The present application is a reissue application of U.S. Pat. No. 8,178,971; the entire contents of which are incorporated herein by reference.
This application is based upon and claims the benefit of priority from Japanese patent application No. 2008-056842, filed on Mar. 6, 2008, the disclosure of which is incorporated herein in its entirety by reference.
1. Field of the Invention
This invention relates to a semiconductor device and, in particular, relates to a semiconductor device improved in strength of a bump array to which thermal stress is particularly applied among bumps that serve as external terminals of the semiconductor device, and further relates to a method of manufacturing such a semiconductor device.
2. Description of the Related Art
Semiconductor devices are widely known having a structure in which a semiconductor chip is mounted on one surface of a wiring substrate and bumps are arranged on the other surface thereof. When a semiconductor device having such a structure is used while being disposed on a mounting board, there are instances where thermal stress is applied to bumps due to a difference in thermal expansion coefficient between a wiring substrate and the mounting board to cause the bumps to fracture, thus leading to the occurrence of connection failure.
Particularly, in a semiconductor device in which a semiconductor chip is mounted so as to be offset or shifted from the center of a wiring substrate for the purpose of ensuring a space for wire bonding, greater thermal stress is applied to a bump array located at a farther position from the center of the wiring substrate in the chip shift direction due to asymmetry of the structure of the device. This will be explained for a BGA (ball grid array) semiconductor device mounted with a plurality of chips, which is illustrated in
In the mounting temperature cycle evaluation of a semiconductor device, fracture of bumps such as solder balls occurs due to the influence of stress generated by a difference in thermal expansion coefficient (α) between a wiring substrate 2 and chips 6 forming the semiconductor device or a difference in a between the semiconductor device and a non-illustrated mounting board. This fracture often occurs mainly at bumps 5 disposed at four corners or bumps 5 disposed under chip corners, which are most subjected to stress among all bumps 5 in the generally grid-shaped bump arrangement of the semiconductor device.
More specifically, in the chip shift direction (on the side A in
As shown in
On the other hand, as shown in
These prior art structures are each considered to have some effect against the occurrence of bump fracture at the four corners of the generally grid-shaped bump arrangement, but the effect is not sufficient. This is because it is not necessarily only at the four corners of the semiconductor device where the stress tends to concentrate and cause bump fracture.
Japanese Unexamined Patent Application Publication (JP-A) No. 2005-183934 (Patent Document 3) discloses a multi-chip semiconductor device in which upper and lower chips are bump-connected to each other and the upper chip is disposed so as to be shifted relative to the lower chip, wherein the center of gravity of the upper chip is set to fall within a connecting bump region between the upper and lower chips, thereby improving the connection between the upper and lower chips. However, even if the bump connection between the upper and lower chips in the semiconductor device can be improved, no teaching is given about a measure for improving the bump connection between the semiconductor device and a mounting board.
As another known example of strengthening the bump connection, Japanese Unexamined Patent Application Publication (JP-A) No. 2000-138447 (Patent Document 4) discloses a structure in which lands on the mounting board side each have a concave-convex shape. On the other hand, Japanese Unexamined Patent Application Publication (JP-A) No. 2004-079559 (Patent Document 5) discloses a technique of shifting bump arrays by a half pitch to narrow bump intervals, thereby achieving a high-density bump arrangement.
Japanese Unexamined Patent Application Publication (JP-A) No. Hei 10-012620 (Patent Document 6) discloses a structure in which large-diameter bumps or dummy bumps are disposed as auxiliary bumps at the outer peripheral portions of a bump arrangement.
However, any of the above related art technologies cannot be said to be a measure against fracture of specific bumps caused by biased stress concentration on those bumps which is generated by disposing a semiconductor chip so as to be shifted in one direction from the center of a wiring substrate.
The present invention provides a semiconductor device with an improved bump structure of a wiring substrate, wherein a semiconductor chip is mounted so as to be shifted from the center of the wiring substrate.
