Cognitive (e.g., memory) devices may contain materials that cannot be dry etched in fabrication facilities via reactive ion etching (ME) due to safety and chamber contamination concerns. Such materials can include, for example, phase change material (PCM), such as germanium-antimony-tellurium (GeSbTe), ovonic threshold switch (OTS) material including, for example, silicon germanium arsenide selenide (SiGeAsSe), and electrochemical metallization (ECM) material, such as AgGeSe. Additive patterning integrations allow capping these materials with a conductive electrode.
Physical vapor deposition (PVD) is a facile way to deposit metal/metal nitrides forming the conductive electrodes at low temperatures which are compatible with low-temperature technologies. However, PVD deposited films often damage common dielectrics (e.g., low-k dielectrics) that surround the memory materials (e.g., memory elements). Subsequent wet processing from additive patterning integration often removes the damaged dielectric, leading to unwanted recesses in the dielectric layer adjacent to the conductive electrodes. The recesses in the dielectric layer can expose sensitive memory elements to the environment, which can negatively impact device performance.
Accordingly, there is a need for techniques to form electrodes on memory materials which allows for low temperature processing while avoiding damage to surrounding dielectric layers.
According to an exemplary embodiment of the present invention, a method for manufacturing a semiconductor device includes forming a memory element in a dielectric layer. A first conductive layer is deposited on the on the dielectric layer and the memory element by atomic layer deposition, and a second conductive layer is deposited on the first conductive layer by physical vapor deposition. In the method, the first and second conductive layers are patterned into an electrode on the memory element.
According to an exemplary embodiment of the present invention, a method for manufacturing a semiconductor device includes forming a phase change material in a dielectric layer, and forming a bottom electrode under the phase change material. In the method, a conductive liner layer is deposited on the dielectric layer and the phase change material by atomic layer deposition, and a conductive layer is deposited on the conductive liner layer. The method further includes patterning the conductive liner layer and the conductive layer into a top electrode on the phase change material.
According to an exemplary embodiment of the present invention, a method for manufacturing a semiconductor device includes forming a contact in a first dielectric layer, and forming a bottom electrode on the contact. In the method, a second dielectric layer including a low-k dielectric is formed on the first dielectric layer. A memory element is formed on the bottom electrode, and is surrounded by the second dielectric layer. The method further includes depositing by atomic layer deposition a first conductive layer on the second dielectric layer and the memory element, and depositing a second conductive layer on the first conductive layer. The first and second conductive layers are patterned into a top electrode on the memory element.
These and other exemplary embodiments of the invention will be described in or become apparent from the following detailed description of exemplary embodiments, which is to be read in connection with the accompanying drawings.
Exemplary embodiments of the present invention will be described below in more detail, with reference to the accompanying drawings, of which:
Exemplary embodiments of the invention will now be discussed in further detail with regard to semiconductor devices and methods of manufacturing same and, in particular, to methods and structures to prevent recessing (e.g., gouge) in a dielectric layer surrounding a storage element, while still gaining the electrical benefits of using low-k materials for memory elements.
It is to be understood that the various layers and/or regions shown in the accompanying drawings are not drawn to scale, and that one or more layers and/or regions of a type commonly used in, for example, phase-change memory (PCM), phase-change random-access memory (PCRAM), resistive random-access memory (RRAM or ReRAM), three-dimensional (3D) RRAM, magnetic random-access memory (MRAM), fuse/anti-fuse, diode, ovonic threshold switch (OTS), bipolar junction transistor (BJT), complementary metal-oxide semiconductor (CMOS), field-effect transistor (FET), nanowire FET, nanosheet FET, fin field-effect transistor (FinFET), metal-oxide-semiconductor field-effect transistor (MOSFET) and/or other semiconductor devices may not be explicitly shown in a given drawing. This does not imply that the layers and/or regions not explicitly shown are omitted from the actual devices. In addition, certain elements may be left out of particular views for the sake of clarity and/or simplicity when explanations are not necessarily focused on the omitted elements. Moreover, the same or similar reference numbers used throughout the drawings are used to denote the same or similar features, elements, or structures, and thus, a detailed explanation of the same or similar features, elements, or structures will not be repeated for each of the drawings.
The semiconductor devices and methods for forming same in accordance with embodiments of the present invention can be employed in applications, hardware, and/or electronic systems. Suitable hardware and systems for implementing embodiments of the invention may include, but are not limited to, personal computers, communication networks, electronic commerce systems, portable communications devices (e.g., cell and smart phones), solid-state media storage devices, functional circuitry, etc. Systems and hardware incorporating the semiconductor devices are contemplated embodiments of the invention. Given the teachings of embodiments of the invention provided herein, one of ordinary skill in the art will be able to contemplate other implementations and applications of embodiments of the invention.
