This application is a national phase entry under 35 U.S.C. 371 of PCT International Application No. PCT/FI2020/050466 filed Jun. 26, 2020, which claims priority to Finnish Patent Application No. 20195591, filed Jun. 28, 2019, the disclosure of each of these applications is expressly incorporated herein by reference in their entirety.
The present invention relates to an atomic layer deposition apparatus.
Atomic layer deposition method utilizes conventionally precursor materials having low vapour pressure. Usually these kinds of materials are solid precursor materials. However, also some liquid precursors may be considered as low vapour pressure materials. During atomic layer deposition method, the precursors are supplied to a deposition chamber of an atomic layer deposition apparatus in gas phase. Thus, the solid or liquid precursor materials are vaporized and dosed in gaseous form into the deposition chamber for subjecting a surface of a substrate to the precursor material. In order to supply these low vapour pressure precursors to the deposition chamber such that dose is large enough and the operating speed or dosing speed is good enough, the precursor materials need to be heated. Thus, these precursor sources or source arrangements are usually called hot sources.
In the prior art precursors are supplied from precursor sources to the deposition chamber through channels that extend from source arrangements that are arranged further away from the deposition chamber. One of the disadvantages of the prior art precursor source arrangements and atomic layer deposition apparatuses is that maintaining an increasing temperature gradient along the supply path of the precursor material is compromised such that the temperature of the precursor material may locally decrease during supplying to the deposition chamber. When the temperature of the precursor material decreases, the gaseous precursor tends to condensate into liquid. Liquid condensate deteriorates the atomic layer deposition process and apparatus.
An object of the present invention is to provide an atomic layer deposition apparatus for processing substrates which the apparatus provides efficient thermal conditions for heated precursors to be supplied from precursor sources to a deposition chamber such that temperature gradient is rising to prevent the formation of cold spots and condensation with them.
The objects of the invention are achieved by an atomic layer deposition apparatus which is characterized by what is stated in the independent claim. The preferred embodiments of the invention are disclosed in the dependent claims.
The invention is based on the idea of providing an atomic layer deposition apparatus for processing substrates according to principles of atomic layer deposition having short passages for heated precursors to flow from precursor sources to the deposition chamber. The atomic layer deposition apparatus according to the invention comprises a vacuum chamber, a deposition chamber within the vacuum chamber, an inlet channel extending from outside of the vacuum chamber to the deposition chamber such that the inlet channel is connected to the deposition chamber for supplying gases to the deposition chamber and a discharge channel extending from the deposition chamber to outside of the vacuum chamber for discharging gases from the deposition chamber. The apparatus further comprises one or more first precursor supply sources connected to the inlet channel, and one or more second precursor supply sources connected to the inlet channel. The vacuum chamber is arranged between the one or more first precursor supply sources and the one or more second precursor supply sources. In other words, the vacuum chamber is arranged such that the one or more first precursor supply sources are arranged on first side of the vacuum chamber and the one or more second precursor sources are arranged on the second side of the vacuum chamber which is opposite to the first side of the vacuum chamber. The one or more first precursor sources, the vacuum chamber and the one or more second precursor sources are preferably arranged at the same horizontal level. The first precursor sources and the second precursor sources are liquid or solid precursor sources which are supplied to the deposition chamber inside the vacuum chamber through the inlet channel. The first precursor sources and the second precursor sources are preferably different precursor sources having different process temperatures such that the first precursor sources are high temperature precursor sources and the second precursor sources are low temperature precursor sources.
The apparatus according to the invention further comprises a first side compartment and a second side compartment such that the vacuum chamber is arranged between the first and second side compartments. The one or more first precursor supply sources are arranged inside the first side compartment, and the one or more second precursor supply sources are arranged inside the second side compartment. In other words, the first side compartment, the vacuum chamber and the second side compartment are preferably arranged side by side such that the vacuum chamber is arranged to separate the first and second side compartments from each other and such that the first and second precursor supply channels coming from the first and second precursor sources are arranged to enter the vacuum chamber on opposite sides of the vacuum chamber.