According to one aspect of one embodiment, a ball grid array (BGA) semiconductor device comprises a wiring substrate, a semiconductor chip disposed on one surface side of the wiring substrate, and a bump arrangement as external terminals disposed on a surface side, opposite to the one surface side, of the wiring substrate. The semiconductor chip is mounted so that a center of the semiconductor chip is shifted from a center of the semiconductor device by one pitch or more of the bump arrangement, and the bump arrangement has a reinforcing structure for a bump array located at a position farthest from the center of the semiconductor device in a shift direction of the semiconductor chip.
Preferably, the reinforcing structure is a structure in which dummy bumps are formed on an outer side of the bump array located at the position farthest from the center of the semiconductor device in the shift direction of the semiconductor chip.
Alternatively, the reinforcing structure may be a structure in which a center of the bump arrangement is shifted from the center of the semiconductor device by one pitch or more of the bump arrangement in the shift direction of the semiconductor chip.
The reinforcing structure may be a structure in which lands of the wiring substrate, fixed with the bump array located at the position farthest from the center of the semiconductor device in the shift direction of the semiconductor chip, each have a concave-convex shape.
Alternatively, the reinforcing structure may be a structure in which bumps of the bump array, located at the position farthest from the center of the semiconductor device in the shift direction of the semiconductor chip, are formed to be larger in size than bumps of bump arrays at other positions.
In another embodiment, a ball grid array (BGA) semiconductor device comprises a wiring substrate, a plurality of semiconductor chips disposed on one surface side of the wiring substrate, and a bump arrangement as external terminals disposed on a surface side, opposite to the one surface side, of the wiring substrate; wherein at least one of the plurality of semiconductor chips is mounted so that a center of the at least one of the plurality of semiconductor chips is shifted from a center of the semiconductor device by one pitch or more of the bump arrangement, the bump arrangement has a reinforcing structure for a bump array located at a position farthest from the center of the semiconductor device in a shift direction of the at least one of the plurality of semiconductor chips, and the plurality of semiconductor chips have a stacked structure in which the semiconductor chips are mounted so as to be shifted farther from the center of the semiconductor device as the semiconductor chips are located farther from the wiring substrate in a stacking direction.
In a further embodiment, there is provided a method of manufacturing ball grid array (BGA) semiconductor devices each comprising a wiring substrate, a plurality of semiconductor chips disposed on one surface side of the wiring substrate, and a bump arrangement as external terminals disposed on a surface side, opposite to the one surface side, of the wiring substrate. The method comprises the steps of: preparing a wiring base substrate having a plurality of wiring substrate regions arranged in a matrix; and forming a chip-mounted wiring base substrate having a semiconductor chip on one surface side of each of the wiring substrate regions of the wiring base substrate, the semiconductor chip disposed so as to be shifted in one direction with respect to a position which is to be a center of a semiconductor device. The method further comprises forming a multichip-mounted wiring base substrate by stacking another semiconductor chip so as to be shifted in the one direction with respect to the semiconductor chip in each of the wiring substrate regions of the chip-mounted wiring base substrate; forming a sealed wiring base substrate by covering entirely the semiconductor chips of the multichip-mounted wiring base substrate with a sealing resin; forming a bump-mounted wiring base substrate having a bump arrangement on a surface side, opposite to the one surface side where the semiconductor chips are stacked, of each of the wiring substrate regions of the sealed wiring base substrate, the bump arrangement having a reinforcing structure for a bump array located at a position farthest in the one direction from the position which is to be the center of the semiconductor device; and dicing the bump-mounted wiring base substrate into pieces for the wiring substrate regions, respectively, to provide the semiconductor devices.
According to this invention, in a semiconductor device having a structure in which a semiconductor chip is largely shifted to one side, a bump arrangement has a reinforcing structure for a bump array located at a position farthest from the center of the semiconductor device in a shift direction of the semiconductor chip and, therefore, it is possible to relax stress concentration on specific bumps or strengthen those specific bumps.
In an embodiment, since a bump arrangement has a reinforcing structure for a bump array located at a position farthest from the center of a semiconductor device in a shift direction of a semiconductor chip, it is possible to relax stress concentration on specific bumps or strengthen those specific bumps.
