This application is a National Phase of PCT Patent Application No. PCT/CN2020/106817 having International filing date of Aug. 4, 2020, which claims the benefit of priority of Chinese Patent Application No. 202010653155.0 filed on Jul. 8, 2020. The contents of the above applications are all incorporated by reference as if fully set forth herein in their entirety.
The present disclosure relates to the field of display technologies, and more particularly, relates to a display panel and a display device.
Conventionally, a substrate of micro light-emitting diode (micro-LED) display panels is double layers of yellow polyimide. However, when the micro-LED display panels are manufactured, the double layers of yellow polyimide may be curled at high temperatures. Therefore, warpage of thin-film transistors may occur, resulting in warpage of the micro-LED display panels. Furthermore, the polyimide in a lower layer may be carbonized when laser is emitted on a glass. Conclusively, in conventional manufacturing processes, warpage may occur on the micro-LED display panels, and yellow polyimide may be curled and carbonized.
As a result, in conventional micro-LED display panels, yellow polyimide may be curled, resulting in warpage of the micro-LED display panels.
An embodiment of the present disclosure provides a display panel and a display device to solve following technical problems: in conventional micro-LED display panels, yellow polyimide may be curled, resulting in warpage of the micro-LED display panels.
To solve the above problems, technical solutions provided by the present disclosure are described below.
An embodiment of the present disclosure provides a display panel, including:
In some embodiments, the material of the first flexible layer includes yellow polyimide, and the material of the second flexible layer includes colorless polyimide.
In some embodiments, the material of the first flexible layer includes colorless polyimide, and the material of the second flexible layer includes yellow polyimide.
In some embodiments, a thickness of the first flexible layer is greater than or equal to a thickness of the second flexible layer.
In some embodiments, a material of the sacrificial layer includes one of silicon oxide, silicon nitride, amorphous silicon, or indium tin oxide.
In some embodiments, a thickness range of the sacrificial layer is one-tenth to one-fifth of a thickness of the first flexible layer.
In some embodiments, a barrier layer is disposed between the sacrificial layer and the first flexible layer.
In some embodiments, a thickness range of the barrier layer is one-tenth to one-fifth of a thickness of the first flexible layer.
In some embodiments, a material of the barrier layer includes silicon dioxide.
In some embodiments, a material of the first block layer includes at least one of silicon oxide or silicon nitride.
Furthermore, an embodiment of the present disclosure provides a display device, including a display panel and a cover plate, wherein the display panel includes:
In some embodiments, the small-sized LED chip includes a micro light-emitting diode (micro-LED chip) or a mini light-emitting diode (mini-LED) chip.
In some embodiments, the material of the first flexible layer includes yellow polyimide, and the material of the second flexible layer includes colorless polyimide.
In some embodiments, the material of the first flexible layer includes colorless polyimide, and the material of the second flexible layer includes yellow polyimide.
In some embodiments, a thickness of the first flexible layer is greater than or equal to a thickness of the second flexible layer.
In some embodiments, a material of the sacrificial layer includes one of silicon oxide, silicon nitride, amorphous silicon, or indium tin oxide.
In some embodiments, a thickness range of the sacrificial layer is one-tenth to one-fifth of a thickness of the first flexible layer.
In some embodiments, a barrier layer is disposed between the sacrificial layer and the first flexible layer.
In some embodiments, a thickness range of the barrier layer is one-tenth to one-fifth of a thickness of the first flexible layer.
In some embodiments, a material of the barrier layer includes silicon dioxide.
Regarding the beneficial effects: an embodiment of the present disclosure provides a display panel and a display device. The display panel includes a sacrificial layer, a first flexible layer, a first block layer, a second flexible layer, a second block layer, and a driving circuit layer. The first flexible layer is disposed on the sacrificial layer, the first block layer is disposed on the first flexible layer, the second flexible layer is disposed on the first block layer, the second block layer is disposed on the second flexible layer, the driving circuit layer is disposed on the second block layer, and a small-sized LED chip is disposed on the driving circuit layer. A material of the first flexible layer and a material of the second flexible layer are different, and a direction of an internal stress of the first flexible layer is opposite to a direction of an internal stress of the second flexible layer. Therefore, when the display panel is manufactured, the internal stress of the first flexible layer and the internal stress of the second flexible layer eliminate each other, so that the first flexible layer and the second flexible layer will not be curled, and warpage will not occur on the display panel. In addition, due to the sacrificial layer, the first flexible layer is prevented from being carbonized. As a result, a following technical problem is solved: in conventional micro-LED display panels, yellow polyimide may be curled, resulting in warpage of the micro-LED display panels.
