The present invention is related to an apparatus and method for increasing the reliability and performance of an electronic device enclosed within a flip-chip package.
Commonly available electronic devices exist in the form of a thin sheet of semiconductor material, or die, with electronic circuitry disposed thereon by way of various photolithographic processes. To protect the circuitry from damage, the die is often enclosed in a package designed to facilitate the attachment of the electronic device to a printed circuit board.
Improvements in electrical signal characteristics, as well as increased flexibility in power consumption and die size, have been realized through the use of packages such as the “flip-chip” or “controlled collapsed chip connection” (C4) package which typically integrates a lid made of aluminum or other thermally conductive material that serves as a heatsink (also known as a “heat spreader”), and a substrate made of an organic compound that incorporates electrically conductive materials used to provide electrical connections between the die and a circuitboard to which the package is attached.
A drawback to disposing sealant 214 in an unbroken line is that a complete seal is formed between the lid and substrate 212 that can prevent differences in pressure between the interior of package 200 and the ambient air surrounding the exterior of package 200 from being equalized. This becomes especially significant where substrate 212 is made of organic or other material that is susceptible to absorbing moisture from the ambient air surrounding package 200, and then releasing moisture into the interior of package 200. During thermal testing or normal use, when the temperature of die 230 increases, moisture present within the interior of package 200 become steam, causing an increase in pressure within package 200, and tending to push the lid and substrate 212 apart. As can best be appreciated by reviewing
Still another drawback arising from the presence of moisture being converted to steam under pressure, is that steam could be forced between either thermal attach 116 and die 130, or between thermal attach 116 and lid 110. This reduces the contact between thermal attach 116 and either lid 110 or die 130, and thereby also reduces the effectiveness of thermal attach 116 in conducting heat away from die 130 and towards lid 110. Furthermore, depending on the composition of thermal attach 116, steam may also penetrate the thermal attach material, itself, thereby forming gaps within thermal attach 116 which would block the transmission of heat from die 130 through thermal attach 116.
In addition to undesirable effects resulting from a buildup of pressure and the presence of moisture, there are drawbacks arising from the use of an unbroken line of sealant as a result of differences in the rates of expansion and contraction between the lid, the substrate and the die. Referring once again to
The objects, features, and advantages of the present invention will be apparent to one skilled in the art in view of the following detailed description in which:
In the following description, for purposes of explanation, numerous details are set forth in order to provide a thorough understanding of the present invention. However, it will be apparent to one skilled in the art that these specific details are not required in order to practice the present invention.
The present invention concerns “flip-chip” or “controlled collapsed chip connection” (C4) packages for integrated circuits where an organic substrate is used. Such a package is also known as an “organic land grid array” or OLGA. Particularly, the present invention concerns the use of such packages to hold particularly large dies. However, as those skilled in the art will appreciate, the present invention is also applicable where other porous substrate materials are used, or where smaller dies are used upon which is disposed circuitry that generates considerable amounts of heat. The present invention is also applicable where the package is to be used in high heat environments.
a is a top side view similar to that of
Like sealant 214 of
Referring variously to both
Also, by allowing this release in pressure, substrate 112/312 is not caused to bow outward, thereby causing substrate 112/312 to become curved, and potentially causing cracks to form in die 130/330 in the vicinity of the corners.
Furthermore, disposing sealant 314a–d in a pattern with breaks results in the sealant forming a less rigid connection between lid 110 and substrate 112/312, thereby allowing a degree of relative movement between lid 110 and substrate 112/312. Allowing some degree of relative movement allows lid 110 and substrate 112/312 to expand and contract at different rates relative to each other in response to changes in temperature, thereby reducing the tendency for lid 110 or substrate 112/312 to bow outwardly. This in turn, serves to reduce the earlier described loss in effectiveness of thermal attach 116 and/or the earlier described cracking or delamination in die 130/330.
In one embodiment, the sealant is disposed in multiple segments, resulting in multiple breaks. In another embodiment, the sealant is disposed in a single segment, but not forming a complete loop surrounding die 330, thereby resulting in a single break. In one embodiment, the breaks comprise at least 10% of the total length of what would otherwise be a complete loop of sealant, while in another embodiment, the breaks comprise less than 10% of that length. In still another embodiment, the sealant is disposed in a pattern of small spots or dots of sealant leaving breaks between the spots of sealant, rather than segments defining breaks.
In one embodiment, the sealant is comprised of a relatively flexible material permitting substrate 312 and lid 310 to move relative to each other with a high degree of freedom. In another embodiment, the sealant is comprised of a more rigid material limiting the relative movement of substrate 312 and lid 310.
