The present application relates to the field of semiconductor technologies, and in particular, to a semiconductor apparatus and a manufacturing method thereof.
Embodiments of the present disclosure provide a semiconductor apparatus and a manufacturing method thereof. In the semiconductor apparatus, a contact area between a thermal interface material layer and a circuit device is increased by using a disposed packaging layer, so as to greatly improve thermal conductivity effectiveness of an entire heat conduction path, thereby better meeting a heat dissipation requirement of a high-power-consumption circuit device.
According to a first aspect, an embodiment of the present disclosure provides a semiconductor apparatus, including a circuit device and a heat sink fin that are disposed in a laminated manner, and a thermal interface material layer located between the circuit device and the heat sink fin, where
In the foregoing solution, because the packaging layer is disposed around the circuit device, and the packaging layer and the circuit device are both thermally coupled to the thermal interface material layer, a contact area between the circuit device and the thermal interface material layer is increased. In addition, heat generated on the side wall of the circuit device may be transferred to the thermal interface material layer through the packaging layer, and then transferred to the heat sink fin, thereby improving a heat dissipation effect of the semiconductor apparatus. In addition, one packaging layer is disposed around an exterior side of the circuit device, so as to increase a laying area of the thermal interface material layer, increase an area of a contact surface of the thermal interface material layer, reduce an interface stress, and correspondingly improve component reliability.
The packaging layer uses a plastic film layer. The plastic film layer has a desirable heat transfer effect, and can rapidly transfer the heat generated on the side wall of the circuit device to the thermal interface material layer, thereby improving heat dissipation efficiency of the circuit device.
The thermal interface material layer includes: a first alloy layer, thermally coupled to the circuit device and the packaging layer; a nano-metal particle layer, thermally coupled to the first alloy layer, where the nano-metal particle layer includes multiple nano-metal particles that are coupled to each other and an intermediate mixture, and the intermediate mixture is filled between the multiple nano-metal particles; and a second alloy layer, thermally coupled to the nano-metal particle layer and the heat sink fin. The used thermal interface material layer no longer includes high polymer materials with a relatively low thermal conductivity in silver adhesive materials, but includes nano-metal particles instead. The thermal interface material in this embodiment of the present disclosure has a relatively high thermal conductivity, so as to greatly improve thermal conductivity effectiveness of an entire heat conduction path, thereby better meeting a heat dissipation requirement of a high-power chip.
In specific disposition, a sintered continuous phase structure is formed at a contact portion between the first alloy layer and the nano-metal particle layer, sintered continuous phase structures are formed at contact portions between the multiple nano-metal particles, and a sintered continuous phase structure is formed at a contact portion between the second alloy layer and the nano-metal particle layer. A connection effect between the circuit device and the heat sink fin is improved by using the sintered continuous phase structure, and a heat transfer effect between the circuit device and the heat sink fin is improved.
In a specific implementation solution, the nano-metal particles include silver, and have a desirable heat transfer effect. In addition, in specific disposition, diameters of the nano-metal particles are between 50 nanometers and 200 nanometers.
The semiconductor apparatus provided in this embodiment is used for a flip chip ball grid array package structure.
The first alloy layer includes a first adhesive layer and a first co-sintered layer, the first adhesive layer is thermally coupled to the circuit device and the packaging layer, the first co-sintered layer is coupled to the nano-metal particle layer, and a sintered continuous phase structure is formed at a contact portion between the first co-sintered layer and the nano-metal particle layer. By using the foregoing structure, connection strength of thermal coupling of the first alloy layer to the circuit device and the packaging layer is increased, and a desirable heat transfer effect is achieved.
In specific disposition, the first adhesive layer includes any one of the following materials: titanium, chromium, nickel, or a nickel-vanadium alloy, and the first co-sintered layer includes any one of the following materials: silver, gold, or copper. The foregoing materials all have relatively desirable heat transfer effects.
In addition, in a solution, the first alloy layer further includes a first buffer layer, located between the first adhesive layer and the first co-sintered layer, and the first buffer layer includes any one of the following materials: aluminum, copper, nickel, or a nickel-vanadium alloy.