According to the invention the one or more first precursor sources are connected to the inlet channel with one or more first precursor supply channels such that the one or more first precursor supply channels are arranged to extend from the one or more first precursor supply sources to the inlet channel inside the vacuum chamber. Further according to the invention, the one or more second precursor supply sources are connected to the inlet channel with one or more second precursor supply channels such that the one or more second precursor supply channels are arranged to extend from the one or more second precursor supply sources to the inlet channel inside the vacuum chamber. The inlet channel is arranged to extend inside the vacuum chamber such that the connection between the one or more first precursor supply channels and the inlet channel is provided perpendicularly, i.e. the connection between the inlet channel and the first precursor supply channel is perpendicular such that the first precursor supplied through the first precursor supply channel is arranged to enter the inlet channel perpendicularly so that the first precursor will mix with gas coming through the inlet channel. The same applies to the connection between the one or more second precursor supply channels and the inlet channel.
The first and second precursors in the first and second precursor sources are preferably different such that they require different temperature levels. Therefore, the apparatus according to an embodiment of the invention comprises one or more first chambers arranged within the first side compartment. The one or more first chambers comprising the one or more first precursor supply sources inside the one or more first chambers. The one or more first chambers are preferably a heated chamber receiving heating energy outside the chamber or the chamber comprises a heating element for heating the chamber. Alternatively, the first side compartment is a first chamber comprising at least one heater for heating the one or more first precursor supply sources arranged within the first side compartment. The difference between the compartment and the chamber is that the compartment is an outer structure of the apparatus for covering the precursor source inside the compartment and therefore comprises structural elements associated with covering the physical source, such as a source bottle, arranged inside the compartment, but the chamber comprises features and elements associated with pressurization or heating the chamber required by the liquid or solid properties of the precursor substance provided within the source.
According to an embodiment of the invention the first chamber is insulated from the vacuum chamber which means that the first compartment is arranged to form the first chamber. Alternatively, the first chamber is insulated from the first side compartment which means that the first chamber is provided inside the first side compartment and is a separate chamber inside the first side compartment.
According to an embodiment of the invention the apparatus comprises a first lead-through connection between the first side compartment and the vacuum chamber such that the one or more first precursor supply channels are extending from the first side compartment to the vacuum chamber through the first lead-through connection. The apparatus further comprises a second lead-through connection between the second side compartment and the vacuum chamber such that the one or more second precursor supply channels are extending from the second side compartment to the vacuum chamber through the second lead-through connection. The first lead-through connection and the second lead-through connection are provided on opposite sides of the vacuum chamber. The vacuum chamber comprises a first end wall and a second end wall opposite to the first end wall and an opening to the vacuum chamber at the first end wall. Further a chamber axis is extending between the first and second end walls such that the vacuum chamber can be divided by an imaginary vertical partition wall through the chamber axis into two parts. The first lead-through connection is provided at a wall of the vacuum chamber in the first part of the vacuum chamber and the second lead-through connection is provided at a wall of the vacuum chamber in the second part of the vacuum chamber, i.e. the first lead-through connection is provided on opposite side of the vacuum chamber than the second lead-through connection which the vacuum chamber is divided into two parts with a plane extending vertically through the chamber axis. The vacuum chamber can also be divided into two parts, an upper part and a lower part, with a plane extending horizontally through the chamber axis. The apparatus further comprises a third lead-through connection at a bottom wall of the vacuum chamber. The bottom wall of the vacuum chamber is provided at the lower part of the vacuum chamber. The inlet channel and the discharge channel are arranged to extend downward from the deposition chamber. The inlet channel is extending from the deposition chamber inside the vacuum chamber through the third lead-through connection to outside of the vacuum chamber.
According to the invention the first and second side compartments are arranged on opposite sides of the vacuum chamber in a direction transverse to the chamber axis, more particularly in a direction horizontally transverse to the chamber axis.
According to an embodiment of the invention the inlet channel is arranged to extend inside the vacuum chamber in a transverse direction relative to the chamber axis. Alternatively or in addition, the inlet channel is arranged to extend inside the vacuum chamber in a perpendicular direction relative to the chamber axis.
