The present disclosure relates to substrate processing systems, and more particularly to systems and methods for remote plasma atomic layer deposition.
The background description provided here is for the purpose of generally presenting the context of the disclosure. Work of the presently named inventors, to the extent it is described in this background section, as well as aspects of the description that may not otherwise qualify as prior art at the time of filing, are neither expressly nor impliedly admitted as prior art against the present disclosure.
A resulting film on the substrate has negligible damage to an extreme low k (ELK) dielectric layer and conformal step coverage. However, the film has poor film density, typically around 8.8 g/cm3. This causes poor barrier performance in Cu thermal diffusion and moisture out-diffusion from the ELK dielectric layer.
In contrast, ion-induced atomic layer deposition (iALD) or plasma-enhanced atomic layer deposition (PEALD) processes use a capacitively-coupled plasma (CCP) treatment with a combination of argon, hydrogen, and ammonia at 16 in
A method for depositing a film on a substrate includes introducing a precursor gas into a reaction volume of a processing chamber, wherein a substrate is arranged in the reaction volume; after a predetermined soak period, purging the precursor gas from the reaction volume; and exposing the substrate with plasma gas using a remote plasma source.
In other features, the method further includes arranging a plasma dome above a dual plenum showerhead; locating the substrate on a pedestal in the reaction volume adjacent to the dual plenum showerhead; supplying the precursor gas to a first plenum defined between first and second plates of the dual plenum showerhead, wherein the precursor gas flows through first distribution holes in the dual plenum showerhead to the reaction volume; and supplying the plasma gas to a second plenum of the plasma dome The second plenum is defined between the plasma dome and the dual plenum showerhead. The plasma gas flows through second distribution holes in the dual plenum showerhead to the reaction volume.
In other features, the plasma gas is generated remotely in the second plenum by supplying a process gas to the second plenum; arranging coils around the plasma dome; and supplying current to the coils to generate the plasma gas in the second plenum.
In other features, the method further includes purging the plasma gas from the reaction volume. The precursor gas includes one of tantalum, nitrogen and carbon. The plasma gas includes one of argon and hydrogen (Ar/H2), nitrogen and hydrogen (N2/H2), nitrogen and ammonia (N2/NH3), helium and hydrogen (He/H2) and/or hydrogen (H2). The plasma gas includes one of nitrogen and hydrogen (N2/H2) and nitrogen and ammonia (N2/NH3).
In other features, the precursor gas and the plasma gas flow through the dual plenum showerhead using separate paths. The method further includes performing a post plasma treatment using the plasma gas. The method further includes purging the post plasma treatment.
In other features, the method further includes, prior to the exposing the substrate with the plasma gas using the remote plasma source, introducing a reactant gas dose into the reaction volume and purging the reactant gas dose.
In other features, the method further includes performing a post plasma treatment using the plasma gas. The method further includes purging the post plasma treatment.
A substrate processing system for depositing a film on a substrate includes a processing chamber including a reaction volume. A substrate is arranged on a pedestal in the reaction volume. A dual plenum showerhead is arranged between the plasma dome and the reaction volume. A first plenum defined by the dual plenum showerhead and a second plenum is defined between the plasma dome and the dual plenum showerhead. Plasma gas is generated remotely in the second plenum. A precursor source supplies a precursor gas to the first plenum. The precursor gas flows through first distribution holes in the dual plenum showerhead to the reaction volume. The plasma gas flows through second distribution holes in the dual plenum showerhead to the reaction volume. A controller is configured to introduce the precursor gas into the reaction volume. After a predetermined period, the controller is configured to purge the precursor gas from the reaction volume. The controller is configured to expose the substrate to the plasma gas.
In other features, the controller is configured to purge the plasma gas from the reaction volume. The precursor gas includes one of tantalum, nitrogen and carbon. The plasma gas includes one of argon and hydrogen (Ar/H2), nitrogen and hydrogen (N2/H2), nitrogen and ammonia (N2/NH3), helium and hydrogen (He/H2) and/or hydrogen (H2). The plasma gas includes one of nitrogen and hydrogen (N2/H2) and nitrogen and ammonia (N2/NH3). The controller is configured to perform a post plasma treatment using the plasma gas. The controller is configured to purge the post plasma treatment.
In other features, the controller is configured to, prior to the exposing the substrate with the plasma gas, introduce a reactant dose into the reaction volume and purge the reactant dose. The controller is configured to perform a post plasma treatment using the plasma gas. The controller is configured to purge the post plasma treatment.
Further areas of applicability of the present disclosure will become apparent from the detailed description, the claims and the drawings. The detailed description and specific examples are intended for purposes of illustration only and are not intended to limit the scope of the disclosure.
The present disclosure will become more fully understood from the detailed description and the accompanying drawings, wherein:
In the drawings, reference numbers may be reused to identify similar and/or identical elements.
