This application is based on Japanese Patent Application No. 2005-340940 filed on Nov. 25, 2005, the disclosure of which is incorporated herein by reference.
The present invention relates to a semiconductor device having a super junction MOS transistor and a method for manufacturing the same.
As an inverter device for operating an alternating current motor with high efficiency, a circuit having a switching element (IGBT element, etc.) and a reflux diode (FWD) set to be parallel is used in an equivalent circuit of one phase amount of an inverter shown in
A device of low loss is required in the switching elements Q1, Q2 and the reflux diodes Df1, Df2 to reduce loss of the inverter circuit.
IGBT has been used as the switching elements Q1, Q2 at middle and high withstand voltages of 100 volts or more. However, the development of super junction type MOS is advanced from this requirement of low loss formation.
On the other hand, reductions in loss of the reflux electric current shown in
U.S. Pat. No. 5,915,179 proposes a structure in which power MOS and the Schottky barrier diode (SBD) are adjacently integrated on one chip and are electrically connected in parallel.
Further, JP-A-2002-76370 proposes a structure in which the Schottky barrier diode (SBD) is formed in a super junction substrate and is formed by silicon (Si) so as to withstand high voltage.
In U.S. Pat. No. 5,915,179, when the Schottky barrier diode is formed in an N− layer of silicon (Si), it is impossible to realize that the reduction of the forward voltage and the high withstand voltage formation are reconciled. Therefore, a problem exists in that no integration with a high withstand voltage power MOS transistor can be performed. Further, no Schottky barrier diode can be integrated without increasing an area of the power MOS transistor.
Further, in JP-A-2002-76370, the MOS transistor and this Schottky barrier diode (SBD) are separate parts as a free wheel diode when an inverter system is formed. Therefore, it is large-sized and there is a difficulty in mounting.
In view of the above-described problem, it is an object of the present disclosure to provide a semiconductor device having a super junction MOS transistor. It is another object of the present disclosure to provide a method for manufacturing a semiconductor device having a super junction MOS transistor.
According to a first aspect of the present disclosure, a semiconductor device having a super junction MOS transistor includes: a semiconductor substrate having a first conductive type and a high impurity concentration; a first semiconductor layer disposed on the substrate, wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; a second semiconductor layer having the first conductive type disposed on the first semiconductor layer, wherein the second semiconductor layer has a low impurity concentration, which is lower than that of the semiconductor substrate; a channel forming region having the second conductive type disposed on a first surface portion of the second semiconductor layer; a source region having the first conductive type disposed on a first surface portion of the channel forming region; a source contact region having the second conductive type disposed on a second surface portion of the channel forming region; a gate electrode disposed on a third surface portion of the channel forming region through a gate insulation film, the third surface portion which is exposed from the source region and the source contact region; a source electrode disposed on the source region and the source contact region; a drain electrode disposed on a backside of the substrate, which is opposite to the first semiconductor layer; and an anode electrode disposed on a second surface portion of the second semiconductor layer, the second surface portion which is exposed from the channel forming region. The anode electrode provides a Schottky barrier diode so that the super junction MOS transistor and the Schottky barrier diode are integrated in the semiconductor device.
In the above device, the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, the MOS transistor has high withstand voltage and low loss.
According to a second aspect of the present disclosure, a semiconductor device having a super junction MOS transistor includes: a semiconductor substrate having a first conductive type and a high impurity concentration; a first semiconductor layer disposed on the substrate, wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; a second semiconductor layer having the first conductive type disposed on the first semiconductor layer, wherein the second semiconductor layer has a low impurity concentration, which is lower than that of the semiconductor substrate; a channel forming region having the second conductive type disposed on a first surface portion of the second semiconductor layer; a source region having the first conductive type disposed on a first surface portion of the channel forming region; a source contact region having the second conductive type disposed on a second surface portion of the channel forming region; an anode electrode disposed on a second surface portion of the second semiconductor layer, the second surface portion which is exposed from the channel forming region; a trench disposed on a third surface portion of the second semiconductor layer to penetrate the source region and the channel forming region; a gate electrode disposed on an inner wall of the trench through a gate insulation film; a source electrode disposed on the source region and the source contact region; and a drain electrode disposed on a backside of the substrate, which is opposite to the first semiconductor layer. The anode electrode provides a Schottky barrier diode so that the super junction MOS transistor and the Schottky barrier diode are integrated in the semiconductor device.
