Embodiments of the invention are in the field of semiconductor metrology and, in particular, systems and approaches for semiconductor metrology and surface analysis using Secondary Ion Mass Spectrometry (SIMS).
Secondary ion mass spectrometry (SIMS) is a technique used to analyze the composition of solid surfaces and thin films by sputtering the surface of the specimen with a focused primary ion beam and collecting and analyzing ejected secondary ions. The mass/charge ratios of these secondary ions are measured with a mass spectrometer to determine the elemental, isotopic, or molecular composition of the surface to a depth of 1 to 2 nanometers. Due to the large variation in ionization probabilities among different materials, SIMS is generally considered to be a qualitative technique, although quantitation is possible with the use of standards. SIMS is the most sensitive surface analysis technique, with elemental detection limits ranging from parts per million to parts per billion.
Generally, SIMS requires a high vacuum with pressures below 10−4 Pa. High vacuum is needed to ensure that secondary ions do not collide with background gases on their way to the detector (i.e., the mean free path of gas molecules within the detector must be large compared to the size of the instrument), and it also prevents surface contamination that otherwise may occur by adsorption of background gas particles during measurement.
Three basic types of ion guns are employed in SIMS analysis. In one, ions of gaseous elements are usually generated with duoplasmatrons or by electron ionization, for instance noble gases (40Ar+, Xe+), oxygen (16O−, 16O2+, 16O2−), or even ionized molecules such as SF5+ (generated from SF6) or C60+ (fullerene). This type of ion gun is easy to operate and generates roughly focused but high current ion beams. A second source type, the surface ionization source, generates 133Cs+ primary ions. Cesium atoms vaporize through a porous tungsten plug and are ionized during evaporation. Depending on the gun design, fine focus or high current can be obtained. A third source type, the liquid metal ion gun (LMIG), operates with metals or metallic alloys, which are liquid at room temperature or slightly above. The liquid metal covers a tungsten tip and emits ions under influence of an intense electric field. While a gallium source is able to operate with elemental gallium, recently developed sources for gold, indium and bismuth use alloys which lower their melting points. The LMIG provides a tightly focused ion beam (less than 50 nanometers) with moderate intensity and is additionally able to generate short pulsed ion beams. It is therefore commonly used in static SIMS devices.
The choice of the ion species and ion gun respectively depends on the required current (pulsed or continuous), the required beam dimensions of the primary ion beam and on the sample which is to be analyzed. Oxygen primary ions are often used to investigate electropositive elements due to an increase of the generation probability of positive secondary ions, while cesium primary ions often are used when electronegative elements are being investigated. For short pulsed ion beams in static SIMS, LMIGs are most often deployed for analysis. LMIGs can be combined with either an oxygen gun or a cesium gun during elemental depth profiling, or with a C60+ or gas cluster ion source during molecular depth profiling.
Depending on the SIMS type, there are three basic analyzers available: sector, quadrupole, and time-of-flight. A sector field mass spectrometer uses a combination of an electrostatic analyzer and a magnetic analyzer to separate the secondary ions by their mass to charge ratio. A quadrupole mass analyzer separates the masses by resonant electric fields, which allow only the selected masses to pass through. The time of flight mass analyzer separates the ions in a field-free drift path according to their velocity. Since all ions possess the same kinetic energy, the velocity and therefore time of flight varies according to mass. The time of flight mass analyzer requires pulsed secondary ion generation using either a pulsed primary ion gun or a pulsed secondary ion extraction. The time of flight mass analyzer is the only analyzer type able to detect all generated secondary ions simultaneously, and is the standard analyzer for static SIMS instruments.
In the field of surface analysis, it is usual to distinguish static SIMS and dynamic SIMS. Static SIMS is the process involved in surface atomic monolayer analysis, or surface molecular analysis, usually with a pulsed ion beam and a time of flight mass spectrometer. Meanwhile, dynamic SIMS is the process involved in bulk analysis, closely related to the sputtering process. Dynamic SIMS employs a DC primary ion beam and a magnetic sector or quadrupole mass spectrometer.
SIMS is a very powerful technique. However, advances are needed in the area of SIMS measurement equipment, systems, and methodologies.
Embodiments of the present invention includes systems and approaches for semiconductor metrology and surface analysis using Secondary Ion Mass Spectrometry (SIMS).
