The present invention relates to methods for producing optical surfaces by smoothing surface roughness using atomic layer deposition.
Surface roughness affects the performance of optical devices in that it is at least partially determinative of how light is scattered, reflected and transmitted. There are many processes used to smooth surfaces. These include chemical etching, chemical mechanical polishing (CMP), magnetorheological finishing, electrochemical micromachining, and ion beam erosion. These processes can smooth with high precision, but can also be abrasive, change the surface curvature, or damage the underlying substrate. Many smoothing processes would benefit from an alternative smoothing technique that removes roughness without negatively impacting the surface.
Atomic layer deposition (ALD) is a thin film deposition process that coats materials with atomic scale control. Gas-phase reactants are introduced to a substrate one at a time to precisely build up the material. These sequential surface reactions are self-limiting, meaning once all surface sites have reacted, the reaction effectively saturates. This allows for precise digital control of film thickness. ALD has been used to deposit many materials including numerous oxides, nitrides and sulfides. Due to the self-limiting nature of the surface reactions, films deposited by ALD are highly conformal and cover the surface with a uniform layer of material. This conformality allows ALD to act as the reverse of CMP. Rather than etching away the surface asperities, ALD can “pinch-off” surface roughness by filling in the gaps between the surface features.
Atomic layer deposition involves growing a film on a substrate by exposing its surface to alternate gaseous species (typically referred to as precursors or reactants). In contrast to chemical vapor deposition, the precursors are never present simultaneously in the reactor, but they are inserted as a series of sequential, non-overlapping pulses. In each of these pulses the precursor molecules react with the surface in a self-limiting way, so that the reaction terminates once all the reactive sites on the surface are consumed. By varying the number of cycles, it is possible to grow materials uniformly and with high precision on a host of complex and large substrates.
According to some implementations, a method of producing an optical surface (e.g., a surface of a mirror) is provided. According to a first step, a substrate is obtained having an exterior on which the optical surface is to reside, the exterior including laterally spaced-apart asperities having peaks that are spaced <1000 nm apart and affect optical performance of the produced optical surface absent a smoothing of the exterior surface. According to a second step, the exterior of the substrate is smoothed using an atomic layer deposition process to sequentially deposit a first plurality of ALD layers (e.g., Al2O3 layers) to produce an ALD film that fills spaces between the laterally spaced-apart asperities existing on the exterior surface. According to a third step, a reflective material (e.g., silver) is deposited on the smoothed exterior of the substrate that includes the ALD film surface to produce the optical surface. The smoothing resulting from depositing the ALD film on the exterior of the substrate causes the grain size of the reflective material to be reduced in comparison to the grain size that would otherwise exists without having deposited the ALD film on the exterior of the substrate. The ALD film has a thickness sufficient to cause a reduction in the grain size of the reflective material that results in a reduction in plasmon absorption in the optical surface in comparison to the plasmon absorption that would otherwise exist without having reduced the grain size of the reflective material. According to some implementations the grain size of the reflective material is caused to be in the range of 50 to 1000 nanometers.
According to some implementations, each of the laterally spaced-apart asperities of the exterior of the substrate has a peak and the ALD film has a thickness of no more than one half an average lateral distance between the peaks.
According to some implementations the power spectral density of a surface topography of the exterior of the substrate that includes the ALD film surface is determined using atomic force microscopy as a function of spatial frequency after the smoothing of the exterior of the substrate using the atomic layer deposition process. Thereafter, the determined power spectral density is compared to a predetermined target power spectral density at one or more spatial frequencies, the predetermined target power spectral density at the one or more spatial frequencies corresponding to a target roughness of the exterior of the substrate before the step of depositing the reflective material. Upon a determining that the exterior of the substrate that includes the ALD film surface has a roughness greater than the target roughness, an additional step of smoothing the exterior of the substrate (including the ALD film surface) is performed, using the atomic layer deposition process to sequentially deposit a second plurality of ALD layers onto the exterior of the substrate prior to depositing the reflective material.
According to other implementations, the producing of an optical surface may comprise a first step of obtaining a substrate having an exterior on which the optical surface is to reside, the exterior including laterally spaced-apart asperities having peaks that are spaced <1000 nm apart and affect optical performance of the produced optical surface absent a smoothing of the exterior surface. Thereafter, the exterior of the substrate is processed using an atomic layer deposition process to sequentially deposit a first plurality of ALD layers to produce a first ALD film that fills spaces between the laterally spaced-apart asperities existing on the exterior surface. This is followed by depositing one or more layers of a metal onto a surface of the first ALD film using a physical vapor deposition process to form a metal film over the surface of the first ALD film. Next, the surface of the metal film is smoothed using an atomic layer deposition process to sequentially deposit a second plurality of ALD layers to produce a second ALD film over the metal film. Subsequently, a reflective material (e.g., silver) is deposited on a surface of the second ALD film to produce the optical surface.
These and other advantages and features will become evident in view of the drawings and detailed description.
Surface roughness can affect performance of high reflectivity mirrors. The main mechanism of reflectance loss in optical devices is through optical scattering. When light interacts with a rough surface, some light will specularly reflect at the same angle as the incident photon. Other light will be diffusely reflected at non-specular angles. A surface with roughness can be described as a superposition of sinusoidal structures that will lead to diffuse scattering resulting from diffraction. Conventional techniques can smooth mirror surfaces, but can affect the mirror curvature and require additional processing steps. ALD may be able to smooth the surface roughness of a mirror without affecting its curvature. In addition, ALD can be scaled up to accommodate larger mirror substrates. Compared with other smoothing techniques, ALD is also an additive process that can improve surface roughness without being destructive.
