Hereinafter, descriptions will be given in detail of a semiconductor device according to a preferred embodiment of the present invention with reference to
As shown in
The N type epitaxial layer 3 is formed on the P type single crystal silicon substrate 2. Note that, although only one epitaxial layer 3 is formed on the substrate 2 in this embodiment, the preferred embodiment of the present invention is not limited to this case. For example, a plurality of epitaxial layers may be stacked on the substrate.
The N type buried diffusion layer 4 is formed on both regions of the substrate 2 and the epitaxial layer 3. As illustrated in
The P type diffusion layer 5 is formed in the epitaxial layer 3. The P type diffusion layer 6 is formed in the P type diffusion layer 5 in a manner of overlapping the P type diffusion layer 5. The P type diffusion layer 5 is used as the back gate region, and the P type diffusion layer 6 is used as a back gate leading region. Moreover, the P type diffusion layer 5 positioned below the gate electrodes 11 and 12 is used as a channel region. Note that, although detailed descriptions will be given later, an impurity concentration of the channel region is adjusted only by the P type diffusion layer 5, achieving an appropriate threshold voltage (Vth) of the MOS transistor 1. Furthermore, an impurity concentration in a deep portion of the back gate region is increased only by the P type diffusion layer 5, and thereby a resistance value of the back gate region is reduced.
The N type diffusion layers 7 and 8 are formed in the P type diffusion layer 5. The N type diffusion layers 7 and 8 are used as the source region. The N type diffusion layers 7 and 8, and the P type diffusion layer 6 are connected to a source electrode 25, and are equal in electric potential. Note that the N type diffusion layers 7 and 8 can be circularly formed around the P type diffusion layer 6.
The N type diffusion layers 9 and 10 are formed in the epitaxial layer 3. The N type diffusion layers 9 and 10 are used as the drain regions.
The gate electrodes 11 and 12 are formed on a gate oxide film 13. Each of the gate electrodes 11 and 12 is formed of, for example, a polysilicon film 14 and a tungsten silicon film 15 so as to have a desired thickness. Incidentally, the gate electrodes 11 and 12 can be circularly formed.
LOCOS (Local Oxidation of Silicon) oxide films 16, 17, 18 and 19 are formed in the epitaxial layer 3. The thickness of each flat portion of the LOCOS oxide films 16, 17, 18 and 19 is approximately 3000 Å to 5000 Å, for example.
An insulating layer 20 is formed over the epitaxial layer 3. The insulating layer 20 is formed of a BPSG (Boron Phospho Silicate Glass) film, a SOG (Spin On Glass) film or the like. In addition, with a known photolithography technique, contact holes 21, 22 and 23 are formed in the insulating layer 20 by dry etching using CHF3 or CF4 gas, for example.
In each of the contact holes 21, 22 and 23, an aluminum alloy film made of, for example, an Al—Si film, an Al—Si—Cu film or an Al—Cu film is selectively formed, so that drain electrodes 24 and 26, and the source electrode 25 are formed respectively in the contact holes 21, 22 and 23. Incidentally, the drain electrodes 24 and 26 can be circularly formed around the source electrode 25. In addition, although a layer of wiring to the gate electrodes 11 and 12 is not illustrated in the cross-section shown in
Next, descriptions will be given of a structure of the back gate region in the MOS transistor 1 and characteristics of the MOS transistor 1 with reference to the
As shown in
As shown in
Here, the parasitic NPN transistor comes into an ON state due to the following operations. Firstly, when the MOS transistor 1 is in the ON state, conductivity modulation occurs in the N type epitaxial layer 3 as a drain region. Free carriers (holes) are generated, which are paired up with free carriers (electrons), in the N type epitaxial layer 3 constituting a current path. Then, when the MOS transistor 1 is in an OFF state, the free carriers (holes) generated in the N type epitaxial layer 3 flow into the P type diffusion layer 5, and forward biases between the emitter and the base of the parasitic NPN transistor. Thereby the parasitic NPN transistor comes into the ON state in some cases. In other words, in a case where the resistance value of the P type diffusion layer 5 is large, the flow of the free carriers (holes) into the base region increases an electric potential of the base region, and thereby the parasitic NPN transistor is easily to be operated.
As described above, in this embodiment, the P type diffusion layer 5 expands into the deep portion of the N type epitaxial layer 3. This structure makes a base width W1 of the parasitic NPN transistor increase, and makes a resistance value of the base region decrease. Moreover, it is possible to suppress the increase in the electric potential caused by the flowing of the free carriers (holes) into the P type diffusion layer 5 when the MOS transistor 1 is in the OFF state. As a result it is possible to prevent the ON state operation of the parasitic NPN transistor, and to prevent breakdown of the MOS transistor 1 caused by the operation of the parasitic NPN transistor. That is, it is possible to improve a breakdown voltage characteristic of the MOS transistor 1.
