicon layer form a stack layer;
10. Pattern the stack layer to form a flash memory cell and a select device, the patterning step may include a photolithography and an etching process;
11. Form source/drain regions using ion implantation;
12. Deposit an inter-metal layer dielectric material overlying the patterned stack layer and the source/drain regions;
13. Form an opening through the inter-metal layer dielectric material overlying the select device;
14. Fill the opening with a conducting material to connect the first polysilicon layer and the second polysilicon layer of the select device; and
15. Perform other steps, as desired.
The above sequence of steps is a method according to an embodiment of the present invention. As shown, the method provides processing steps of forming a select device coupled to a memory device, which has improved packing features. The memory device is an ETOX type memory structure, which can be packed in an array structure that is much denser than conventional split gate structures. Further details are provided throughout the present specification and more particularly below.
The method forms field isolation regions (not shown) within the substrate. The field isolation regions can be formed using a variety of techniques such as local oxidation of silicon, commonly called LOCOS, alternatively, isolation regions can be formed using trench isolation structures. A surface of the silicon wafer is exposed and cleaned before the formation of a gate dielectric layer 420. The gate dielectric layer is formed overlying the surface of the substrate. The gate dielectric layer can be a high quality oxide layer, a silicon oxynitride layer, silicon nitride layer, any combination of these, and the like.
The method forms a stack layer, including a first polysilicon layer 405, an oxide layer 406, and a second polysilicon layer 407. Here, the method forms the first polysilicon layer overlying the gate dielectric layer. The polysilicon layer is preferably doped using implantation, diffusion, or other techniques. More preferably, the polysilicon layers are in-situ doped with an impurity having a concentration of about 1020 atoms/cm3 depending upon the embodiment. The impurity can be phosphorous and/or arsenic and the like. The method forms an overlying oxide layer 406 overlying the first polysilicon layer. In an embodiment, the oxide layer includes forming a first oxide layer overlying the dielectric layer, and forming a nitride layer over the first oxide layer. The method further includes forming a second oxide layer over the nitride layer to form an oxide-nitride-oxide (ONO) layer. The first polysilicon layer, the ONO layer and the second polysilicon layer form a stack layer that is then patterned and etched to obtain a select device 501 and a flash memory device 503 as shown in
Referring to
In a specific embodiment, the oxide layer 420 has a thickness of 100 Angstroms; the first polysilicon layer has a thickness of 1000 to about 2000 Angstroms, preferably 1500 Angstroms, the ONO layer has a thickness of about 200 Angstroms, and the second polysilicon layer has a thickness of about 1500 Angstroms to about 2500 Angstroms, and preferably 2000 Angstroms. In another embodiment, the inter-metal layer dielectric material has a thickness ranging from about 3000 Angstroms to about 6000 Angstrom measuring from a surface of the gate dielectric layer 420. In yet another embodiment, the inter-metal layer dielectric material has a thickness ranging from about 400 Angstroms to about 3000 Angstroms measuring from a top surface of the second polysilicon layer.
Referring to
It is also understood that the examples and embodiments described herein are for illustrative purposes only and that various modifications or changes in light thereof will be suggested to persons skilled in the art and are to be included within the spirit and purview of this application and scope of the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
200910199993.9 | Dec 2009 | CN | national |