In an embodiment, a secondary ion mass spectrometry (SIMS) system includes a sample stage. A primary ion beam is directed to the sample stage. An extraction lens is directed at the sample stage. The extraction lens is configured to provide a low extraction field for secondary ions emitted from a sample on the sample stage. A magnetic sector spectrograph is coupled to the extraction lens along an optical path of the SIMS system. The magnetic sector spectrograph includes an electrostatic analyzer (ESA) coupled to a magnetic sector analyzer (MSA).
In an embodiment, a method of measurement and control of the surface potential of a sample involves measuring kinetic energy of charged particles emitted from a surface of a sample. The method also involves determining a shift in kinetic energy of the charged particles. The surface potential of the surface of the sample is changed in response the shift in kinetic energy of the charged particles.
In an embodiment, a method of determining wafer backside contact resistance involves measuring a gap distance value of a surface of a wafer based on a comparison of a main capacitive sensor electrode driven with a first drive signal and a compensating capacitive sensor electrode driven with a second drive signal that is amplitude or phase shifted as compared to the first drive signal. A value of the second drive signal is measured. The value of the second drive signal is calibrated to a reference impedance standard to determine an impedance value of the wafer to ground. A contact resistance value is determined for the surface of the wafer based on the gap distance value and the impedance value of the wafer to ground.
Systems and approaches for semiconductor metrology and surface analysis using Secondary Ion Mass Spectrometry (SIMS) are described. In the following description, numerous specific details are set forth, such as SIMS analysis techniques and system configurations, in order to provide a thorough understanding of embodiments of the present invention. It will be apparent to one skilled in the art that embodiments of the present invention may be practiced without these specific details. In other instances, well-known features such as entire semiconductor device stacks are not described in detail in order to not unnecessarily obscure embodiments of the present invention. Furthermore, it is to be understood that the various embodiments shown in the Figures are illustrative representations and are not necessarily drawn to scale.
In a first aspect, embodiments of the present invention are directed to systems and methods for characterization and process control of structures on semiconductor wafers during manufacturing using Secondary Ion Mass Spectrometry (SIMS).
To provide context, state of the art semiconductor manufacturing entails many hundreds of process operations. Each process operations are subject to processing variations which can lead to variation and degradation of the performance of the finished device. As such, many measurements and inspections are performed during the manufacturing process to both ensure that a manufacturing operation has been executed correctly and within specification and also to provide feedforward and feedback to control the manufacturing process. Process control requires several key attributes that enable its effectiveness.
First, the cost of a measurement or inspection must be consistent with the economical manufacturing of devices. Practically, this means that the cost of a tool, the cost of consumables, the cost of ownership (including maintenance, calibration and other costs), its useful lifetime, the time required to take a measurement and the labor costs associated with its effective use are consistent with the manufacturing environment. Perhaps most importantly, it is critical that the characterization be nondestructive, as the cost of a semiconductor wafer during processing can be very high, and techniques which require destructive testing are not necessarily viable.
Second, the inspection and measurement must measure a sample which is directly relevant to the process control requirements. While techniques that can only measure “monitor” wafers, i.e., those wafers that have only undergone one or a few process operations, can be useful for tool qualification or coarse quality control, effective process control requires that the measured structures are as similar to actual device structures as possible and that measurement sampling can be as frequent as possible compared to the rate of process variation and drift.
Third, and perhaps most importantly, the inspection or measurement operation must have the desired information content, i.e., the required relevancy, resolution, accuracy and precision, required for process control.
To provide further context, Secondary Ion Mass Spectrometry (SIMS) is a well-known materials characterization technique which is capable of determining the depth profile of elemental composition with great accuracy and precision. Because of this unique capability, SIMS is widely used in materials science and analytical laboratory settings. While SIMS is currently used in an “offline” mode in semiconductor manufacturing, its use in “inline” process control is currently not viable due to its inability to address the practical issues outlined above. What is needed, therefore, is a Secondary Ion Mass Spectrometry system which provides the well known capabilities of SIMS while addressing the gaps which prevent its use in inline process control.
In order to satisfy the requirements of an in-line semiconductor manufacturing environment, several gaps in current SIMS designs must be addressed. Such gaps include particular challenges associated with measurement on typical product wafers, the time it takes to make the measurements, the availability/uptime of the tool (e.g., including time for calibration and verification), and the costs associated with the maintenance of the tool. Design specifics addressing one or more of the above issues are described below, in accordance with one or more embodiments of the present invention.