In the above device, the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, the MOS transistor has high withstand voltage and low loss.
According to a third aspect of the present disclosure, a semiconductor device having a super junction MOS transistor includes: a semiconductor substrate having a first conductive type and a high impurity concentration; a first semiconductor layer disposed on the substrate, wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; a low concentration channel forming region having the second conductive type disposed on the first semiconductor layer; a well region having the first conductive type disposed on a first surface portion of the low concentration channel forming region, wherein the well region reaches the first semiconductor layer; a high concentration channel forming region having the second conductive type disposed on a second surface portion of the low concentration channel forming region, wherein the high concentration channel forming region has a high impurity concentration, which is higher than that of the low concentration channel forming region; a source region having the first conductive type disposed on a first surface portion of the high concentration channel forming region; a source contact region having the second conductive type disposed on a second surface portion of the high concentration channel forming region; a gate electrode disposed on a third surface portion of the low concentration channel forming region and a third surface portion of the high concentration channel forming region through a gate insulation film, each third surface portion which is exposed from the source region and the source contact region; a source electrode disposed on the source region and the source contact region; a drain electrode disposed on a backside of the substrate, which is opposite to the first semiconductor layer; and an anode electrode disposed on the well region, which is exposed from the low concentration channel forming region. The anode electrode provides a Schottky barrier diode so that the super junction MOS transistor and the Schottky barrier diode are integrated in the semiconductor device.
In the above device, the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, the MOS transistor has high withstand voltage and low loss.
According to a fourth aspect of the present disclosure, a semiconductor device having a super junction MOS transistor includes: a semiconductor substrate having a first conductive type and a high impurity concentration; a first semiconductor layer disposed on the substrate, wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; a channel forming region having a second conductive type disposed on a first surface portion of the first semiconductor layer; a source region having the first conductive type disposed on a first surface portion of the channel forming region; a source contact region having the second conductive type disposed on a second surface portion of the channel forming region; a gate electrode disposed on a third surface portion of the channel forming region through a gate insulation film, the third surface portion which is exposed from the source region and the source contact region; a source electrode disposed on the source region and the source contact region; a drain electrode disposed on a backside of the substrate, which is opposite to the first semiconductor layer; and an anode electrode disposed on a second surface portion of the first semiconductor layer, the second surface portion which is exposed from the channel forming region. The anode electrode provides a Schottky barrier diode so that the super junction MOS transistor and the Schottky barrier diode are integrated in the semiconductor device.
In the above device, the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, the MOS transistor has high withstand voltage and low loss.
According to a fifth aspect of the present disclosure, a method for manufacturing a semiconductor device includes: forming a first semiconductor layer on a semiconductor substrate, wherein the semiconductor substrate has a first conductive type and a high impurity concentration, and wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; forming a second semiconductor layer having the first conductive type on the first semiconductor layer by using an epitaxial growth method; forming a planar gate electrode on the second semiconductor layer through a gate insulation film; forming a channel forming region having the second conductive type on a first surface portion of the second semiconductor layer by using the planar gate electrode as a self-alignment member; forming a source region having the first conductive type disposed on a first surface portion of the channel forming region; forming a source contact region having the second conductive type disposed on a second surface portion of the channel forming region; forming an opening on the planar gate electrode by using a photo lithography etching method, wherein the opening corresponds to an anode electrode, which provides a Schottky barrier diode; forming an insulation film on whole area of the second semiconductor layer; removing a part of the insulation film, which corresponds to a source electrode and the anode electrode by using a photo lithography etching method; forming the source electrode on the source region and the source contact region; forming the anode electrode on a second surface portion of the second semiconductor layer, the second surface portion which is exposed from the channel forming region through the opening of the planar gate electrode; and forming a drain electrode on a backside of the substrate, which is opposite to the first semiconductor layer. The second semiconductor layer has a low impurity concentration, which is lower than that of the semiconductor substrate, and the gate electrode is disposed on a third surface portion of the channel forming region through the gate insulation film, the third surface portion which is exposed from the source region and the source contact region.