In
In both cases of the solid line and the dotted line, the PN junction region 27 (see
Specifically, a valley-shaped region of the impurity concentration profile, where each of the solid line and the dotted line intersects the dashed line, is the PN junction region 27. The valley-shape is formed because, in the PN junction region 27, a P type impurity concentration and an N type impurity concentration are compensated each other, and thereby a low impurity concentration region is formed. Then, a region on the left side of the PN junction region 27 in
In
In both cases of the solid line and the dotted line, the PN junction region 27 (see
Specifically, a valley-shaped region of the impurity concentration profile, where each of the solid line and the dotted line intersects the dashed line, is the PN junction region 27. The valley-shape is formed because, in the PN junction region 27, the P type impurity concentration and the N type impurity concentration are compensated each other, and thereby a low impurity concentration region is formed. Then, a region on the left side of the PN junction region 27 in
As described above, it is necessary to reduce the resistance value of the base region in order to prevent the parasitic NPN transistor from operating. On the other hand, in order to achieve the appropriate threshold voltage (Vth) of the MOS transistor 1, conditions for forming the P type diffusion layer 5, for example, an impurity concentration profile, diffusion depth, and the like, are designed. In this embodiment, when the P type diffusion layer 5 is formed, ions are implanted and thermally diffused so that the diffusion layer 5 has the impurity concentration peak in the deep portion of the N type epitaxial layer 3. Thereby, the impurity concentration of the P type diffusion layer 5 in the deep portion of the N type epitaxial layer 3 can be increased and also the impurity concentration in the channel region can be set to a desired value. As a result, by increasing the impurity concentration in the deep portion of the P type diffusion layer 5, it is possible to reduce the resistance value of base region of the parasitic NPN transistor. Moreover, it is possible to suppress the increase in the electric potential caused by the flowing of the free carriers (holes) into the P type diffusion layer 5 when the MOS transistor 1 is in the OFF state. Consequently, it is possible to prevent the ON state operation of the parasitic NPN transistor, and to prevent breakdown of the MOS transistor 1, which might be deteriorated by the operation of the parasitic NPN transistor.
In other words, the impurity concentration profile of the P type diffusion layer 5 is designed to prevent the ON state operation of the parasitic NPN transistor. Thereby, impurity concentration ratios (the line A-A direction/the line B-B direction) in the vicinity of the PN junction region 27 on the P type diffusion region 5 side are approximately 3.21 in the case of the solid line, and approximately 1.49 in the case of the dotted line. In this embodiment, the P type diffusion layer S is formed so that the impurity concentration ratio becomes larger than 3.0 or more. Thus, it is possible to prevent the ON state operation of the parasitic NPN transistor, and to improve the breakdown voltage characteristic of the MOS transistor, which might be deteriorated by the operation of the parasitic NPN transistor.
Note that, in this embodiment, the descriptions have been given of the case of the lamination structure where the gate electrodes 11 and 12 are formed of the polysilicon film 14 and the tungsten silicon film 15, but the preferred embodiment of the present invention is not limited to the above-described case. For example, a single-layer structure of the polysilicon film or the tungsten silicon film can be employed, as long as the gate electrodes 11 or 12 have a thickness enough to prevent the impurity from penetrating therethrough in the step of performing ion implantation to form the P type diffusion layer 5. Moreover, various modifications are possible to be made on the preferred embodiment of the present invention without departing from the spirit of the preferred embodiment of the present invention.
Next, descriptions will be given in detail of a method of manufacturing a semiconductor device according to another preferred embodiment of the present invention with reference to
Firstly, as shown in
Next, as shown in
Next, as shown in
Next, by means of the known photolithography technique, P type diffusion layers 46 and 47 are formed in the epitaxial layer 3. Then, LOCOS oxide films 16, 17, 18 and 19 are formed in desired regions of the epitaxial layer 3.
Next, as shown in
Next, a photoresist 48 is formed on the silicon oxide film to be used as the gate oxide film 13. By means of the known photolithography technique, an opening is formed in the photoresist 48 on a region where a P type diffusion layer 5 is to be formed. Then, ions of a P type impurity, for example, boron (B) are implanted from the surface of the epitaxial layer 3 at an accelerating voltage of 60 to 90 (keV) and a dose of 1.0×1014 to 1.0×1016 (/cm2). Subsequently, the photoresist 48 is removed, and then the P type diffusion layer 5 is formed by thermal diffusion.
At this time, the P type diffusion layer 5 is formed by self-alignment using the gate electrodes 11 and 12 as a mask. As described above, since the thickness of the tungsten silicon film 15 is approximately 2000 to 3000 (Å), it is possible to prevent ions of boron (B) from being implanted into a region below the gate electrodes 11 and 12 exposed from the opening in the photoresist 48. In addition, as described by use of
Specifically, suppose a case where the P type diffusion layer 5 is formed by an ion implantation technique using the gate electrodes 11 and 12 as a mask, each of the gate electrodes 11 and 12 is formed of only the polysilicon film 14 whose thickness is 4000 (Å). If an accelerating voltage is applied at 40 or more (KeV), the ions of boron (B) penetrate through the gate electrodes 11 and 12. On the other hand, suppose a structure in which each thickness of the gate electrodes 11 and 12 is 4000 (Å), while the thickness of the polysilicon film 14 is 1500 (Å) and that of the tungsten silicon film 15 is 2500 (Å). This structure makes it possible to prevent the ions of boron (B) from penetrating through the gate electrodes 11 and 12 even in a case where the ions of boron (B) are implanted at an accelerating voltage of 80 (KeV). In other words, by using, in the gate electrodes 11 and 12, the tungsten silicon film 15 through which the ions of boron (B) hardly penetrate, the P type diffusion layer 5 can be formed by self alignment without increasing the thickness of the gate electrodes 11 and 12.