According to an embodiment of the invention the inlet channel is connected to the deposition chamber inside the vacuum chamber such that a distance from a connection of the inlet channel and the deposition chamber to the second side compartment is smaller than a distance from the connection of the inlet channel and the deposition chamber to the first side compartment. In other words, the inlet channel is preferably arranged to extend inside the vacuum chamber from the bottom of the vacuum chamber to the deposition chamber on that side of the vacuum chamber comprising the second lead-through connection to the second side compartment. In this embodiment, a distance that the first precursor supply channel is arranged to extend from the first side compartment through the lead-through connection to the inlet channel is greater than the distance of the second precursor supply channel extending from the second side compartment to the inlet channel. This is particularly preferable in embodiments in which the first precursor of the first precursor source should maintain its high temperature from the first precursor source all the way to the inlet channel. The vacuum chamber is most preferably a heated vacuum chamber comprising one or more heaters inside the vacuum chamber.
In an embodiment of the invention the vacuum chamber comprises a first end wall having an opening to the vacuum chamber and a second end wall opposite to the first end wall and the inlet channel is arranged in the vacuum chamber such that a connection of inlet channel and the deposition chamber is closer to the second end wall than to the first end wall.
In an embodiment of the invention the apparatus further comprises a lower compartment connected to the vacuum chamber such that the vacuum chamber is arranged above the lower compartment and the inlet channel is arranged to extend from the lower compartment to the deposition chamber arranged inside the vacuum chamber. The third lead-through connection is arranged between the lower compartment and the vacuum chamber to provide a passage for the inlet channel to extend from the lower compartment to the vacuum chamber. The first and the second side compartments are also arranged above the lower compartment.
The first lead-through connection from the first side compartment to the vacuum chamber and the second lead-through connection from the second side compartment to the vacuum chamber are preferably arranged such that the precursor supply channels extending through the lead-throughs are transverse relative to the chamber axis when the precursor supply channels enter the vacuum chamber on opposite sides of the vacuum chamber divided into two parts by an imaginary vertical plane passing through the chamber axis. The third lead-through connection from the lower compartment to the vacuum chamber is arranged such that the inlet channel extending through the third lead-through is transverse to the chamber axis when entering to the vacuum chamber. In a preferable embodiment of the invention the inlet channel is arranged to extend in a vertical direction inside the vacuum chamber and such that the first and second precursor supply channels that are connected to the inlet channel extend transversely relative to the inlet channel. In a preferred embodiment of the invention the first and second precursor supply channels are connected to the inlet channel perpendicularly. The third lead-through connection is arranged between the lower compartment and the vacuum chamber such that the inlet channel is arranged to extend vertically or substantially vertically through the third lead-through connection whereas the first lead-through connection is arranged between the first side compartment and the vacuum chamber such that the first precursor supply channel is arranged to extend through the first lead-through connection in a transverse direction to the inlet channel and the second lead-through connection is arranged between the second side compartment and the vacuum chamber such that the second precursor supply channel is arranged to extend through the second lead-through connection in a transverse direction to the inlet channel on the opposite side of the vacuum chamber than the first precursor supply channel.
According to the invention the apparatus comprises a gas source arranged within the lower compartment. Alternatively or in addition, the apparatus comprises a suction device arranged within the lower compartment.
According to the invention the vacuum chamber is arranged between the first precursor source and the second precursor source, more specifically between the first side compartment comprising the first precursor source and the second side compartment comprising the second precursor source. The term “between” in this connection means that the vacuum chamber is provided next to the first side compartment and next to the second side compartment such that first side compartment is on the opposite side of the vacuum chamber than the second side compartment. The vacuum chamber is connected to the side compartments such that a passage from the side compartments to the vacuum chamber are arranged with the lead-throughs.
An advantage of the invention is that the precursor supply channels are arranged such that distance from the precursor source to the inlet channel connected to the deposition chamber is minimized in order to provide optimal precursor flows from the precursor source to the inlet channel. Another advantage of the invention is that the minimized distance from the precursor sources to the inlet channel and rising temperature gradient due to vacuum chamber heating prevent effectively the formation of cold spots, especially when the precursor is supplied from a heated chamber surrounding the precursor source in the side compartment.
