This application is a National Stage of International Application No. PCT/CN2018/086604, filed May 11, 2018, which claims priority to Chinese Patent Application No. 201710493209.X, submitted on Jun. 26, 2017 to the Chinese Patent Office and entitled “Encapsulating Cover Plate, Organic Light-Emitting Diode Display and Fabricating Method Thereof”, the entire content of which is incorporated herein by reference.
The present disclosure relates to the technical field of displays, in particular to an encapsulating cover plate, an organic light-emitting diode display, and a fabricating method thereof.
In an OLED (Organic Light-Emitting Diode) display, most of the organic substances in a light-emitting layer are sensitive to pollutants, oxygen, and water vapor in the atmosphere. Oxygen and carbonyl compound formed by the oxidation of the light-emitting layer are an effective quencher, which may significantly reduce the light-emitting quantum efficiency of the organic light-emitting diode display; water vapor may hydrolyze the organic layer compound and affect the conductivity, resulting in great stability reduction of the organic light-emitting diode display; metal materials used to form the cathode of the organic light-emitting diode display are mostly chemically active metals, which are prone to erosion in the air or other oxygen-containing atmospheres, especially in environments containing water vapor, more prone to electrochemical corrosion. These can seriously affect the service life of devices in organic light-emitting diode displays. Therefore, the encapsulation of the OLED device ensures good internal sealing of the device, and contact with the external environment is reduced as little as possible, which is essential for stable light emitting of the OLED device.
At present, the encapsulating of the organic light-emitting diode display is mainly used to prevent the organic light-emitting diode device from being eroded by water and oxygen using film encapsulation or encapsulation resin. The water and oxygen have a certain erosion path through the edge of the encapsulation, and after a period of time of testing or placement, organic light-emitting diode devices are all subject to different degrees of erosion. Therefore, it is a very important task to improve the encapsulation effect for the organic light-emitting diode display to ensure long service life.
The present disclosure provides an encapsulating cover plate, an organic light-emitting diode display, and a fabricating method thereof, to improve the encapsulating effect and prolong the service life of the organic light-emitting diode display.
In order to achieve the above objects, the present disclosure provides the following technical solutions.
The present disclosure provides an encapsulating cover plate. The encapsulating cover plate includes a cover plate body, having an open groove configured for introducing a drying gas; cap plugs, configured for covering both ends of the open groove; and a water absorption layer, configured for covering at least an open of the open groove.
The encapsulating cover plate according to the present disclosure can facilitate the introduction of the drying gas through the open groove; furthermore, the water absorption layer absorbs water vapor; the introduced drying gas dries the water absorption layer; the drying gas in circulation flow can take away the water vapor and oxygen in the water absorption layer, thus reducing the damage of water vapor and oxygen to the device, and the encapsulating effect is better. The cap plugs can seal the open groove when drying is not needed. The encapsulating cover plate according to the present disclosure can repeatedly absorb the water vapor, and can prolong the service life of the organic light-emitting diode display.
In some optional embodiments, the encapsulating cover plate further includes: a chemical drying agent doped in the water absorption layer, the chemical drying agent changes color when absorbing water. The chemical drying agent can further increase the water absorption intensity, and the change of the color can remind an operator to introduce the drying gas in time for drying.
In some optional embodiments, the chemical drying agent includes any one of copper sulfate and silica gel. The chemical drying agent can absorb water to form a substance with a new color, or can be dehydrated to regain the original color.
In some optional embodiments, the water absorption layer is a water absorption layer made of an organic material, which facilitates the bonding between film layers.
In some optional embodiments, the open groove is of a fold line shape.
In some optional embodiments, the open groove includes: a plurality of first strip-shaped grooves spaced apart along a first direction of the cover plate body, a first strip-shaped groove at a first position in an arranging direction and a first strip-shaped groove at a last position in the arranging direction having openings provided with the cap plugs, respectively; and a second strip-shaped groove for connecting two adjacent first strip-shaped grooves, the second strip-shaped groove having a length direction perpendicular to the first direction; the open groove has a large coverage area and a good water absorbing effect.