The present disclosure describes systems and methods for using remote plasma atomic layer deposition (RPALD) to deposit film such as tantalum nitride (TaN) film or another film where a remote plasma source is used in a plasma dose step or a post-plasma treatment step. In some examples, a dual plenum showerhead blocks the intermixing of precursor gas and reactant gas. Using the remote plasma source, the systems and methods described herein improve film density and produce film with fewer impurities (carbon, oxygen). The systems and methods also provide conformal step coverage and minimize extreme low dielectric (ELK) damage.
The systems and methods described herein utilize a remote plasma source as a reactant and/or as a post-plasma treatment. The remote plasma source generates a high density of hydrogen-containing radicals involved in the reaction with the precursor gas. Most of the ions associated with ELK damage may be filtered during delivery to the substrate. In some examples, the precursor gas includes tantalum (Ta), nitrogen (N), and carbon (C). The precursor gas is introduced to a first plenum of a dual plenum showerhead. In some examples, process gases including argon and hydrogen (Ar/H2), nitrogen and hydrogen (N2/H2), nitrogen and ammonia (N2/NH3), helium and hydrogen (He/H2) and/or hydrogen (H2) are supplied to a plasma dome to generate the remote plasma source.
In some examples, the dual plenum showerhead delivers the remotely-generated plasma to the wafer. In some examples, gas compositions with N2/H2 and N2/NH3 are used to achieve desired film properties, although other gas compositions such as, but not limited to, those described herein can be used. Due to the high density and non-directionality of hydrogen radicals that are generated, the systems and methods described herein can be applied to various small features that require thin, continuous step coverage and minimal plasma damage.
Referring now to
Process gases 62 are supplied via a mass flow controller 63 to a second plenum defined between the plasma dome 52 and the dual plenum showerhead 56. A diffuser 65 may be used to diffuse the process gas. A remote plasma generator 82 is connected to electromagnetic coils 54. The remote plasma generator 82 may include a current source to supply current to the coils 54. Process gas is supplied to the second plenum and the plasma gas is remotely generated by an induced magnetic field and an electric field when the remote plasma generator 82 flows current along the coils 54 around the plasma dome 52. Alternately, the plasma gas may be generated outside of the plasma dome 52 and delivered to the plasma dome 52.
In
The first plenum is defined between upper and lower plates of the dual plenum showerhead 56 as will be described further below. A valve 79 and a pump 80 may be used to purge gas from the reaction volume 51.
The dual plenum showerhead 56 separately delivers precursor or plasma to the reaction volume. In other words, the precursor gas travels from the precursor source to the first plenum of the dual plenum showerhead 56 and through first distribution holes in the dual plenum showerhead 56 to the reaction volume 51. In contrast, the plasma flows from the second plenum through a second set of distribution holes in the dual plenum showerhead 56 to the reaction volume 51. A controller 90 may be used to control the process and may be connected to the valves 76 and 79, the mass flow controller 73, the pump 80, and the remote plasma generator 82.
In some examples, the plasma dome 52 and the dual plenum showerhead 56 may be implemented in a manner similar to that described in commonly-assigned “Dual Plenum, Axi-Symmetric Showerhead with Edge-To-Center Gas Delivery”, U.S. patent application Ser. No. 13/531,254, filed on Jun. 22, 2012, which is hereby incorporated by reference in its entirety.
The dual plenum showerhead 56 may be made from any suitable material such as aluminum, ceramic, or other materials compatible with a semiconductor processing environment. While the upper faceplate 112 and the lower faceplate 114 are shown fastened together, they can be fabricated in other ways. For example, the upper faceplate 112 and the lower faceplate 114 may be bonded together, for example, with a diffusion bond or brazing.
Second channels 140 may be formed within the faceplate 112 and may extend in a substantially circumferential direction with respect to the center axis 126. The second channels 140 may have different nominal diameters and may be spaced apart such that they are distributed across the faceplate 112. While the second channels 140 that are shown are concentric annular channels that extend through 360 degrees, other examples may feature other channel path shapes. For example, instead of multiple annular second channels 140, one or multiple spiral second channels centered on the center axis 126 may be used in some examples.
The faceplates 112 and 114 may feature two different sets of gas distribution holes, each serving to exhaust a different plenum volume. For example, the faceplates 112 and 114 may include first gas distribution holes 132 and second gas distribution holes 134. The second gas distribution holes 134 may allow gas within the second plenum volume to escape towards the reaction volume 51.