The invention is described in detail by means of specific embodiments with reference to the enclosed figures, in which
Although figures do not specifically show the vacuum chamber 20 is preferably heated such that the vacuum chamber 20 comprises at least one heater connected to an interior surface of the vacuum chamber.
The vacuum chamber 20 comprises a deposition chamber 2 provided inside the vacuum chamber 20. The deposition chamber 2 comprises a space within the deposition chamber into which a substrate to be coated is placed. The inlet channel 5 is connected to the deposition chamber 5 for supplying gas flows into the deposition chamber 2 during processing of the substrate. The inlet channel 5 supplies the first precursor supplied from the first precursor source through the first precursor supply channel 31 to the deposition chamber 2 and also the second precursor supplied from the second precursor source through the second precursor supply channel 41 to the deposition chamber 2 as well as other gases such as purge gases from the lower compartment 10 comprising a gas source 50 arranged within the lower compartment 10. The inlet channel 5 is preferably arranged to extend from the gas source 50 through the third lead-through connection 100 to the vacuum chamber 20 and further to the deposition chamber 2 such that the inlet channel 5 and the deposition chamber 2 are connected together.
The lower compartment 10 further comprises a suction device 60 or other equipment relating to discharging gases from the deposition chamber 2 through the discharge channel 6 connected to the deposition chamber 2 and extending through the third lead-through connection 100 from the vacuum chamber 2 to the lower compartment 10. The lower compartment 10 also comprises means for moving the deposition chamber 2 such as mechanical construction for opening and closing the deposition chamber 2 which is preferably arranged such that a bottom of the deposition chamber 2 is arranged to be moved downwards in the vacuum chamber 2 for opening the deposition chamber 2 and further to be moved upwards for closing the deposition chamber 2.
The vacuum chamber 20 comprises a deposition chamber 2 provided inside the vacuum chamber 20. The inlet channel 5 extending from the lower compartment substantially vertically to the vacuum chamber 20 is connected to the deposition chamber such that the connections from the first and second precursor supply channel 31, 41, 41′ to the inlet channel 5 are provided at the inlet channel 5 in an area between the third lead-through connection 100 and the connection to the deposition chamber 2. The discharge channel 6 connected to the deposition chamber 2 for discharging gases from the deposition chamber 2 is preferably arranged to extend vertically from the deposition chamber 2 to the lower compartment 10. In the embodiment shown in
The invention has been described above with reference to the examples shown in the figures. However, the invention is in no way restricted to the above examples but may vary within the scope of the claims.
Number | Date | Country | Kind |
---|---|---|---|
20195591 | Jun 2019 | FI | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/FI2020/050466 | 6/26/2020 | WO |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2020/260770 | 12/30/2020 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
20060126700 | Wilcox | Jun 2006 | A1 |
20080063798 | Kher et al. | Mar 2008 | A1 |
20080193643 | Dip | Aug 2008 | A1 |
20100136313 | Shimizu et al. | Jun 2010 | A1 |
20100183825 | Becker | Jul 2010 | A1 |
20120058630 | Quinn | Mar 2012 | A1 |
20120222751 | Okabe | Sep 2012 | A1 |
20120266819 | Sanchez et al. | Oct 2012 | A1 |
20150184297 | Kim et al. | Jul 2015 | A1 |
20170067163 | Papasouliotis et al. | Mar 2017 | A1 |
Number | Date | Country |
---|---|---|
2013064737 | May 2013 | WO |
Entry |
---|
International Search Report issued by the Finnish Patent and Registration Office acting as the International Searching Authority in relation to International Application No. PCT/FI2020/050466 dated Dec. 2, 2020 (4 pages). |
Written Opinion of the International Searching Authority issued by the Finnish Patent and Registration Office acting as the International Searching Authority in relation to International Application No. PCT/FI2020/050466 dated Dec. 2, 2020 (5 pages). |
Finnish Search Report issued by the Finnish Patent and Registration Office in relation to Finnish Application No. 20195591 dated Jan. 29, 2020 (1 page). |
Number | Date | Country | |
---|---|---|---|
20220205097 A1 | Jun 2022 | US |