In some optional embodiments, the water absorption layer covers only the open of the open groove, and the open groove is filled with liquid metal.
In some optional embodiments, the water absorption layer covers one surface of the cover plate body, provided with the open groove.
The present disclosure also provides an organic light-emitting diode display. The organic light-emitting diode display includes: a substrate having an organic light-emitting diode device, and further includes: the encapsulating cover plate according to any one of the above embodiments. The encapsulating cover plate is configured to encapsulate the organic light-emitting diode device. Since the encapsulating cover plate has a better encapsulating effect and can prolong the service life of the organic light-emitting diode device, the organic light-emitting diode display according to the present disclosure has a long service life.
The present disclosure also provides a fabricating method of an organic light-emitting diode display. The method includes: providing a substrate on which an organic light-emitting diode device is formed; providing a cover plate body; forming an open groove for introducing a drying gas in the cover plate body; sealing both ends of the open groove by cap plugs; forming a water absorption layer for covering at least an open of the open groove; forming a sealant on the water absorption layer; and sealing and pressing the cover plate on which the sealant is formed and the substrate on which the organic light-emitting diode device is formed.
The technical solutions in embodiments of the present disclosure are clearly and completely described in detail below with reference to the accompanying drawings in the embodiments of the present disclosure. It is obvious that the described embodiments are only a part of the embodiments of the present disclosure, and not all of the embodiments. All other embodiments obtained by those skilled in the art based on the embodiments of the present disclosure without creative efforts shall fall into the scope of the present disclosure.
As shown in
The encapsulating cover plate according to the present disclosure is configured with the open groove 2 to facilitate the introduction of the drying gas through the open groove 2. Furthermore, the water absorption layer 4 absorbs water vapor; the introduced drying gas dries the water absorption layer 4; the drying gas in circulation flow can take away the water vapor and oxygen in the water absorption layer 4, thus reducing the damage of water vapor and oxygen to the device, and the encapsulation effect is better. The cap plugs 3 can seal the open groove 2 when there is no need to dry. The encapsulating cover plate according to the present disclosure can repeatedly absorb the water vapor, and can prolong the service life of the organic light-emitting diode display.
In order to improve the encapsulation effect of the encapsulating cover plate, the encapsulating cover plate further includes: chemical drying agent 5 doped in the water absorption layer 4, and the chemical drying agent 5 changes color when absorbing water. The chemical drying agent 5 can further increase the water absorption intensity, and the change of the color can remind an operator to introduce the drying gas in time for drying.
The water absorption layer 4 can be formed by coating or vapor deposition. The shapes of the cap plugs 3 can be set according to the shape of the openings at both ends of the open groove.
Optionally, the chemical drying agent 5 includes any one of copper sulfate and silica gel. The chemical drying agent 5 can absorb water to form a substance with a new color, or can be dehydrated to regain the original color. The copper sulfate absorbs water to become blue, and the silica gel absorbs water to become pink, and water in the chemical drying agent 5 with changed color can be taken away by the introduced drying gas to regain the chemical drying agent 5 with the original color.
The chemical drying agent 5 can be added to the water absorption layer 4 in various ways. Optionally, the chemical drying agent 5 can be added after the water absorption layer 4 is formed, specifically, by coating, printing, etc.; alternatively, the chemical drying agent 5 may be first doped into a material configured for forming the water absorption layer 4, and then the water absorption layer 4 with the chemical drying agent 5 is formed.
The drying gas may be a hot drying gas, and the drying gas may be nitrogen or argon, etc., and will not be further described herein.
Since the organic light-emitting diode display device is generally made of an organic material, the water absorption layer 4 is made of an organic material in order to improve the bonding stability between the water absorption layer 4 and the organic light-emitting diode display element. The specific materials of the water absorption layer may be various. For example, the material of the water absorption layer 4 may be resin, silica gel or the like.