This manufacturing method makes it possible to omit a forming step of a diffusion layer which is formed in a conventional manufacturing method for reducing a resistance value of the back gate region. In other words, it is not necessary to take account of an impurity concentration of a channel region to be disturbed by mask misalignment at the time of forming the back gate region. This allows the gate electrodes 11 and 12 to be formed with a processing technique without taking account of a degree of the mask misalignment at the time of forming the back gate region. Moreover, each cell pitch can be shortened by reducing a separation distance W2 between the gate electrodes 11 and 12, and thereby the device size can be reduced. In other words, when the back gate region is formed of only the P type diffusion layer 5, the on-resistance per area of a MOS transistor 1 can be reduced. Furthermore, by reducing the number of P type diffusion layers which constitute the back gate region, it is possible to reduce the manufacturing cost, for example, reducing the number of masks. Incidentally, the P type diffusion layer 6 as a back gate leading region is formed in the P type diffusion layer 5 in a manner of overlapping the P type diffusion layer 5 in the latter step of the manufacturing method.
Next, as shown in
Next, as shown in
(P) are implanted from the surface of the epitaxial layer 3 at an accelerating voltage of 90 to 110 (keV) and a dose of 1.0×1014 to 1.0×1016 (/cm2). Subsequently, the photoresist 50 is removed, and then the N type diffusion layers 7, 8, 9 and 10 are formed by thermal diffusion.
Next, as shown in
Noted that, in this embodiment descriptions have been given of the case where the accelerating voltage of 60 to 90 (KeV) is applied when the P type diffusion layer 5 is formed. However, the preferred embodiment of the present invention is not limited to the above-described case. It is only necessary that the impurity, for example, at the time of forming the P type diffusion layer 5, be prevented from penetrating through the gate electrodes. Thus, for example, the thickness of the gate electrode may allow the accelerating voltage to be applied at 90 (KeV) or more. In this case, the impurity concentration peak of the P type diffusion layer 5 is in the deep portion of the epitaxial layer and the diffusion width increases. As the result, it is possible to prevent the parasitic NPN transistor from operating. Meanwhile, descriptions have been given of the case where the gate electrodes 11 and 12 are formed of the polysilicon film and the tungsten silicon film as a two-layer structure, but the preferred embodiment of the present invention is not limited to the above-described case. The gate electrode can be formed of, for example, a polysilicon film or a tungsten silicon film as a single-layer structure. In this case, it is only necessary that the polysilicon film or the tungsten silicon film has a thickness enough to prevent implanted ions of boron (B) from penetrating through the film. Moreover, various modifications are possible to be made on the preferred embodiment of the present invention without departing from the spirit of the preferred embodiment of the present invention.
In the preferred embodiment of the present invention, the impurity concentration peak of the back gate region of the MOS transistor is formed in the deep portion of the semiconductor layer. This structure makes it possible to reduce the resistance value in the deep portion of the back gate region due to the impurity concentration, and to prevent the parasitic bipolar transistor in the MOS transistor from operating. As a result, the breakdown voltage characteristic of the MOS transistor can be improved.
In addition, in the preferred embodiment of the present invention, the appropriate threshold voltage of the MOS transistor is achieved, while the impurity concentration peak of the back gate region is formed in the deep portion of the semiconductor layer. This structure makes it possible to reduce the resistance value of the back gate region, and to prevent the parasitic bipolar transistor in the MOS transistor from operating.
Moreover, in the preferred embodiment of the present invention, the gate electrode of the MOS transistor is formed as a lamination structure with the polysilicon film and the tungsten silicon film. This structure makes it possible to form the diffusion layer as the back gate region in a desired region, thereby to reduce the device size. As a result, the on-resistance of the MOS transistor can be reduced.
Furthermore, in the preferred embodiment of the present invention, when the back gate region is formed, the back gate region is formed in the deep portion of the semiconductor layer by self-alignment using the gate electrode. This manufacturing method makes it possible to form the back gate region in a desired region, and to reduce the device size. As a result, the on-resistance per area of the MOS transistor can be reduced.
Still furthermore, in the preferred embodiment of the present invention, in the step of forming the back gate region by self-alignment using the gate electrode, the ion implantation technique is used at a highly accelerating voltage. This manufacturing method makes it possible to form the back gate region in the deep portion of the semiconductor layer, and to prevent the parasitic bipolar transistor in the MOS transistor from operating.
Yet still furthermore, in the preferred embodiment of the present invention, the gate electrode is formed by using the tungsten silicon film on the polysilicon film. This manufacturing method makes it possible to form the back gate region in a desired region by self-alignment using the gate electrode.
| Number | Date | Country | Kind |
|---|---|---|---|