The first plenum may be formed, at least in part, by volume defined by the first channels and the second channels. The first gas distribution holes 132 may allow gas within the first plenum to escape towards the reaction volume 51. The first gas distribution holes 132 may be smaller than the second gas distribution holes 134. The second gas distribution holes 134 may also extend completely through the faceplates 112 and 114, i.e., from top surface 128 to bottom surface 130. In some examples, since the remote plasma may be generated in the second plenum, it may be desirable to increase the number of free radicals that are released into the reaction volume 51. The second gas distribution holes 134 may thus have a diameter that, within certain constraints, is configured to maximize, to the extent possible, the number of free radicals that pass into the reaction volume 51.
For example only, a method based on
For example only, a method based on
Referring now to
Referring now to Table 1 below, the RPALD processes described herein are expected to yield high growth rate of 1 A/cycle, almost stoichiometric TaN composition with reduced carbon impurity of 3 at. %, and improved film density of 11.2 g/cm3. The high growth rate might be attributed to the enhanced chemisorptions of precursor molecules on hydrogen radicals terminated surface.
Referring now to
RP ALD TaN provides the thin and conformal step coverage on small features due to non-directional distribution of radicals. RPALD TaN process with H2/N2 or NH3/N2 achieved the improved film properties such as chemical composition and film density with minimized ELK underlayer damage.
The foregoing description is merely illustrative in nature and is in no way intended to limit the disclosure, its application, or uses. The broad teachings of the disclosure can be implemented in a variety of forms. Therefore, while this disclosure includes particular examples, the true scope of the disclosure should not be so limited since other modifications will become apparent upon a study of the drawings, the specification, and the following claims. As used herein, the phrase at least one of A, B, and C should be construed to mean a logical (A or B or C), using a non-exclusive logical OR. It should be understood that one or more steps within a method may be executed in different order (or concurrently) without altering the principles of the present disclosure.
In this application, including the definitions below, the term module may be replaced with the term circuit. The term module may refer to, be part of, or include an Application Specific Integrated Circuit (ASIC); a digital, analog, or mixed analog/digital discrete circuit; a digital, analog, or mixed analog/digital integrated circuit; a combinational logic circuit; a field programmable gate array (FPGA); a processor (shared, dedicated, or group) that executes code; memory (shared, dedicated, or group) that stores code executed by a processor; other suitable hardware components that provide the described functionality; or a combination of some or all of the above, such as in a system-on-chip.
The term code, as used above, may include software, firmware, and/or microcode, and may refer to programs, routines, functions, classes, and/or objects. The term shared processor encompasses a single processor that executes some or all code from multiple modules. The term group processor encompasses a processor that, in combination with additional processors, executes some or all code from one or more modules. The term shared memory encompasses a single memory that stores some or all code from multiple modules. The term group memory encompasses a memory that, in combination with additional memories, stores some or all code from one or more modules. The term memory may be a subset of the term computer-readable medium. The term computer-readable medium does not encompass transitory electrical and electromagnetic signals propagating through a medium, and may therefore be considered tangible and non-transitory. Non-limiting examples of a non-transitory tangible computer readable medium include nonvolatile memory, volatile memory, magnetic storage, and optical storage.
The apparatuses and methods described in this application may be partially or fully implemented by one or more computer programs executed by one or more processors. The computer programs include processor-executable instructions that are stored on at least one non-transitory tangible computer readable medium. The computer programs may also include and/or rely on stored data.
| Number | Name | Date | Kind |
|---|---|---|---|
| 5614026 | Williams | Mar 1997 | A |
| 6883733 | Lind | Apr 2005 | B1 |
| 7049226 | Chung et al. | May 2006 | B2 |
| 8083853 | Choi et al. | Dec 2011 | B2 |
| 8328939 | Choi et al. | Dec 2012 | B2 |
| 8419959 | Bettencourt et al. | Apr 2013 | B2 |
| 8869742 | Dhindsa et al. | Oct 2014 | B2 |
| 20060228496 | Choi et al. | Oct 2006 | A1 |
| 20100003406 | Lam et al. | Jan 2010 | A1 |
| 20110114601 | Lubomirsky et al. | May 2011 | A1 |
| 20110227037 | Su | Sep 2011 | A1 |
| 20120077349 | Li et al. | Mar 2012 | A1 |
| 20120115325 | Park et al. | May 2012 | A1 |
| 20120161405 | Mohn et al. | Jun 2012 | A1 |
| 20130260488 | Kim et al. | Oct 2013 | A1 |
| 20130306758 | Park et al. | Nov 2013 | A1 |
| 20130341433 | Roy et al. | Dec 2013 | A1 |
| 20140179114 | van Schravendijk | Jun 2014 | A1 |
| 20140235069 | Breiling et al. | Aug 2014 | A1 |
| 20150007770 | Chandrasekharan et al. | Jan 2015 | A1 |
| Entry |
|---|
| U.S. Appl. No. 13/531,254, filed Jun. 22, 2012, Shambhu N. Roy et al. |
| Number | Date | Country | |
|---|---|---|---|
| 20140272185 A1 | Sep 2014 | US |