The above features and advantages of the present invention will be more apparent from the following description of certain preferred embodiments taken in conjunction with the accompanying drawings, in which:
Embodiments of this invention will be described with reference to the drawings.
The semiconductor device, generally denoted by numeral 1, of the first embodiment comprises a generally square wiring substrate 2. The wiring substrate 2 is, for example, a glass epoxy substrate with a thickness of 0.25 mm and is formed with predetermined wiring patterns. A plurality of connection pads 3 are formed on one surface of the wiring substrate 2. Further, a plurality of lands 4 are formed on the other surface of the wiring substrate 2. The connection pads 3 and the corresponding lands 4 are electrically connected together by the wiring patterns of the wiring substrate 2. Further, bumps 5 such as, for example, solder balls that respectively serve as external terminals are mounted on the lands 4, respectively.
In
On the one surface of the wiring substrate 2, a plurality of semiconductor chips 6 are fixedly mounted in a stacked manner through an insulating adhesive such as, for example, a DAF (die attach film) 7. For the purpose of ensuring a space for wires 9 that connect the chips 6 and the wiring substrate 2 to each other, there is one or more chips 6 disposed so that the center or centers thereof are largely shifted (shifted by one pitch or more of the bump arrangement) in one direction (to the side A in
The electrode pads 8 of the semiconductor chips 6 are electrically connected to the corresponding connection pads 3 of the wiring substrate 2 through the conductive wires 9, respectively, each made of a conductive material such as, for example, Au or Cu.
Further, a sealing body 10 is formed over the one surface of the wiring substrate 2 so as to cover the semiconductor chips 6 and the wires 9. The sealing body 10 is made of a thermosetting resin such as, for example, an epoxy resin.
As described above, the bumps 5 are mounted on the lands 4 formed on the other surface of the wiring substrate 2 whose one surface is covered with the sealing body 10. As also described above, the bumps 5 are arranged as the external terminals in the generally grid pattern at the predetermined interval as shown in
As shown in
The relationship among the wiring substrate 2, the semiconductor chips 6, and the bump arrangement in this embodiment will be further described. In the grid-shaped bump arrangement, the bumps 5 are arranged at rectangular grid points, a first arrangement direction is substantially parallel to a first side of the generally square wiring substrate 2, and a second arrangement direction perpendicular to the first arrangement direction is substantially parallel to a second side, perpendicular to the first side, of the wiring substrate 2. Each semiconductor chip 6 has a substantially rectangular shape and is mounted with its mutually perpendicular sides arranged parallel to the first and second sides of the wiring substrate 2, respectively.
Referring now to
A wiring base substrate for use in manufacturing the semiconductor devices each according to the first embodiment is a substrate made of a glass epoxy material and has a plurality of product forming regions. The product forming regions are arranged in a matrix and dicing lines are formed between the respective product forming regions. Each product forming region defined by the dicing lines will serve as a wiring substrate 2 of each semiconductor device. Each product forming region has the same structure as that of the wiring substrate 2 of the semiconductor device illustrated in
Then, the wiring base substrate is subjected to a die bonding process where, as shown in
Then, the wiring base substrate having been subjected to the die bonding process is subjected to a wire bonding process where, as shown in
In the case of a multichip structure, the die bonding process and the wire bonding process are carried out a plurality of times so as to dispose a predetermined number of chips 6 at predetermined positions and to establish wire connection between electrode pads 8 on the predetermined chip 6 and corresponding electrode pads 8 on the predetermined chip 6 or corresponding connection pads 3 on the wiring base substrate in each product forming region. In the case of stacking three chips 6, the die bonding and the wire bonding are repeated in order of
As another manufacturing method, the die bonding process may be performed in advance for all necessary chips to thereby complete the die bonding process and then the wire bonding process may be performed collectively. In the case of this manufacturing method, it is possible to prevent the occurrence of manufacturing failure of damaging wire-bonded wires by the die bonding operation for second or subsequent chips and to shorten the apparatus setting time by continuously performing the die bonding operation and continuously performing the wire bonding operation.