In one embodiment package 300 would be formed by first attaching die 330 to substrate 312, thereby forming physical and electrical connections between die 330 and substrate 312. The sealant would then be disposed on substrate 312 in the four segments 314a–d, where lid 310 is to be attached to substrate 312. Thermal attach 316 would then be disposed on die 330, where lid 310 is to be attached to die 330. Then lid 310 would be attached to substrate 312 (via sealant 314a–d) and die 330 (via thermal attach 316). As those skilled in the art will understand, the order in which these occur may be changed without departing from the spirit of the invention.
In one embodiment, package assembly equipment originally designed to dispose sealant in an unbroken line is modified to dispose the sealant as sealant segments 314a–d. In another embodiment, new package assembly equipment specifically designed to dispose the sealant as sealant segments 314a–d is used.
In one embodiment, substrate 312 is comprised of an organic material, and this organic material may be porous such that it is susceptible to absorbing moisture from the ambient air external to package 300. In another embodiment, substrate 312 is comprised of a non-organic material, but a material that still suffers the drawback of absorbing moisture. In one embodiment, the package and/or the die within the package is tested by applying heat to the exterior of the package by exposing the package to steam at high pressure.
In one embodiment, lid 310 has one or more vent-holes, such as vent-hole 311, formed therethrough, that could also serve to permit the release of pressure within the interior of package 300, but which may be blocked as a result of the manner in which package 300 is installed, either for testing or for normal use. In another embodiment, the lid has no vent-holes formed therethrough, and the breaks between sealant segments 314a–314d are the sole means provided for release of pressure.
In one embodiment, thermal attach 316 is a thermal grease, while in another embodiment, thermal attach 316 is a thermal adhesive.
In one embodiment, lid 310 is made of material capable of conducting heat away from die 330, such as copper or aluminum. In one embodiment, lid 310 releases the heat conducted away from die 330 to ambient air surrounding package 300. In another embodiment, lid 310 conducts the heat to other thermally conductive apparatus with which lid 310 is in contact, such as a heatsink (or heat spreader), heat pipe, or thermal electric cooler.
In one embodiment, package 300 is a ball grid array package where substrate 312 is attached to a circuitboard (not shown) by way of solderballs corresponding generally to solder balls 124 of
In one embodiment, circuitry comprising the core logic (e.g., random access memory controller, bus interface, I/O device interface, or timers) of a microcomputer system is disposed on a surface of die 330. In another embodiment, circuitry comprising a central processing unit of a microcomputer system is disposed on a surface of die 330.
a is a top side view similar to that of
The invention has been described in conjunction with the preferred embodiment. It is evident that numerous alternatives, modifications, variations and uses will be apparent to those skilled in the art in light of the foregoing description. It will be understood by those skilled in the art, that the present invention may be practiced in support of other combinations of functions in a computer system.
The example embodiments of the present invention are described in the context of ball grid array and pin grid array packages carrying a die on which is disposed electronic circuitry. However, the present invention is applicable to a variety of package types and to a variety of electronic, microelectronic and micromechanical devices. Although the present invention is described in the context of packages attached to rigid printed circuit boards that are commonly in use, the present invention is also applicable to packages being attached to sheets of flexible material or other surfaces providing electrical connections. Also, although the present invention is described in the context of packages with the sealant be disposed in a substantially rectangular pattern, the present invention is applicable to other patterns in which the sealant may disposed, regardless of whether the pattern in which the sealant is disposed is influenced by the shape of the lid and/or the substrate, or not. Indeed, the sealant may be disposed in circular or other polygonal patterns, or the sealant may be disposed as a plurality of spots rather than line segments. Furthermore, although the present invention is described in the context of packages that enclose a single die on which electronic circuitry is disposed, the present invention is applicable to packages enclosing multiple separate dies, and/or dies comprised of smaller dies.
Number | Name | Date | Kind |
---|---|---|---|
5081327 | Graham et al. | Jan 1992 | A |
6136128 | Chung | Oct 2000 | A |
6215180 | Chen et al. | Apr 2001 | B1 |
6232652 | Matsushima | May 2001 | B1 |
6410981 | Tao | Jun 2002 | B2 |
Number | Date | Country |
---|---|---|
63029555 | Jul 1986 | JP |
61256656 | Nov 1986 | JP |
63084051 | Apr 1988 | JP |
04083363 | Jul 1990 | JP |
06140523 | Oct 1992 | JP |
06232284 | Aug 1994 | JP |
20000349178 | Dec 2000 | JP |
Number | Date | Country | |
---|---|---|---|
20020084532 A1 | Jul 2002 | US |