The above method provides the device, in which the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, in the device, the MOS transistor has high withstand voltage and low loss.
According to a sixth aspect of the present disclosure, a method for manufacturing a semiconductor device includes: forming a first semiconductor layer on a semiconductor substrate, wherein the semiconductor substrate has a first conductive type and a high impurity concentration, and wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; forming a second semiconductor layer having the first conductive type on the first semiconductor layer by using an epitaxial growth method; forming a trench on a third surface portion of the second semiconductor layer; embedding a gate electrode on an inner wall of the trench through a gate insulation film; forming a channel forming region having the second conductive type on a first surface portion of the second semiconductor layer by using the gate electrode as a self-alignment member; forming a source region having the first conductive type on a first surface portion of the channel forming region; forming a source contact region having the second conductive type on a second surface portion of the channel forming region; forming an insulation film on whole area of the second semiconductor layer; removing a part of the insulation film, which corresponds to a source electrode and an anode electrode by using a photo lithography etching method, wherein the anode electrode provides a Schottky barrier diode; forming the source electrode on the source region and the source contact region; forming the anode electrode on a second surface portion of the second semiconductor layer, the second surface portion which is exposed from the channel forming region; and forming a drain electrode on a backside of the substrate, which is opposite to the first semiconductor layer. The second semiconductor layer has a low impurity concentration, which is lower than that of the semiconductor substrate, and the trench penetrates the source region and the channel forming region.
The above method provides the device, in which the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, in the device, the MOS transistor has high withstand voltage and low loss.
According to a seventh aspect of the present disclosure, a method for manufacturing a semiconductor device includes: forming a first semiconductor layer on a semiconductor substrate, wherein the semiconductor substrate has a first conductive type and a high impurity concentration, and wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; forming a low concentration channel forming region having the second conductive type on the first semiconductor layer by using an epitaxial growth method; forming a well region having the first conductive type on a first surface portion of the low concentration channel forming region, wherein the well region reaches the first impurity diffusion regions; forming a planar gate electrode on the low concentration channel forming region through a gate insulation film; forming a high concentration channel forming region having the second conductive type on a second surface portion of the low concentration channel forming region by using the planar gate electrode as a self-alignment member, wherein the high concentration channel forming region has a high impurity concentration, which is higher than that of the low concentration channel forming region; forming a source region having the first conductive type on a first surface portion of the high concentration channel forming region; forming a source contact region having the second conductive type on a second surface portion of the high concentration channel forming region; forming an opening on the planar gate electrode by using a photo lithography etching method, wherein the opening corresponds to an anode electrode, which provides a Schottky barrier diode; forming an insulation film on whole area of the low concentration channel forming region; removing a part of the insulation film, which corresponds to a source electrode and the anode electrode by using a photo lithography etching method; forming the source electrode on the source region and the source contact region; forming the anode electrode on the well region, which is exposed from the low concentration channel forming region; and forming a drain electrode on a backside of the substrate, which is opposite to the first semiconductor layer. The planar gate electrode having the opening is disposed on a third surface portion of the low concentration channel forming region and a third surface portion of the high concentration channel forming region through the gate insulation film, each third surface portion which is exposed from the source region and the source contact region.
The above method provides the device, in which the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, in the device, the MOS transistor has high withstand voltage and low loss.