With respect to measurement on product wafers, performing a SIMS measurement on a product wafer entails three challenges that constrain the design. First, measurements on product wafers must typically be confined to a small designated area, such as a 50 μm by 50 μm pad. Second, at the same time, the manufacturer is typically interested in changes of composition over very small changes in depth. Third, there will be an unpredictable grounding path to the measurement site. In cases where the grounding is poor or non-existent the wafer will charge during the SIMS measurement, which leads to several problems including a deflection of the primary beam away from the intended site, a decrease in detected secondary ion signal, and a reduction in the ability to correctly identify and resolve secondary ion masses.
Addressing one or more of the above issues concerning measurements performed on product wafer, in accordance with an embodiment of the present invention, a SIMS approach described herein involves use of a low extraction Voltage at a secondary extraction lens of a SIMS measurement system. In particular, only a very weak electric field is used between the collection lens and the sample under measurement. Such an approach is contrary to a typical SIMS design which uses a strong electric field between the extraction lens and the sample to attract the secondary ions towards the lens and boost the number of collected ions. In one embodiment, the extraction field threshold is at most approximately 10 Volts/mm (as an absolute value).
Referring to
Referring again to
Referring again to
Referring again to
In one embodiment, referring again to system 100, by using a low extraction Voltage between the extraction lens 108 and the sample 102, as much as 80% of a signal otherwise obtainable by a typical SIMS measurement is sacrificed. However, in return, it is much easier to accurately place the primary beam. For example, in systems where the extraction field is strong, the primary beam is deflected as much as tens or even hundreds of microns as it passes through the field, which means that the aim of the primary beam must be altered to compensate. This leads to a tricky control problem with typical SIMS measurements, making the precise rastering of the beam in a small 50 μm area very difficult.
Such deflection of the primary beam by the extraction field is more severe the lower the energy of the primary ions. Accordingly, under typical or conventional SIMS operation, there is incentive to maintain a high primary energy in order to minimize the beam deflection. However, high-energy primary beams lead to two effects that degrade the depth resolution. First, a high-energy primary beam penetrates more deeply into the sample leading to ions being created over a range of depths rather than at the surface. Second, the higher energies can drive surface atoms of the sample deep into the substrate, essentially smearing the material over depth. In an embodiment, in contrast to high-energy primary beams used in typical SIMS measurements, fine depth resolution required by the semiconductor industry is benefited from use of a low-energy primary beam. Accordingly, in one embodiment, the above described advantage of using a low-extraction field design is even greater when also designing for maximum depth resolution since otherwise severe deflection of a low-energy primary beam is mitigated by the low-extraction field design.
Additionally, in an embodiment, using a low extraction field makes it easier to deal with sample charging in cases of poor grounding. For example, reducing the field above the sample enables the use of a low-energy electron flood to neutralize the charge. By contrast, in a more typical SIMS design using a strong extraction field, a charge-compensating beam must be run at high energy and precisely steered in order to overcome the deflection by the field and to place the beam accurately at the measurement site, which is a vastly more complicated process.
Referring to
With respect to throughput, the time needed to make a set of measurements on a wafer is a critical factor in the economical application of a measurement technique. In accordance with one or more embodiment of the present invention several secondary ion species are measured in parallel for increased throughput.
To provide context for throughput considerations, common SIMS designs can be grouped into three categories: (1) time-of-flight (TOF), (2) quadrupole detection, and (3) magnetic sector detection. In TOF SIMS, the primary beam is pulsed and the sputtered secondary ion species are sorted according to the time it takes for them to reach a detector. TOF SIMS has the advantage that a wide range of secondary ion species are collected in parallel, but the pulsed nature of the measurement reduces the measurement speed. In the quadrupole approach, the primary beam is applied continuously, but the detector can only measure one ion species at a time (although switching from one species to another can be done quickly). Finally, the third common approach, magnetic sector, separates the ion species according to mass/charge using a combination of electric and magnetic fields. As with the quadrupole system, the primary beam is on continuously. However, in typical magnetic sector systems the spectrometer uses a single detector, which again limits the detection to a single species at a time.