The present disclosure provides a display panel and a display device. Embodiments are further described below in detail with reference to accompanying drawings to make objectives, technical solutions, and effects of the present disclosure clearer and more precise. It should be noted that described embodiments are merely used to construct the present disclosure and are not intended to limit the present disclosure.
An aim of an embodiment of the present disclosure is to solve a following technical problem: in conventional micro-LED display panels, yellow polyimide may be curled, resulting in warpage of the micro-LED display panels.
As shown in
As shown in
An embodiment of the present disclosure provides a display panel, including a sacrificial layer, a first flexible layer, a first block layer, a second flexible layer, a second block layer, and a driving circuit layer. The first flexible layer is disposed on the sacrificial layer, the first block layer is disposed on the first flexible layer, the second flexible layer is disposed on the first block layer, the second block layer is disposed on the second flexible layer, the driving circuit layer is disposed on the second block layer, and a small-sized LED chip is disposed on the driving circuit layer. A material of the first flexible layer and a material of the second flexible layer are different, and a direction of an internal stress of the first flexible layer is opposite to a direction of an internal stress of the second flexible layer. Therefore, when the display panel is manufactured, the internal stress of the first flexible layer and the internal stress of the second flexible layer eliminate each other, so that the first flexible layer and the second flexible layer will not be curled, and warpage will not occur on the display panel. In addition, due to the sacrificial layer, the first flexible layer is prevented from being carbonized. As a result, a following technical problem is solved: in conventional micro-LED display panels, yellow polyimide may be curled, resulting in warpage of the micro-LED display panels.
In one embodiment, the material of the first flexible layer is yellow polyimide, and the material of the second flexible layer is colorless polyimide. In conventional micro-LED display panels, the first flexible layer and the second flexible layer are made of yellow polyimide, leading to warpage of the micro-LED display panels. In the present embodiment, a direction of an internal stress of colorless polyimide is opposite to a direction of an internal stress of yellow polyimide. For example, as shown in
In one embodiment, the material of the first flexible layer is colorless polyimide, and the material of the second flexible layer is yellow polyimide. Specifically, to prevent warpage from occurring on the first flexible layer and the second flexible layer, which curls the first flexible layer and the second flexible layer, the first flexible layer may be colorless polyimide, and the second flexible layer may be yellow polyimide. As such, the internal stress of the first flexible layer and the internal stress of the second flexible layer may eliminate each other, thereby preventing warpage from occurring on the display panel.
In one embodiment, the first flexible includes a first area and a second area, a material of the first area is colorless polyimide, and a material of the second area is yellow polyimide. The second flexible layer includes a third area and a fourth area, a projection of the third area overlaps with a projection of the first area on the first block layer, and a projection of the fourth area overlaps with a projection of the second area on the first block area. A material of the third area is yellow polyimide, and a material of the fourth area is colorless polyimide. Specifically, as long as flatness and flexibility of the first flexible layer and the second flexible, and capability to block moisture and oxygen of the blocking layer are not affected, the first flexible layer may simultaneously include colorless polyimide and yellow polyimide, and the second flexible layer may correspondingly include colorless polyimide and yellow polyimide. Therefore, the internal stress of the first flexible layer and the internal stress of the second flexible layer may eliminate each other. In the present embodiment, an arrangement method of the material of the first flexible layer and an arrangement method of the material of the second flexible layer are not limited. Both the first flexible layer and the second flexible layer may include colorless polyimide and yellow polyimide which are alternately disposed.
In one embodiment, a thickness of the first flexible layer is greater than or equal to a thickness of the second flexible layer. When deciding on the thickness of the first flexible layer and the thickness of the second flexible layer, the thickness of the first flexible layer may be greater than or equal to the thickness of the second flexible layer. Given that the first flexible layer is disposed under the second flexible layer, the thickness of the first flexible layer may be greater than the thickness of the second flexible layer, thereby preventing the first block layer from being exposed when the first flexible is damaged. Moreover, flexibility of the display panel may be improved due to the first flexible layer. In addition, given that the direction of the internal stress of the first flexible layer and the direction of the internal stress of the second flexible layer are opposite, the thickness of the first flexible layer and the thickness of the second flexible layer may be the same. Therefore, the internal stress of the first flexible layer and the internal stress of the second flexible layer may also be the same and may eliminate each other. In actual processes, considering internal stresses of other layers, the thickness of the first flexible layer and the thickness of the second flexible layer may also be different. For example, the thickness of the first flexible layer is greater than the thickness of the second flexible layer, or the thickness of the first flexible layer is less than the thickness of the second flexible layer. As such, internal stresses of the entire display panel may be eliminated and warpage will not occur on the display panel.