According to an eighth aspect of the present disclosure, a method for manufacturing a semiconductor device includes: forming a first semiconductor layer on a semiconductor substrate, wherein the semiconductor substrate has a first conductive type and a high impurity concentration, and wherein the first semiconductor layer includes a plurality of first impurity diffusion regions having the first conductive type and a plurality of second impurity diffusion regions having a second conductive type, which are alternately arranged so that the first semiconductor layer provides a drift region; forming a planar gate electrode on the first semiconductor layer through a gate insulation film; forming a channel forming region having the second conductive type on a first surface portion of the first semiconductor layer by using the planar gate electrode as a self-alignment member; forming a source region having the first conductive type disposed on a first surface portion of the channel forming region; forming a source contact region having the second conductive type disposed on a second surface portion of the channel forming region; forming an opening on the planar gate electrode by using a photo lithography etching method, wherein the opening corresponds to an anode electrode, which provides a Schottky barrier diode; forming an insulation film on whole area of the first semiconductor layer; removing a part of the insulation film, which corresponds to a source electrode and the anode electrode by using a photo lithography etching method; forming the source electrode on the source region and the source contact region; forming the anode electrode on a second surface portion of the first semiconductor layer, the second surface portion which is exposed from the channel forming region through the opening of the planar gate electrode; and forming a drain electrode on a backside of the substrate, which is opposite to the first semiconductor layer. The gate electrode is disposed on a third surface portion of the channel forming region through the gate insulation film, the third surface portion which is exposed from the source region and the source contact region.
The above method provides the device, in which the super junction MOS transistor and the Schottky barrier diode having the super junction construction are integrated, so that the diode has high withstand voltage and low loss. Further, in the device, the MOS transistor has high withstand voltage and low loss.
The above and other objects, features and advantages of the present invention will become more apparent from the following detailed description made with reference to the accompanying drawings. In the drawings:
FIGS. 4 to 6 are cross sectional views explaining an operation of the device in
This semiconductor device is a semiconductor device having a super junction MOS structure, and a super junction MOS transistor and a Schottky barrier diode are integrated. The MOS transistor is an N channel transistor.
A silicon layer 2 as a semiconductor layer is laminated on an N+ silicon substrate 1 as a high concentration semiconductor substrate of a first electric conductivity type. An impurity diffusive area 2a of an N type (first electric conductivity type) and an impurity diffusive area 2b of a P type (second electric conductivity type) as a drift area are adjacently alternately arranged in the silicon layer 2. Thus, the super junction structure is constructed by adjacently alternately arranging the N type impurity diffusive area 2a and the P type impurity diffusive area 2b.
An N− silicon layer 3 as a low concentration semiconductor layer of the first electric conductivity type is laminated on the silicon layer 2. A channel forming area (P well layer) 4 of the P type (second electric conductivity type) is formed in a surface layer portion of the N− silicon layer 3. A lower end of the channel forming area (P well layer) 4 reaches the impurity diffusive area 2b of the P type. Further, an N+ source area 5 is formed in the surface layer portion of the N− silicon layer 3 within the channel forming area 4. Further, a P+ source contact area 6 is formed in the surface layer portion of the N− silicon layer 3 within the channel forming area 4 so as to be adjacent to the N+ source area 5.
A gate electrode 8 is arranged on a part exposing the channel forming area 4 on an upper face of the N− silicon layer 3 through a gate oxide film 7 as a gate insulating film. A source electrode 9 is arranged in a part exposing the source area 5 and the source contact area 6 on the upper face of the N− silicon layer 3. The source electrode 9 is electrically connected to the N+ source area 5 and the P+ area 6 for a contact. A drain electrode 10 is arranged on a rear face of the N+ silicon substrate 1, and is electrically connected to the N+ silicon substrate 1. The super junction MOS transistor is constructed by such a structure.