None of the above conventional approaches provide the speed and parallel detection possibly needed for the semiconductor manufacturing environment. By contrast, in accordance with one or more embodiments of the present invention, a magnetic sector spectrograph is used. Like the spectrometer, a magnetic sector spectrograph separates the various mass species by sending the beam through a magnetic field. However, the spectrograph design focuses the different masses along a line, or “focal plane.” By placing multiple detectors at various positions along the focal plane, different masses can be measured in parallel. In a particular embodiment, a SIMS system design includes 10 different detectors, enabling measurement of a vast majority of species present in any single semiconductor measurement. It is to be appreciated that fewer than or greater than 10 detectors may be used. It is also to be appreciated that although the entire available range of masses may not be collected in parallel in such an arrangement, as is the case for TOF SIMS, the multi-detector approach is not a detriment since the number of species typically used in any given semiconductor process is limited and the manufacturer usually has a good notion of which species are likely to be present. It should also be noted that the plurality of detectors can be mounted onto translation stages so that their locations along the focal plane, and hence the collected species, can be tailored according to the needs of a specific measurement.
With respect to availability and serviceability, due to the time-critical nature of process control measurements, it is essential that the tool be available for use at the time when a wafer becomes available for measurement. For this reason, it is important that the mean time between failures of the tool is long and the mean time to repair is short. It is further required that the measurement tool is in calibration at all times. Accordingly, the SIMS tool must be capable of checking and updating its calibration automatically.
In accordance with one or more embodiments herein, several design aspects of a SIMS system are tailored to address such issues concerning availability and serviceability. In one embodiment, to improve the overall stability of the hardware, a monolithic system structure is implemented. For example, every major sub-system, such as the extraction optics, the lower primary column, and the mass spectrometer, may be rigidly mounted to one another. There may be a tradeoff with respect to alignment flexibility, but the advantages include a resulting system that can hold on to an alignment more reliably. In addition, in one embodiment, as depicted in
In accordance with one or more embodiments herein, to maintain measurement consistency, several internal checks and calibrations are added to a SIMS system. Such internal checks and calibrations may include one or more of (1) a Faraday cup, as depicted in
In an embodiment, a set of internal reference samples is included in a SIMS system. The internal samples can be automatically moved to the measurement site to periodically check various crucial aspects of the beam. These may include layered materials of predetermined thickness to monitor the primary sputtering rates and raster uniformity, patterned boxes of known dimensions to check the raster size and position, and simple chips of various composition to monitor the overall signal strengths. Many of the tests can be performed at a multitude of primary energies and currents. As an example,
Referring to
In a second aspect, one or more embodiments involve measuring the surface potential of a sample by observing the shift in kinetic energy of emitted charged particles or ions. One or more embodiments involve measuring and controlling the surface potential by using shifts of kinetic energy as a feedback mechanism.
To provide context, secondary ions are generated by removing atoms from a surface, some of which are ionized. The secondary ions are emitted with a range of velocities, or equivalently, a range of kinetic energies. As the ions travel along an optical path, their kinetic energy at an arbitrary point A will be the sum of the initial kinetic energy (KE), the surface potential of the sample, the local potential at A, and any KE contribution from electrodynamic elements (e.g., buncher, cyclotron, etc.). Determining the KE distribution and comparing it to a distribution from a reference sample with known surface potential provides a measure of the sample potential.
A primary reason to measure surface potential is charging of insulating samples caused by an unequal flow of positive and negative charges to the sample. Secondary ions may be formed by impinging atoms, ions, electrons, or photons onto a surface. Ions and electrons add charge to the surface, while any secondary charged particles emitted from the surface removes charge. If the sample is electrically conducting, it will dissipate any imbalance of charge transport. Insulating overlayers (e.g., which in some cases are laterally patterned) may charge, and the entire sample may charge if it is not electrically connected to an electrode at a stable potential. Furthermore, the surface potential may be measured as material is removed from the surface, possibly exposing variations in sample conductivity or in the emission of charged particles.
In accordance with an embodiment of the present invention, the emitted secondary ions are passed through an electrostatic analyzer so that ions are dispersed in space according to their energies. The complete KE distribution is measured by varying the electric field in the ESA, such that the dispersed ion beam travels across an ion detector 120. A change in KE can be measured while intercepting only the low and/or high tails of the energy distribution by using one or two detectors positioned at the tails. In one embodiment, the slope of a tail is measured by slightly modulating the ESA deflecting field. To preserve the position of the main transmitted beam, the apparatus may have an arrangement of two ESAs with the ion detector(s) 120 there between. In one such embodiment, the second ESA, or the second ESA in conjunction with a matching lens, has an equal and opposite dispersive strength to that of the first ESA.
