This invention relates to atomic layer deposition methods of depositing an oxide on a substrate.
Integrated circuits are typically formed on a semiconductor substrate such as a silicon wafer or other semiconductive material. In general, layers of various materials, which are one of semiconductive, conducting or insulating, are used to form the integrated circuits. By way of example, the various materials are doped, ion implanted, deposited, etched, grown, etc., using various processes. A continuing goal in semiconductor processing is to reduce the size of individual electronic components, thereby enabling smaller and denser integrated circuitry.
As semiconductor devices continue to shrink geometrically, such has had a tendency to result in greater shrinkage in the horizontal dimension than in the vertical dimension. In some instances, the vertical dimension increases. Regardless, the result is increased aspect ratios (height to width) of the devices, making it increasingly important to develop processes that enable materials to conformally deposit over the surfaces of high aspect ratio features. One such processing is atomic layer deposition, which involves the deposition of successive monolayers over a substrate within a deposition chamber typically maintained at subatmospheric pressure. With typical atomic layer deposition, successive mono-atomic layers are adsorbed to a substrate and/or reacted with the outer layer on the substrate, typically by the successive feeding of different deposition precursors to the substrate surface.
One commonly used class of materials in the fabrication of integrated circuitry is oxides. Some oxides are electrically conductive, while other oxides are electrically insulative.
While the invention was motivated in addressing the above issues, it is in no way so limited. The invention is only limited by the accompanying claims as literally worded, without interpretative or other limiting reference to the specification, and in accordance with the doctrine of equivalents.
The invention includes atomic layer deposition methods of depositing an oxide on a substrate. In one implementation, a substrate is positioned within a deposition chamber. A first species is chemisorbed onto the substrate to form a first species monolayer within the deposition chamber from a gaseous precursor. The chemisorbed first species is contacted with remote plasma oxygen derived at least in part from at least one of O2 and O3 and with remote plasma nitrogen effective to react with the first species to form a monolayer comprising an oxide of a component of the first species monolayer. The chemisorbing and the contacting with remote plasma oxygen and with remote plasma nitrogen are successively repeated effective to form porous oxide on the substrate.
Other aspects and implementations are contemplated.
Preferred embodiments of the invention are described below with reference to the following accompanying drawings.
This disclosure of the invention is submitted in furtherance of the constitutional purposes of the U.S. Patent Laws “to promote the progress of science and useful arts” (Article 1, Section 8).
The invention comprises atomic layer deposition methods of depositing oxides on substrates. Atomic layer depositing (ALD) typically involves formation of successive atomic layers on a substrate. Described in summary, ALD includes exposing an initial substrate to a first chemical species to accomplish chemisorbtion of the species onto the substrate. Theoretically, the chemisorbtion forms a monolayer that is uniformly one atom or molecule thick on the entire exposed initial substrate. In other words, a saturated monolayer is preferably formed. Practically, chemisorbtion might not occur on all portions or completely over the desired substrate surfaces. Nevertheless, such an imperfect monolayer is still considered a monolayer in the context of this document. In many applications, merely a substantially saturated monolayer may be suitable. A substantially saturated monolayer is one that will still yield a deposited layer exhibiting the quality and/or properties desired for such layer.
The first species is purged from over the substrate and a second chemical species is provided to chemisorb onto the first monolayer of the first species. The second species is then purged and the steps are repeated with exposure of the second species monolayer to the first species. In some cases, the two monolayers may be of the same species. Also, a third species or more may be successively chemisorbed and purged just as described for the first and second species. Further, one or more of the first, second and third species can be mixed with inert gas to speed up pressure saturation within a reaction chamber.
Purging may involve a variety of techniques including, but not limited to, contacting the substrate and/or monolayer with a carrier gas and/or lowering pressure to below the deposition pressure to reduce the concentration of a species contacting the substrate and/or chemisorbed species. Examples of carrier gases include nitrogen, Ar, He, Ne, Kr, Xe, etc. Purging may instead include contacting the substrate and/or monolayer with any substance that allows chemisorption byproducts to desorb and reduces the concentration of a species preparatory to introducing another species. A suitable amount of purging can be determined experimentally as known to those skilled in the art. Purging time may be successively reduced to a purge time that yields an increase in film growth rate. The increase in film growth rate might be an indication of a change to a non-ALD process regime and may be used to establish a purge time limit.
ALD is often described as a self-limiting process in that a finite number of sites exist on a substrate to which the first species may form chemical bonds. The second species might only bond to the first species and thus may also be self-limiting. Once all of the finite number of sites on a substrate are bonded with a first species, the first species will often not bond to other of the first species already bonded with the substrate. However, process conditions can be varied in ALD to promote such bonding and render ALD not self-limiting. Accordingly, ALD may also encompass a species forming other than one monolayer at a time by stacking of a species, forming a layer more than one atom or molecule thick. Further, local chemical reactions can occur during ALD (for instance, an incoming reactant molecule can displace a molecule from an existing surface rather than forming a monolayer over the surface). To the extent that such chemical reactions occur, they are generally confined within the uppermost monolayer of a surface.
Traditional ALD can occur within frequently-used ranges of temperature and pressure and according to established purging criteria to achieve the desired formation of an overall ALD layer one monolayer at a time. Even so, ALD conditions can vary greatly depending on the particular precursors, layer composition, deposition equipment, and other factors according to criteria known by those skilled in the art. Maintaining the traditional conditions of temperature, pressure, and purging minimizes unwanted reactions that may impact monolayer formation and quality of the resulting overall ALD layer. Accordingly, operating outside the traditional temperature and pressure ranges may risk formation of defective monolayers.