Further, an anode electrode 20 constituting the Schottky barrier diode is arranged in a part exposing a low concentration area 3a of the N type on the upper face of the N− silicon layer 3. Thus, the super junction MOS (SJ-MOS) transistor and the Schottky barrier diode (SBD) are integrated.
At this time, the super junction structure is commonly used in the MOS transistor and the Schottky barrier diode in withstand voltage support.
In particular, the anode electrode 20 is arranged in the part exposing the low concentration area 3a of the N type between the adjacent channel forming areas 4 on the upper face of the N− silicon layer 3 within a transistor cell forming area. Namely, similar to the channel forming area 4 constituting the MOS transistor, SBD is constructed by forming the anode electrode 20 on the surface of the N− silicon layer 3 sandwiched by the channel forming area 4 constituting an adjacent separate MOS transistor. More particularly, an opening portion 8a is formed in the common gate electrode 8 within each cell within the transistor cell forming area. The anode electrode 20 is formed in the opening portion 8a. Further, the anode electrode 20 and the source electrode 9 are short-circuited within a chip.
As shown in
The operation of the semiconductor device of this embodiment mode will next be explained by using
As shown in
In this case, only the super junction MOS (SJ-MOS) transistor attains a turning-on state, and an electric current is flowed from the drain electrode 10 to the source electrode 9 through the N+ silicon substrate 1, the N type impurity diffusive area 2a, the low concentration area 3a (N− silicon layer 3) of the N type, an inverting layer formed in a part opposed to the gate electrode 8 in the channel forming area 4, and the N+ source area 5.
Further, as shown in
In this case, both the super junction MOS (SJ-MOS) transistor and the Schottky barrier diode attain a turning-off state, and a depletion layer is formed in the silicon layer 2 (a portion in which the N type impurity diffusive area 2a and the P type impurity diffusive area 2b are adjacently alternately arranged). Thus, withstand voltage is supported by the super junction structure.
Further, as shown in
In this case, only the Schottky barrier diode attains the turning-on state, and an electric current is flowed from the anode electrode 20 to the drain electrode 10 through the low concentration area 3a (N− silicon layer 3) of the N type, the N type impurity diffusive area 2a and the N+ silicon substrate 1. At this time, the built-in diodes D1, D2 have high forward voltages, and are not almost turned on. In other words, the impurity concentration of the N− silicon layer 3 is set such that the forward voltage of the Schottky barrier diode becomes lower than the forward voltages of the built-in diodes (PN diodes) D1, D2 (the impurity concentration of the N− silicon layer 3 is set to be low).
Thus, high withstand voltage and low loss can be formed with respect to the transistor and the diode by setting a structure in which the MOS transistor and the Schottky barrier diode are set to be parallel and a portion for supporting the withstand voltage is commonly used in the super junction. More particularly, with respect to the diode, the forward voltage can be reduced (low loss can be set). More precisely, the Schottky barrier diode (SBD) can be integrated without increasing the area of the power MOS transistor, and the withstand voltage is supported by the super junction (SJ). The MOS transistor and the Schottky barrier diode (SBD) can be set to high withstand voltage and low resistance. Further, carrier accumulation can be reduced (short-circuit breakdown restraint and noise reduction). Further, gate capacity can be reduced by an amount for forming the opening portion 8a in the gate electrode 8.
A manufacturing method will next be explained.
First, as shown in
Subsequently, as shown in
Thereafter, as shown in
As shown in
The following effects are obtained when the semiconductor device (a device for integrating SJ-MOS and SBD) of this structure is used in an inverter circuit as shown in
In
Here, since the Schottky barrier diode (SBD) can be formed with respect to the reflux diodes (Df1, Df2), carrier accumulation at a reverse restoring time can be restrained and the recovery electric current is reduced. Thus, short-circuit breakdown due to a passing-through electric current is also restrained.