Particular embodiments of the present invention are directed to measurement and control of the surface potential of a sample by observing the shift in kinetic energy of emitted charged particles and by using shifts of kinetic energy as a feedback mechanism. It is to be appreciated that although exemplary embodiments are described in association with SIMS measurements, embodiments described herein may be applicable to other measurement and metrology techniques and systems.
One or more embodiments are directed to a system of at least one electrostatic analyzer with an energy slit that is equipped with ion current sensors. One or more embodiments are directed to a system and/or approach for measuring energy distribution and energy shift of the total secondary charged particles transported from a sample surface prior to a mass analyzer. One or more embodiments are directed to implementation of an electrostatic analyzer and energy slit feedback system to monitor surface charging. One or more embodiments are directed to utilization of an active control system to adjust the surface potential. In an embodiment, the system of at least one electrostatic analyzer with an energy slit that is equipped with ion current sensors, the system and/or approach for measuring energy distribution and energy shift of the total secondary charged particles transported from a sample surface prior to a mass analyzer, and the electrostatic analyzer and energy slit feedback system implemented to monitor surface charging are used together as a feedback system for surface potential changes.
In an embodiment applicable to SIMS measurements in which the main ion beam is sent through a mass spectrometer, it is often analytically desirable to reject secondary ions which originate near the edge of the eroded area, since these can confound a depth profile. The complete KE distribution may be measured while the main beam is rejected. In one embodiment, the tails of the distribution are measured while the main beam should travel through the mass spectrometer.
Referring to
Referring to
Referring again to
Referring again to
Referring to
Referring again to
In an embodiment, the high energy slit sensor signal can in turn be used to monitor the effect of a charge neutralization system (for positive secondary ions). For negative secondary ions or electrons, a positive surface potential results in a shift of the energy distribution toward the low-energy slit sensor and may in the extreme effectively suppress secondary ion emission from the sample surface altogether (as the negative charged particles are attracted to the positive sample potential).
Referring to
In an embodiment, if the sample surface accumulates a negative potential, positive secondary ions will shift toward apparent lower secondary ion energy. This shift may occur when the overall sample potential is changes from positive to less positive potential. The cause of such shifts may be due to one or more of the following factors: (a) an intentional sample bias used to reject low-energy secondary ions, (b) if a constant positive surface potential is induced on a semi-insulating sample and the sample is irradiated with higher energy electrons that cause a net negative surface charge, and/or (c) the overall sample bias is set to a more negative potential for a conducting sample to reject low-energy secondary ions from the measurement.
Referring to
Referring to
Referring to
Referring to
Referring to
Thus, embodiments include approaches to controlling the surface potential of a sample. In an embodiment, the potential at the sample surface can be controlled using one or more of: (1) adjusting the bias voltage of the sample substrate (described in greater detail below, in association with
Referring to
Referring to
Referring to
In a third aspect, embodiments of the present invention are directed to methods for determining wafer backside contact resistance using multiple capacitive height sensors.
To provide context, in metrology equipment for semiconductor wafers it is common to use either charged particle (electrons/ions) beams as a primary exciting source, or measure the properties of charged particles that are emitted from the wafer, or both. Charging of the wafer can cause either errors in measuring the properties of the emitted particles or cause the primary charged particle to be deflected into neighboring regions causing damage to these areas. To keep the wafer from charging it is common to make contact to the backside of the wafer with a conductive electrode. However, in some instances, due to contamination on the electrode or insulating films on the back of the wafer, there is a high resistance between the electrode and the wafer. It may be desirable to measure the backside contact resistance in order to be assured that it is safe to apply an associated primary ion or electron beam to the sample.
In accordance with an embodiment of the present invention, approaches for measuring a contact resistance by using multiple capacitive height sensors are described. To exemplify the concepts described herein, a case of a single sensor being used to measure the height to a well-grounded wafer is first considered. The sensor includes a parallel plate electrode that is within sensing distance to the wafer. The structure forms a parallel plate capacitor where one plate is the sensor and the other is the wafer. If an AC voltage is applied to the sensor, then current flows across the gap between the plates. The amount of current that flows across the gap is determined by the voltage, the area of the plates, the material that separates the plates, and the distance between the plates.