In one embodiment, a material of the sacrificial layer includes one of silicon oxide, silicon nitride, amorphous silicon, or indium tin oxide. When the glass is stripped off by laser, the first flexible layer may be damaged by laser. Therefore, the sacrificial layer, including silicon oxide, silicon nitride, amorphous silicon, or indium tin oxide, may be disposed under the first flexible layer, thereby protecting the first flexible layer when the glass is stripped off by laser. As a result, the first flexible layer may be prevented from being curled or carbonized. Although the sacrificial layer may be damaged when the glass is stripped off by laser, the display panel can work normally because the damaged sacrificial layer will not affect the display panel. Furthermore, if the sacrificial layer is not damaged, the sacrificial layer can block moisture and oxygen because it is made of an inorganic material. Therefore, capability to block moisture and oxygen of the display panel is improved.
In one embodiment, the material of the sacrificial layer includes an organic material. To prevent the sacrificial layer from affecting the display panel as much as possible, the sacrificial layer may be made of an organic material.
In one embodiment, a thickness range of the sacrificial layer is one-tenth to one-fifth of the thickness of the first flexible layer. Considering that the sacrificial layer may affect a thickness of the display panel, the sacrificial layer may be designed to be relatively thin. For example, the thickness of the sacrificial layer is one-eighth of the thickness of the first flexible layer. Therefore, the sacrificial layer can be stripped off as much as possible when the glass is stripped off by laser, so that it will not be retained on the display panel. The sacrificial layer is thick enough to protect the first flexible layer, thereby preventing the first flexible layer from being damaged.
In on embodiment, as shown in
In one embodiment, a thickness range of the barrier layer is one-tenth to one-fifth of the thickness of the first flexible layer. The barrier layer may be relatively thin to prevent the display panel from being overly thick. For example, the thickness of the barrier layer is one-tenth of the thickness of the first flexible layer, thereby protecting the first flexible layer. Furthermore, because the barrier layer is relatively thin, the total thickness of the display panel is slightly affected.
In one embodiment, a material of the barrier layer includes at least one of silicon dioxide or silicon nitride. By using silicon dioxide to form the barrier layer, not only can the first flexible layer be protected by the silicon nitride, but also capability to prevent moisture and oxygen of the display panel can be improved due to the silicon nitride.
In one embodiment, a material of the first block layer includes at least one of silicon oxide or silicon nitride. By using silicon oxide, silicon nitride, or a stacked layer thereof to form the first block layer, moisture and oxygen can be blocked.
In one embodiment, a material of the second block layer includes at least one of silicon oxide or silicon nitride. By using silicon oxide, silicon nitride, or a stacked layer thereof to form the second block layer, moisture and oxygen can be blocked. When a structure including the first flexible layer, the first block layer, the second flexible layer, and the second block is used to block moisture and oxygen, the first block layer and the second block layer are made of an inorganic material, and the material of the first block layer and the material of the second block layer may be the same or different. Therefore, moisture and oxygen can be blocked by the first block layer, the second block layer, and the second flexible layer. In addition, flexibility of the display panel can be improved due to the first flexible layer and the second flexible layer, and bendability of the display panel can be improved as well.
In one embodiment, as shown in
In one embodiment, a recess is defined on the first flexible layer. Apart from the above-mentioned method (an internal stress of the first flexible layer and an internal stress of the second flexible layer eliminate each other), defining the recess on the first flexible layer to reduce the internal stress of the first flexible layer may also prevent warpage from occurring on the display panel due to the internal stress of the flexible layer.
In one embodiment, a recess is defined on the second flexible layer. Apart from the above-mentioned method (an internal stress of the first flexible layer and an internal stress of the second flexible layer eliminate each other), defining the recess on the second flexible layer to reduce the internal stress of the second flexible layer may also prevent warpage from occurring on the display panel due to the internal stress of the flexible layer.
In one embodiment, both the first flexible layer and the second flexible layer are provided with a recess. By defining the recesses on the first flexible layer and the second flexible layer, the internal stress of the first flexible layer and the internal stress of the second flexible layer can be reduced. Furthermore, by allowing the internal stress of first flexible layer and the internal stress of the second flexible layer to eliminate each other, warpage can be prevented from occurring on the display panel.
In one embodiment, the first flexible layer is provided with a first recess, and the second flexible layer is provided with a second recess. A material of the first flexible layer is yellow polyimide, and a material of the second flexible layer is colorless polyimide. The first recess is filled with colorless polyimide, and the second recess is filled with yellow polyimide. Specifically, in the present embodiment, the recesses are defined to reduce the internal stress of the first flexible layer and the internal stress of the second flexible layer. Meanwhile, colorless polyimide is filled in yellow polyimide of the first flexible layer, and yellow polyimide is filled in colorless polyimide of the second flexible layer. Therefore, the internal stress of the first flexible layer and the internal stress of the second flexible layer can be in part or even completely eliminated by themselves. Furthermore, the direction of the internal stress of the first flexible layer and the direction of the internal stress of the second flexible layer are opposite, so that the internal stress of the first flexible layer and the internal stress of the second flexible layer can eliminate each other, thereby preventing warpage from occurring on the display panel.