Thus, both the power MOS transistor and the Schottky barrier diode (SBD) can be set to high withstand voltage and low loss. As its result, the power MOS transistor and a free wheel diode in a high withstand voltage inverter can be used as an integrated low loss device so that a system can be made compact and reduced in loss. In other words, the Schottky barrier diode (SBD) can be built-in without increasing the area of the power MOS transistor, and the number of parts can be reduced.
The following effects can be obtained in accordance with the above embodiment mode.
(1) The anode electrode 20 constituting the Schottky barrier diode is arranged in a part exposing the low concentration area 3a of the N type on the upper face of the silicon layer (low concentration semiconductor layer) 3, and the super junction MOS transistor and the Schottky barrier diode are integrated. Thus, since the Schottky barrier diode of the super junction structure is integrated with the super junction MOS transistor, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated.
(2) In particular, the anode electrode 20 constituting the Schottky barrier diode is arranged in a part exposing the low concentration area 3a of the N type between the adjacent channel forming areas 4 on the upper face of the N− silicon layer 3 within the transistor cell forming area. The super junction MOS transistor and the Schottky barrier diode are then integrated. Thus, the Schottky barrier diode can be integrated with the super junction MOS transistor of high withstand voltage and low loss without increasing an area. As its result, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated in a small area.
Therefore, the opening portion 8a is formed in the common gate electrode 8 within each cell within the transistor cell forming area, and the anode electrode 20 is formed in the opening portion 8a. Accordingly, the anode electrode 20 can be easily arranged in the transistor cell forming area, which is preferable from the viewpoint that no increase of an area is caused.
A modified example will next be explained.
In
Further, as shown in
Thus, widths W1, W2 of the areas 2a, 2b (column) and pitches P1, P2 of the MOS transistor and the Schottky barrier diode can be independently set (designed).
Further, as shown in
Further, as shown in
Furthermore, as shown in
Next, a second embodiment mode will be explained in accordance with the drawings with different points from the first embodiment mode as a center.
In
Further, an anode electrode 20 constituting the Schottky barrier diode is arranged in a part exposing the low concentration area 3a of the N type on the upper face of the N− silicon layer (low concentration semiconductor layer) 3. The super junction MOS transistor and the Schottky barrier diode are integrated. Accordingly, since the Schottky barrier diode of the super junction structure is integrated with the super junction MOS transistor, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated. In particular, the anode electrode 20 constituting the Schottky barrier diode is arranged in the part exposing the low concentration area 3a of the N type between the adjacent channel forming areas 4 on the upper face of the N− silicon layer 3 within the transistor cell forming area. The super junction MOS transistor and the Schottky barrier diode are integrated. Thus, the Schottky barrier diode can be integrated with the super junction MOS transistor of high withstand voltage and low loss without increasing an area. As its result, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated in a small area.
Further, the impurity concentration of the N− silicon layer 3 is set such that the forward voltage of the Schottky barrier diode becomes lower than the forward voltage of a built-in PN diode. Further, the anode electrode 20 and the source electrode 9 are short-circuited within a chip. Further, extending directions of the gate electrode 52 and the anode electrode 20 are perpendicular to the extending directions of the impurity diffusive area 2a of the N type and the impurity diffusive area 2b of the P type as a drift area in the silicon layer 2.
A manufacturing method will next be explained.