Before now, optical mirrors were produced with little to no consideration of nanometer-sized roughness features residing on their surface. This is because the nanometer-sized features were thought to be too small to significantly affect the reflectivity of light at the mirror's surface. However, it has been discovered that in some applications nanometer-sized features at a mirror's surface can in fact negatively affect the mirror's ability to reflect light due to plasmon absorption that exists in the metal nanoparticles that make up the reflective surface. When an incident light beam strikes the metal nanoparticles it causes free electrons at the surface of the metal (e.g., silver) to oscillate. The energy expended by the incident light beam to produce the oscillating electrons results in some of the light being lost.
As will be discussed in more detail below, to properly assess a roughness of an optical surface (e.g., a mirror surface) having nanometer-sized features, traditional RMS surface roughness measurement techniques can be inadequate. For this reason, according to some implementations power spectral density analysis is in some cases used to determine when a sufficient smoothing has been obtained. Hence, rather than relying on the evaluation of distinct features at the optical surface to determine if a target roughness has been met, a statistical distribution of roughness is instead used.
In the examples that follows, the optical surfaces are regarded to be surfaces of a mirror. It is appreciated, however, that the methods and structures disclosed herein are applicable to other types of optical surfaces and are in no way limited to those associated with mirrors.
Surface plasmon absorption can affect mirror reflectivity when light interacts with features smaller than the light wavelength on some metallic surfaces. The surface plasmon absorption is most noticeable in nanostructures of metals, such as silver, that have a large number of free electrons that may oscillate when there is light incident on the surface. As noted above, the energy expended by the incident light beam to produce the oscillating electrons results in some of the light being lost. In mirrors, this adversely affects its reflectance. In regard to reflective materials, such as silver, the strength of the coupling between the light and the plasmon oscillation depends on the surface topology where larger grain sizes result in higher surface absorption of light in comparison to smaller grain sizes. For this reason, in some applications it is important to minimize the roughness of the surface on which the reflective material is deposited in order to minimize the grain size of the reflective material.
Generally, surface plasmons (electron oscillations) are excited by light incident on a metallic surface. It is a specific type of oscillation that is bound to the interface, does not radiate, and propagates. (In some microscopic treatments of reflection, other oscillations that radiate simply lead to specular reflection; this is not that type of oscillation associated with plasmons). The plasmon excitation losses energy as it propagates through electrical resistance in the metal or secondary scattering mechanisms. Excitation of surface plasmons by light only occurs under specific conditions when evanescent waves are generated, e.g., under conditions of total internal reflection or even after scattering at a rough surface. The strength of the excitation (amount of energy coupled from the light to the plasmon) depends strongly on geometry such as the surface topography and angles of incidence, though of course the dielectric constants a materials at the metal interface, and the wavelength of light are also relevant. In fact, for perfectly smooth metallic surfaces it is impossible to excite a surface plasmon in the absence of total internal reflection (for example on the backside of a prism). Detailed analysis shows that the loss is greater for large grain sizes typical of rough surfaces. Thus, reducing the grain size to create a smoother surface reduces the ability to lose energy through exciting surface plasmons.
According to some implementations, as shown in
Upon having deposited the ALD film 20 onto the exterior surface 11 of the substrate 10, a reflective material 40 is deposited on the smoothed exterior of the substrate (that includes the ALD film surface 21) to produce the optical surface 50. According to one implementation, the reflective material 40 is deposited using an e-beam physical vapor deposition process. The smoothing is carried out such that the depositing of the ALD film 20 on the exterior surface 11 of the substrate 10 causes the grain size of the reflective material 40 to be reduced in comparison to the grain size that would otherwise exists without having deposited the ALD film 20 on the exterior surface of the substrate. The ALD film 20 is produced to have a thickness sufficient to cause a reduction in the grain size of the reflective material 40 that results in a reduction in plasmon absorption in the optical surface 50 in comparison to the plasmon absorption that would otherwise exist without having applied the ALD film to the substrate surface 11. According to one implementation, the smoothing of the substrate surface 11 is carried out to cause the grain size of the reflective material 40 to be in a range of 50 to 1000 nanometers as measured using high resolution transmission microscopy.
According to some implementations the ALD layers are comprised of one of Al2O3 layers, SiO2 layers, TiO2 layers, ZrO2 layers, ZnO or SiNx. According to other implementations the ALD layers comprise two or more of Al2O3 layers, SiO2 layers, TiO2 layers, ZrO2 layers, ZnO and SiNx.
According to some implementations, the reflective material is silver, gold, aluminum, germanium or chromium.
The obtaining or making of the substrate 10 may comprise a smoothing of the exterior surface 11, which according to one example includes a chemical mechanical polishing (CMP) of surface 11.
As shown in
In the implementation of
According to some implementations power spectral density analysis is used to determine when a sufficient smoothing has been obtained before the reflective material 40 is applied to the exterior-most surface of the substrate 10. (In the examples disclosed herein, prior to depositing the reflective material 40 the exterior-most surface of the substrate 10 includes a surface of an ALD film.) In some instances, this includes determining the power spectral density of a surface topography of the exterior-most surface of the substrate using atomic force microscopy as a function of spatial frequency after the smoothing of the exterior of the substrate using the atomic layer deposition process. Thereafter, the determined power spectral density is compared to a predetermined target power spectral density at one or more spatial frequencies (see
Although only a number of examples have been disclosed herein, other alternatives, modifications, uses and/or equivalents thereof are possible. Furthermore, all possible combinations of the described examples are also covered. Thus, the scope of the present disclosure should not be limited by the particular examples disclosed herein.
This application is a continuation of U.S. patent application Ser. No. 17/733,575, filed Apr. 29, 2022, the entire contents of each of which are hereby incorporated by reference.
| Number | Date | Country | |
|---|---|---|---|
| Parent | 17733575 | Apr 2022 | US |
| Child | 19042836 | US |