The relevant equations to describe the current are: iac=x*C*V, where iac=ac current (in amps), C=capacitance (in farads), V=voltage, and x is a constant that depends only on the ac frequency. Capacitance (C) in turn is defined as: C=K*E0*A/D, where C=capacitance (in farads), K=the dielectric constant of the material between the plates (e.g., Air=1.0), E0=permittivity of free space (a constant), A=area of the plates (in square meters), D=distance between the plates (in meters). Thus, if the area of the sensor is maintained as constant, the distance (D) is proportional to the voltage (V) divided by the current (iac). For an AC voltage, this is directly proportional to the impedance of the circuit.
The control electronic for the sensor can be implemented several ways. For example, some capacitive sensors hold the current constant and allow the voltage to vary. These are called constant current capacitive sensors. Other capacitive sensors hold the voltage constant and allow the current to vary. These are constant voltage designs. There is no inherent advantage of one design over the other.
The above description assumes that the wafer is well grounded to the measurement electronics such that the impedance that is measured is due to the sensor to wafer gap. If the wafer is not well grounded, then the sum of the impedance due to the sensor to wafer gap and the impedance of the wafer to ground is what is measured. This, unfortunately, results in a distance being reported that is the sum of the wafer to sensor gap and the error from the wafer impedance. Approaches for using a second sensor or compensating electrode to minimize the wafer to ground current have been described for reducing the error in the distance measurement. The general idea is to feed the second electrode with an AC voltage that is amplitude and/or phase shifted version of the drive signal that is fed to the main sensor electrode. When the net current of the two electrodes is zero then the value from the main electrode is an accurate measure of the gap distance.
It is to be appreciated that, in accordance with an embodiment of the present invention, it is of interest to further determine the value of the signal being driven to the compensating electrode. The value is a measure of the wafer impedance to ground. By determining the signal and calibrating it with known reference impedance standards added between ground and a conductive wafer, the signal can be calibrated such that an unknown contact resistance can be determined.
In accordance with an embodiment of the present invention, there are several options for performing a measurement of a compensating electrode signal. In a first embodiment, an approach involving drive of a compensating electrode with a 180 degree shifted version of the main electrode signal. The amplitude is adjusted until the net current is zero (or until the distance measured by the main electrode is minimized). The amplitude of the voltage on the compensating electrode can then be calibrated to the impedance. In a second embodiment, the distance indicated by the main sensor is measured as the compensating electrode is being driven by a phase shifted version of the main signal. The distances are plotted for a number of different phase angles and a curve fitting algorithm is used to determine the phase angle for the minimum distance. The obtained phase angle is then calibrated to the impedance. In a third embodiment, the distance of the compensating electrode to the wafer or the exposed area of the compensating electrode is varied. The distance on the main electrode is measured to determine the minimum and, thus, a value is obtained that can be calibrated to the impedance.
Embodiments of the present invention may be provided as a computer program product, or software, that may include a machine-readable medium having stored thereon instructions, which may be used to program a computer system (or other electronic devices) to perform a process according to the present invention. A machine-readable medium includes any mechanism for storing or transmitting information in a form readable by a machine (e.g., a computer). For example, a machine-readable (e.g., computer-readable) medium includes a machine (e.g., a computer) readable storage medium (e.g., read only memory (“ROM”), random access memory (“RAM”), magnetic disk storage media, optical storage media, flash memory devices, etc.), a machine (e.g., computer) readable transmission medium (electrical, optical, acoustical or other form of propagated signals (e.g., infrared signals, digital signals, etc.)), etc.
The exemplary computer system 1500 includes a processor 1502, a main memory 1504 (e.g., read-only memory (ROM), flash memory, dynamic random access memory (DRAM) such as synchronous DRAM (SDRAM) or Rambus DRAM (RDRAM), etc.), a static memory 1506 (e.g., flash memory, static random access memory (SRAM), etc.), and a secondary memory 1518 (e.g., a data storage device), which communicate with each other via a bus 1530.
Processor 1502 represents one or more general-purpose processing devices such as a microprocessor, central processing unit, or the like. More particularly, the processor 1502 may be a complex instruction set computing (CISC) microprocessor, reduced instruction set computing (RISC) microprocessor, very long instruction word (VLIW) microprocessor, processor implementing other instruction sets, or processors implementing a combination of instruction sets. Processor 1502 may also be one or more special-purpose processing devices such as an application specific integrated circuit (ASIC), a field programmable gate array (FPGA), a digital signal processor (DSP), network processor, or the like. Processor 1502 is configured to execute the processing logic 1526 for performing the operations discussed herein.