In specific disposition, the second alloy layer includes a second adhesive layer and a second co-sintered layer, the second adhesive layer is thermally coupled to the heat sink fin, the second co-sintered layer is thermally coupled to the nano-metal particle layer, and a sintered continuous phase structure is formed at a contact portion between the second co-sintered layer and the nano-metal particle layer. By using the foregoing structure, connection strength of thermal coupling of the second alloy layer to the heat sink fin is increased, and a desirable heat transfer effect is achieved.
In addition, in specific disposition, the second adhesive layer includes any one of the following materials: titanium, chromium, nickel, or a nickel-vanadium alloy, and the second co-sintered layer includes any one of the following materials: silver, gold, or copper. The foregoing materials all have relatively desirable heat transfer effects.
In a solution, the second alloy layer further includes a second buffer layer, located between the second adhesive layer and the second co-sintered layer, and the second buffer layer includes any one of the following materials: aluminum, copper, nickel, or a nickel-vanadium alloy.
Diameters of the nano-metal particles are not greater than 1 micrometer.
Different materials may be selected for the intermediate mixture. In a specific implementation, the intermediate mixture includes either of the following materials: air or resin.
An embodiment of the present disclosure provides a semiconductor apparatus manufacturing method, including: disposing a packaging layer around a side wall of a circuit device, where the circuit device includes an integrated circuit die, the integrated circuit die is provided with a pin, one surface that is of the integrated circuit die and on which the pin is disposed is a mounting surface, and the side wall of the circuit device is a wall that is of the integrated circuit die and that is adjacent to the mounting surface;
In the foregoing solution, because the packaging layer is disposed around the circuit device, and the packaging layer and the circuit device are both thermally coupled to the thermal interface material layer, a contact area between the circuit device and the thermal interface material layer is increased. In addition, heat generated on the side wall of the circuit device may be transferred to the thermal interface material layer through the packaging layer, and then transferred to the heat sink fin, thereby improving a heat dissipation effect of the semiconductor apparatus. In addition, one packaging layer is disposed around an exterior side of the circuit device, so as to increase a laying area of the thermal interface material layer, increase an area of a contact surface of the thermal interface material layer, reduce an interface stress, and correspondingly improve component reliability.
During specific fabrication, the generating a thermal interface material layer, where the thermal interface material layer has a first surface facing the circuit device and the packaging layer and a second surface facing the heat sink fin is specifically:
The manufacturing method further includes: forming a sintered continuous phase structure at a contact portion between the first alloy layer and the nano-metal particle layer, forming sintered continuous phase structures at contact portions between the nano-metal particles, and forming a sintered continuous phase structure at a contact portion between the second alloy layer and the nano-metal particle layer.
Diameters of the nano-metal particles are not greater than 1 micrometer.
The intermediate mixture includes either of the following materials: air or resin.
During specific fabrication of the first alloy layer, a first adhesive layer and a first co-sintered layer are generated, the first adhesive layer is thermally coupled to the circuit device and the packaging layer, the first co-sintered layer is coupled to the nano-metal particle layer, and a sintered continuous phase structure is formed at a contact portion between the first co-sintered layer and the nano-metal particle layer.
During specific fabrication of the second alloy layer, a second adhesive layer and a second co-sintered layer are generated, the second adhesive layer is thermally coupled to the heat sink fin, the second co-sintered layer is thermally coupled to the nano-metal particle layer, and a sintered continuous phase structure is formed at a contact portion between the second co-sintered layer and the nano-metal particle layer.
The disposing a packaging layer around a side wall of a circuit device includes: disposing the packaging layer around the side wall by using a plastic film as a material for manufacturing the packaging layer. The plastic film has a desirable heat transfer effect. Heat dissipation efficiency of the circuit device is improved by using the disposed packaging layer that is fabricated from the plastic film.
To describe the technical solutions in the embodiments of the present disclosure or in the prior art more clearly, the following briefly describes the accompanying drawings required for describing the embodiments or the prior art. Apparently, the accompanying drawings in the following description show merely some embodiments of the present disclosure, and a person of ordinary skill in the art may still derive other drawings from these accompanying drawings without creative efforts.
The following clearly describes the technical solutions in the embodiments of the present disclosure with reference to the accompanying drawings in the embodiments of the present disclosure. Apparently, the described embodiments are merely some but not all of the embodiments of the present disclosure. All other embodiments obtained by a person of ordinary skill in the art based on the embodiments of the present disclosure without creative efforts shall fall within the protection scope of the present disclosure.