The embodiments of the present invention can be used in connection with semiconductor devices that may require, for example, PCM, PCRAM, RRAM, 3D RRAM, MRAM, fuses/anti-fuses, diodes, OTSs, BJTs, FETs, CMOSs, MOSFETs, nanowire FETs, nanosheet FETs and/or FinFETs. By way of non-limiting example, the semiconductor devices can include, but are not limited to PCM, PCRAM, RRAM, 3D RRAM, MRAM, fuse/anti-fuse, diode, OTS, BJT, FET, CMOS, MOSFET, nanowire FET, nanosheet FET and FinFET devices, and/or semiconductor devices that use PCM, PCRAM, RRAM, 3D RRAM, MRAM, fuse/anti-fuse, diode, OTS, BJT, FET, CMOS, MOSFET, nanowire FET, nanosheet FET and/or FinFET technology.
As used herein, “height” refers to a vertical size of an element (e.g., a layer, trench, hole, opening, etc.) in the cross-sectional views or images measured from a bottom surface to a top surface of the element, and/or measured with respect to a surface on which the element is located. Conversely, a “depth” refers to a vertical size of an element (e.g., a layer, trench, hole, opening, etc.) in the cross-sectional views or images measured from a top surface to a bottom surface of the element.
As used herein, “lateral,” “lateral side,” “lateral surface” refers to a side surface of an element (e.g., a layer, opening, etc.), such as a left or right side surface in the drawings.
As used herein, “width” or “length” refers to a size of an element (e.g., a layer, trench, hole, opening, etc.) in the drawings measured from a side surface to an opposite surface of the element.
As used herein, terms such as “upper”, “lower”, “right”, “left”, “vertical”, “horizontal”, “top”, “bottom”, and derivatives thereof shall relate to the disclosed structures and methods, as oriented in the drawing figures. For example, as used herein, “vertical” refers to a direction perpendicular to the top surface of a layer or substrate in the cross-sectional views or images, and “horizontal” refers to a direction parallel to the top surface of a layer or substrate in the cross-sectional views or images.
As used herein, unless otherwise specified, terms such as “on”, “overlying”, “atop”, “on top”, “positioned on” or “positioned atop” mean that a first element is present on a second element, wherein intervening elements may be present between the first element and the second element. As used herein, unless otherwise specified, the term “directly” used in connection with the terms “on”, “overlying”, “atop”, “on top”, “positioned on” or “positioned atop” or the term “direct contact” mean that a first element and a second element are connected without any intervening elements, such as, for example, intermediary conducting, insulating or semiconductor layers, present between the first element and the second element.
As used herein, “low-k” refers to dielectric materials having a relative dielectric constant less than 7, and includes ultra-low-k dielectric materials.
As used herein, “high-k” refers to dielectric materials having a relative dielectric constant greater than 7.
In accordance with an embodiment of the present invention, an atomic layer deposition (ALD) film is deposited on a memory element (e.g., PCM, OTS, etc.) and a surrounding dielectric layer in which the memory element is formed. The ALD film is deposited between the dielectric layer and a subsequently deposited physical vapor deposition (PVD) film in order to protect the underlying dielectric layer from damage which can occur during patterning of the PVD film into a top electrode on the memory element. A bilayer of the PVD deposited film on the ALD deposited film is patterned into a top electrode on the memory element without damage to (e.g., unwanted recessing) of the dielectric layer. As a result of the dielectric layer remaining intact due to the protection afforded by the ALD film, the memory element is not exposed to the environment, and device degradation is prevented.
As can be understood by one of ordinary skill in the art, the dielectric layer 104 can be on a semiconductor substrate 102, with intervening layers (e.g., lower conductive lines, devices, etc.) between the dielectric layer 104 and the substrate 102. A semiconductor substrate 102 may comprise semiconductor material including, but not limited to, Si, SiGe, SiC, SiGeC or other like semiconductor. In addition, multiple layers of the semiconductor materials can be used as the semiconductor material of the substrate 102. A plurality of devices can be on the substrate 102, such as, for example, transistors, capacitors, and resistors.
A liner layer 108 comprising, for example titanium nitride, tantalum nitride or tungsten nitride is conformally formed on the sidewalls and bottom surfaces of trenches in which the landing pads 106 are formed. The landing pads 106 include, for example, tungsten, cobalt, zirconium, tantalum, titanium, aluminum, ruthenium, copper, metal carbides (e.g., tantalum carbide, titanium carbide, tantalum magnesium carbide), metal nitrides (e.g., titanium nitride), transition metal aluminides or combinations thereof deposited on the liner layers 108 using deposition techniques, including, but not necessarily limited to, PVD, chemical vapor depositions (CVD), ALD or sputtering. In accordance with an embodiment of the present invention, the landing pads 106 can be electrically connected to or form contact lines, such as, for example, wordlines, of a resulting memory cell array. The number of landing pads 106 shown in the figures is illustrative, and the embodiments of the present invention are not necessarily limited to the number of landing pads shown.