In one embodiment, as shown in
As shown in
An embodiment of the present disclosure provides a display device, including a display panel and a cover plate. The display panel includes a sacrificial layer, a first flexible layer, a first block layer, a second flexible layer, a second block layer, and a driving circuit layer. The first flexible layer is disposed on the sacrificial layer, the first block layer is disposed on the first flexible layer, the second flexible layer is disposed on the first block layer, the second block layer is disposed on the second flexible layer, the driving circuit layer is disposed on the second block layer, and a small-sized LED chip is disposed on the driving circuit layer. A material of the first flexible layer and a material of the second flexible layer are different, and a direction of an internal stress of the first flexible layer is opposite to a direction of an internal stress of the second flexible layer. Therefore, when the display panel is manufactured, the internal stress of the first flexible layer and the internal stress of the second flexible layer eliminate each other, so that the first flexible layer and the second flexible layer will not be curled, and warpage will not occur on the display panel. In addition, due to the sacrificial layer, the first flexible layer is prevented from being carbonized. As a result, a following technical problem is solved: in conventional micro-LED display panels, yellow polyimide may be curled, resulting in warpage of the micro-LED display panels.
In one embodiment, the small-sized LED chip includes a micro-LED chip or a mini-LED chip.
In one embodiment, the material of the first flexible layer includes yellow polyimide, and the material of the second flexible layer includes colorless polyimide.
In one embodiment, the material of the first flexible layer includes colorless polyimide, and the material of the second flexible layer includes yellow polyimide.
In one embodiment, a thickness of the first flexible layer is greater than or equal to a thickness of the second flexible layer.
In one embodiment, a material of the sacrificial layer includes one of silicon oxide, silicon nitride, amorphous silicon, or indium tin oxide.
In one embodiment, a thickness range of the sacrificial layer is one-tenth to one-fifth of a thickness of the first flexible layer.
In one embodiment, a barrier layer is disposed between the sacrificial layer and the first flexible layer.
In one embodiment, a thickness range of the barrier layer is one-tenth to one-fifth of a thickness of the first flexible layer.
In one embodiment, a material of the barrier layer includes silicon dioxide.
An embodiment of the present disclosure provides a method of manufacturing a display panel, including the following steps:
A display panel and a manufacturing method thereof are provided. By disposing a sacrificial layer under a first flexible layer, the first flexible layer can be protected by the sacrificial layer when a glass substrate is stripped off by laser. Only the sacrificial layer will be damaged by laser, or will not even be damaged. Furthermore, a material of the first flexible layer and a material of the second flexible layer are different, and a direction of an internal stress of the first flexible layer is opposite to a direction of an internal stress of the second flexible layer. Therefore, the internal stress of the first flexible layer and the internal stress of the second flexible layer can eliminate each other. As a result, the first flexible layer and the second flexible layer will not be curled, so that warpage will not occur on the display panel. As such, a following technical problem is solved: in conventional micro-LED display panels, yellow polyimide may be curled, resulting in warpage of the micro-LED display panels.
According to the above embodiments:
In summary, many changes and modifications to the described embodiment can be carried out by those skilled in the art, and all such changes and modifications are intended to be included within the scope of the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
202010653155.0 | Jul 2020 | CN | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/CN2020/106817 | 8/4/2020 | WO |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2022/007076 | 1/13/2022 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
20140145587 | Yoon | May 2014 | A1 |
20150028362 | Chan et al. | Jan 2015 | A1 |
20160079320 | Kim et al. | Mar 2016 | A1 |
20200006703 | Zhang | Jan 2020 | A1 |
20200220092 | Liu | Jul 2020 | A1 |
20210184181 | Ding | Jun 2021 | A1 |
20210234129 | Zhang | Jul 2021 | A1 |
20210376024 | Zheng | Dec 2021 | A1 |
Number | Date | Country |
---|---|---|
104505467 | Apr 2015 | CN |
107507927 | Dec 2017 | CN |
109192878 | Jan 2019 | CN |
109638178 | Apr 2019 | CN |
110391294 | Oct 2019 | CN |
110676292 | Jan 2020 | CN |
111276052 | Feb 2020 | CN |
111276052 | Jun 2020 | CN |
Number | Date | Country | |
---|---|---|---|
20230107568 A1 | Apr 2023 | US |