For convenience of description, a side wall of a circuit device is defined in the embodiments. In the embodiments, the side wall of the circuit device is a wall that is of the circuit device and that is adjacent to one surface (a mounting surface) on which a pin is disposed. In
An embodiment of the present disclosure provides a semiconductor apparatus. The semiconductor apparatus includes: a circuit device and a heat sink fin 105 that are disposed in a laminated manner, and a thermal interface material layer 104 located between the circuit device and the heat sink fin 105, where
Referring to
In addition, in specific disposition, the packaging layer 120 is attached on the side wall of the circuit device. Therefore, during heat dissipation, heat on the side wall of the circuit device is transferred to the thermal interface material layer 104 through the packaging layer 120, and is further dissipated to the heat sink fin 105. By using the foregoing structure, it may be known that a heat dissipation manner of the circuit device is dissipating heat on a top surface of the circuit device along a path from the thermal interface material layer 104 to the heat sink fin 105 and dissipating the heat on the side wall of the circuit device along a path from the packaging layer 120 through the thermal interface material layer 104 to the heat sink fin 105, so as to increase a heat dissipation area of the circuit device, thereby improving a heat dissipation effect of the circuit device.
In a specific implementation, the packaging layer 120 uses a plastic film layer. The plastic film layer has a desirable packaging effect and a desirable heat transfer effect, so that the plastic film layer can rapidly transfer heat to the thermal interface material layer, thereby improving the heat dissipation effect of the circuit device.
As shown in
The integrated circuit die 103, the packaging layer 120 disposed around the circuit device 103, the thermal interface material layer 104, and the heat sink fin 105 may be some or all of components of a semiconductor apparatus. The semiconductor apparatus may be used for the flip chip ball grid array package structure shown in the figure, but no limitation is set thereto.
The nano-metal particle layer 110 is thermally coupled to the integrated circuit die 103 and the packaging layer 120 by using the first alloy layer 109. More specifically, as shown in
The nano-metal particle layer 110 includes nano-metal particles and an intermediate mixture. The intermediate mixture includes, but is not limited to, either of the following materials: air or resin. The intermediate mixture is filled between multiple nano-metal particles, to make the multiple nano-metal particles form a whole. The nano-metal particles include, but are not limited to, silver. Diameters of the nano-metal particles are not greater than 1 micrometer. In an embodiment, the diameters of the nano-metal particles are between 50 nanometers and 200 nanometers. The nano-metal particle layer 110 has a relatively low thermal resistance, and forms a relatively desirable heat conduction path.
The second alloy layer 112 is thermally coupled to the nano-metal particle layer 110 and the heat sink fin 105. More specifically, as shown in the figure, the second alloy layer 112 may be located on the nano-metal particle layer 110 and under the heat sink fin 105. That is, the second alloy layer 112 may be located between the nano-metal particle layer 110 and the heat sink fin 105. The second alloy layer 112 increases adhesive strength between the nano-metal particle layer 110 and the heat sink fin 105.
In an embodiment, a sintered continuous phase structure is formed at a contact portion between the first alloy layer 109 and the nano-metal particle layer 110, sintered continuous phase structures are formed at contact portions between the nano-metal particles, and a sintered continuous phase structure is formed at a contact portion between the second alloy layer 112 and the nano-metal particle layer 110. The sintered continuous phase structure in this specification includes, but is not limited to, a whole structure formed of metal particles as metal atoms near contact portions of the metal particles spread to metal particle interfaces and fuse with the metal particle interfaces because the metal particles are sintered.
In conclusion, because the thermal interface material layer in this embodiment of the present disclosure no longer includes high polymer materials with a relatively low thermal conductivity in silver adhesive materials, but includes nano-metal particles instead. The thermal interface material in this embodiment of the present disclosure has a relatively high thermal conductivity, so as to greatly improve thermal conductivity effectiveness of an entire heat conduction path, thereby better meeting a heat dissipation requirement of a high-power chip. In addition, one packaging layer 120 is disposed around an exterior side of the integrated circuit die 103, so as to increase a laying area of the thermal interface material layer, increase an area of a contact surface of the thermal interface material layer, reduce an interface stress, and correspondingly improve component reliability.