As shown in
A low-k dielectric layer 120 is formed on the dielectric layer 115 using, for example, deposition techniques, including, but not necessarily limited to, PVD, CVD, ALD or sputtering. According to an embodiment of the present invention, the low-k dielectric layer 120 includes, for example, TEOS, SiO2, SiCOH, SiLK® dielectrics, and/or porous forms of these low-k dielectric films. A thickness (e.g., vertical height) of the low-k dielectric layer 120 is in the range of about 100 nm to about 120 nm.
As can be seen in
The memory element 116 is deposited in a trench surrounded by the dielectric layers 120 and 115 and lined on side and bottom surfaces with a liner layer 118 including, for example, TaN or TiN deposited using techniques such as ALD or PVD. According to an embodiment of the present invention, a horizontal width of the bottom electrode is in the range of about 36 nm to about 56 nm, and includes, for example, TaN. A thickness of the bottom electrode is the same or substantially the same as a thickness of the dielectric layer 115, and the bottom electrode 112 is in electrical contact with the memory element 116 and a corresponding landing pad 106.
According to an embodiment of the present invention, a conductive liner layer 125 including, for example, ALD TaN, is deposited on the low-k dielectric layer 120 including the memory element 116 formed therein. The liner layer 125 can also be formed from ALD TiN or other conductive nitride, as long as the liner layer is an ALD film with low reactivity. The liner layer 125 has a thickness (e.g., vertical height) in the range of about 3 nm to about 5 nm so as to limit the liner layer 125 from contributing to a resistance of the device 100. The liner layer 125 is deposited using ALD. A conductive layer 130 is formed on the conductive liner layer 125. In accordance with an embodiment of the present invention, the conductive layer 130 includes, for example, PVD TaN or a PVD TiN/TaN bilayer, and has a thickness (e.g., vertical height) in the range of about 20 nm to about 30 nm. The conductive layer 130 is deposited using PVD. As noted herein, the liner layer 125 functions as a protective layer for the low-k dielectric layer 120 to protect the underlying low-k dielectric layer 120 from damage which can occur during patterning of the PVD conductive layer 130 on the liner layer 125 into a top electrode of the memory element 116.
According to an embodiment of the present invention, the hardmask layer 135 includes, for example, SiN, silicon boron nitride (SiBN), siliconborocarbonitride (SiBCN) and/or silicon oxycarbonitride (SiOCN) and has a thickness (e.g., vertical height) in the range of about 50 nm-about 200 nm. The hardmask layer 135 is deposited by one or more deposition techniques, including, but not necessarily limited to, PVD, CVD, ALD or sputtering.
The OPL 140 comprises, but is not necessarily limited to, an organic polymer including C, H, and N. In an embodiment, the OPL material can be free of silicon (Si). According to an embodiment, the OPL material can be free of Si and fluorine (F). As defined herein, a material is free of an atomic element when the level of the atomic element in the material is at or below a trace level detectable with analytic methods available in the art. Non-limiting examples of the OPL material include JSR HM8006, JSR HM8014, AZ UM10M2, Shin Etsu ODL 102, or other similar commercially available materials from such vendors as JSR, TOK, Sumitomo, Rohm & Haas, etc. The OPL 140 can be deposited, for example, by spin coating, to a thickness of about 100 nm-about 200 nm. The SiARC layer 145 is deposited on the OPL 140.
A resist 150 is formed on the SiARC layer 145 over the memory element 116. The resist has a thickness in the range of about 80 nm to about 110 nm, and horizontal width which corresponds to that of the bottom electrode 112 and the memory element 116.
Subsequent downstream processing can be performed to form a contact to the top electrode structure comprising the layers 130 and 125. As can be understood, although one memory element is illustrated, the embodiments of the present invention are not necessarily limited thereto, and more than one memory element 116 and corresponding electrode bilayer structure can be formed by the techniques and processes according to embodiments of the present invention.
In addition to the metallization level including landing pads 206 in dielectric layer 204, device 200 further illustrates another metallization level below the landing pads 206 including a landing pad 205 (e.g., contact) formed on a liner 207 in a trench in a dielectric layer 203 including the same or similar materials as the dielectric layer 204. The landing pad 205 and liner 207 can include the same or similar materials as those of the landing pad and liner 206 and 208.
Although illustrative embodiments of the present invention have been described herein with reference to the accompanying drawings, it is to be understood that the invention is not limited to those precise embodiments, and that various other changes and modifications may be made by one skilled in the art without departing from the scope or spirit of the invention.