First, as shown in
Subsequently, as shown in
As shown in
In this embodiment mode, as explained by using
In a silicon layer (first semiconductor layer) 2 laminated on an N+ silicon substrate 1, an N type impurity diffusive area 2a and a P type impurity diffusive area 2b as a drift area are adjacently alternately arranged. A P type silicon layer (second semiconductor layer) 60 as a low concentration channel forming area is laminated on the silicon layer 2. An N well layer 61 reaching the N type impurity diffusive area 2a is formed in the silicon layer 60. A P type high concentration channel forming area 62 is formed in a surface layer portion of the silicon layer 60. An N+ source area 5 and a P+ source contact area 6 are formed within the high concentration channel forming area 62. A gate electrode 8 is arranged through a gate oxide film 7 on a part exposing the high concentration channel forming area 62 and a low concentration channel forming area 60a on the upper face of the silicon layer 60. A source electrode 9 is arranged in a part exposing the source area 5 and the source contact area 6 on the upper face of the silicon layer 60. Further, a drain electrode 10 is arranged on the rear face of the N+ silicon substrate 1. An anode electrode 20 constituting the Schottky barrier diode is arranged in a part exposing the well layer 61 on the upper face of the silicon layer 60. A super junction MOS transistor and the Schottky barrier diode are integrated. Accordingly, since the Schottky barrier diode of a super junction structure is integrated with the super junction MOS transistor, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated. In particular, the anode electrode 20 constituting the Schottky barrier diode is arranged in a part exposing the well layer 61 of the N type between adjacent high concentration channel forming area 62 and low concentration channel forming area 60a on the upper face of the silicon layer 60 within a transistor cell forming area. The super junction MOS transistor and the Schottky barrier diode are integrated. Thus, the Schottky barrier diode can be integrated with the super junction MOS transistor of high withstand voltage and low loss without causing an increase of an area. As its result, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated in a small area.
Further, an opening portion 8a is formed in the common gate electrode 8 within each cell within the transistor cell forming area, and the anode electrode 20 is formed in the opening portion 8a. Further, the impurity concentration of the well layer 61 is set such that the forward voltage of the Schottky barrier diode becomes lower than the forward voltage of a built-in PN diode. Further, the anode electrode 20 and the source electrode 9 are short-circuited within a chip.
As an operation, only the super junction MOS transistor attains a turning-on state by adjusting a gate electric potential in a state in which a positive bias voltage is applied as the voltage between the drain and the source. An electric current is then flowed from the drain electrode 10 to the source electrode 9 through the substrate 1, the drift area (2a), the well layer 61, an inverting layer formed in a part opposed to the gate electrode 8 in the high concentration and low concentration channel forming areas 62, 60a, and the source area 5. Further, when the voltage between the gate and the source is set to 0 volt in a state in which a positive bias voltage is applied as the voltage between the drain and the source, both the super junction MOS transistor and the Schottky barrier diode attain a turning-off state, and a depletion layer is formed in the silicon layer 2 (a portion in which the impurity diffusive area 2a of the N type and the impurity diffusive area 2b of the P type are adjacently alternately arranged). Thus, withstand voltage is supported by the super junction structure. Further, when a negative bias voltage is applied as the voltage between the drain and the source and the voltage between the gate and the source is set to 0 volt, only the Schottky barrier diode attains the turning-on state, and an electric current is flowed from the anode electrode 20 through the well layer 61, the drift area (2b) and the substrate 1.
Thus, high withstand voltage and low loss can be formed by setting a structure in which the MOS transistor and the Schottky barrier diode are set to be parallel and a portion for supporting the withstand voltage is commonly used in the super junction.
A manufacturing method will next be explained.