Then, the wiring base substrate having been subjected to the die bonding and the wire bonding is subjected to a molding process. In the molding process, while clamping the wiring base substrate between upper and lower dies of a transfer molding apparatus (not illustrated), a molten sealing resin such as, for example, a molten thermosetting epoxy resin is filled into a cavity between the upper and lower dies and then is heat-cured, thereby forming a sealing portion collectively covering all the product forming regions as shown in
Then, the wiring base substrate formed with the sealing portion is subjected to a ball mounting process. In the ball mounting process, external terminals are formed by mounting solder balls 5 on the lands 4 arranged on the other surface side of the wiring base substrate as shown in
Then, the wiring base substrate formed with the bumps 5 is subjected to a substrate dicing process. In the substrate dicing process, as shown in
In
Referring to
In
Referring to
In
Referring to
While the several embodiments have been described above, this invention is not limited thereto, but is applicable to any types of bonding portions such as precoats by solder printing, half bumps, and flip-chip bumps.
Further, there is no limitation to the number of semiconductor chips as long as a semiconductor chip is shifted with respect to the center of a semiconductor device.
Further, in the foregoing embodiments, the reinforcement is carried out only for the outermost bump array in the chip shift direction. However, the reinforcement may also be applied to the second bump array or the second and third bump arrays from the outermost bump array and, in this case, a further lifetime improving effect for a semiconductor device is expected.
According to this invention, particularly in the case of a semiconductor device having a structure in which one or more semiconductor chips are largely shifted to one side like a MCP (multichip package), improvement in reliability of a semiconductor device itself is expected by relaxing biased stress concentration on specific bumps or strengthening those specific bumps.
Further, since this invention relates to a reinforcing structure for a portion where the stress concentrates, the required area on a bump mounting surface of a wiring substrate may remain the same as that on a conventional product and only partial improvement is sufficient for embodying this invention. Therefore, new package development with significant changes such as a change in size is not required and thus it is possible to suppress the cost such as the development cost.
Although this invention has been described in conjunction with exemplary embodiments thereof, it will be appreciated by those skilled in the art that those embodiments are provided for illustrating the invention, and should not be relied upon to construe the appended claims in a limiting sense.
Number | Date | Country | Kind |
---|---|---|---|
2008-056842 | Mar 2008 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
6444563 | Potter et al. | Sep 2002 | B1 |
6736306 | Byun et al. | May 2004 | B2 |
6781245 | Huang | Aug 2004 | B2 |
7015590 | Jeong et al. | Mar 2006 | B2 |
7145247 | Kawano et al. | Dec 2006 | B2 |
7642632 | Kang | Jan 2010 | B2 |
7683485 | Nikaido | Mar 2010 | B2 |
9018761 | Oomori | Apr 2015 | B2 |
9018774 | Lee | Apr 2015 | B2 |
9093322 | Meyer | Jul 2015 | B2 |
9111818 | Lin | Aug 2015 | B2 |
20020141171 | Bohr | Oct 2002 | A1 |
20030071284 | Kanai et al. | Apr 2003 | A1 |
20030092326 | Nishikawa et al. | May 2003 | A1 |
20040017008 | Ueda | Jan 2004 | A1 |
20040164385 | Kado et al. | Aug 2004 | A1 |
20050093153 | Liu | May 2005 | A1 |
20060170102 | Ko | Aug 2006 | A1 |
20060231949 | Park et al. | Oct 2006 | A1 |
20070013083 | Kikuchi et al. | Jan 2007 | A1 |
20070029673 | Yamaguchi | Feb 2007 | A1 |
20090206490 | Koide et al. | Aug 2009 | A1 |
20130043583 | Wu et al. | Feb 2013 | A1 |
Number | Date | Country |
---|---|---|
09-162531 | Jun 1997 | JP |
10-012620 | Jan 1998 | JP |
2000-138447 | May 2000 | JP |
2001-210749 | Aug 2001 | JP |
2004-079559 | Mar 2004 | JP |
2004111543 | Apr 2004 | JP |
2005-183934 | Jul 2005 | JP |
Number | Date | Country | |
---|---|---|---|
Parent | 12379916 | Mar 2009 | US |
Child | 14278877 | US |