An exemplary preferred embodiment is initially described with reference to
Referring to
The porous oxide which is formed might be an electrically insulative oxide or an electrically conductive oxide. By way of example only, exemplary preferred insulative oxides include SiO2 and Al2O3. Further by way of example only, exemplary preferred electrically conductive oxides include tin oxide and indium oxide. By way of example only, for the formation of porous Al2O3, an exemplary gaseous precursor for chemisorbing the first species is trimethyl aluminum, with a likely first species being aluminum chemisorbed to the substrate, with methyl groups pending from the chemisorbed aluminum. Accordingly, the contacting with remote plasma oxygen and with remote plasma nitrogen forms an oxide with an aluminum component of the first species monolayer.
By way of example only, where the porous oxide comprises SiO2, an exemplary gaseous precursor comprises at least one of tetraethylorthosilicate (TEOS) and a silane. Accordingly, the chemisorbed first species will comprise silicon, which will combine with the remote plasma oxygen to form an oxide. Further by way of example only, where the porous oxide comprises tin oxide, an exemplary gaseous precursor is trimethyl tin. Accordingly, the chemisorbed first species will comprise tin, which combines with the remote plasma oxygen to form tin oxide. Further by way of example only, where the porous oxide comprises indium oxide, an exemplary gaseous precursor is trimethyl indium. Accordingly, the chemisorbed first species will comprise indium, which combines with the remote plasma oxygen to form indium oxide.
Further by way of example only, the porous oxide might comprise multiple cations. By way of example only, one such porous oxide comprises InxSnyO, which is an electrically conductive oxide. By way of example only, exemplary indium and tin precursors are trimethyl tin and trimethyl indium. Such might be fed to the deposition chamber simultaneously in desired ratios towards achieving the desired quantity of tin and indium in the oxide being formed. Further by way of example only, such simultaneous feeding might as a mixture or separately to the chamber. Further by way of example only, the tin containing precursor and the indium containing precursor might be fed to the deposition chamber at different times. Such different times might overlap with one another, or be spaced from one another such that there is no overlap.
By way of example only,
Referring to
Exemplary preferred remote plasma nitrogen is derived from any one or combination of N2, N2O and NOx. Further, the remote plasma oxygen might comprise one or a combination of O2 and O3.
The remote plasma oxygen and the remote plasma nitrogen are most preferably fed to the deposition chamber simultaneously, meaning over the same identical time interval (for example as depicted in
In one preferred implementation, the remote plasma oxygen and the remote plasma nitrogen are fed as a mixture to the deposition chamber.
By way of example only, an alternate lesser preferred embodiment system 40 is depicted in
Regardless of whether mixing or fed separately, when the remote plasma oxygen and the remote plasma nitrogen are fed to the deposition chamber at the same time, a preferred quantity or concentration of the remote plasma nitrogen is from 0.01% to 90% by volume of all remote plasma oxygen and remote plasma nitrogen fed to the deposition chamber. More preferably, the remote plasma nitrogen is from 0.1% to 10%, and more preferably from 0.1% to 3% by volume of all remote plasma oxygen and remote plasma nitrogen fed to the deposition chamber. Very low quantities of remote plasma nitrogen have been found effective to produce porous oxide in accordance with the invention, with another preferred concentration range for the remote plasma nitrogen being from 0.01% to 1% by volume of all remote plasma oxygen and remote plasma nitrogen fed to the deposition chamber.
An exemplary preferred temperature range for the stated chemisorbings and contactings is from 100° C. to 500° C., and more preferably from 200° C. to 350° C. Exemplary preferred pressure within the chamber during the stated chemisorbings and contactings is from 200 mTorr to 10 Torr, with from 500 mTorr to 2.5 Torr being more preferred. An exemplary preferred remote plasma generating power is from 1000 watts to 6000 watts, with 4000 watts being a specific example. An exemplary preferred frequency for the remote plasma generation is 13.5 mHz, with such powers and frequencies being for an exemplary total two liters feed of gases to the remote plasma generator. Of course, some of the remote plasma material generated might be diverted to not flow to the chamber. Further, the chamber might, of course, be a cold wall reactor or a hot wall reactor.
The invention was reduced-to-practice utilizing the embodiment system of
The invention was reduced-to-practice and considered in the fabrication of integrated circuitry in semiconductor processing. However, porous oxides have other uses beyond integrated circuitry fabrication, with the invention not being so limited. By way of example only, exemplary uses for the technology would be to insulate sidewalls of deep structures, or steep sidewalls and steep steps, or in forming very low k insulator layers as well as conductive layers, in integrated circuitry fabrication. Further, porous oxides formed in accordance with the invention may have a myriad of other uses, whether existing or yet-to-be developed, for example as anti-reflective coatings in semiconductor processing or on display screens; as coatings in photolithography; as mechanical, chemical or chemical/mechanical fluid filters; as catalyst support beds, etc.
In compliance with the statute, the invention has been described in language more or less specific as to structural and methodical features. It is to be understood, however, that the invention is not limited to the specific features shown and described, since the means herein disclosed comprise preferred forms of putting the invention into effect. The invention is, therefore, claimed in any of its forms or modifications within the proper scope of the appended claims appropriately interpreted in accordance with the doctrine of equivalents. For example and by way of example only, the invention does not preclude and contemplates combination of the claimed atomic layer depositing with other deposition methods before or after the claimed atomic layer depositing in forming porous oxide on the substrate.
| Number | Date | Country | |
|---|---|---|---|
| Parent | 10733201 | Dec 2003 | US |
| Child | 11491383 | Jul 2006 | US |