The computer system 1500 may further include a network interface device 1508. The computer system 1500 also may include a video display unit 1510 (e.g., a liquid crystal display (LCD) or a cathode ray tube (CRT)), an alphanumeric input device 1512 (e.g., a keyboard), a cursor control device 1514 (e.g., a mouse), and a signal generation device 1516 (e.g., a speaker).
The secondary memory 1518 may include a machine-accessible storage medium (or more specifically a computer-readable storage medium) 1531 on which is stored one or more sets of instructions (e.g., software 1522) embodying any one or more of the methodologies or functions described herein. The software 1522 may also reside, completely or at least partially, within the main memory 1504 and/or within the processor 1502 during execution thereof by the computer system 1500, the main memory 1504 and the processor 1502 also constituting machine-readable storage media. The software 1522 may further be transmitted or received over a network 1520 via the network interface device 1508.
While the machine-accessible storage medium 1531 is shown in an exemplary embodiment to be a single medium, the term “machine-readable storage medium” should be taken to include a single medium or multiple media (e.g., a centralized or distributed database, and/or associated caches and servers) that store the one or more sets of instructions. The term “machine-readable storage medium” shall also be taken to include any medium that is capable of storing or encoding a set of instructions for execution by the machine and that cause the machine to perform any one or more of the methodologies of the present invention. The term “machine-readable storage medium” shall accordingly be taken to include, but not be limited to, solid-state memories, and optical and magnetic media.
Thus, systems and approaches for semiconductor metrology and surface analysis using Secondary Ion Mass Spectrometry (SIMS) have been described.
In an embodiment, a secondary ion mass spectrometry (SIMS) system includes a sample stage. A primary ion beam is directed to the sample stage. An extraction lens is directed at the sample stage. The extraction lens is configured to provide a low extraction field for secondary ions emitted from a sample on the sample stage. A magnetic sector spectrograph is coupled to the extraction lens along an optical path of the SIMS system. The magnetic sector spectrograph includes an electrostatic analyzer (ESA) coupled to a magnetic sector analyzer (MSA).
In one embodiment, the sample stage includes a Faraday cup.
In one embodiment, the SIMS system further includes a plurality of detectors spaced along a plane of the magnetic sector spectrograph.
In one embodiment, the plurality of detectors is for detecting a corresponding plurality of different species from a beam of the secondary ions emitted from the sample.
In one embodiment, the SIMS system further includes a first additional ESA coupled along the optical path of the SIMS system, between the extraction lens and the ESA of the magnetic sector spectrograph, and a second additional ESA coupled along the optical path of the SIMS system, between the first additional ESA and the ESA of the magnetic sector spectrograph.
In one embodiment, the first additional ESA is configured to spread a beam of the secondary ions emitted from the sample, and wherein the second additional ESA is configured to concentrate the beam of the secondary ions received from the first additional ESA.
In one embodiment, the SIMS system further includes one or more slits along the optical path of the SIMS system, between the first additional ESA and the second additional ESA.
In one embodiment, the first additional ESA, the second additional ESA, and the one or more slits are included in a charge compensation system of the SIMS system.
In one embodiment, the first additional ESA and the second additional ESA together direct the optical path of the SIMS system from above the sample stage to below the sample.
In one embodiment, a magnet of the MSA is located below the sample stage.
In one embodiment, the low extraction field has an absolute value of at most approximately 10 Volts/mm.
In one embodiment, the SIMS system further includes a transfer robot coupled to the sample stage.
In one embodiment, the SIMS system further includes a receptacle coupled to the transfer robot, the receptacle comprises calibration standards.
In an embodiment, a method of measurement and control of the surface potential of a sample involves measuring kinetic energy of charged particles emitted from a surface of a sample. The method also involves determining a shift in kinetic energy of the charged particles. The surface potential of the surface of the sample is changed in response the shift in kinetic energy of the charged particles.
In one embodiment, the surface potential of the surface of the sample comprises adjusting a bias voltage of an electrode supporting the sample.
In one embodiment, changing the surface potential of the surface of the sample comprises directing a beam of electrons at the surface of the sample.
In one embodiment, directing the beam of electrons at the surface of the sample comprises varying a current delivered to the surface of the sample.
In one embodiment, directing the beam of electrons at the surface of the sample comprises varying an impact energy of the beam of electrons at the surface of the sample.