The specific shapes of the open groove 2 may be various. Optionally, the shape of the open groove 2 is a fold line. Of course, the shape of the open groove 2 is not limited to a fold line. Optionally, the area of the open groove 2 covering the cover plate body 1 is as large as possible.
As shown in
The water absorption layer 4 may be of a full layer structure or of a split structure.
In an optional embodiment, as shown in
In another optional embodiment, as shown in
As shown in
Usually, the encapsulating cover plate seals the organic light-emitting diode device by a sealant 6 and adheres to the substrate 7.
As shown in
S601 is to provide a substrate on which an organic light-emitting diode device is formed; the organic light-emitting diode device may be formed by vapor deposition, and generally includes a functional layer, a light-emitting layer, and the like.
S602 is to provide a cover plate body.
S603 is to form an open groove configured for introducing a drying gas in the cover plate body.
S604 is to seal both ends of the open groove by cap plugs.
S605 is to form a water absorption layer configured for covering at least the open of the open groove.
S606 is to form a sealant on the water absorption layer.
S607 is to seal and press the cover plate on which the sealant is formed and the substrate on which the organic light-emitting diode device is formed.
The organic light-emitting diode display fabricated by the method can facilitate the introduction of the drying gas through the open groove formed in and the cap plugs provided on the cover plate body during use; furthermore, the water absorption layer absorbs water vapor and oxygen; the introduced drying gas dries the water absorption layer; the drying gas in circulation flow can take away the water vapor and oxygen in the water absorption layer, thus reducing the damage of the water vapor to the device, and the encapsulating effect is better, and the drying gas can be repeatedly and circularly introduced into the encapsulating cover plate provided by the present disclosure to absorb the water vapor, when there is water vapor again, the encapsulating cover plate can be dried by introducing the drying gas again. Such a structural arrangement can prolong the service life of the organic light-emitting diode display.
It will be apparent to those skilled in the art that various modifications and changes can be made in the present disclosure without departing from the spirit and scope of the present disclosure. Thus, if such modifications and changes of the present disclosure are within the scope of the appended claims and their equivalent technology, it is intended that the present invention cover the modifications and the changes.
Number | Date | Country | Kind |
---|---|---|---|
201710493209.X | Jun 2017 | CN | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/CN2018/086604 | 5/11/2018 | WO | 00 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2019/001151 | 1/3/2019 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
3784443 | Vercasson | Jan 1974 | A |
4357557 | Inohara | Nov 1982 | A |
4381463 | Branover | Apr 1983 | A |
4441318 | Theckston | Apr 1984 | A |
4679317 | Bailleul | Jul 1987 | A |
4810931 | McKenna | Mar 1989 | A |
5239228 | Taniguchi | Aug 1993 | A |