In addition, the disposing a packaging layer around a side wall of a circuit device includes: disposing the packaging layer around the side wall by using a plastic film as a material for manufacturing the packaging layer. The plastic film layer has a desirable heat transfer effect, and can rapidly transfer heat generated on the side wall of the circuit device to the thermal interface material layer, thereby improving heat dissipation efficiency of the circuit device.
During specific manufacturing, the thermal interface material layer is generated. The thermal interface material layer has the first surface facing the circuit device and the packaging layer and the second surface facing the heat sink fin.
A first alloy layer is generated. A nano-metal particle layer is generated by using nano-metal particles that are coupled to each other and an intermediate mixture. Diameters of the nano-metal particles are not greater than 1 micrometer. For example, the diameters of the nano-metal particles are between 50 nanometers and 200 nanometers. The intermediate mixture includes, but is not limited to, either of the following materials: air or resin. In an embodiment, the nano-metal particles include, but are not limited to, silver. A second alloy layer is generated. The nano-metal particle layer is thermally coupled to the circuit device and the packaging layer by using the first alloy layer. The second alloy layer is thermally coupled to the nano-metal particle layer and the heat sink fin.
In an embodiment, the method further includes: forming a sintered continuous phase structure at a contact portion between the first alloy layer and the nano-metal particle layer, forming sintered continuous phase structures at contact portions between the nano-metal particles, and forming a sintered continuous phase structure at a contact portion between the second alloy layer and the nano-metal particle layer.
In an embodiment, the method may be used for a flip chip ball grid array package structure, but no limitation is set thereto.
In an embodiment, the generating a first alloy layer includes: generating a first adhesive layer and a first co-sintered layer, thermally coupling the first adhesive layer to the circuit device and the packaging layer, coupling the first co-sintered layer to the nano-metal particle layer, and forming a sintered continuous phase structure at a contact portion between the first co-sintered layer and the nano-metal particle layer. The first adhesive layer includes, but is not limited to, any one of the following materials: titanium, chromium, nickel, or nickel/vanadium. The first co-sintered layer includes, but is not limited to, any one of the following materials: silver, gold, or copper. In another embodiment, the generating a first alloy layer further includes: generating a first buffer layer between the first adhesive layer and the first co-sintered layer. The first buffer layer includes, but is not limited to, any one of the following materials: aluminum, copper, nickel, or nickel/vanadium.
In an embodiment, the generating a second alloy layer includes: generating a second adhesive layer and a second co-sintered layer, thermally coupling the second adhesive layer to the heat sink fin, thermally coupling the second co-sintered layer to the nano-metal particle layer, and forming a sintered continuous phase structure at a contact portion between the second co-sintered layer and the nano-metal particle layer. The second adhesive layer includes, but is not limited to, any one of the following materials: titanium, chromium, nickel, or nickel/vanadium. The second co-sintered layer includes, but is not limited to, any one of the following materials: silver, gold, or copper. In another embodiment, the generating a second alloy layer further includes: generating a second buffer layer between the second adhesive layer and the second co-sintered layer. The second buffer layer includes, but is not limited to, any one of the following materials: aluminum, copper, nickel, or nickel/vanadium.
The circuit device may include the integrated circuit die. Thermally coupling the first alloy layer to the circuit device and the packaging layer includes thermally coupling the first alloy layer to a substrate in the integrated circuit die and the packaging layer.
The foregoing disclosed above is merely examples of embodiments of the present disclosure, and certainly is not intended to limit the protection scope of the present disclosure. Therefore, equivalent variations made in accordance with the claims of the present disclosure shall fall within the scope of the present disclosure.
Number | Date | Country | Kind |
---|---|---|---|
201610799678.X | Aug 2016 | CN | national |
This application is a continuation of International Application No. PCT/CN2017/074449, filed on Feb. 22, 2017, which claims priority to Chinese Patent Application No. 201610799678.X, filed on Aug. 31, 2016, the disclosures of the aforementioned applications are hereby incorporated by reference in their entireties.
Number | Date | Country | |
---|---|---|---|
Parent | PCT/CN2017/074449 | Feb 2017 | US |
Child | 16287629 | US |