In one embodiment, changing the surface potential of the surface of the sample comprises directing photons of variable intensity to the sample surface.
In one embodiment, directing photons of variable intensity to the sample surface comprises generating charge carriers in the sample to vary a conductivity of the sample.
In one embodiment, directing photons of variable intensity to the sample surface comprises emitting photoelectrons from the sample to drive a sample potential to more positive.
In one embodiment, changing the surface potential of the surface of the sample comprises directing photons of variable intensity away from the sample surface.
In one embodiment, the method further includes, subsequent to changing the surface potential of the surface of the sample, performing a secondary ion mass spectrometry (SIMS) measurement of the surface of the sample.
In an embodiment, a method of determining wafer backside contact resistance involves measuring a gap distance value of a surface of a wafer based on a comparison of a main capacitive sensor electrode driven with a first drive signal and a compensating capacitive sensor electrode driven with a second drive signal that is amplitude or phase shifted as compared to the first drive signal. A value of the second drive signal is measured. The value of the second drive signal is calibrated to a reference impedance standard to determine an impedance value of the wafer to ground. A contact resistance value is determined for the surface of the wafer based on the gap distance value and the impedance value of the wafer to ground.
In one embodiment, measuring the value of the second drive signal comprises driving the compensating capacitive sensor with the second drive signal that is a 180 degree shifted version of the first drive signal, and adjusting an amplitude of the second drive signal to obtain an amplitude value when a net current of the main capacitive sensor electrode and the compensating capacitive sensor electrode is zero, and wherein calibrating the value of the second drive signal to the reference impedance standard comprises calibrating the amplitude value to the reference impedance standard.
In one embodiment, measuring the value of the second drive signal comprises driving the compensating capacitive sensor with the second drive signal that is a phase shifted version of the first drive signal, and adjusting a phase angle of the second drive signal to obtain a phase angle value when a minimum gap distance value is obtained, and wherein calibrating the value of the second drive signal to the reference impedance standard comprises calibrating the phase angle value to the reference impedance standard.
In one embodiment, measuring the value of the second drive signal comprises varying a distance of the compensating capacitive sensor electrode from the surface of the wafer to obtain minimum gap distance value, and wherein calibrating the value of the second drive signal to the reference impedance standard comprises calibrating the minimum gap distance value to the reference impedance standard.
In one embodiment, measuring the gap distance value comprises measuring the gap distance value when a net current of the main capacitive sensor electrode and the compensating capacitive sensor electrode is zero.
In one embodiment, the method further includes contacting a conductive electrode to the surface of the wafer, and directing a charged particle beam to a second surface of the wafer when the contact resistance value for the surface of the wafer is below a threshold value.
In one embodiment, directing the charged particle beam to the second surface of the wafer comprises initiating a secondary ion mass spectrometry (SIMS) measurement of the second surface of the wafer.
This patent application is a continuation application of U.S. patent application Ser. No. 16/039,292, filed on Jul. 18, 2018 (now U.S. Pat. No. 10,403,489), which is a continuation application of U.S. patent application Ser. No. 15/550,014, filed on Aug. 9, 2017 (now U.S. Pat. No. 10,056,242), which is a U.S. National Phase application under 35 U.S.C. § 371 of International Application No. PCT/US2016/017370, filed on Feb. 10, 2016, which claims the benefit of U.S. Provisional Application No. 62/114,521, filed on Feb. 10, 2015, U.S. Provisional Application No. 62/114,519, filed on Feb. 10, 2015, and U.S. Provisional Application No. 62/114,524, filed on Feb. 10, 2015, the entire contents of which are hereby incorporated by reference in their entireties.
| Number | Name | Date | Kind |
|---|---|---|---|
| 5271724 | van Lintel | Dec 1993 | A |
| 20150337367 | Kim | Nov 2015 | A1 |
| Number | Date | Country | |
|---|---|---|---|
| 20190385831 A1 | Dec 2019 | US |
| Number | Date | Country | |
|---|---|---|---|
| 62114521 | Feb 2015 | US | |
| 62114519 | Feb 2015 | US | |
| 62114524 | Feb 2015 | US |
| Number | Date | Country | |
|---|---|---|---|
| Parent | 16039292 | Jul 2018 | US |
| Child | 16557197 | US | |
| Parent | 15550014 | US | |
| Child | 16039292 | US |