5405808 | Rostoker | Apr 1995 | A |
5909057 | McCormick | Jun 1999 | A |
5962962 | Fujita | Oct 1999 | A |
5981312 | Farquhar | Nov 1999 | A |
5990615 | Sakaguchi | Nov 1999 | A |
6016006 | Man | Jan 2000 | A |
6284342 | Ebisawa | Sep 2001 | B1 |
6737176 | Otsuki | May 2004 | B1 |
6758713 | Wei | Jul 2004 | B2 |
6784612 | Park | Aug 2004 | B2 |
6882041 | Cheah | Apr 2005 | B1 |
7178927 | Seo | Feb 2007 | B2 |
7482686 | Zhao | Jan 2009 | B2 |
8202746 | Lee | Jun 2012 | B2 |
9345169 | Campbell | May 2016 | B1 |
9660222 | Ikeda | May 2017 | B2 |
10643924 | Shen | May 2020 | B1 |
20040075115 | Fery | Apr 2004 | A1 |
20040082089 | Cheng | Apr 2004 | A1 |
20040189196 | Cok | Sep 2004 | A1 |
20040191566 | Kikuchi | Sep 2004 | A1 |
20040201347 | Park | Oct 2004 | A1 |
20050248270 | Ghosh | Nov 2005 | A1 |
20050276947 | Huang | Dec 2005 | A1 |
20060118925 | Macris | Jun 2006 | A1 |
20060289985 | Bettinelli | Dec 2006 | A1 |
20070013292 | Inoue | Jan 2007 | A1 |
20070023873 | Park | Feb 2007 | A1 |
20070029928 | Choi | Feb 2007 | A1 |
20070046198 | Kuan | Mar 2007 | A1 |
20070152212 | Cho | Jul 2007 | A1 |
20080180923 | Grespan | Jul 2008 | A1 |
20090051724 | Katoh | Feb 2009 | A1 |
20090066243 | Sakurai | Mar 2009 | A1 |
20090288695 | Jaisinghani | Nov 2009 | A1 |
20100237453 | Bonekamp | Sep 2010 | A1 |
20100248966 | Lynch | Sep 2010 | A1 |
20100283384 | Lifka | Nov 2010 | A1 |
20110114840 | Yamazaki | May 2011 | A1 |
20110140119 | Oh | Jun 2011 | A1 |
20110147916 | Su | Jun 2011 | A1 |
20120037893 | Tanaka | Feb 2012 | A1 |
20120098119 | Refai-Ahmed | Apr 2012 | A1 |
20130183471 | Luhmann | Jul 2013 | A1 |
20140110685 | Hong | Apr 2014 | A1 |
20140159017 | Ikeda et al. | Jun 2014 | A1 |
20140346476 | Yao | Nov 2014 | A1 |
20150162568 | Bai | Jun 2015 | A1 |
20150294919 | Notsu | Oct 2015 | A1 |
20150337174 | Keite-Telgenbuscher | Nov 2015 | A1 |
20160056089 | Taniguchi | Feb 2016 | A1 |
20160104861 | Zeng | Apr 2016 | A1 |
20160118620 | Yoo | Apr 2016 | A1 |
20160136851 | Campbell | May 2016 | A1 |
20160240597 | Chen | Aug 2016 | A1 |
20160254491 | Wang | Sep 2016 | A1 |
20160293887 | Chen | Oct 2016 | A1 |
20160308161 | Qian | Oct 2016 | A1 |
20160315282 | Qian | Oct 2016 | A1 |
20160329519 | Yu | Nov 2016 | A1 |
20160372700 | Baisl | Dec 2016 | A1 |
20170194597 | Pang | Jun 2017 | A1 |
20170213976 | Luo | Jul 2017 | A1 |
20180315954 | Wu | Nov 2018 | A1 |
20190140206 | Liu | May 2019 | A1 |
20190393118 | Rawlings | Dec 2019 | A1 |
20200194341 | Cheng | Jun 2020 | A1 |
20200350231 | Shen | Nov 2020 | A1 |
20210102757 | Colson | Apr 2021 | A1 |
20210249632 | Wang | Aug 2021 | A1 |
Number | Date | Country |
---|---|---|
1505442 | Jun 2004 | CN |
1507084 | Jun 2004 | CN |
203407114 | Jan 2014 | CN |
103872260 | Jun 2014 | CN |
104979373 | Oct 2015 | CN |
106784381 | May 2017 | CN |
106784381 | May 2017 | CN |
107331787 | Nov 2017 | CN |
0776147 | May 1997 | EP |
9134781 | May 1997 | JP |
Entry |
---|
Office Action for corresponding Chinese Application 201710493209.X dated Jul. 26, 2018. |
Office Action for corresponding Chinese Application 201710493209.X dated Mar. 7, 2019. |
International Search Report for PCT/CN2018/086604 dated Aug. 6, 2018. |
Number | Date | Country | |
---|---|---|---|
20210249632 A1 | Aug 2021 | US |