First, as shown in
Subsequently, as shown in
Subsequently, as shown in
Thereafter, as shown in
In this embodiment mode, as explained by using
In this embodiment mode, a channel forming area (P well layer) 4 of the P type, an N+ source area 5 and a P+ area 6 for a contact are directly formed in an N type silicon layer 70 without arranging the surface N− layer 3 in
In the silicon layer (semiconductor layer) 70 laminated on an N+ silicon substrate 1, an N type impurity diffusive area 2a and a P type impurity diffusive area 2b as a drift area are adjacently alternately arranged. Further, the P type channel forming area 4 is formed in a surface layer portion on the upper face of the silicon layer 70. The N type source area 5 and the P type source contact area 6 are formed within the channel forming area 4. A gate electrode 8 is arranged through a gate oxide film 7 on a part exposing the channel forming area 4 on the upper face of the silicon layer 70. A source electrode 9 is arranged in a part exposing the source area 5 and the source contact area 6 on the upper face of the silicon layer 70, and a drain electrode 10 is arranged on the rear face of the substrate 1. An anode electrode 20 constituting the Schottky barrier diode is arranged in a part exposing the impurity diffusive area 2a of the N type as a drift area on the upper face of the silicon layer 70. A super junction MOS transistor and the Schottky barrier diode are integrated. Accordingly, since the Schottky barrier diode of a super junction structure is integrated with the super junction MOS transistor, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated. In particular, the anode electrode 20 constituting the Schottky barrier diode is arranged in the part exposing the impurity diffusive area 2a of the N type as the drift area between the adjacent channel forming areas 4 on the upper face of the silicon layer 70 within a transistor cell forming area. The super junction MOS transistor and the Schottky barrier diode are integrated. Thus, the Schottky barrier diode can be integrated with the super junction MOS transistor of high withstand voltage and low loss without increasing an area. As its result, the diode can be set to high withstand voltage and low loss, and this diode and the MOS transistor of high withstand voltage and low loss can be integrated in a small area.
Further, an opening portion 8a is formed in the common gate electrode 8 within each cell within the transistor cell forming area, and the anode electrode 20 is formed in the opening portion 8a. Further, the impurity concentration of the impurity diffusive area 2a of the N type as the drift area is set such that the forward voltage of the Schottky barrier diode becomes lower than the forward voltage of a built-in PN diode. Further, the anode electrode 20 and the source electrode 9 are short-circuited within a chip. Further, extending directions of the gate electrode 8 and the anode electrode 20 are perpendicular to the extending directions of the impurity diffusive area 2a of the N type and the impurity diffusive area 2b of the P type as the drift area in the silicon layer 70.
As an operation, only the super junction MOS transistor attains a turning-on state by adjusting a gate electric potential in a state in which a positive bias voltage is applied as the voltage between the drain and the source. An electric current is then flowed from the drain electrode 10 to the source electrode 9 through the substrate 1, the drift area (2a), an inverting layer formed in a part opposed to the gate electrode 8 in the channel forming area 4, and the source area 5. Further, when the voltage between the gate and the source is set to 0 volt in a state in which a positive bias voltage is applied as the voltage between the drain and the source, both the super junction MOS transistor and the Schottky barrier diode attain a turning-off state, and a depletion layer is formed in the silicon layer 70 (a portion in which the impurity diffusive area 2a of the N type and the impurity diffusive area 2b of the P type are adjacently alternately arranged). Thus, withstand voltage is supported by the super junction structure. Further, when a negative bias voltage is applied as the voltage between the drain and the source and the voltage between the gate and the source is set to 0 volt, only the Schottky barrier diode attains the turning-on state, and an electric current is flowed from the anode electrode 20 through the drift area (2a) and the substrate 1.
Thus, high withstand voltage and low loss can be formed by setting a structure in which the MOS transistor and the Schottky barrier diode are set to be parallel and a portion for supporting the withstand voltage is commonly used in the super junction.
A manufacturing method will next be explained.
First, as shown in
Subsequently, as shown in
Further, as shown in
In this embodiment mode, as explained by using
In each of the above embodiment modes, the stripe shape is set as a planar shape with respect to the PN junction using the N type impurity diffusive area 2a and the P type impurity diffusive area 2b in the silicon layers 2, 70. However, a hexagonal shape may be also formed as shown in
Further, the N channel transistor has been explained so far, but the invention may be also applied to a P channel transistor. In this case, the first electric conductivity type becomes the P type, and the second electric conductivity type becomes the N type.
While the invention has been described with reference to preferred embodiments thereof, it is to be understood that the invention is not limited to the preferred embodiments and constructions. The invention is intended to cover various modification and equivalent arrangements. In addition, while the various combinations and configurations, which are preferred, other combinations and configurations, including more, less or only a single element, are also within the spirit and scope of the invention.
Number | Date | Country | Kind |
---|---|---|---|